Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate
Received date: 2021-01-14
Revised date: 2021-04-22
Online published: 2021-07-19
Supported by
National Natural Science Foundation of China(51871043);Fundamental Research Funds for the Central Universities of China(180212010);Natural Science Foundation of Liaoning Province(2019-MS-113)
7N01 aluminum alloy is the main load-bearing structure material for bullet train bodies due to its high specific strength, high specific stiffness, good magnetic-shielding ability, strong corrosion resistance, and good formability and weldability. The fatigue performance of materials and components used in bullet trains determines their security. It is unavoidable that there is pre-deformation during the assembly process of aluminum alloy components, which will influence the active service and fatigue performance of the aluminum alloy. It is important not only to clarify the relationship between pre-deformation and fatigue performance but also to reveal the mechanism of pre-deformation on the fatigue fracture of 7N01 aluminum alloy, to ensure the security of the bullet train. In this study, the effect of pre-tensile deformation on the fatigue property, fatigue fracture initiation, and fatigue crack propagation characteristics of a commercial 7N01 aluminum alloy plate at under-aged conditions was studied using tensile and fatigue tests combined with microstructure analysis. As the pre-tensile deformation increased to 20%, the results showed that the shape, size, number, distribution of second phase particles, as well as the size and morphology of thin strips grain of under-aged 7N01 aluminum alloy plate were almost the same. However, the under-aged 7N01 aluminum alloy plate has a significant strain-hardening effect after pre-tensile at room temperature, with the yield strength, tensile strength, and hardness increased from 181 MPa, 233 MPa, and 95 HV (without pre-tensile deformation) to 254 MPa, 271 MPa, and 117 HV (after 20% pre-tensile deformation), while the elongation decreased from 23.2% to 5.2%. Under the 175 MPa pulsating tensile load condition (stress ratio R = 0), the overall fatigue life of the under-aged 7N01 aluminum alloy plate first reduced, then prolonged, and then decreased as pre-tensile deformation increased. Without pre-tensile deformation, the fatigue life of under-aged 7N01 aluminum alloy plate is about 6.06 × 105 cyc, and when prolonged by about 75%, it reaches about 1.06 × 106 cyc after 5% pre-tensile deformation. However, the fatigue life of the under-aged 7N01 aluminum alloy plate is decreased to 4.21 × 105 and 2.89 × 105 cyc after 3% and 20% pre-tensile deformation, respectively. The evenly distributed high-density dislocations or dislocation cells resulted in 5%-16% pre-tensile deformation in the under-aged 7N01 aluminum alloy plate, which can prolong the fatigue life of the alloy plate by over 23%.
Key words: 7N01 aluminum alloy plate; pre-tensile deformation; under-aged; dislocation; fatigue
Ni TIAN , Xu SHI , Wei LIU , Chuncheng LIU , Gang ZHAO , Liang ZUO . Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate[J]. Acta Metall Sin, 2022 , 58(6) : 760 -770 . DOI: 10.11900/0412.1961.2021.00017
| 1 | Deschamps A, Texier G, Ringeval S, et al. Influence of cooling rate on the precipitation microstructure in a medium strength Al-Zn-Mg alloy [J]. Mater. Sci. Eng., 2009, A501: 133 |
| 2 | Heinz A, Haszler A, Keidel C, et al. Recent development in aluminium alloys for aerospace applications [J]. Mater. Sci. Eng., 2000, A280: 102 |
| 3 | Liu W H, Liu W B, Bao A L. Microstructure and properties of ceramic coatings on 7N01 aluminum alloy by micro-arc oxidation [J]. Procedia Eng., 2012, 27: 828 |
| 4 | Branco R, Costa J D, Borrego L P, et al. Effect of tensile pre-strain on low-cycle fatigue behaviour of 7050-T6 aluminium alloy [J]. Eng. Fail. Anal., 2020, 114: 104592 |
| 5 | Branco R, Borrego L P, Costa J D, et al. Effect of pre-strain on cyclic plastic behaviour of 7050-T6 aluminium alloy [J]. Procedia Struct. Integr., 2019, 17: 177 |
| 6 | Niendorf T, Lotze C, Canadinc D, et al. The role of monotonic pre-deformation on the fatigue performance of a high-manganese austenitic TWIP steel [J]. Mater. Sci. Eng., 2009, A499: 518 |
