Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories
Received date: 2021-01-26
Revised date: 2021-05-25
Online published: 2021-07-20
High-performance nickel-based superalloys are highly desired in the aerospace industry. A drawback of vacuum induction melting for processing nickel-based superalloys is that oxide refractories contaminate the molten alloy through crucible-melt interaction. Therefore, crucibles used for producing nickel-based superalloys should be carefully selected to avoid melt contamination. In this study, the interfacial reaction between a molten nickel-based superalloy (K417G) and various oxide refractories, including Al2O3, CaO, MgO, ZrO2 + 12%Y2O3 (mass fraction) (Y-PSZ), ZrO2 + 20%CaO (CSZ), and Y2O3, formed by cold isostatic pressing was investigated at 1600oC by XRD, SEM, and EDS. The effects of the oxide crucibles on the impurity contents of K417G were also evaluated. The results show that physical erosion is the primary mechanism of the interaction between Al2O3 crucibles and alloy melt. The readily detached Al2O3 particles formed inclusions in the alloy. The Ca3Al2O6 liquid phase generated at the melt-crucible interface promoted wettability between the alloy and CaO crucible, resulting in a high adhesion at the interface. The reaction of the MgO crucible with Al in the alloy resulted in the formation of MgAl2O4 at the melt-crucible interface, which subsequently entered the alloy to form inclusions. Al2O3 was generated at the Y-PSZ-crucible-alloy interface. However, there was no corrosion of Al2O3 in the Y-PSZ crucible, indicating the crucible exhibits excellent corrosion resistance to Al2O3 slags. The interaction between the CSZ crucible and alloy melt generated a CaAl2O4 liquid phase, making the crucible unstable to dissolve into the alloy. An Al2Y4O9 reaction layer is mainly formed at the Y2O3-crucible-alloy interface. The dissolution of Y2O3 into the alloy melt was high compared to that of other oxide refractories. The melt-crucible interaction also significantly affected the oxygen content of K417G. The oxygen concentration of the alloy fused by CaO, Y2O3, and Y-PSZ crucibles did not increase, whereas that of the alloy melted in CSZ, MgO, and Al2O3 crucibles increased from 0.0007% to 0.0011%, 0.0034%, and 0.0135%, respectively.
Key words: interfacial reaction; K417G; refractory; Al2O3; CaO; MgO; ZrO2; Y2O3
Qingzhong SONG , Kun QIAN , Lei SHU , Bo CHEN , Yingche MA , Kui LIU . Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories[J]. Acta Metall Sin, 2022 , 58(7) : 868 -882 . DOI: 10.11900/0412.1961.2021.00048
| 1 | Shi C X, Zhong Z Y. Development and innovation of superalloy in China [J]. Acta Metall. Sin., 2010, 46: 1281 |
| 1 | 师昌绪, 仲增墉. 我国高温合金的发展与创新 [J]. 金属学报, 2010, 46: 1281 |
| 2 | Akca E, Gürsel A. A review on superalloys and IN718 nickel-based INCONEL superalloy [J]. Period. Eng. Nat. Sci., 2015, 3: 15 |
| 3 | Huang Q Y, Li H K. Superalloy [M]. Beijing: Metallurgical Industry Press, 2000: 4 |
| 3 | 黄乾尧, 李汉康. 高温合金 [M]. 北京: 冶金工业出版社, 2000: 4 |
| 4 | Jiang Z H, Zhang X F, Liu F B, et al. Harmful impurities control of raw material used in Ni-based superalloy production [J]. Iron Steel, 2017, 52(9): 1 |
| 4 | 姜周华, 张新法, 刘福斌 等. 镍基高温合金生产用原材料有害杂质的控制 [J]. 钢铁, 2017, 52(9): 1 |
