Research paper

Effects of Heat Treatment on Microstructure and Mechanical Properties of a Bimodal Grain Ultra-Low Carbon 9Cr-ODS Steel

  • Jiarong ZHANG ,
  • Yanfen LI ,
  • Guangquan WANG ,
  • Feiyang BAO ,
  • Xiang RUI ,
  • Quanqiang SHI ,
  • Wei YAN ,
  • Yiyin SHAN ,
  • Ke YANG
Expand
  • 1.School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
    2.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3.CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    4.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
LI Yanfen, professor, Tel: (024)23978990, E-mail: yfli@imr.ac.cnSHAN Yiyin, professor, Tel: (024)23971517, E-mail: yyshan@imr.ac.cn

Received date: 2020-12-18

  Revised date: 2021-02-09

  Online published: 2021-03-09

Supported by

National Natural Science Foundation of China(51971217);Excellent Scholar Funding of Institute of Metal Research, Chinese Academy of Sciences(JY7A7A111A1)

Abstract

Oxide dispersion strengthened (ODS) steel is a promising structural material for advanced nuclear power systems. In this study, an ultra-low carbon 9Cr-ODS steel with a bimodal grain structure was prepared using powder metallurgy, and a superior matching of strength and plasticity was expected by adjusting the soft-hard matching of the coarse-grained and fine-grained regions. The effects of heat treatment on microstructure and mechanical properties of the ultra-low carbon 9Cr-ODS steel were evaluated through OM, SEM, TEM, microhardness, and tensile tests. The results demonstrated that the ultra-low carbon 9Cr-ODS steel exhibited a tempered martensite structure after normalizing at 1050-1200oC, and then tempering at 700 and 750oC. Moreover, it presented the microstructure characteristics of coarse-grained and fine-grained regions, in which the average grain size of fine-grained regions was 1.6 μm and that of coarse-grained regions was 4.3 μm. The dislocation density in the ultra-low carbon 9Cr-ODS steel was very high and the number density of nano-scale oxide particles was up to about 1022 m-3. The microhardness in fine-grained regions was higher than that in coarse-grained regions. As the normalizing temperature increased, the microhardness of the ultra-low carbon 9Cr-ODS steel first increased and then decreased. The microhardness reached the highest after normalizing at 1100oC. When the normalizing temperature increased to 1200oC, the microhardness decreased due to the growth of austenitic grains. Regarding the tempering temperature, the microhardness first decreased and then increased as the tempering temperature increased from 700oC to 800oC. Furthermore, the decrease in microhardness when tempering at 700 and 750oC was because the microstructure was recovered and softened. The higher the tempering temperature, the lower the microhardness. However, when tempering at 800oC, the microhardness increased significantly, mainly due to the partial austenite transformation of martensite. The tensile test results at 25oC showed that the strength of the ultra-low carbon 9Cr-ODS steel first decreased and then increased by increasing the tempering temperature, which was consistent with the microhardness change while the opposite was observed for elongation. The tensile test results at 700oC showed that the strength of the ultra-low carbon 9Cr-ODS steel slightly decreased by increasing the tempering temperature. Moreover, the fracture morphology was dominated by fine dimples and secondary tearing, indicating that the ultra-low carbon 9Cr-ODS steel underwent ductile fracture. Combined with the mechanical property and fracture analysis results, the ultra-low carbon 9Cr-ODS steel exhibited superior matching of strength and plasticity after normalizing at 1150oC for 1 h and tempering at 750oC for 1 h.

Cite this article

Jiarong ZHANG , Yanfen LI , Guangquan WANG , Feiyang BAO , Xiang RUI , Quanqiang SHI , Wei YAN , Yiyin SHAN , Ke YANG . Effects of Heat Treatment on Microstructure and Mechanical Properties of a Bimodal Grain Ultra-Low Carbon 9Cr-ODS Steel[J]. Acta Metall Sin, 2022 , 58(5) : 623 -636 . DOI: 10.11900/0412.1961.2020.00507

