Research paper

As-Cast Spot Segregation of Gear Steel and Its Evolution in the Rolled Products

  • Zhuang ZHANG ,
  • Haiyang LI ,
  • Lei ZHOU ,
  • Huasong LIU ,
  • Haiyan TANG ,
  • Jiaquan ZHANG
Expand
  • 1.School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
    2.Special Steel Department, Nanjing Iron & Steel Co. , Ltd. , Nanjing 210035, China
ZHANG Jiaquan, professor, Tel: (010)62334222, E-mail: jqzhang@metall.ustb.edu.cn

Received date: 2020-12-02

  Revised date: 2021-02-10

  Online published: 2021-03-19

Supported by

National Natural Science Foundation of China(U1860111、51874033);Project to Strengthen Industrial Development at the Grass-Roots Level(TC180A3Y1/14)

Abstract

As a crucial transmission component and basic component in mechanical equipment, gears have extremely high requirements for homogeneity of elements. However, the banded segregation defects in a rolled bar will reduce the hardenability of the finished gear and cause uneven deformation in heat treatment. Generally, the formation of banded defects is believed to inseparable from semimacro segregation in the bloom castings. Spot segregation in gear steel bloom and banded segregation defects in a rolled bar were experimentally studied to explore its evolution. The correlation between the spot segregation and banded defects was clarified from the aspects of morphology characteristics, position distribution, element segregation, and spacing statistics using hot acid etching, dendritic etching, electron probe microanalysis (EPMA), and statistical calculations. The evolution law of spot segregation and the possibility of elimination of banded defects in the heat treatment stage were also discussed. Experimental results show that spot segregation mainly exists in the central equiaxed crystal area of the castings, and solute elements such as C, Mn, and Cr in the segregated spot show positive segregation. The wide banded defects are consistent with the spot segregation in their geometrical location and element distribution pattern. Morphologically, there are two types of banded defects in which the dendrite microsegregation and the independently existing spot segregation are changed into separate band structures during the hot rolling process, while the interconnected spot segregations convert into a type of converged band defect through the hot deformation. Thus, more fine and coarse banded defects have been observed in the final rolled bar products than the numbers of as-cast spot segregation. Heat treatment through heating and insulation at 1200oC can reduce the degree of solute segregation in the banded defects with a width less than 40 μm, but it shows little beneficial effect on the more coarse-sized banded defects, which suggests that they should be controlled from the original as-cast dendrite morphology during the casting process.

Cite this article

Zhuang ZHANG , Haiyang LI , Lei ZHOU , Huasong LIU , Haiyan TANG , Jiaquan ZHANG . As-Cast Spot Segregation of Gear Steel and Its Evolution in the Rolled Products[J]. Acta Metall Sin, 2021 , 57(10) : 1281 -1290 . DOI: 10.11900/0412.1961.2020.00482

