Microstructure and Tribological Properties of WC-Ni Matrix Cermet Coatings Prepared by Electrospark Deposition on H13 Steel Substrate
Received date: 2020-09-09
Revised date: 2021-01-04
Online published: 2021-03-10
Supported by
Fundamental Research Funds for the Central Universities(45120031B004);Co-Construction Project of Jilin University and Jilin Province(440050316A14)
H13 steel is one of the most promising materials for molds owing to its outstanding hardenability, high toughness, and thermal cracking resistance. To reinforce the surface performance and extend service life of H13 steel, a WC-Ni matrix cermet composite coating with a Ni or Mo transition layer was prepared by electrospark deposition on an H13 steel substrate. The phase compositions, microstructure, microhardness, and tribological properties of the coating were investigated in detail. The surface of the WC-Ni coating contained accumulated sputtered deposition spots. The cross section of WC-Ni coating is composed of a coating, a transition layer, and a substrate with a clear boundary; the WC hard phases are dispersed in the coating. The Ni/WC-Ni composite coating surface is relatively smooth and flat, and its phase composition is consistent with that of the WC-Ni coating. The WC hard phases show abnormal growth at the interface. The surface of a Mo/WC-Ni composite coating exhibits microcracks and indicates the formation of a new Fe9.7Mo0.3 phase. Hardness values of the composite coatings are greater than that of the WC-Ni coating, and their friction coefficient and wear loss are lower than that of the H13 steel substrate and WC-Ni coating. In addition, the antiabrasive performance of the Mo/WC-Ni composite coating is better than that of the Ni/WC-Ni composite coating.
Wenquan WANG , Ming DU , Xinge ZHANG , Mingzhang GENG . Microstructure and Tribological Properties of WC-Ni Matrix Cermet Coatings Prepared by Electrospark Deposition on H13 Steel Substrate[J]. Acta Metall Sin, 2021 , 57(8) : 1048 -1056 . DOI: 10.11900/0412.1961.2020.00360
| 1 | Zhao X Y. Research on metal based ceramic composite coatings and the wear resistance prepared by laser cladding on H13 die steel [D]. Guangzhou: Jinan University, 2016 |
| 1 | 赵雪阳. H13钢表面激光熔覆制备金属基陶瓷复合涂层及其耐磨性的研究 [D]. 广州: 暨南大学, 2016 |
| 2 | Liao F. PN + PECVD duplex treatment on the surface of H13 steel: Preparation and mechanical properties [D]. Guangzhou: South China University of Technology, 2012 |
| 2 | 廖 芳. H13钢表面PN + PECVD复合处理工艺及性能的研究 [D]. 广州: 华南理工大学, 2012 |
| 3 | Cen S B, Chen H, Liu Y, et al. Effect of CeO2 on corrosion behavior of WC-12Co coatings by high velocity oxygen fuel [J]. Acta Metall. Sin., 2016, 52: 1441 |
| 3 | 岑升波, 陈 辉, 刘 艳等. CeO2对超音速火焰喷涂WC-12Co涂层腐蚀行为的影响 [J]. 金属学报, 2016, 52: 1441 |
| 4 | Xue P. Study on modification of WC-10Ni cemented carbide [D]. Nanchang: Nanchang Hangkong University, 2017 |
| 4 | 薛 萍. WC-10Ni硬质合金的改性研究 [D]. 南昌: 南昌航空大学, 2017 |
| 5 | Chen H Y, Wang Z C, Luo L M, et al. Effect of Ni content on microstructure and properties of WC-Ni composites prepared by electroless plating and powder metallurgy [J]. Rare Met. Mater. Eng., 2017, 46: 2820 |
| 6 | Wada K, Yagi T, Gotou H, et al. Development of new WC-Ni hardmetals for use in high pressure experiments [J]. High Pressure Res., 2015, 35: 263 |
| 7 | Chen Q Y, Fu W, Du D M, et al. Comparison of microstructure and properties of WC-Ni coating by atmospheric plasma spraying and high velocity oxygen-fuel spraying [J]. Rare Met. Mater. Eng., 2019, 48: 3680 |
| 7 | 陈清宇, 富 伟, 杜大明等. 大气等离子喷涂和超音速火焰喷涂WC-Ni涂层组织结构和性能的对比 [J]. 稀有金属材料与工程, 2019, 48: 3680 |
| 8 | Zhang X Y. A study of microstructure and interface of WC-Ni by flame spraying [D]. Dalian: Dalian University of Technology, 2016 |
| 8 | 张翔宇. 火焰喷涂WC-Ni涂层组织与界面研究 [D]. 大连: 大连理工大学, 2016 |
