Research paper

Ultrasonic Emulsification Preparation of Metallic Rubidium Sol and Its Ignition Performance

  • Yujing GUO ,
  • Haoming BAO ,
  • Hao FU ,
  • Hongwen ZHANG ,
  • Wenhong LI ,
  • Weiping CAI
Expand
  • 1.Institute of Solid State Physics, Hefei Institutes of Physical Science, Chinese Academy of Sciences, Hefei 230031, China
    2.Graduate School of Science Island, University of Science and Technology of China, Hefei 230026, China
    3.Hebei Rubidium Cesium Technology Co. Ltd., Chengde 063000, China
BAO Haoming, Tel: (0551)65591837, E-mail: baohm@issp.ac.cn

Received date: 2021-01-05

  Revised date: 2021-05-07

  Online published: 2021-06-30

Supported by

Key Research and Development Project of Hebei Province(19211002D)

Abstract

Metallic rubidium (Rb) has great potential in various fields, such as energy, catalysis, and medical treatment. Fragmenting bulk Rb to the nanoscale is essential for its efficient application in these fields. However, as an alkali metal with a high chemical activity, Rb reacts violently with trace water, oxygen, and others; thus, preparing nanosized Rb is challenging. This study proposes a sample solid-liquid transformation and ultrasonic dispersion method to prepare Rb nanoparticles (NPs) utilizing Rb's low melting point. This method uses the ultrasonic emulsification of liquid Rb in a specific liquid (toluene) to form a colloidal Rb solution. Typically prepared Rb NPs are nearly spherical with an average size of approximately 45 nm. Further, the average size increases with a decrease in ultrasonic power. When the ultrasonic power falls to 320 and 240 W, the average NP size rises to 55 and 70 nm, respectively, demonstrating good controllability of the proposed method. Further experiments demonstrated that Rb NPs can ignite toluene at relatively low temperatures (say 120oC) within 1 s. When the temperature is up to 250oC, toluene can be ignited in 0.25 s. This study not only provides a new method for synthesizing Rb NPs but also offers new opportunities for novel energy-containing materials and ignition devices.

Cite this article

Yujing GUO , Haoming BAO , Hao FU , Hongwen ZHANG , Wenhong LI , Weiping CAI . Ultrasonic Emulsification Preparation of Metallic Rubidium Sol and Its Ignition Performance[J]. Acta Metall Sin, 2022 , 58(6) : 792 -798 . DOI: 10.11900/0412.1961.2021.00001

