Microstructure and Mechanical Properties of 14Cr-ODS Steel Fabricated by Ultra-High Pressure Sintering
Received date: 2021-03-03
Revised date: 2021-04-27
Online published: 2021-05-14
Supported by
National Key Research and Development Program of China(2017YFB0701801);National Natural Science Foundation of China(51974199)
Due to its superior mechanical, processing, and service properties, oxide dispersion-strengthened (ODS) alloy (particularly Fe base ODS steel) has emerged as the most promising future candidate for advanced reactor structural materials. However, there are some problems with hot isostatic pressing sintering ODS steels, such as higher sintering temperature, longer sintering time, and relatively coarse grains. In this work, 14Cr-ODS steels were prepared by ultra-high pressure sintering with a sintering pressure of 3, 4, and 5 GPa, respectively. The microstructure and mechanical properties of the ultra-high pressure sintered 14Cr-ODS steel samples were characterized by density test, SEM, TEM, hardness test, and tensile test. Based on the contrast analysis of microstructure and mechanical properties, the effect of sintering pressure on the microstructure and mechanical properties of ultra-high pressure sintered 14Cr-ODS steel was investigated, and the effect mechanism was thoroughly analyzed. Analysis results show that the main oxide precipitate of ultra-high pressure sintered 14Cr-ODS steel is Ti2O3, and the average grain size of 14Cr-ODS steel prepared by ultra-high pressure sintering is less than 300 nm, which is approximately 5% of the average grain size of 14Cr-ODS steel prepared by conventional hot isostatic pressing sintering. The average grain size of samples prepared by ultra-high pressure sintering decreased initially and then increased as sintering pressure increased. The Vickers hardness of ODS steel samples sintered at 4 GPa can reach 604 HV, and the tensile strength is approximately 1.5 GPa, which is 1.6 times than that of 14Cr-ODS steel samples with a similar composition prepared by conventional hot isostatic pressing sintering. Ultra-high pressure sintered 14Cr-ODS steel with good sintering formability and a density greater than 99% can be obtained at lower sintering temperatures and shorter sintering times. Its excellent performance can be mainly associated with the comprehensive influence of the plastic deformation effect produced by ultra-high pressure sintering on grain nucleation and atom diffusion in sintered samples.
Tao WANG , Dijun LONG , Liming YU , Yongchang LIU , Huijun LI , Zumin WANG . Microstructure and Mechanical Properties of 14Cr-ODS Steel Fabricated by Ultra-High Pressure Sintering[J]. Acta Metall Sin, 2022 , 58(2) : 184 -192 . DOI: 10.11900/0412.1961.2021.00099
| 1 | Yan P Y , Yu L M , Liu Y C , et al . Effects of Hf addition on the thermal stability of 16Cr-ODS steels at elevated aging temperatures [J]. J. Alloys Compd., 2018, 739: 368 |
| 2 | Dai L , Liu Z , Yu L M , et al . Microstructural characterization of Mg-Al-O rich nanophase strengthened Fe-Cr alloys [J]. Mater. Sci. Eng., 2020, A771: 138664 |
| 3 | Mukhopadhyay D . Development of low activation oxide-dispersion strengthened ferritic steels for fusion reactors [D]. Ann Arbor: University of Idaho, 1996 |
| 4 | Hosemann P , Frazer D , Fratoni M , et al . Materials selection for nuclear applications: Challenges and opportunities [J]. Scr. Mater., 2018, 143: 181 |
| 5 | Odette G R , Alinger M J , Wirth B D . Recent developments in irradiation-resistant steels [J]. Annu. Rev. Mater. Res., 2008, 38: 471 |
| 6 | Lescoat M L , Ribis J , Gentils A , et al . In situ TEM study of the stability of nano-oxides in ODS steels under ion-irradiation [J]. J. Nucl. Mater., 2012, 428: 176 |
| 7 | Shao Y , Yu L M , Liu Y C , et al . Hot deformation behaviors of a 9Cr oxide dispersion-strengthened steel and its microstructure characterization [J]. Int. J. Min. Met. Mater., 2019, 26: 597 |
| 8 | Ren J , Yu L M , Liu Y C , et al . Microstructure evolution and tensile properties of an Al added high-Cr ODS steel during thermal aging at 650℃ [J]. Fusion Eng. Des., 2020, 157: 111700 |
| 9 | Abe F . Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants [J]. Sci. Technol. Adv. Mater., 2008, 9: 013002 |
| 10 | Capdevila C , Miller M K , Russell K F , et al . Phase separation in PM 2000TM Fe-base ODS alloy: Experimental study at the atomic level [J]. Mater. Sci. Eng., 2008, A490: 277 |
| 11 | Kobayashi S , Takasugi T . Mapping of 475℃ embrittlement in ferritic Fe-Cr-Al alloys [J]. Scr. Mater., 2010, 63: 1104 |
| 12 | Capdevila C , Miller M K , Toda I , et al . Influence of the α-α' phase separation on the tensile properties of Fe-base ODS PM 2000 alloy [J]. Mater. Sci. Eng., 2010, A527: 7931 |