References

1 Rong J, Liu Z. Development and prospect of advanced nuclear energy technology [J]. Atom. Energy Sci. Technol., 2020, 54: 1638
1 荣 健, 刘 展. 先进核能技术发展与展望 [J]. 原子能科学技术, 2020, 54: 1638
2 Li G X, Zhou B X, Xiao M, et al. Overall development strategy of China's new-generation nuclear fuel [J]. Strateg. Study CAE, 2019, 21: 6
2 李冠兴, 周邦新, 肖 岷 等. 中国新一代核能核燃料总体发展战略研究 [J]. 中国工程科学, 2019, 21: 6
3 Xu Y P, Lü Y M, Zhou H S, et al. A review on the development of the structural materials of the fusion blanket [J]. Mater. Rev., 2018, 32: 2897
3 徐玉平, 吕一鸣, 周海山 等. 核聚变堆包层结构材料研究进展及展望 [J]. 材料导报, 2018, 32: 2897
4 Zinkle S J, Boutard J L, Hoelzer D T, et al. Development of next generation tempered and ODS reduced activation ferritic/martensitic steels for fusion energy applications [J]. Nucl. Fusion, 2017, 57: 092005
5 Hsiung L L, Fluss M J, Tumey S J, et al. Formation mechanism and the role of nanoparticles in Fe-Cr ODS steels developed for radiation tolerance [J]. Phys. Rev., 2010, 82B: 184103
6 Feng Y C, Xing W W, Wang S L, et al. First-principles study of hydrogen behaviors at oxide/ferrite interface in ODS steels [J]. Acta Metall. Sin., 2018, 54: 325
6 冯宇超, 邢炜伟, 王寿龙 等. ODS钢中氧化物/铁素体界面捕氢行为的第一原理研究 [J]. 金属学报, 2018, 54: 325
7 Suryanarayana C. Mechanical alloying and milling [J]. Prog. Mater. Sci., 2001, 46: 1
8 Laurent-Brocq M, Legendre F, Mathon M H, et al. Influence of ball-milling and annealing conditions on nanocluster characteristics in oxide dispersion strengthened steels [J]. Acta Mater., 2012, 60: 7150
9 Zilnyk K D, Oliveira V B, Sandim H R Z, et al. Martensitic transformation in Eurofer-97 and ODS-Eurofer steels: A comparative study [J]. J. Nucl. Mater., 2015, 462: 360
10 Jarugula R, Koppoju S, Jeyaraam R, et al. On the understanding of microstructural evolution during hot deformation of n-ODS-18Cr ferritic steel containing heterogeneous microstructure [J]. Mater. Sci. Eng., 2021, A800: 140343
11 Alam M E, Pal S, Fields K, et al. Tensile deformation and fracture properties of a 14YWT nanostructured ferritic alloy [J]. Mater. Sci. Eng., 2016, A675: 437
12 Steckmeyer A, Praud M, Fournier B, et al. Tensile properties and deformation mechanisms of a 14Cr ODS ferritic steel [J]. J. Nucl. Mater., 2010, 405: 95
13 Guo L, Jia C C, Hu B F, et al. Microstructure and mechanical properties of an oxide dispersion strengthened ferritic steel by a new fabrication route [J]. Mater. Sci. Eng., 2010, A527: 5220
14 Kim J H, Byun T S, Hoelzer D T, et al. Temperature dependence of strengthening mechanisms in the nanostructured ferritic alloy 14YWT: Part I—Mechanical and microstructural observations [J]. Mater. Sci. Eng., 2013, A559: 101
15 Ma E. Eight routes to improve the tensile ductility of bulk nanostructured metals and alloys [J]. JOM, 2006, 58(4): 49
16 Wang Y M, Chen M W, Zhou F H, et al. High tensile ductility in a nanostructured metal [J]. Nature, 2002, 419: 912
17 Lu K. Making strong nanomaterials ductile with gradients [J]. Science, 2014, 345: 1455
18 Cheng Z, Zhou H F, Lu Q H, et al. Extra strengthening and work hardening in gradient nanotwinned metals [J]. Science, 2018, 362: eaau1925
19 Zhang Z, Vajpai S K, Orlov D, et al. Improvement of mechanical properties in SUS304L steel through the control of bimodal microstructure characteristics [J]. Mater. Sci. Eng., 2014, A598: 106
