Carrier Mobility Optimization in Thermoelectric Materials
Received date: 2021-03-31
Revised date: 2021-05-06
Online published: 2021-05-19
Supported by
National Key Research and Development Program of China(2018YFA0702100);National Natural Science Foundation of China(51772012);National Science Fund for Distinguished Young Scholars(51925101);National Postdoctoral Program for Innovative Talents(BX20190028);Postdoctoral Science Foundation of China(2019M660399);Programme of Introducing Talents of Discipline to Universities(B17002);Beijing Natural Science Foundation(JQ18004);Shenzhen Peacock Plan team(KQTD2016022619565991)
Thermoelectric (TE) materials are functional materials that can realize the direct and reversible conversion between heat and electricity. Their conversion efficiency is determined by their average figure of merit (ZTave). Generally, high ZTave requires TE materials to possess both excellent electrical transport properties and low thermal conductivity, called “electron crystal-phonon glass.” To date, although commonly used band manipulation and defect designing strategies can optimize the carrier effective mass and lattice thermal conductivity, they reduce the carrier mobility and thus limit the improvement of ZTave. Therefore, maintaining high carrier mobility is essential for improving ZTave over a wide temperature range. In this review, the methods to optimize carrier mobility, including crystal defect manipulations and multiple coupling parameter manipulations, were summarized. Specifically, crystal defect manipulations include strategies of crystal growth, crystal symmetry manipulation, and point defect manipulation, and the multiple coupling parameter manipulations include band alignment strategies, modulation doping, and band sharpening. Further, the applications of these strategies in multiple TE material systems were discussed, such as in SnSe/S, PbTe/Se/S, BiCuSeO, and BiAgSeS compounds. It was proven that the above strategies can well optimize the TE performance over the entire working temperature by effectively balancing carrier and phonon scattering and synergistically manipulating the coupling relationships between carrier mobility, effective mass, and carrier density. The importance of carrier mobility optimization in TE materials and a new research idea for developing high-efficiency TE materials were presented.
Li-Dong ZHAO , Sining WANG , Yu XIAO . Carrier Mobility Optimization in Thermoelectric Materials[J]. Acta Metall Sin, 2021 , 57(9) : 1171 -1183 . DOI: 10.11900/0412.1961.2021.00130
| 1 | Bell L E. Cooling, heating, generating power, and recovering waste heat with thermoelectric systems [J]. Science, 2008, 321: 1457 |
| 2 | Xiao Y, Zhao L D. Seeking new, highly effective thermoelectrics [J]. Science, 2020, 367: 1196 |
| 3 | DiSalvo F J. Thermoelectric cooling and power generation [J]. Science, 1999, 285: 703 |
| 4 | Yang J H, Stabler F R. Automotive applications of thermoelectric materials [J]. J. Electron. Mater., 2009, 38: 1245 |
| 5 | Zhang X, Zhao L D. Thermoelectric materials: Energy conversion between heat and electricity [J]. J. Materiomics, 2015, 1: 92 |
| 6 | Chang C, Zhao L D. Anharmoncity and low thermal conductivity in thermoelectrics [J]. Mater. Today Phys., 2018, 4: 50 |
