Research paper

Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel

  • Xueda LI ,
  • Chunyu LI ,
  • Ning CAO ,
  • Xueqiang LIN ,
  • Jianbo SUN
Expand
  • School of Materials Science and Engineering, China University of Petroleum (East China), Qingdao 266580, China
LI Xueda, associate professor, Tel: 15621003950, E-mail: lixuedachina@163.com

Received date: 2020-07-31

  Revised date: 2020-09-24

  Online published: 2021-03-03

Supported by

National Natural Science Foundation of China(51801233)

Abstract

Low carbon microalloyed high-strength pipeline steels processed by the thermomechanical controlled process have a good strength-toughness combination. However, after welding, the microstructure and mechanical properties of the heat-affected zone (HAZ) become deteriorated. Previous studies show that martensite-austenite (M-A) constituent formed in the HAZ is a key factor that lowers the toughness, especially necklace-type M-A constituent formed in the intercritically reheated coarse-grained HAZ (ICCGHAZ). However, the phase transformation mechanism of necklace-type M-A constituent in the ICCGHAZ is unclear. In this study, the crystallography of reverted austenite (γr) during the reversion phase transformation upon heating the ICCGHAZ of a high-strength pipeline steel was studied using Gleeble thermal simulation and electron backscatter diffraction (EBSD) technique. Two thermal cycles with peak temperatures of 1300oC and 760oC/800oC/840oC were conducted to simulate the phase transformation process in the ICCGHAZ. The samples were directly quenched to room temperature after been reheated to the second peak temperature, and the reversion behavior, distribution, and crystallography of γr were studied. The results showed that the volume fraction of γr formed at 760, 800, and 840oC was 4.1%, 8.9%, and 25.2%, respectively. γr preferred to nucleate along prior austenite grain boundaries (PAGB), and posterior the block boundaries within the prior austenite grains. γr preferred to grow to blocky type along the PAGB, and the acicular type γr between bainite laths was suppressed. The crystallographic study showed that the formation of γr at PAGB was not free nucleation. However, γr was formed based on the crystallographic orientation of PAGB alongside prior austenite grain complying with Kurdjuov-Sachs (K-S) relationship, while having non K-S relationship with the prior austenite grain on the other side. After nucleation at PAGB, and at a low second peak temperature (760oC), γr transformed to prior austenite grain with non K-S relationship, and the γr formed in blocky and necklace-type along the PAGB. With an increase in the second peak temperature (800-840oC), γr transformed to the prior austenite grains on both sides. The analysis showed that the reversion behavior and crystallography of γr during the second pass reheating have a big impact on the phase transformation upon cooling and the corresponding microstructure and mechanical properties.

Cite this article

Xueda LI , Chunyu LI , Ning CAO , Xueqiang LIN , Jianbo SUN . Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel[J]. Acta Metall Sin, 2021 , 57(8) : 967 -976 . DOI: 10.11900/0412.1961.2020.00287

