Inconel 718 alloy is an Fe-Ni based superalloy precipitation-strengthened by γ″ phase (Ni3Nb) and γ′ phase (Ni3(AlTi)). It has been widely used in aviation, energy, chemicals, and other fields because of its outstanding mechanical properties, resistance to high-temperature oxidation, and corrosion resistance. Because the mechanical properties of Inconel 718 alloy are primarily determined by the γ″ precipitates, Nb becomes one of the most important alloying elements. Due to the high content, large atomic radius, and small partition coefficient of Nb, Nb segregation occurs easily during the solidification process of casting, welding, and laser cladding. The segregation drastically degrades mechanical properties and increases the difficulty of subsequent heat treatment. The composition of Inconel 718 alloy comprises many elements, and some trace elements are inevitably introduced from the raw materials. The interaction of the elements has a certain effect on Nb segregation. In this study, the effect of the interaction of elements caused by doping of Cu on Nb segregation in Inconel 718 alloy was studied by first-principles calculation and experiment. The Ni-Fe-Cr-Nb supercell model was constructed with and without Cu doping. The enthalpy of formation, cohesive energy, state density, electron density difference, and population analysis was calculated. The calculation results show that the doping of Cu reduces the stability of the system. Doping will change the interaction between elements and affects the strength and density distribution ratio of the charged density between atomic bonds in the system. The addition of Cu increases the bond strength between the Fe atoms and Cr atoms and the repulsive force between Fe atoms and Nb atoms in the matrix. The experimental results show that the addition of 0.1%Cu (mass fraction) decreases the segregation of Fe and Cr, but promotes the segregation of Nb. Experimental results and first-principles calculations show that the increase in the repulsive force between the Nb atom and Fe atom, which is caused by the interaction between the alloying elements after doping with Cu, is the essential reason for Cu to promote Nb segregation.
Yamin LI , Yaoyao ZHANG , Wang ZHAO , Shengrui ZHOU , Hongjun LIU . First-Principles Study on the Effect of Cu on Nb Segregation in Inconel 718 Alloy[J]. Acta Metall Sin, 2022 , 58(2) : 241 -249 . DOI: 10.11900/0412.1961.2020.00495
| 1 | Pereira J M , Lerch B A . Effects of heat treatment on the ballistic impact properties of Inconel 718 for jet engine fan containment applications [J]. Int. J. Impact Eng., 2001, 25: 715 |
| 2 | Qi H . Review of INCONEL 718 alloy: Its history, properties, processing and developing substitutes [J]. J. Mater. Eng., 2012, (8): 92 |
| 2 | 齐 欢 . INCONEL 718(GH4169)高温合金的发展与工艺 [J]. 材料工程, 2012, (8): 92 |
| 3 | Tian Y , Zhao M C . Segregation of Nb and its formation mechanism of high strength casing steel [J]. J. Iron Steel Res., 2020, 32: 344 |
| 3 | 田 研, 赵明纯 . 高强度油井管钢中的Nb偏析及形成机制分析 [J]. 钢铁研究学报, 2020, 32: 344 |
| 4 | Sun K , Lin H B , He Y B , et al . Microscopic inspection and improvement of GH4169G alloy forging banded structure defects [J]. Spec. Cast. Nonferrous Alloys, 2020, 40: 694 |
| 4 | 孙 凯, 蔺虹宾, 何跃斌 等 . GH4169G合金锻件条带缺陷微观检测及改进 [J]. 特种铸造及有色合金, 2020, 40: 694 |
| 5 | Chen Y , Guo Y B , Xu M J , et al . Study on the element segregation and Laves phase formation in the laser metal deposited IN718 superalloy by flat top laser and gaussian distribution laser [J]. Mater. Sci. Eng., 2019, A754: 339 |
| 6 | Zhang Y , Li X X , Wei K , et al . Element segregation in GH4169 Superalloy large-scale ingot and billet manufactured by triple-melting [J]. Acta Metall. Sin., 2020, 56: 1123 |
| 6 | 张 勇, 李鑫旭, 韦 康 等 . 三联熔炼GH4169合金大规格铸锭与棒材元素偏析行为 [J]. 金属学报, 2020, 56: 1123 |
| 7 | DuPont J N , Rohino C V . The influence of Nb and C on the solidification microstructures of Fe-Ni-Cr alloys [J]. Scr. Mater., 1999, 41: 449 |
| 8 | Li A L , Tang X , Gai Q D , et al . Effect of heat treatment on microstructure of K4169 superalloy [J]. J. Aeronaut. Mater., 2006, 26: 311 |