| 7 | Gustavsson A, Melander A. Fatigue of a highly prestrained dual-phase sheet steel [J]. Fatigue Fract. Eng. Mater. Struct., 1995, 18(2): 201 |
| 8 | Uemura T. A fatigue life estimation of specimens excessively prestrained in tension [J]. Fatigue Fract. Eng. Mater. Struct., 1998, 21: 151 |
| 9 | Al-Rubaie K S, Del Grande M A, Travessa D N, et al. Effect of pre-strain on the fatigue life of 7050-T7451 aluminium alloy [J]. Mater. Sci. Eng., 2007, A464: 141 |
| 10 | Schijve J. The effect of pre-strain on fatigue crack growth and crack closure [J]. Eng. Fract. Mech., 1976, 8: 575 |
| 11 | Froustey C, Lataillade J L. Influence of large pre-straining of aluminium alloys on their residual fatigue resistance [J]. Int. J. Fatigue, 2008, 30(5): 908 |
| 12 | Arora P R, Raghavan M R. Effect of tensile prestrain on fatigue strength of aluminum alloy in high cycle fatigue [J]. J. Eng. Mater. Technol., 1973, 95: 76 |
| 13 | Hodgson P, Parker B A. The composition of insoluble intermetallic phases in aluminium alloy 6010 [J]. J. Mater. Sci., 1981, 16: 1343 |
| 14 | Adrien J, Maire E, Estevez R, et al. Influence of the thermomechanical treatment on the microplastic behaviour of a wrought Al-Zn-Mg-Cu alloy [J]. Acta Mater., 2004, 52: 1653 |
| 15 | Benoit S G, Chalivendra V B, Rice M A, et al. Characterization of the microstructure, fracture, and mechanical properties of aluminum alloys 7085-O and 7175-T7452 hollow cylinder extrusions [J]. Metall. Mater. Trans., 2016, 47A: 4476 |
| 16 | Hou L G, Xiao W L, Su H, et al. Room-temperature low-cycle fatigue and fracture behaviour of asymmetrically rolled high-strength 7050 aluminium alloy plates [J]. Int. J. Fatigue, 2021, 142: 105919 |
| 17 | Wen K, Fan Y Q, Wang G J, et al. Aging behavior and fatigue crack propagation of high Zn-containing Al-Zn-Mg-Cu alloys with zinc variation [J]. Prog. Nat. Sci., 2017, 27: 217 |
| 18 | Tian N, Zhao G, Zuo L, et al. Study on the strain hardening behavior of Al-Mg-Si-Cu alloy sheet for automotive body [J]. Acta. Metall. Sin., 2010, 46: 613 |
| 18 | 田 妮, 赵 刚, 左 良 等. 汽车车身用Al-Mg-Si-Cu合金薄板应变强化行为的研究 [J]. 金属学报, 2010, 46: 613 |
| 19 | Wang Z X, Li H, Wei X Y, et al. Effects of prior strain on static tensile properties and fatigue lives of 2E12 aluminum alloy [J]. Rare Met. Mater. Eng., 2010, 39(): 138 |
| 19 | 王芝秀, 李 海, 魏修宇 等. 预变形对2E12铝合金拉伸性能和疲劳寿命的影响 [J]. 稀有金属材料与工程, 2010, 39(): 138 |
| 20 | Schijve J, translated by Wu X R, et al. Fatigue of Structures and Materials [M]. 2nd Ed., Beijing: Aviation Industry Press, 2014: 30 |
| 20 | Schijve J著, 吴学仁等译 . 结构与材料的疲劳 [M]. 第2版, 北京: 航空工业出版社, 2014: 30 |
| 21 | Wang X S, Liang F, Zeng Y P, et al. SEM in situ observations to the effects of inclusion on initiation and propagation of the low cyclic fatigue crack in super strength steel [J]. Acta. Metall. Sin, 2005, 41: 1272 |
| 21 | 王习术, 梁 锋, 曾燕屏, 等. 夹杂物对超高强度钢低周疲劳裂纹萌生及扩展影响的原位观测 [J]. 金属学报, 2005, 41(12): 1272 |
| 22 | Bai S, Liu Z Y, Gu Y X, et al. Microstructures and fatigue fracture behavior of an Al-Cu-Mg-Ag alloy with a low Cu/Mg ratio [J]. Mater. Sci. Eng., 2011, A530: 473 |
| 23 | Xu L P, Wang Q Y, Zhou M. Micro-crack initiation and propagation in a high strength aluminum alloy during very high cycle fatigue [J]. Mater. Sci. Eng., 2018, A715: 404 |
| 24 | Yao W X, Guo S J. Gigacycle fatigue life distribution of aluminum alloy LC4CS [J]. Acta. Metall. Sin., 2007, 43: 399 |
| 24 | 姚卫星, 郭盛杰. LC4CS铝合金的超高周疲劳寿命分布 [J]. 金属学报, 2007, 43: 399 |
| 25 | Zang X C, Xie L Y, Hu J X, et al. Effect of service on fracture mechanical properties of 7N01 aluminum alloy [J]. J. Northeast. Univ. (Nat. Sci.), 2017, 38: 1442 |
| 25 | 张啸尘, 谢里阳, 胡杰鑫, 等. 服役经历对7N01铝合金断裂力学性能的影响 [J]. 东北大学学报(自然科学版), 2017, 38: 1442 |
| 26 | Jian H G, Jiang F, Wei L L, et al. Crystallographic mechanism for crack propagation in the T7451 Al-Zn-Mg-Cu alloy [J]. Mater. Sci. Eng., 2010, A527: 5879 |
| 27 | Nandana M S, Udaya Bhat K, Manjunatha C M. Influence of retrogression and re-ageing heat treatment on the fatigue crack growth behavior of 7010 aluminum alloy [J]. Procedia Struct. Integr., 2019, 14: 314 |
/
| 〈 |
|
〉 |