References

1 Zhang Y, Huo S B, Huang Y X. Developing and producing of gear steel [J]. Metall. Standard. Qual., 2003, 41(1): 17
1 张 悦, 霍松波, 黄一新. 齿轮钢的开发与生产 [J]. 冶金标准化与质量, 2003, 41(1): 17
2 Guo F J, Wang X L, Wang J L, et al. The significance of central segregation of continuously cast billet on banded microstructure and mechanical properties of section steel [J]. Metals, 2020, 10: 76
3 Navas V G, Gonzalo O, Quintana I, et al. Residual stresses and structural changes generated at different steps of the manufacturing of gears: Effect of banded structures [J]. Mater. Sci. Eng., 2011, A528: 5146
4 Thompson S W, Howell P R. Factors influencing ferrite/pearlite banding and origin of large pearlite nodules in a hypoeutectoid plate steel [J]. Mater. Sci. Technol., 1992, 8: 777
5 Hunkel M, Kagathara J, Prahl U. The influence of segregations after forming on the heat treatment result of bevel gears [J]. Steel. Res. Int., 2019, 90: 1800427
6 Lan P, Tie Z P, Zhang W, et al. Research progress on spot segregation defects in continuously cast semi-products [J]. Iron Steel, 2020, 55(2): 11
6 兰 鹏, 铁占鹏, 张 伟等. 连铸坯点状偏析缺陷研究进展 [J]. 钢铁, 2020, 55(2): 11
7 Tsuchida Y, Nakada M, Sugawara I, et al. Behavior of semi-macroscopic segregation in continuously cast slabs and technique for reducing the segregation [J]. Trans. Iron Steel Inst. Japan, 1984, 24: 899
8 Fang J, He Y D, Tian D, et al. Study on spot segregation and internal bubble defects of low carbon gear steel [J]. Spec. Steel, 1991, 12(4): 31
8 方 军, 何英达, 田 党等. 低碳齿轮钢中点状偏析及内部气泡缺陷的研究 [J]. 特殊钢, 1991, 12(4): 31
9 Ji Y, Lan P, Geng H, et al. Behavior of spot segregation in continuously cast blooms and the resulting segregated band in oil pipe steels [J]. Steel Res. Int., 2018, 89: 1700331
10 Geng H, Zhang Z H, Tang H Y, et al. Study on segregation and Nb-bearing precipitates of high-strength oil well casing steel [J]. J. Iron. Steel Res., 2019, 31: 387
10 耿 豪, 张忠铧, 唐海燕等. 高强度油井套管钢偏析与含Nb析出相研究 [J]. 钢铁研究学报, 2019, 31: 387
11 Xu Z G, Wang X H, Huang F X, et al. Solidification structure and semi-macro segregation of pipeline steel continuous casting slabs [J]. J. Univ. Sci. Technol. Beijing., 2014, 36: 751
11 许志刚, 王新华, 黄福祥等. 管线钢连铸板坯的半宏观偏析和凝固组织 [J]. 北京科技大学学报, 2014, 36: 751
12 Yang C, Min Y A, Ouyang J X. Influence of banded microstructure on quenching dilatometry in 22CrMo steel bars [J]. Trans. Mater. Heat Treat., 2014, 35(8): 80
12 杨 超, 闵永安, 欧阳剑雄. 带状组织对22CrMo钢棒材淬火特性的影响 [J]. 材料热处理学报, 2014, 35(8): 80
13 Liu Y X. Reason of formation, harmful effect and removal of band structure in low carbon alloy steel [J]. Heat Treat., 2000, (12): 1
13 刘云旭. 低碳合金钢中带状组织的成因、危害和消除 [J]. 金属热处理, 2000, (12): 1
14 Groβterlinden R, Kawalla R, Lotter U, et al. Formation of pearlitic banded structures in ferritic-pearlitic steels [J]. Steel Res., 1992, 63: 331
15 Krauss G. Solidification, segregation, and banding in carbon and alloy steels [J]. Metall. Mater. Trans., 2003, 34B: 781
16 Offerman S E, van Dijk N H, Rekveldt M T, et al. Ferrite/pearlite band formation in hot rolled medium carbon steel [J]. Mater. Sci. Technol., 2002, 18: 297
17 He X F, Wang X H, Wang Y, et al. Formation and effects of banded structures in 55SiCrA spring steel wire rod [J]. Metall. Res. Technol., 2015, 112: 606
18 Preβlinger H, Mayr M, Tragl E, et al. Assessment of the primary structure of slabs and the influence on hot-and cold-rolled strip structure [J]. Steel Res. Int., 2006, 77: 107
19 Zhang Y L, Liu H Y, Ruan X J, et al. Microsegregation behaviors of alloy elements and their effects on the formation of banded structure in pinion steels [J]. J. Univ. Sci. Technol. Beijing, 2009, 31(suppl.1): 199
19 张延玲, 刘海英, 阮小江等. 中低碳齿轮钢中合金元素的偏析行为及其对带状组织的影响 [J]. 北京科技大学学报, 2009, 31(): 199
20 Zhang Y H, Lai H Z, Zhao H J. Research status of banded structure in steel [J]. Steel Rolling, 2014, 31(3): 45
20 张迎晖, 赖泓州, 赵鸿金. 钢中带状组织的研究现状 [J]. 轧钢, 2014, 31(3): 45
21 Ji Y, Min Y F, Li P S, et al. Research status of banding phenomena in steels [J]. China Metall., 2016, 26(4): 1
21 纪 元, 闵云峰, 李鹏善等. 钢中带状组织及其研究现状 [J]. 中国冶金, 2016, 26(4): 1
22 Zhang Z Q, Wang X H, Huang F X, et al. Relationship between solidification microstructure and centerline segregation in pipeline steel slabs with soft-reduction condition [J]. Iron Steel, 2012, 47(12): 39
22 张正群, 王新华, 黄福祥等. 轻压下条件下管线钢铸坯凝固组织与中心偏析的关系 [J]. 钢铁, 2012, 47(12): 39
23 Ji Y, He Q, Geng H, et al. Effect of dendritic structure on the spot segregation of continuously cast round bloom [A]. AISTech 2017-Proceedings of the Iron and Steel Technology Conference [C]. Nashiville: Association for Iron and Steel Technology (AISTECH), 2017: 2599
24 Xu X J, Deng A Y, Wang E G, et al. Effect mechanism of high frequency electro-magnetic field on the surface quality and equiaxed crystal ratio of 15CrMo billet [J]. Acta Metall. Sin., 2009, 45: 1330
24 许秀杰, 邓安元, 王恩刚等. 高频电磁场对15CrMo连铸坯表面质量和等轴晶率的影响机理 [J]. 金属学报, 2009, 45: 1330
25 Nuri Y, Ohashi T, Hiromoto T, et al. Solidification macrostructure of ingots and continuously cast slabs treated with rare earth metal [J]. Trans. Iron Steel Inst. Japan, 1982, 22: 408
26 Li G, Lan P, Zhang J Q. Solidification structure refinement in TWIP steel by Ce inoculation [J]. Acta Metall. Sin., 2020, 56: 704
26 李 根, 兰 鹏, 张家泉. 基于Ce变质处理的TWIP钢凝固组织细化 [J]. 金属学报, 2020, 56: 704
27 Li B, Zhang Z H, Liu H S, et al. Characteristics and evolution of the spot segregations and banded defects in high strength corrosion resistant tube steel [J]. Acta Metall. Sin., 2019, 55: 762
27 李 博, 张忠铧, 刘华松等. 高强耐蚀管钢点状偏析及带状缺陷的特征与演变 [J]. 金属学报, 2019, 55: 762
28 Haida O, Kitaoka H, Habu Y, et al. Macro-and semi-macroscopic features of the centerline segregation in CC slabs and their effect on product quality [J]. Trans. Iron Steel Inst. Japan, 1984, 24: 891
29 Xu Z G, Wang X H, Zhou L, et al. Effects of soft reduction parameters on semi-macro segregation in continuously cast slab [J]. Iron Steel, 2014, 49(3): 36
29 许志刚, 王新华, 周 力等. 轻压下参数对连铸板坯半宏观偏析的影响 [J]. 钢铁, 2014, 49(3): 36
30 Oh K S, Chang Y W. Macro and microscopic segregation behavior of center segregations in high carbon steel CC blooms during the final stage of solidification [J]. Process. Technol., 1995, 13: 381
31 Rivera-Díaz-Del-Castillo P E J, Van Der Zwaag S, Sietsma J. A model for ferrite/pearlite band formation and prevention in steels [J]. Metall. Mater. Trans., 2004, 35A: 425
Outlines

/