| 7 | Case E D. Thermal fatigue and waste heat recovery via thermoelectrics [J]. J. Electron. Mater., 2012, 41: 1811 |
| 8 | Zhao L D, He J Q, Hao S Q, et al. Raising the thermoelectric performance of p-type PbS with endotaxial nanostructuring and valence-band offset engineering using CdS and ZnS [J]. J. Am. Chem. Soc., 2012, 134: 16327 |
| 9 | Snyder G J, Snyder A H. Figure of merit ZT of a thermoelectric device defined from materials properties [J]. Energy Environ. Sci., 2017, 10: 2280 |
| 10 | Hu X K, Zhang S M, Zhao F, et al. Thermoelectric device: Contact interface and interface materials [J]. J. Inorg. Mater., 2019, 34: 269 |
| 10 | 胡晓凯, 张双猛, 赵 府等. 热电器件的界面和界面材料 [J]. 无机材料学报, 2019, 34: 269 |
| 11 | Zhang Q H, Bai S Q, Chen L D. Technologies and applications of thermoelectric devices: Current status, challenges and prospects [J]. J. Inorg. Mater., 2019, 34: 279 |
| 11 | 张骐昊, 柏胜强, 陈立东. 热电发电器件与应用技术: 现状、挑战与展望 [J]. 无机材料学报, 2019, 34: 279 |
| 12 | Kanatzidis M G. Nanostructured thermoelectrics: The new paradigm? [J]. Chem. Mater., 2010, 22: 648 |
| 13 | Snyder G J, Toberer E S. Complex thermoelectric materials [J]. Nat. Mater., 2008, 7: 105 |
| 14 | Xiao Y, Li W, Chang C, et al. Synergistically optimizing thermoelectric transport properties of n-type PbTe via Se and Sn co-alloying [J]. J. Alloys Compd., 2017, 724: 208 |
| 15 | Sales B C. Electron crystals and phonon glasses: A new path to improved thermoelectric materials [J]. MRS Bull., 1998, 23: 15 |
| 16 | Zhao L D, Dravid V P, Kanatzidis M G. The panoscopic approach to high performance thermoelectrics [J]. Energy Environ. Sci., 2014, 7: 251 |
| 17 | Ren P, Liu Y M, He J, et al. Recent advances in inorganic material thermoelectrics [J]. Inorg. Chem. Front., 2018, 5: 2380 |
| 18 | Wang H, Pei Y Z, LaLonde A D, et al. Weak electron-phonon coupling contributing to high thermoelectric performance in n-type PbSe [J]. Proc. Natl. Acad. Sci. USA, 2012, 109: 9705 |
| 19 | Zhang G, Li B W. Impacts of doping on thermal and thermoelectric properties of nanomaterials [J]. Nanoscale, 2010, 2: 1058 |
| 20 | Pan L, Mitra S, Zhao L D, et al. The role of ionized impurity scattering on the thermoelectric performances of rock salt AgPbm-SnSe2+m [J]. Adv. Funct. Mater., 2016, 26: 5149 |
| 21 | Zhao L D, Wu H J, Hao S Q, et al. All-scale hierarchical thermoelectrics: MgTe in PbTe facilitates valence band convergence and suppresses bipolar thermal transport for high performance [J]. Energy Environ. Sci., 2013, 6: 3346 |
| 22 | Zhang L J, Qin P, Han C, et al. Enhanced thermoelectric performance through synergy of resonance levels and valence band convergence via Q/In (Q = Mg, Ag, Bi) co-doping [J]. J. Mater. Chem., 2018, 6A: 2507 |
| 23 | Pei Y Z, Shi X Y, LaLonde A, et al. Convergence of electronic bands for high performance bulk thermoelectrics [J]. Nature, 2011, 473: 66 |
| 24 | Jaworski C M, Kulbachinskii V, Heremans J P. Resonant level formed by tin in Bi2Te3 and the enhancement of room-temperature thermoelectric power [J]. Phys. Rev., 2009, 80B: 233201 |
| 25 | Skipetrov E P, Pichugin N A, Slyn'ko E I, et al. On the resonant level of chromium in the rhombohedral and cubic phases of Pb1-x-yGexCryTe alloys [J]. Semiconductors, 2013, 47: 729 |
| 26 | Qin Y X, Xiao Y, Zhao L D. Carrier mobility does matter for enhancing thermoelectric performance [J]. APL Mater., 2020, 8: 010901 |