| 5 | Niu J P, Sun X F, Jin T, et al. Super refining of superalloys by VIM [J]. Mater. Rev., 2001, 15(11): 27 |
| 5 | 牛建平, 孙晓峰, 金 涛 等. 高温合金的真空感应超纯净熔炼 [J]. 材料导报, 2001, 15(11): 27 |
| 6 | Wan X J, Zhang H X, Yu A, et al. Superrefining of Ni-base superalloy by VIDP [J]. Vacuum, 2018, 55(3): 48 |
| 6 | 万旭杰, 张华霞, 于 昂 等. 镍基高温合金VIDP真空超纯净熔炼 [J]. 真空, 2018, 55(3): 48 |
| 7 | Li N. Reaction Between Refractory and Steel and Its Effect on Steel Quality [M]. Beijing: Metallurgical Industry Press, 2005: 26 |
| 7 | 李 楠. 耐火材料与钢铁的反应及对钢质量的影响 [M]. 北京: 冶金工业出版社, 2005: 26 |
| 8 | Xie K W, Chen B, Zhang M S, et al. Desulfurization mechanism of K4169 superalloy using CaO crucible in vacuum induction melting process [A]. High Performance Structural Materials [C]. Yinchuan, China: Springer, 2017: 575 |
| 9 | Niu J P, Yang K N, Sun X F, et al. Investigation on deoxidation during VIM refining Ni-base superalloy by using CaO crucible [J]. Acta Metall. Sin., 2002, 38: 303 |
| 9 | 牛建平, 杨克努, 孙晓峰 等. 用CaO坩埚真空感应熔炼镍基高温合金脱氧研究 [J]. 金属学报, 2002, 38: 303 |
| 10 | Song R K, Ma D, Wu S J. Microstructure, mechanical properties and thermal fatigue behavior of K417G alloy used in turbine guide vane [J]. Rare Met. Mater. Eng., 2019, 48: 1517 |
| 10 | 宋若康, 马 东, 吴素君. K417G服役涡轮导向叶片的组织性能及热疲劳损伤机理分析 [J]. 稀有金属材料与工程, 2019, 48: 1517 |
| 11 | Choudhury A. State of the art of superalloy production for aerospace and other application using VIM/VAR or VIM/ESR [J]. ISIJ Int., 1992, 32: 563 |
| 12 | Qian K, Chen B, Shu L, et al. Nitrogen solubility in liquid Ni-V, Ni-Ta, Ni-Cr-V, and Ni-Cr-Ta alloys [J]. Metals, 2019, 9: 1184 |
| 13 | Qian K, Chen B, Zhang L, et al. Kinetics study of nitrogen removal from liquid IN718 alloy during vacuum induction melting [J]. Vacuum, 2020, 179: 109521 |
| 14 | Bodnar R L, Ohhashi T, Jaffee R I. Effects of Mn, Si, and purity on the design of 3.5NiCrMoV, 1CrMoV, and 2.25Cr-1Mo bainitic alloy steels [J]. Metall. Mater. Trans., 1989, 20A: 1445 |
| 15 | Yue J B. Technical progress and characteristics of vacuum induction melting furnaces [J]. Shanxi Metall., 2017, 40(2): 33 |
| 15 | 岳江波. 真空感应熔炼炉工艺特点及其技术进展 [J]. 山西冶金, 2017, 40(2): 33 |
| 16 | Fashu S, Lototskyy M, Davids M W, et al. A review on crucibles for induction melting of titanium alloys [J]. Mater. Des., 2020, 186: 108295 |
| 17 | Zhu S G, Li L, Chang T Q, et al. Effect of impurity elements on microstructure and castability of directionally solidified superalloy DZ125L [J]. Non-Ferrous Mining Metall., 2017, 33(6): 31 |
| 17 | 朱石刚, 李 琳, 常涛歧 等. 杂质元素含量对定向凝固镍基高温合金DZ125L微观组织及铸造性能的影响 [J]. 有色矿冶, 2017, 33(6): 31 |
| 18 | Jiang L, Guo S Q, Bian Y Y, et al. Interfacial behaviors of magnesia partially stabilized zirconia with nickel-based superalloy [J]. Mater. Lett., 2016, 181: 313 |
| 19 | Li J P, Zhang H R, Gao M, et al. High-temperature wettability and interactions between Y-containing Ni-based alloys and various oxide ceramics [J]. Materials, 2018, 11: 749 |
| 20 | Li Q, Song J X, Wang D G, et al. Effect of Cr, Hf and temperature on interface reaction between nickel melt and silicon oxide core [J]. Rare Met., 2011, 30: 405 |
| 21 | Valenza F, Nowak R, Sobczak N, et al. Interactions between superalloys and mould materials for investment casting of turbine blades [J]. Adv. Sci. Technol., 2010, 70: 130 |