20 Zheng P F, Li Y F, Zhang J R, et al. On the thermal stability of a 9Cr-ODS steel aged at 700oC up to 10000 h—Mechanical properties and microstructure [J]. Mater. Sci. Eng., 2020, A783: 139292
21 Yang X, Liao B, Xiao F R, et al. Ripening behavior of M23C6 carbides in P92 steel during aging at 800oC [J]. J. Iron Steel Res. Int., 2017, 24: 858
22 Xu Y T, Zhang X Y, Tian Y B, et al. Study on the nucleation and growth of M23C6 carbides in a 10%Cr martensite ferritic steel after long-term aging [J]. Mater. Charact., 2016, 111: 122
23 Grybėnas A, Makarevičius V, Baltušnikas A, et al. Correlation between structural changes of M23C6 carbide and mechanical behaviour of P91 steel after thermal aging [J]. Mater. Sci. Eng., 2017, A696: 453
24 Hu X, Huang L X, Yan W, et al. Evolution of microstructure and changes of mechanical properties of CLAM steel after long-term aging [J]. Mater. Sci. Eng., 2013, A586: 253
25 Ohtsuka S, Ukai S, Fujiwara M. Nano-mesoscopic structural control in 9CrODS ferritic/martensitic steels [J]. J. Nucl. Mater., 2006, 351: 241
26 Das A, Chekhonin P, Altstadt E, et al. Microstructure and fracture toughness characterization of three 9Cr ODS EUROFER steels with different thermo-mechanical treatments [J]. J. Nucl. Mater., 2020, 542: 152464
27 Ukai S, Narita T, Alamo A, et al. Tube manufacturing trials by different routes in 9CrW-ODS martensitic steels [J]. J. Nucl. Mater., 2004, 329-333: 356
28 Sandim H R Z, Renzetti R A, Padilha A F, et al. Annealing behavior of ferritic-martensitic 9%Cr-ODS-Eurofer steel [J]. Mater. Sci. Eng., 2010, A527: 3602
29 Wang G Q, Li Y F, Zhang J R, et al. Design and preliminary characterization of a novel carbide-free 9Cr-ODS martensitic steel [J]. Fusion Eng. Des., 2020, 160: 111824
30 Shen J J, Yang H L, Li Y F, et al. Microstructural stability of an as-fabricated 12Cr-ODS steel under elevated-temperature annealing [J]. J. Alloys Compd., 2017, 695: 1946
31 He P, Hoffmann J, Möslang A. Effect of milling time and annealing temperature on nanoparticles evolution for 13.5%Cr ODS ferritic steel powders by joint application of XAFS and TEM [J]. J. Nucl. Mater., 2018, 501: 381
32 Lu H, Zhang C, Xu J X, et al. Effects of N addition and annealing treatment on microstructures and mechanical properties of ODS steels [J]. J. Nucl. Mater., 2019, 527: 151796
33 Oskooie M S, Asgharzadeh H. Strength and ductility enhancement in nanostructured AI6063 with a bimodal grain size distribution [J]. IOP Conf. Ser.: Mater. Sci. Eng., 2014, 63: 012022
34 Sun S L, He W W, Zhang M G, et al. Grain growth rule of austenite grain in the heating process of P92 heat-resistant steel [J]. J. Plast. Eng., 2013, 20(3): 92
34 孙述利, 何文武, 张敏刚 等. P92耐热钢加热过程中奥氏体晶粒长大规律 [J]. 塑性工程学报, 2013, 20(3): 92
35 Christ B W, Smith G V. Comparison of the Hall-Petch parameters of zone-refined iron determined by the grain size and extrapolation methods [J]. Acta Metall., 1967, 15: 809
36 Lu K, Liu X D, Hu Z Q. The Hall-Petch relation in nanocrystalline materials [J]. Chin. J. Mater. Res., 1994, 8: 385
36 卢 柯, 刘学东, 胡壮麒. 纳米晶体材料的Hall-Petch关系 [J]. 材料研究学报, 1994, 8: 385
37 Sun J J, Yang C, Guo S W, et al. A novel process to obtain lamella structured low-carbon steel with bimodal grain size distribution for potentially improving mechanical property [J]. Mater. Sci. Eng., 2020, A785: 139339
38 Guo M X, Zhu J, Zhang Y, et al. The formation of bimodal grain size distribution in Al-Mg-Si-Cu alloy and its effect on the formability [J]. Mater. Charact., 2017, 132: 248
Outlines

/