| 27 | Liu Y, Zhao L D, Zhu Y C, et al. Synergistically optimizing electrical and thermal transport properties of bicuseo via a dual-doping approach [J]. Adv. Energy Mater., 2016, 6: 1502423 |
| 28 | Tan G J, Zhao L D, Kanatzidis M G. Rationally designing high-performance bulk thermoelectric materials [J]. Chem. Rev., 2016, 116: 12123 |
| 29 | Qin B C, Wang D Y, He W K, et al. Realizing high thermoelectric performance in p-type SnSe through crystal structure modification [J]. J. Am. Chem. Soc., 2019, 141: 1141 |
| 30 | Xiao Y, Wang D Y, Zhang Y, et al. Band sharpening and band alignment enable high quality factor to enhance thermoelectric performance in n-type PbS [J]. J. Am. Chem. Soc., 2020, 142: 4051 |
| 31 | Li J F, Liu W S, Zhao L D, et al. High-performance nanostructured thermoelectric materials [J]. NPG Asia Mater., 2010, 2: 152 |
| 32 | Shen J J, Fang T, Fu T Z, et al. Lattice thermal conductivity in thermoelectric materials [J]. J. Inorg. Mater., 2019, 34: 260 |
| 32 | 沈家骏, 方 腾, 傅铁铮等. 热电材料中的晶格热导率 [J]. 无机材料学报, 2019, 34: 260 |
| 33 | Wan C L, Pan W, Xu Q, et al. Effect of point defects on the thermal transport properties of (LaxGd1-x)2Zr2O7: Experiment and theoretical model [J]. Phys. Rev., 2006, 74B: 144109 |
| 34 | Ge Z H, Qiu Y, Chen Y X, et al. Multipoint defect synergy realizing the excellent thermoelectric performance of n-type polycrystalline SnSe via Re doping [J]. Adv. Funct. Mater., 2019, 29: 1902893 |
| 35 | Liu W S, Zhang B P, Li J F, et al. Effects of Sb compensation on microstructure, thermoelectric properties and point defect of CoSb3 compound [J]. J. Phys., 2007, 40D: 6784 |
| 36 | Hu L P, Zhu T J, Liu X H, et al. Point defect engineering of high-performance bismuth-telluride-based thermoelectric materials [J]. Adv. Funct. Mater., 2014, 24: 5211 |
| 37 | Medlin D L, Snyder G J. Interfaces in bulk thermoelectric materials: a review for current opinion in colloid and interface science [J]. Curr. Opin. Colloid Interface Sci., 2009, 14: 226 |
| 38 | Rowe D M, Shukla V S, Savvides N. Phonon scattering at grain boundaries in heavily doped fine-grained silicon-germanium alloys [J]. Nature, 1981, 290: 765 |
| 39 | Mun H, Choi S M, Lee K H, et al. Boundary engineering for the thermoelectric performance of bulk alloys based on bismuth telluride [J]. ChemSusChem, 2015, 8: 2312 |
| 40 | Chang C, Wu M H, He D S, et al. 3D charge and 2D phonon transports leading to high out-of-plane ZT in n-type SnSe crystals [J]. Science, 2018, 360: 778 |
| 41 | Zhao L D, Tan G J, Hao S Q, et al. Ultrahigh power factor and thermoelectric performance in hole-doped single-crystal SnSe [J]. Science, 2016, 351: 141 |
| 42 | He W K, Wang D Y, Wu H J, et al. High thermoelectric performance in low-cost SnS0.91Se0.09 crystals [J]. Science, 2019, 365: 1418 |
| 43 | Li S, Wang Y M, Chen C, et al. Heavy doping by bromine to improve the thermoelectric properties of n-type polycrystalline SnSe [J]. Adv. Sci., 2018, 5: 1800598 |
| 44 | Wei T R, Tan G J, Zhang X M, et al. Distinct impact of alkali-ion doping on electrical transport properties of thermoelectric p-type polycrystalline SnSe [J]. J. Am. Chem. Soc., 2016, 138: 8875 |
| 45 | Yang H Q, Wang X Y, Wu H, et al. Sn vacancy engineering for enhancing the thermoelectric performance of two-dimensional SnS [J]. J. Mater. Chem. C, 2019, 7: 3351 |