References

1 Feng Y R, Ji L K, Li W W, et al. Progress and prospects of research and application of X80 pipeline steel and steel pipe in China [J]. Oil Gas Storage Transp., 2020, 39: 612
1 冯耀荣, 吉玲康, 李为卫等. 中国X80管线钢和钢管研发应用进展及展望 [J]. 油气储运, 2020, 39: 612
2 Xia D X, Wang X L, Li X C, et al. Properties and microstructure of third generation X90 pipeline steel [J]. Acta Metall. Sin., 2013, 49: 271
2 夏佃秀, 王学林, 李秀程等. X90级别第三代管线钢的力学性能与组织特征 [J]. 金属学报, 2013, 49: 271
3 Shang C J, Wang X M, Yang S W, et al. Microstructure refinement of high strength low carbon bainitic steel [J]. Acta Metall. Sin., 2003, 39: 1019
3 尚成嘉, 王学敏, 杨善武等. 高强度低碳贝氏体钢的工艺与组织细化 [J]. 金属学报, 2003, 39: 1019
4 Shang C J, Wang X X, Liu Q Y, et al. Weldability of higher niobium X80 pipeline steel [A]. Proceedings of International Seminar on Welding of High Strength Pipeline Steels [C]. Araxa, Brazil: TMS, 2011: 435
5 Chen Y Q, Du Z Y, Xu L H. Microstructure and mechanical properties of heat affected zone for X80 pipeline steel [J]. Trans. China Weld. Inst., 2010, 31(5): 101
5 陈延清, 杜则裕, 许良红. X80管线钢焊接热影响区组织和性能分析 [J]. 焊接学报, 2010, 31(5): 101
6 Li X D. Study on the weldability of the third generation pipeline steels [D]. Beijing: University of Science & Technology Beijing, 2015
6 李学达. 第三代管线钢的焊接性能研究 [D]. 北京: 北京科技大学, 2015
7 Miao C L, Shang C J, Wang X M, et al. Microstructure and toughness of HAZ in X80 pipeline steel with high Nb content [J]. Acta Metall. Sin., 2010, 46: 541
7 缪成亮, 尚成嘉, 王学敏等. 高Nb X80管线钢焊接热影响区显微组织与韧性 [J]. 金属学报, 2010, 46: 541
8 Nie W J, Shang C J, You Y, et al. Microstructure and toughness of the simulated welding heat affected zone in X100 pipeline steel with high deformation resistance [J]. Acta Metall. Sin., 2012, 48: 797
8 聂文金, 尚成嘉, 由 洋等. 抗变形X100管线钢模拟焊接热影响区的组织与韧性研究 [J]. 金属学报, 2012, 48: 797
9 Matsuda F, Fukada Y, Okada H, et al. Review of mechanical and metallurgical investigations of martensite-austenite constituent in welded joints in Japan [J]. Weld. World, 1996, 37: 134
10 Shi Y W, Han Z X. Effect of weld thermal cycle on microstructure and fracture toughness of simulated heat-affected zone for a 800 MPa grade high strength low alloy steel [J]. J. Mater. Process. Technol., 2008, 207: 30
11 Lan L Y, Qiu C L, Zhao D W, et al. Microstructural characteristics and toughness of the simulated coarse grained heat affected zone of high strength low carbon bainitic steel [J]. Mater. Sci. Eng., 2011, A529: 192
12 Davis C L, King J E. Cleavage initiation in the intercritically reheated coarse-grained heat-affected zone: Part I. Fractographic evidence [J]. Metall. Mater. Trans., 1994, 25A: 563
13 Li X D, Shang C J, Han C C, et al. Influence of necklace-type M-A constituent on impact toughness and fracture mechanism in the heat affected zone of X100 pipeline steel [J]. Acta Metall. Sin., 2016, 52: 1025
13 李学达, 尚成嘉, 韩昌柴等. X100管线钢焊接热影响区中链状M-A组元对冲击韧性和断裂机制的影响 [J]. 金属学报, 2016, 52: 1025
14 Li X D, Ma X P, Subramanian S V, et al. Influence of prior austenite grain size on martensite-austenite constituent and toughness in the heat affected zone of 700 MPa high strength linepipe steel [J]. Mater. Sci. Eng., 2014, A616: 141
15 You Y, Shang C J, Chen L, et al. Investigation on the crystallography of the transformation products of reverted austenite in intercritically reheated coarse grained heat affected zone [J]. Mater. Des., 2013, 43: 485
16 Di X J, An X, Cheng F J, et al. Effect of martensite-austenite constituent on toughness of simulated inter-critically reheated coarse-grained heat-affected zone in X70 pipeline steel [J]. Sci. Technol. Weld. Join., 2016, 21: 366
17 Li X D, Fan Y R, Ma X P, et al. Influence of martensite-austenite constituents formed at different intercritical temperatures on toughness [J]. Mater. Des., 2015, 67: 457
18 Zhang X G, Miyamoto G, Toji Y, et al. Orientation of austenite reverted from martensite in Fe-2Mn-1.5Si-0.3C alloy [J]. Acta Mater., 2018, 144: 601
19 Zhang X G, Miyamoto G, Kaneshita T, et al. Growth mode of austenite during reversion from martensite in Fe-2Mn-1.5Si-0.3C alloy: A transition in kinetics and morphology [J]. Acta Mater., 2018, 154: 1
20 Nakada N, Tsuchiyama T, Takaki S, et al. Temperature dependence of austenite nucleation behavior from lath martensite [J]. ISIJ Int., 2011, 51: 299
21 Nakada N, Tsuchiyama T, Takaki S, et al. Variant selection of reversed austenite in lath martensite [J]. ISIJ Int., 2007, 47: 1527
22 Xie Z J, Han G, Zhou W H, et al. A novel multi-step intercritical heat treatment induces multi-phase microstructure with ultra-low yield ratio and high ductility in advanced high-strength steel [J]. Scr. Mater., 2018, 155: 164
23 Luo H W, Shi J, Wang C, et al. Experimental and numerical analysis on formation of stable austenite during the intercritical annealing of 5Mn steel [J]. Acta Mater., 2011, 59: 4002
24 Xie Z J, Shang C J, Subramanian S V, et al. Atom probe tomography and numerical study of austenite stabilization in a low carbon low alloy steel processed by two-step intercritical heat treatment [J]. Scr. Mater., 2017, 137: 36
25 Fairchild D P, Macia M L, Bangaru N V, et al. Girth welding development for X120 linepipe [A]. Proceedings of the 13th International Offshore and Polar Engineering Conference [C]. Hawaii: ISOPE-2003, 2003: 26
26 Zhong Y, Xiao F R, Zhang J W, et al. In situ TEM study of the effect of M/A films at grain boundaries on crack propagation in an ultra-fine acicular ferrite pipeline steel [J]. Acta Mater., 2006, 54: 435
27 Guo Z, Lee C S, Morris Jr J W. On coherent transformations in steel [J]. Acta Mater., 2004, 52: 5511
28 Gourgues A F, Flower H M, Lindley T C. Electron backscattering diffraction study of acicular ferrite, bainite, and martensite steel microstructures [J]. Mater. Sci. Technol., 2000, 16: 26
29 Li X D, Ma X P, Subramanian S V, et al. EBSD characterization of secondary microcracks in the heat affected zone of a X100 pipeline steel weld joint [J]. Int. J. Fract., 2015, 193: 131
30 You Y, Wang X M, Shang C J. Influence of austenitizing temperature on the microstructure and impact toughness of a high strength low alloy HSLA100 steel [J]. Acta Metall. Sin., 2012, 48: 1290
30 由 洋, 王学敏, 尚成嘉. 奥氏体化温度对HSLA100高强度低合金钢组织及冲击韧性的影响 [J]. 金属学报, 2012, 48: 1290
31 Zhang X G, Miyamoto G, Furuhara T. Effects of heating rate on microstructure of reverted austenite [J]. Iron Steel, 2019, 54(2): 83
31 张献光, 宫本吾郎, 古原忠. 加热速率对逆转变奥氏体微观组织的影响 [J]. 钢铁, 2019, 54(2): 83
32 Li X D, Shang C J, Ma X P, et al. Elemental distribution in the martensite-austenite constituent in intercritically reheated coarse-grained heat-affected zone of a high-strength pipeline steel [J]. Scr. Mater., 2017, 139: 67
Outlines

/