References

1 Tan Y N, Liu Y. Properties and research progress of rubidium and its compounds [J]. Chin. J. Nonferrous Met., 2017, 27: 272
1 谭彦妮, 刘 咏. 铷及含铷材料的性能与应用研究进展 [J]. 中国有色金属学报, 2017, 27: 272
2 Cui Y J, Liu Y, Yang B. The design of high precision time reference measurement system based on rubidium disciplined crystal oscillator and double TDC GP2 [J]. Chin. J. Electron Dev., 2017, 40: 1072
2 崔永俊, 刘 阳, 杨 兵. 基于铷原子钟和双TDC-GP2的高精度时间基准测量系统的设计 [J]. 电子器件, 2017, 40: 1072
3 Chang S M, Guo Y. Influences of alkali metal Rb doped Mn as catalyst on catalytic combustion activity of soot particle [J]. China Adhes., 2017, 26(5): 25
3 常三毛, 郭 耘. 碱金属Rb掺锰对碳烟颗粒催化燃烧活性的影响 [J]. 中国胶粘剂, 2017, 26(5): 25
4 Yang Y, Zhang Y, Guo Q, et al. Effect of extracellular potassium on the activity of distal renal tubule in mice [J]. J. Shanghai Jiaotong Univ. (Med. Sci.), 2019, 39(9): 85
4 杨 阳, 张 娅, 郭 琴 等. 细胞外钾对小鼠远端肾小管离子通道活性的影响 [J]. 上海交通大学学报(医学版), 2019, 39(9): 985
5 Qian J M, Li X X, Huang H Y. Properties of nanometer materials and its preparing methods [J]. New Chem. Mater., 2001, 29(7): 1
5 钱军民, 李旭祥, 黄海燕. 纳米材料的性质及其制备方法 [J]. 化工新型材料, 2001, 29(7): 1
6 Li X H, Guo S H, Su J, et al. Efficient raman enhancement in molybdenum disulfide by tuning the interlayer spacing [J]. ACS Appl. Mater. Interfaces, 2020, 12: 28474
7 Zhu M Y, Chen Q, Tong W J, et al. Preparation and application of Fe3O4 nanomaterials [J]. Prog. Chem., 2017, 29: 1366
7 朱脉勇, 陈 齐, 童文杰 等. 四氧化三铁纳米材料的制备与应用 [J]. 化学进展, 2017, 29: 1366
8 Yang M Q, Ji Y H, Liang Q, et al. Preparation, doping modulation and field emission properties of square-shaped GaN nanowires [J]. Acta Phys. Sin., 2020, 69: 167805
8 杨孟骐, 姬宇航, 梁 琦 等. 四方结构GaN纳米线制备、掺杂调控及其场发射性能研究 [J]. 物理学报, 2020, 69: 167805
9 Sun Q S, Ni C L, Yu Y C, et al. Design principle of all-inorganic halide perovskite-related nanocrystals [J]. J. Mater. Chem., 2018, 6C: 12484
10 Liu H G, Tian R Y, Jiang Y, et al. On the drastically improved performance of Fe-doped LiMn2O4 nanoparticles prepared by a facile solution-gelation route [J]. Electrochim. Acta, 2015, 180: 138
11 Xu X Y, Wang Y L, Wang R, et al. Creating carbon-oxygen bonds over TiO2 nanofibers for synergistic benefits of visible-light response and charge separation toward photocatalysis [J]. Adv. Mater. Interfaces, 2017, 4: 1600795
12 Bozlee B, Lian B, Kahn J, et al. Characterization of alkali-metal sols in diethyl ether. Visible extinction and surface-enhanced Raman spectra [J]. Chem. Phys. Lett., 1992, 196: 437
13 Bozlee B, Clark S, Marr C, et al. Characterization and surface-enhanced Raman spectroscopy of alkali metal sols [J]. J. Raman Spectrosc., 1996, 27: 75
14 Roginsky S, Schalnikoff A. A new method of production of colloid solutions [J]. Kolloid Z., 1927, 43: 67
15 Tomaschewsky N. Concerning the manufacture of colloids from the condensation method of molecular rays [J]. Kolloid Z., 1931, 54: 79
16 Modarres-Gheisari S M M, Gavagsaz-Ghoachani R, Malaki M, et al. Ultrasonic nano-emulsification—A review [J]. Ultrason. Sonochem., 2019, 52: 88
17 Baissac L, Buron C C, Hallez L, et al. Synthesis of sub-micronic and nanometric PMMA particles via emulsion polymerization assisted by ultrasound: Process flow sheet and characterization [J]. Ultrason. Sonochem., 2018, 40: 183
18 Behbahani E S, Ghaedi M, Abbaspour M, et al. Optimization and characterization of ultrasound assisted preparation of curcumin-loaded solid lipid nanoparticles: Application of central composite design, thermal analysis and X-ray diffraction techniques [J]. Ultrason. Sonochem., 2017, 38: 271
19 Jia Q P, Ma Z L, Han B, et al. Effects on SPR of Au/TiO2 by preparation methods [J]. J. Hebei Univ. (Nat. Sci. Ed.), 2020, 40: 385
19 贾群鹏, 马志领, 韩 冰 等. Au/TiO2的制备方法对其SPR的影响 [J]. 河北大学学报(自然科学版), 2020, 40: 385
20 Zhu W Z, Liu Y Q, Meng G. Preparation and characterization of nano-gold particles by seeding method [J]. Chin. J. Veter. Med., 2019, 55(10): 33
20 朱文壮, 刘轶群, 孟 赓. 纳米金颗粒的晶种法制备及表征 [J]. 中国兽医杂志, 2019, 55(10): 33
21 Li C X, Wang Z H. Applications of ultrasound in preparation of nanosized materials [J]. Chemistry, 2001, 64: 268
21 李春喜, 王子镐. 超声技术在纳米材料制备中的应用 [J]. 化学通报, 2001, 64: 268
22 Vyas N, Manmi K, Wang Q X, et al. Which parameters affect biofilm removal with acoustic cavitation? A review [J]. Ultrasound Med. Biol., 2019, 45: 1044
23 Jiang R P. Effect rules and function mechanism of ultrasonic field on the solidification of high strength aluminum alloy [D]. Changsha: Central South University, 2014
23 蒋日鹏. 超声场对高强铝合金凝固过程的影响规律与作用机理研究 [D]. 长沙: 中南大学, 2014
24 Ma L. Mechanism for ultrasonic driving filling of liquid solder and acoustic cavitation [D]. Harbin: Harbin Institute of Technology, 2015
24 马 琳. 液态钎料超声驱动填缝机理及声空化作用研究 [D]. 哈尔滨: 哈尔滨工业大学, 2015
25 Sajjadi B, Raman A A A, Shah R S S R E, et al. Review on applicable breakup/coalescence models in turbulent liquid-liquid flows [J]. Rev. Chem. Eng., 2013, 29: 131
26 Kulawik-Pióro A, Tal-Figiel B. Influence of preparation method on size distribution of the dispersed phase of primary emulsions [J]. Chem. Eng. Technol., 2017, 40: 412
27 Li X T, Gao X P, Li T J, et al. A experimental study of grain refinement by ultrasonic treatment during continuous casting [J]. Rare Met. Mater. Eng., 2007, 36: 377
27 李新涛, 高学鹏, 李廷举 等. 连铸过程中超声细晶技术研究 [J]. 稀有金属材料与工程, 2007, 36: 377
Outlines

/