| 8 | 李爱兰, 汤 鑫, 盖其东 等 . 热处理工艺对K4169合金微观组织的影响 [J]. 航空材料学报, 2006, 26: 311 |
| 9 | Long Y T , Nie P L , Li Z G , et al . Segregation of niobium in laser cladding Inconel 718 superalloy [J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 431 |
| 10 | Zhang M C , Zheng L , Yao Z H , et al . Effect of Nb content on micro-segregation evolution of GH4169 ingots [J]. Hot Work. Technol., 2013, 42(10): 45 |
| 10 | 张麦仓, 郑 磊, 姚志浩 等 . Nb含量对GH4169合金钢锭偏析规律的影响 [J]. 热加工工艺, 2013, 42(10): 45 |
| 11 | Mo Y , Wang D Z , Jiang B , et al . Effect of micro alloying vanadium on micro-segregation behavior of niobium in 718 alloy [J]. Heat Treat. Met., 2017, 42(4): 37 |
| 11 | 莫 燕, 王东哲, 蒋 斌 等 . 钒微合金化对718合金中铌元素偏析行为的影响 [J]. 金属热处理, 2017, 42(4): 37 |
| 12 | Sun W R , Guo S R , Lu D Z , et al . Effect of Si on solidification and segregation in Inconel 718 alloy [J]. J. Aeronaut. Mater., 1996, 16(2): 7 |
| 12 | 孙文儒, 郭守仁, 卢德忠 等 . Si对In718合金凝固过程及元素偏析的影响 [J]. 航空材料学报, 1996, 16(2): 7 |
| 13 | Meng F X , Li J H , Zhao X . First-principles study on the effects of Zn-segregation in CuΣ5 grain boundary [J]. Acta Phys. Sin., 2014, 63: 237102 |
| 13 | 孟凡顺, 李久会, 赵 星 . 第一性原理研究Zn偏析对CuΣ5晶界的影响 [J]. 物理学报, 2014, 63: 237102 |
| 14 | Wang J L , Enomoto M , Shang C J . First-principles study on the interfacial segregation at coherent Cu precipitate/Fe matrix interface [J]. Scr. Mater., 2020, 185: 42 |
| 15 | Peng L J . Study on microstructure evolution of Cu-Cr-Zr system alloys and interaction mechanism between alloying elements [D]. Beijing: General Research Institute for Nonferrous Metals, 2014 |
| 15 | 彭丽军 . Cu-Cr-Zr系合金微观组织演变规律及合金元素交互作用机理的研究 [D]. 北京: 北京有色金属研究总院, 2014 |
| 16 | Huang Z W , Zhao Y H , Hou H , et al . Point defects structure and alloying effects of V atoms into Ni3Al alloy: A first-principles study [J]. Rare Met. Mater. Eng., 2011, 40: 2136 |
| 16 | 黄志伟, 赵宇宏, 侯 华 等 . V掺杂Ni3Al点缺陷结构及合金化效应的第一性原理研究 [J]. 稀有金属材料与工程, 2011, 40: 2136 |
| 17 | Perdew J P , Wang Y . Accurate and simple analytic representation of the electron-gas correlation energy [J]. Phys. Rev., 1992, 45B: 13244 |
| 18 | Li Y M , Jiang L , Zhao W , et al . First-principle study of the effects of Cu doped on γ' phase [J]. Mater. Rev., 2019, 33: 3085 |
| 18 | 李亚敏, 江 璐, 赵 旺 等 . 铜掺杂对γ′相影响的第一性原理研究 [J]. 材料导报, 2019, 33: 3085 |
| 19 | Zhao Y H , Huang Z W , Li A H , et al . First principles study on substitution behavior and alloying effects of Nb in Ni3Al [J]. Acta Phys. Sin., 2011, 60: 047103 |
| 19 | 赵宇宏, 黄志伟, 李爱红 等 . Nb在Ni3Al中取代行为及合金化效应的第一性原理研究 [J]. 物理学报, 2011, 60: 047103 |
| 20 | Zhang X Y , Zheng B J , Guo B , et al . Theoretical study on bonding characteristics of Cr, Mn, Mo and N in high nitrogen austenitic stainless steel [J]. Mater. Rev., 2017, 31(18): 146 |
| 20 | 张旭昀, 郑冰洁, 郭 斌 等 . 高氮奥氏体不锈钢中N与Cr、Mn、Mo键合性质研究 [J]. 材料导报, 2017, 31(18): 146 |
| 21 | Chen Z M , Yu W Q . Principle of Solidification of Casting Metal [M]. Beijing: Peking University Press, 2014: 116 |
| 21 | 陈宗民, 于文强 . 铸造金属凝固原理 [M]. 北京: 北京大学出版社, 2014: 116 |
| 22 | Hu Z Q , Sun W R , Guo S R , et al . Effect of trace P on Fe-Ni based wrought superalloy [J]. Chin. J. Nonferrous Met., 2001, 11: 947 |
| 22 | 胡壮麒, 孙文儒, 郭守仁 等 . 微量元素磷在铁镍基变形高温合金中的作用 [J]. 中国有色金属学报, 2001, 11: 947 |
| 23 | Xu Z L . Performance, Strength Design and Engineering Application of High Temperature Metal Materials [M]. Beijing: Chemical Industry Press, 2006: 77 |
| 23 | 徐自立 . 高温金属材料的性能、强度设计及工程应用 [M]. 北京: 化学工业出版社, 2006: 77 |
| 24 | Zhang Q C . A new type of turbine disc and blade material—low segregation superalloy [J]. Aeroengine, 1995, (2): 14 |
| 24 | 张庆春 . 新型涡轮盘及叶片材料——低偏析高温合金 [J]. 航空发动机, 1995, (2): 14 |
| 25 | Zhu Y X . Low segregation superalloys [J]. Trans. Mater. Heat Treat., 1997, 18(3): 16 |
| 25 | 朱耀霄 . 低偏析高温合金 [J]. 金属热处理学报, 1997, 18(3): 16 |
| 26 | Wang A C , Li Y Y , Li D F , et al . Effect of Nb and Ti contents on micro-segregation of J-90 alloy [J]. Acta Metall. Sin., 1995, 31: 216 |
| 26 | 王安川, 李依依, 李冬法 等 . Nb, Ti含量对J-90合金凝固偏析的影响 [J]. 金属学报, 1995, 31: 216 |
/
| 〈 |
|
〉 |