| 46 | Xiao Y, Chang C, Pei Y L, et al. Origin of low thermal conductivity in SnSe [J]. Phys. Rev., 2016, 94B: 125203 |
| 47 | He W K, Wang D Y, Dong J F, et al. Remarkable electron and phonon band structures lead to a high thermoelectric performance ZT > 1 in earth-abundant and eco-friendly SnS crystals [J]. J. Mater. Chem., 2018, 6A: 10048 |
| 48 | He W K, Qin B C, Zhao L D. Predicting the potential performance in p-type SnS crystals via utilizing the weighted mobility and quality factor [J]. Chin. Phys. Lett., 2020, 37: 087104 |
| 49 | Zhang X X, Chang C, Zhou Y M, et al. BiCuSeO Thermoelectrics: An update on recent progress and perspective [J]. Materials, 2017, 10: 198 |
| 50 | Li F, Li J F, Zhao L D, et al. Polycrystalline BiCuSeO oxide as a potential thermoelectric material [J]. Energy Environ. Sci., 2012, 5: 7188 |
| 51 | Zhao L D, Berardan D, Pei Y L, et al. Bi1-xSrxCuSeO oxyselenides as promising thermoelectric materials [J]. Appl. Phys. Lett., 2010, 97: 092118 |
| 52 | Wang S Y, Sun Y X, Yang J, et al. High thermoelectric performance in Te-free (Bi,Sb)2Se3via structural transition induced band convergence and chemical bond softening [J]. Energy Environ. Sci., 2016, 9: 3436 |
| 53 | Liu X Y, Wang D Y, Wu H J, et al. Intrinsically low thermal conductivity in BiSbSe3: A promising thermoelectric material with multiple conduction bands [J]. Adv. Funct. Mater., 2019, 29: 1806558 |
| 54 | Wang S N, Su L Z, Qiu Y T, et al. Enhanced thermoelectric performance in Cl-doped BiSbSe3 with optimal carrier concentration and effective mass [J]. J. Mater. Sci. Technol., 2021, 70: 67 |
| 55 | Huang Z W, Zhao L D. Sb2Si2Te6: A robust new thermoelectric material [J]. Trends Chem., 2020, 2: 89 |
| 56 | Luo Y B, Cai S T, Hao S Q, et al. High-performance thermoelectrics from cellular nanostructured Sb2Si2Te6 [J]. Joule, 2020, 4: 159 |
| 57 | Wang D Y, Huang Z W, Zhang Y, et al. Extremely low thermal conductivity from bismuth selenohalides with 1D soft crystal structure [J]. Sci. China Mater., 2020, 63: 1759 |
| 58 | Jiang J, Chen L D, Bai S Q, et al. Thermoelectric properties of textured p-type (Bi,Sb)2Te3 fabricated by spark plasma sintering [J]. Scr. Mater., 2005, 52: 347 |
| 59 | Zhao L D, Zhang B P, Li J F, et al. Enhanced thermoelectric and mechanical properties in textured n-type Bi2Te3 prepared by spark plasma sintering [J]. Solid State Sci., 2008, 10: 651 |
| 60 | Li Y W, Li F, Dong J F, et al. Enhanced mid-temperature thermoelectric performance of textured SnSe polycrystals made of solvothermally synthesized powders [J]. J. Mater. Chem., 2016, 4C: 2047 |
| 61 | Shang P P, Dong J F, Pei J, et al. Highly textured n-type SnSe polycrystals with enhanced thermoelectric performance [J]. Research, 2019, 2019: 9253132 |
| 62 | Sui J H, Li J, He J Q, et al. Texturation boosts the thermoelectric performance of BiCuSeO oxyselenides [J]. Energy Environ. Sci., 2013, 6: 2916 |
| 63 | Li J, Zhang X Y, Chen Z W, et al. Low-symmetry rhombohedral GeTe thermoelectrics [J]. Joule, 2018, 2: 976 |
| 64 | Zhao L D, Lo S H, Zhang Y S, et al. Ultralow thermal conductivity and high thermoelectric figure of merit in SnSe crystals [J]. Nature, 2014, 508: 373 |
| 65 | Duong A T, Nguyen V Q, Duvjir G, et al. Achieving ZT = 2.2 with Bi-doped n-type SnSe single crystals [J]. Nat. Commun., 2016, 7: 13713 |