| 22 | Yao J S, Tang D Z, Liu X G, et al. Interaction between two Ni-base alloys and ceramic moulds [J]. Mater. Sci. Forum, 2013, 747-748: 765 |
| 23 | Hu B Y, Xu Y Q, Zhang H D. Special Refractory Practical Technical Manuals [M]. Beijing: Metallurgical Industry Press, 2004: 1 |
| 23 | 胡宝玉, 徐延庆, 张宏达. 特种耐火材料实用技术手册 [M]. 北京: 冶金工业出版社, 2004: 1 |
| 24 | Kostov A, Friedrich B. Predicting thermodynamic stability of crucible oxides in molten titanium and titanium alloys [J]. Comput. Mater. Sci., 2006, 38: 374 |
| 25 | Gomes F, Barbosa J, Ribeiro C S. Induction melting of γ-TiAl in CaO crucibles [J]. Intermetallics, 2008, 16: 1292 |
| 26 | Chen B, Ma Y C, Gao M, et al. Changes of oxygen content in molten TiAl alloys as a function of superheat during vacuum induction melting [J]. J. Mater. Sci. Technol., 2010, 26: 900 |
| 27 | Sakamoto K, Yoshikawa K, Kusamichi T, et al. Changes in oxygen contents of titanium aluminides by vacuum induction, cold crucible induction and electron-beam melting [J]. ISIJ Int., 1992, 32: 616 |
| 28 | Tetsui T, Kobayashi T, Kishimoto A, et al. Structural optimization of an yttria crucible for melting TiAl alloy [J]. Intermetallics, 2012, 20: 16 |
| 29 | Gao M, Cui R J, Ma L M, et al. Physical erosion of yttria crucibles in Ti-54Al alloy casting process [J]. J. Mater. Process. Technol., 2011, 211: 2004 |
| 30 | Gao P Y, Liu Y Z, Ren Y, et al. Evaluation of the microstructure and property of TiNi SMA prepared using VIM in BaZrO3 crucible [J]. Vacuum, 2019, 168: 108843 |
| 31 | Meng D Z, Chen G Y, Zhang R L, et al. Preparation of Y2O3 doped SrZrO3 refractory and study on its interface reaction with molten TiNi alloys [J]. Key Eng. Mater., 2018, 768: 256 |
| 32 | Kabiri Y, Kermanpur A, Foroozmehr A. Comparative study on microstructure and homogeneity of NiTi shape memory alloy produced by copper boat induction melting and conventional vacuum arc melting [J]. Vacuum, 2012, 86: 1073 |
| 33 | Li C H, He J, Zhang Z, et al. Preparation of TiFe based alloys melted by CaO crucible and its hydrogen storage properties [J]. J. Alloys Compd., 2015, 618: 679 |
| 34 | Wei J W, Han B Q, Wang X C, et al. Improvement in hydration resistance of CaO granules based on CaO-TiO2, CaO-ZrO2 and CaO-V2O5 systems [J]. Mater. Chem. Phys., 2020, 254: 123413 |
| 35 | Chen Z Y. Chemical Thermodynamics of Refractories [M]. Beijing: Metallurgical Industry Press, 2008: 423 |
| 35 | 陈肇友. 化学热力学与耐火材料 [M]. 北京: 冶金工业出版社, 2008: 423 |
| 36 | Boniecki M, Librant Z, Wesołowski W, et al. The thermal shock resistance of Y2O3 ceramics [J]. Ceram. Int., 2016, 42: 10215 |
| 37 | Cheng X, Yuan C, Green N R, et al. Sintering mechanisms of yttria with different additives [J]. Ceram. Int., 2013, 39: 4791 |
| 38 | Jiang L, Guo S Q, Qiao M R, et al. Study on the structure and mechanical properties of magnesia partially stabilized zirconia during cyclic heating and cooling [J]. Mater. Lett., 2017, 194: 26 |
| 39 | Schafföner S. Reactions of alkaline earth zirconate refractories with titanium alloys [A]. The 14th World Conference on Titanium (Ti 2019) [C]. Nantes, France: EDP Sciences, 2020: 10012 |
