Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings

  • Dexin MA ,
  • Yunxing ZHAO ,
  • Weitai XU ,
  • Libo PI ,
  • Zhongxing LI
Expand
  • 1.Wedge Central South Research Institute, Shenzhen 518045, China
    2.Powder Metallurgy Research Institute, Central South University, Changsha 410083, China
ZHAO Yunxing, Tel: 15673119949, E-mail: zhaoyx1@wedge.com.cn

Received date: 2020-10-10

  Revised date: 2020-11-12

  Online published: 2021-06-11

Supported by

Development and Reform Commission of Shenzhen Municipality(SZDRC20181000);Key-Area Research and Development Program of Guangdong Province(2019B010935001)

Abstract

In recent years, surface γ/γ′-eutectics have been observed to form continuous layers along the peripheries of the outer surfaces of Ni-based single crystal (SC) castings. This type of solidification defect poses specific concerns for turbine blade production because large surface eutectics are very difficult to completely dissolve during practical heat treatment. In the present work, a third generation SC superalloy was used to cast turbine blades and cylindrical bars. However, no eutectic layer was observed on the outer surface of the blade aerofoils and bars in hundreds of castings. Instead of the lateral eutectic enrichment on the outer side surface, a non-uniform distribution of eutectics along the solidification length was detected. Eutectics were found to accumulate on the upper surface of solidification units such as platforms whereas less eutectics were observed on the bottom surface. Especially on the inclined upper surface at the junctions between platform and airfoil, a large amount of eutectics were accumulated so that only a small part could dissolve during conventional solution heat treatment. This phenomenon, called the eutectic accumulation on the upper surface, could be attributed to the upward solutal flow of eutectics forming elements through diffusion and convection, which is finally stopped beneath the upper surface. The factors influencing the upward eutectic accumulation are the chemical composition of the alloys, the process conditions, and the local geometry of the castings, such as the platform thickness and the inclination of the upper surface. Another surface effect was also observed on the eutectic dissolution during heat treatment process. It was found that the eutectics in the outer surface area were dissolved completely during heat treatment process than that in the internal one. The possible explanation is that at high temperatures, the eutectic forming elements Al and Ti evaporate from the casting surface faster than the other elements, as experimentally confirmed by chemical measurement.

Cite this article

Dexin MA , Yunxing ZHAO , Weitai XU , Libo PI , Zhongxing LI . Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings[J]. Acta Metall Sin, 2021 , 57(12) : 1539 -1548 . DOI: 10.11900/0412.1961.2020.00404