| 66 | Peng K L, Lu X, Zhan H, et al. Broad temperature plateau for high ZTs in heavily doped p-type SnSe single crystals [J]. Energy Environ. Sci., 2016, 9: 454 |
| 67 | Peng K L, Zhang B, Wu H, et al. Ultra-high average figure of merit in synergistic band engineered SnxNa1-xSe0.9S0.1 single crystals [J]. Mater. Today, 2018, 21: 501 |
| 68 | Hou Z H, Xiao Y, Zhao L D. Investigation on carrier mobility when comparing nanostructures and bands manipulation [J]. Nanoscale, 2020, 12: 12741 |
| 69 | Cha J, Zhou C, Lee Y K, et al. High thermoelectric performance in n-type polycrystalline SnSe via dual incorporation of Cl and PbSe and dense nanostructures [J]. ACS Appl. Mater. Interfaces, 2019, 11: 21645 |
| 70 | Banik A, Vishal B, Perumal S, et al. The origin of low thermal conductivity in Sn1-xSbxTe: Phonon scattering via layered intergrowth nanostructures [J]. Energy Environ. Sci., 2016, 9: 2011 |
| 71 | Sharp J W, Poon S J, Goldsmid H J. Boundary scattering and the thermoelectric figure of merit [J]. Phys. Status Solidi, 2001, 187A: 507 |
| 72 | You L, Zhang J Y, Pan S S, et al. Realization of higher thermoelectric performance by dynamic doping of copper in n-type PbTe [J]. Energy Environ. Sci., 2019, 12: 3089 |
| 73 | Xiao Y, Wu H J, Li W, et al. Remarkable roles of Cu to synergistically optimize phonon and carrier transport in n-Type PbTe-Cu2Te [J]. J. Am. Chem. Soc., 2017, 139: 18732 |
| 74 | Qian X, Wang D Y, Zhang Y, et al. Contrasting roles of small metallic elements M (M = Cu, Zn, Ni) in enhancing the thermoelectric performance of n-type PbM0.01Se [J]. J. Mater. Chem., 2020, 8A: 5699 |
| 75 | Qian X, Wu H, Wang D, et al. Synergistically optimizing interdependent thermoelectric parameters of n-type PbSe through introducing a small amount of Zn [J]. Mater. Today Phys., 2019, 9: 100102 |
| 76 | Pei Y Z, May A F, Snyder G J. Self-tuning the carrier concentration of PbTe/Ag2Te composites with excess Ag for high thermoelectric performance [J]. Adv. Energy Mater., 2011, 1: 291 |
| 77 | Ahn K, Han M K, He J Q, et al. Exploring resonance levels and nanostructuring in the PbTe-CdTe system and enhancement of the thermoelectric figure of merit [J]. J. Am. Chem. Soc., 2010, 132: 5227 |
| 78 | Zhang J, Wu D, He D S, et al. Extraordinary thermoelectric performance realized in n-type PbTe through multiphase nanostructure engineering [J]. Adv. Mater., 2017, 29: 1703148 |
| 79 | Cai S T, Hao S Q, Luo Z Z, et al. Discordant nature of Cd in PbSe: Off-centering and core-shell nanoscale CdSe precipitates lead to high thermoelectric performance [J]. Energy Environ. Sci., 2020, 13: 200 |
| 80 | Zeng L J K, Zhang J Y, You L, et al. Enhanced thermoelectric performance in PbSe-SrSe solid solution by Mn substitution [J]. J. Alloys Compd., 2016, 687: 765 |
| 81 | Zhang X, Wang D Y, Wu H J, et al. Simultaneously enhancing the power factor and reducing the thermal conductivity of SnTe via introducing its analogues [J]. Energy Environ. Sci., 2017, 10: 2420 |
| 82 | Teng W, Wang H C, Su W B, et al. Simultaneous enhancement of thermoelectric and mechanical performance for SnTe by nano SiC compositing [J]. J. Mater. Chem., 2020, 8: 7393 |
| 83 | Zheng Y, Wang S Y, Liu W, et al. Thermoelectric transport properties of p-type silver-doped PbS with in situ Ag2S nanoprecipitates [J]. J. Phys., 2014, 47D: 115303 |