| 40 | Schafföner S, Fruhstorfer J, Ludwig S, et al. Cyclic cold isostatic pressing and improved particle packing of coarse grained oxide ceramics for refractory applications [J]. Ceram. Int., 2018, 44: 9027 |
| 41 | Chang Y W, Lin C C. Compositional dependence of phase formation mechanisms at the interface between titanium and calcia-stabilized zirconia at 1550oC [J]. J. Am. Ceram. Soc., 2010, 93: 3893 |
| 42 | Lin C C, Chang Y W, Lin K L, et al. Effect of yttria on interfacial reactions between titanium melt and hot-pressed yttria/zirconia composites at 1700oC [J]. J. Am. Ceram. Soc., 2008, 91: 2321 |
| 43 | Chen Z Y. Phase Diagrams of Refractories [M]. Beijing: Metallurgical Industry Press, 2014: 32 |
| 43 | 陈肇友. 相图与耐火材料 [M]. 北京: 冶金工业出版社, 2014: 32 |
| 44 | Kishimoto Y, Utada S, Iguchi T, et al. Desulfurization model using solid CaO in molten Ni-based superalloys containing Al [J]. Metall. Mater. Trans., 2020, 51B: 293 |
| 45 | Kumar G, Prabhu K N. Review of non-reactive and reactive wetting of liquids on surfaces [J]. Adv. Colloid Interface Sci., 2007, 133: 61 |
| 46 | Wan C, Kritsalis P, Drevet B, et al. Optimization of wettability and adhesion in reactive nickel-based alloys/alumina systems by a thermodynamic approach [J]. Mater. Sci. Eng., 1996, A207: 181 |
| 47 | Sadrnezhad S K, Raz S B. Interaction between refractory crucible materials and the melted NiTi shape-memory alloy [J]. Metall. Mater. Trans., 2005, 36B: 395 |
| 48 | Zhang T, Wei Y W, Chen J F, et al. Preparation of CaO-MgO-ZrO2 refractory and its desulfurization effect on Ni-based alloy in vacuum induction melting (VIM) [J]. J. Aust. Ceram. Soc., 2020, 56: 885 |
| 49 | Gao X Y, Zhang L, Qu X H, et al. Effect of interaction of refractories with Ni-based superalloy on inclusions during vacuum induction melting [J]. Int. J. Miner. Metall. Mater., 2020, 27: 1551 |
| 50 | Durov A V, Naidich Y V, Kostyuk B D. Investigation of interaction of metal melts and zirconia [J]. J. Mater. Sci., 2005, 40: 2173 |
| 51 | Zi Y, Meng J, Zhang C W, et al. Effect of Y content on interface reaction and wettability between a nickel-base single crystal superalloy melt and ceramic mould [J]. J. Alloys Compd., 2019, 789: 472 |
| 52 | Liu Q M, Huang S Z, Liu F, et al. Effect of boron content on microstructure evolution during solidification and mechanical properties of K417G alloy [J]. Acta Metall. Sin., 2019, 55: 720 |
| 52 | 刘巧沐, 黄顺洲, 刘 芳 等. B含量对K417G合金凝固过程中组织演变和力学性能的影响 [J]. 金属学报, 2019, 55: 720 |
| 53 | Tetsui T, Kobayashi T, Mori T, et al. Evaluation of yttria applicability as a crucible for induction melting of TiAl alloy [J]. Mater. Trans., 2010, 51: 1656 |
| 54 | Li J P, Zhang H R, Gao M, et al. Effect of vacuum level on the interfacial reactions between K417 superalloy and Y2O3 crucibles [J]. Vacuum, 2020, 182: 109701 |
| 55 | Ye D L, Hu J H. Thermodynamic Data Sheet of Practical Inorganic [M]. 2nd Ed., Beijing: Metallurgical Industry Press, 2002: 1 |
| 55 | 叶大伦, 胡建华. 实用无机物热力学数据手册 [M]. 第 2版, 北京: 冶金工业出版社, 2002: 1 |
| 56 | Chen X Y, Jin Z, Bai X F, et al. Effect of C on the interfacial reaction and wettability between a Ni-based superalloy and ceramic mould [J]. Acta Metall. Sin., 2015, 51: 853 |
| 56 | 陈晓燕, 金 喆, 白雪峰 等. C对一种镍基高温合金与陶瓷型壳界面反应及润湿性的影响 [J]. 金属学报, 2015, 51: 853 |
/
| 〈 |
|
〉 |