References

1 Seo S M, Lee J H, Yoo Y S, et al. A comparative study of the γ/γ′ eutectic evolution during the solidification of Ni-base superalloys [J]. Metall. Mater. Trans., 2011, 42A: 3150
2 Brewster G, Dong H B, Green N R, et al. Surface Segregation during directional solidification of Ni-base superalloys [J]. Metall. Mater. Trans., 2008, 39B: 87
3 Cao L. Research on the formation of surface eutectic of Ni-base single crystal superalloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2015
3 曹 亮. 镍基单晶高温合金中表面共晶形成行为研究 [D]. 沈阳: 中国科学院金属研究所, 2015
4 Cao L, Yao L, Zhou Y Z, et al. Formation of the surface eutectic of a Ni-based single crystal superalloy [J]. J. Mater. Sci. Technol., 2017, 33: 347
5 Cao L, Zhou Y Z, Jin T, et al. Effects of Re on surface eutectic formation for Ni-base single crystal superalloys during directional solidification [J]. J. Mater. Sci. Technol., 2017, 33: 1308
6 Sidhu R K, Ojo O A, Chaturvedi M C. Sub-solidus melting of directionally solidified Rene 80 superalloy during solution heat treatment [J]. J. Mater. Sci., 2008, 43: 3612
7 Hegde S R, Kearsey R M, Beddoes J C. Designing homogenization-solution heat treatments for single crystal superalloys [J]. Mater. Sci. Eng., 2010, A527: 5528
8 Chen R Z. A problem in manufacturing and using of cast turbine blades—Surface recrystallization [J]. Aviat. Eng. Maint., 1990, (4): 22
8 陈荣章. 铸造涡轮叶片制造和使用中的一个问题——表面再结晶 [J]. 航空制造工程, 1990, (4): 22
9 Xiong J C, Li J R, Liu S Z, et al. Microstructure of surface recrystallization of single crystal superalloy DD6 [J]. J. Mater. Eng., 2009, (): 110
9 熊继春, 李嘉荣, 刘世忠等. 单晶高温合金DD6表面再结晶组织 [J]. 材料工程, 2009, (): 110
10 Ma D X, Bührig-Polaczek A. Application of heat-conductor technique to production of single crystal turbine blade [J]. Metall. Mater. Trans., 2009, 40B: 738
11 Ma D X, Wu Q, Bührig-Polaczek A. Some new observations on freckle formation in directionally solidified superalloy components [J]. Metall. Mater. Trans., 2012, 43B: 344
12 Ma D X. Development of single crystal solidification technology for production of superalloy turbine blades [J]. Acta Metall. Sin., 2015, 51: 1179
12 马德新. 高温合金叶片单晶凝固技术的新发展 [J]. 金属学报, 2015, 51: 1179
13 Ma D X, Wang F X, Wu Q, et al. Innovations in casting techniques for single crystal turbine blades of superalloys [A]. Superalloys 2016: Proceedings of the 13th Intenational Symposium of Superalloys [C]. Warrendale, PA: TMS, 2016: 237
14 Ma D X, Wang F, Wu Q, et al. Temperature evolution and grain defect formation during single crystal solidification of a blade cluster [J]. Chin. Foundr., 2017, 14: 456
15 Ma D X. Novel casting processes for single-crystal turbine blades of superalloys [J]. Front. Mech. Eng., 2018, 13: 3
16 Giamei A F, Kear B H. On the nature of freckles in nickel base superalloys [J]. Metall. Trans., 1970, 1: 2185
17 Copley S M, Giamei A F, Johnson S M, et al. The origin of freckles in unidirectionally solidified castings [J]. Metall. Trans., 1970, 1: 2193
18 Auburtin P, Cockcroft S L, Mitchell A, et al. Liquid density inversions during the solidification of superalloys and their relationship to freckle formation in castings [A]. Superalloy 1996 [C]. Warrendale, PA: TMS, 1996: 443
19 Beckmann C, Gu J P, Boettinger W J. Development of a freckle predictor via Rayleigh number method for single-crystal nickel-base superalloy castings [J]. Metall. Mater. Trans., 2000, 31A: 2545
20 Ma D X, Bührig-Polaczek A. The geometrical effect on freckle formation in the directionally solidified superalloy CMSX-4 [J]. Metall. Mater. Trans., 2014, 45A: 1435
21 Ma D X. Freckle formation during directional solidification of complex castings of superalloys [J]. Acta Metall. Sin., 2016, 52: 426
21 马德新. 定向凝固的复杂形状高温合金铸件中的雀斑形成 [J]. 金属学报, 2016, 52: 426
22 Hong J P, Ma D X, Wang J, et al. Freckle defect formation near the casting interfaces of directionally solidified superalloys [J]. Materials, 2016, 9: 929
23 Hong J P, Ma D X, Wang J, et al. Geometrical effect of freckle formation on directionally solidified superalloy CM247 LC components [J]. J. Alloys Compd., 2015, 648: 1076
24 Ma D X, Zhou B, Bührig-Polaczek A. Investigation of freckle formation under various solidification conditions [J]. Adv. Mater. Res., 2011, 278: 428
25 Wilson B C, Cutler E R, Fuchs G E. Effect of solidification parameters on the microstructures and properties of CMSX-10 [J]. Mater. Sci. Eng., 2008, A479: 356
26 Khan T. Heat-resistant materials/superalloys [J]. Adv. Mater. Process, 1990, 137: 19
27 General Editorial Board of Aviation Manufacturing Engineering Manual. Aviation Manufacturing Engineering Manual, Heat Treatment Division [M]. Beijing: Aviation Industry Press, 1993: 325
27 《航空制造工程手册》总编委会. 航空制造工程手册——热处理 [M]. 北京: 航空工业出版社, 1993: 325
Outlines

/