| 13 | Kim I S , Choi B Y , Kang C Y , et al . Effect of Ti and W on the mechanical properties and microstructure of 12% Cr base mechanical-alloyed nano-sized ODS ferritic alloys [J]. ISIJ Int., 2003, 43: 1640 |
| 14 | Kim I S , Okuda T , Kang C Y , et al . Effect of oxide species and thermomechanical treatments on the strength properties of mechanically alloyed Fe-17%Cr ferritic ODS materials [J]. Met. Mater., 2000, 6: 513 |
| 15 | Li Z Y , Lu Z , Xie R , et al . Effects of Y2O3, La2O3 and CeO2 additions on microstructure and mechanical properties of 14Cr-ODS ferrite alloys produced by spark plasma sintering [J]. Fusion Eng. Des., 2017, 121: 159 |
| 16 | Li S F . Study on oxide strengthened dispersion alloys for generation IV advanced nuclear systems [D]. Beijing: University of Science and Technology Beijing, 2016 |
| 16 | 李少夫 . 用于第四代先进核能系统的氧化物弥散强化合金的研究 [D]. 北京: 北京科技大学, 2016 |
| 17 | Dadé M , Malaplate J , Garnier J , et al . Influence of microstructural parameters on the mechanical properties of oxide dispersion strengthened Fe-14Cr steels [J]. Acta Mater., 2017, 127: 165 |
| 18 | Zhao Q , Ma Z Q , Yu L M , et al . Tailoring the secondary phases and mechanical properties of ODS steel by heat treatment [J]. J. Mater. Sci. Technol., 2019, 35: 1064 |
| 19 | Gong M Q , Zhou Z J , Hu H L , et al . Effects of aluminum on microstructure and mechanical behavior of 14Cr-ODS steels [J]. J. Nucl. Mater., 2015, 462: 502 |
| 20 | Peng Y Y , Yu L M , Liu Y C , et al . Effect of ageing treatment at 650oC on microstructure and properties of 9Cr-ODS steel [J]. Acta Metall. Sin., 2020, 56: 1075 |
| 20 | 彭艳艳, 余黎明, 刘永长 等 . 650℃时效对9Cr-ODS钢显微组织和性能的影响 [J]. 金属学报, 2020, 56: 1075 |
| 21 | Zhao Q , Yu L M , Liu Y C , et al . Effects of aluminum and titanium on the microstructure of ODS steels fabricated by hot pressing [J]. Int. J. Min. Met. Mater., 2018, 25: 1156 |
| 22 | Oksiuta Z , Ozieblo A , Perkowski K , et al . Influence of HIP pressure on tensile properties of a 14Cr ODS ferritic steel [J]. Fusion Eng. Des., 2014, 89: 137 |
| 23 | Zhao Q , Yu L M , Liu Y C , et al . Microstructure and tensile properties of a 14Cr ODS ferritic steel [J]. Mater. Sci. Eng., 2017, A680: 347 |
| 24 | Ma F K . Isostatic Pressing Technology [M]. Beijing: Metallurgical Industry Press, 1992: 158 |
| 24 | 马福康 . 等静压技术 [M]. 北京: 冶金工业出版社, 1992: 158 |
| 25 | Pazos D , Suárez M , Fernández A , et al . Microstructural comparison of oxide dispersion strengthened Fe-14Cr steels produced by HIP and SPS [J]. Fusion Eng. Des., 2019, 146: 2328 |
| 26 | Zhang Y Z , Li Y G , Han B , et al . Microstructural characteristics of Hadfield steel solidified under high pressure [J]. High Press. Res., 2011, 31: 634 |
| 27 | Gu T , Xu F Q , Zhao Y H , et al . Effects of high pressure heat treatment on microstructure and mechanical properties of aluminum bronze [J]. Mater. Res. Express, 2019, 6: 096508 |
| 28 | Du C C , Jin S B , Fang Y , et al . Ultrastrong nanocrystalline steel with exceptional thermal stability and radiation tolerance [J]. Nat. Commun., 2018, 9: 5389 |
| 29 | Porter D A , Easterling K E , translated by Li C H , Yu Y N . Phase Transformations in Metals and Alloys [M]. Beijing: Metallurgical Industry Press, 1981: 286 |
| 29 | Porter D A, Easterling K E 著, 李长海, 余永宁译. 金属和合金中的相变 [M]. 北京: 冶金工业出版社, 1981: 286 |
| 30 | Xia L F , Zhang Z X . Diffusion in Metals [M]. Harbin: Harbin Institute of Technology Press, 1989: 74 |
| 30 | 夏立芳, 张振信 . 金属中的扩散 [M]. 哈尔滨: 哈尔滨工业大学出版社, 1989: 74 |
| 31 | Sakasegawa H , Chaffron L , Legendre F , et al . Correlation between chemical composition and size of very small oxide particles in the MA957 ODS ferritic alloy [J]. J. Nucl. Mater., 2009, 384: 115 |
| 32 | Seol J B , Haley D , Hoelzer D T , et al . Influences of interstitial and extrusion temperature on grain boundary segregation, Y-Ti-O nanofeatures, and mechanical properties of ferritic steels [J]. Acta Mater., 2018, 153: 71 |
| 33 | Jiang Y , Smith J R , Odette G R . Formation of Y-Ti-O nanoclusters in nanostructured ferritic alloys: A first-principles study [J]. Phys. Rev., 2009, 79B: 064103 |
| 34 | Qian Q , Wang Y R , Jiang Y , et al . Nucleation of Y-X-O (X = Al, Ti, or Zr) NCs in nano-structured ferritic alloys: A first principles comparative study [J]. J. Nucl. Mater., 2019, 518: 140 |
| 35 | Williams C A , Unifantowicz P , Baluc N , et al . The formation and evolution of oxide particles in oxide-dispersion-strengthened ferritic steels during processing [J]. Acta Mater., 2013, 61: 2219 |
| 36 | Zhang W Q . Phase Transformations in Solid Metals and Alloys [M]. Beijing: National Defense Industry Press, 2016: 70 |
| 36 | 张伟强 . 固态金属及合金中的相变 [M]. 北京: 国防工业出版社, 2016: 70 |
/
| 〈 |
|
〉 |