| 84 | Zhao L D, Lo S H, He J Q, et al. High performance thermoelectrics from earth-abundant materials: Enhanced figure of merit in PbS by second phase nanostructures [J]. J. Am. Chem. Soc., 2011, 133: 20476 |
| 85 | Jiang B B, Liu X X, Wang Q, et al. Realizing high-efficiency power generation in low-cost PbS-based thermoelectric materials [J]. Energy Environ. Sci., 2020, 13: 579 |
| 86 | Weidner M, Fuchs A, Bayer T J M, et al. Defect modulation doping [J]. Adv. Funct. Mater., 2019, 29: 1807906 |
| 87 | Zhang X Y, Pei Y Z. Manipulation of charge transport in thermoelectrics [J]. npj Quantum Mater., 2017, 2: 68 |
| 88 | Tsukazaki A, Akasaka S, Nakahara K, et al. Observation of the fractional quantum Hall effect in an oxide [J]. Nat. Mater., 2010, 9: 889 |
| 89 | Yu B, Zebarjadi M, Wang H, et al. Enhancement of thermoelectric properties by modulation-doping in silicon germanium alloy nanocomposites [J]. Nano Lett., 2012, 12: 2077 |
| 90 | Pei Y L, Wu H J, Wu D, et al. High thermoelectric performance realized in a BiCuSeO system by improving carrier mobility through 3D modulation doping [J]. J. Am. Chem. Soc., 2014, 136: 13902 |
| 91 | Zebarjadi M, Joshi G, Zhu G H, et al. Power factor enhancement by modulation doping in bulk nanocomposites [J]. Nano Lett., 2011, 11: 2225 |
| 92 | Hasan N, Wahid H, Nayan N, et al. Inorganic thermoelectric materials: A review [J]. Int. J. Energy Res., 2020, 44: 6170 |
| 93 | Wu D, Pei Y L, Wang Z, et al. Significantly enhanced thermoelectric performance in n-type heterogeneous BiAgSeS composites [J]. Adv. Funct. Mater., 2014, 24: 7763 |
| 94 | Banik A, Shenoy U S, Anand S, et al. Mg alloying in SnTe facilitates valence band convergence and optimizes thermoelectric properties [J]. Chem. Mater., 2015, 27: 581 |
| 95 | Chen Z W, Jian Z Z, Li W, et al. Lattice dislocations enhancing thermoelectric PbTe in addition to band convergence [J]. Adv. Mater., 2017, 29: 1606768 |
| 96 | Skipetrov E P, Skipetrova L A, Knotko A V, et al. Scandium resonant impurity level in PbTe [J]. J. Appl. Phys., 2014, 115: 133702 |
| 97 | Maier S, Ohno S, Yu G, et al. Resonant bonding, multiband thermoelectric transport, and native defects in n-type BaBiTe3-xSex (x = 0, 0.05, and 0.1) [J]. Chem. Mater., 2018, 30: 174 |
| 98 | Xiao Y, Wang D Y, Qin B C, et al. Approaching topological insulating states leads to high thermoelectric performance in n-type PbTe [J]. J. Am. Chem. Soc., 2018, 140: 13097 |
| 99 | Bali A, Chetty R, Sharma A, et al. Thermoelectric properties of In and I doped PbTe [J]. J. Appl. Phys., 2016, 120: 175101 |
| 100 | Sootsman J R, Kong H J, Uher C, et al. Large enhancements in the thermoelectric power factor of bulk PbTe at high temperature by synergistic nanostructuring [J]. Angew. Chem. Int. Ed., 2008, 47: 8618 |
| 101 | Pei Y Z, Lensch-Falk J, Toberer E S, et al. High thermoelectric performance in PbTe due to large nanoscale Ag2Te precipitates and la doping [J]. Adv. Funct. Mater., 2011, 21: 241 |
| 102 | Papageorgiou C, Giapintzakis J, Kyratsi T. Low-temperature synthesis and thermoelectric properties of n-type PbTe [J]. J. Electron. Mater., 2013, 42: 1911 |
| 103 | Zhao M H, Chang C, Xiao Y, et al. Investigations on distinct thermoelectric transport behaviors of Cu in n-type PbS [J]. J. Alloys Compd., 2019, 781: 820 |
/
| 〈 |
|
〉 |