| 9 | Yang J X, Zhang J Q, Chang W Q, et al. High temperature dry sliding friction and wear performance of laser cladding WC/Ni composite coating [J]. J. Mater. Eng., 2016, 44(6): 110 |
| 9 | 杨胶溪, 张健全, 常万庆等. 激光熔覆WC/Ni基复合涂层高温滑动干摩擦磨损性能 [J]. 材料工程, 2016, 44(6): 110 |
| 10 | Zhao W, Zhang K, Liu P, et al. Study on microstructure and properties of laser cladding Ni-based WC composite coating [J]. J. Funct. Mater., 2019, 50: 01098 |
| 10 | 赵 伟, 张 柯, 刘 平等. 激光熔覆Ni基WC复合熔覆层组织与性能的研究 [J]. 功能材料, 2019, 50: 01098 |
| 11 | Tehrani H M, Shoja-Razavi R, Erfanmanesh M, et al. Evaluation of the mechanical properties of WC-Ni composite coating on an AISI 321 steel substrate [J]. Opt. Laser Technol., 2020, 127: 106138 |
| 12 | Wu Z W, Chen J, Piao N, et al. Synthesis and passive property of nanocomposite Ni-WC coating [J]. Acta Metall. Sin., 2013, 49: 1185 |
| 12 | 武占文, 陈 吉, 朴 楠等. Ni-WC纳米复合镀层的制备及钝化性能研究 [J]. 金属学报, 2013, 49: 1185 |
| 13 | Johnson R N, Sheldon G L. Advances in the electrospark deposition coating process [J]. J. Vac. Sci. Technol., 1986, 4A: 2740 |
| 14 | Wei X, Chen Z G, Zhong J, et al. Feasibility of preparing Mo2FeB2-based cermet coating by electrospark deposition on high speed steel [J]. Surf. Coat. Technol., 2016, 296: 58 |
| 15 | Salmaliyan M, Malek G F, Ebrahimnia M. Effect of electro spark deposition process parameters on WC-Co coating on H13 steel [J]. Surf. Coat. Technol., 2017, 321: 81 |
| 16 | Burkov A A. Wear resistance of electrospark WC-Cо coatings with different iron contents [J]. J. Frict. Wear, 2016, 37: 385 |
| 17 | Burkov A A, Pyachin S A. Formation of WC-Co coating by a novel technique of electrospark granules deposition [J]. Mater. Des., 2015, 80: 109 |
| 18 | Suzuki H, Yamamoto T. Effects of carbon content on some properties of WC-10%(Co-Ni) cemented carbides [J]. J. Jpn. Soc. Powder Powder Metall., 1968, 15: 68 |
| 19 | Chen D Y, Luo Z Q. The characteristics development and application of WC-Ni cemented carbide [J]. Cement. Carb., 2007, 24: 43 |
| 19 | 陈德勇, 罗在清. WC-Ni硬质合金的特性、发展及其应用 [J]. 硬质合金, 2007, 24: 43 |
| 20 | Zhang Y, Chen Z G, Wei X, et al. Microstructure and properties of chromium carbide based metal-ceramic coatings prepared by electro-spark deposition [J]. Rare Met. Mater. Eng., 2019, 48: 601 |
| 20 | 张 怡, 陈志国, 魏 祥等. 电火花沉积碳化铬基金属陶瓷涂层的微观组织与性能 [J]. 稀有金属材料与工程, 2019, 48: 601 |
| 21 | Li Q. Study on preparation of novel core/shell structured WC-Ni cemented carbides and properties [D]. Nanchang: Nanchang Hangkong University, 2015 |
| 21 | 李 强. 新型核壳结构WC-Ni硬质合金的制备及性能研究 [D]. 南昌: 南昌航空大学, 2015 |
| 22 | Yang X T, Li X Q, Yang Q B, et al. Effects of WC on microstructure and corrosion resistance of directional structure Ni60 coatings [J]. Surf. Coat. Technol., 2020, 385: 125359 |
| 23 | Wang R J, Qian Y Y, Liu J. Interface behavior study of WC92-Co8 coating produced by electrospark deposition [J]. Appl. Surf. Sci., 2005, 240: 42 |
| 24 | Guo C, Chen J M, Zhou J S, et al. Effects of WC-Ni content on microstructure and wear resistance of laser cladding Ni-based alloys coating [J]. Surf. Coat. Technol., 2012, 206: 2064 |
| 25 | Yang G R, Song W M, Li J, et al. Wear behavior of Ni/WC surface-infiltrated composite coating on copper substrate [J]. Int. J. Mater. Res., 2016, 107: 88 |
| 26 | Wen S Z, Huang P. Principles of Tribology [M]. 2nd Ed., Beijing: Tsinghua University Press, 2002: 283 |
| 26 | 温诗铸, 黄 平. 摩擦学原理 [M]. 第2版, 北京: 清华大学出版社, 2002: 283 |
| 27 | Xu J S, Zhang X C, Xuan F Z, et al. Microstructure and sliding wear resistance of laser cladded WC/Ni composite coatings with different contents of WC particle [J]. J. Mater. Eng. Perform., 2012, 21: 1904 |
| 28 | Bao C G, Gao Y M, Xing J D, et al. Wear behavior of plasma sprayed Ni-WC composite coatings [J]. Key Eng. Mater., 2007, 336-338: 1731 |
/
| 〈 |
|
〉 |