Research paper

Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate

  • Hongyu ZHOU ,
  • Minrui RAN ,
  • Yaqiang LI ,
  • Weidong ZHANG ,
  • Junyou LIU ,
  • Wenyue ZHENG
Expand
  • 1.National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China
    2.Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China
    3.School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
ZHENG Wenyue, professor, Tel: (010)62334996, E-mail: zheng_wenyue@ustb.edu.cn

Received date: 2020-09-30

  Revised date: 2021-02-05

  Online published: 2021-03-01

Supported by

Fundamental Research Funds for the Central Universities(FRF-TP-19-012A1);Beijing Municipal Science and Technology Project(Z121100001312012)

Abstract

Rapid development of high-power electronic equipment for 5G and other advanced communication devices leads to a highly compact component size with increased heat flux density in integrated circuits, which requires electronic packaging materials to meet excellent heat dissipation performance. In this work, a novel liquid-solid separation technology was used to prepare a 40% (volume fraction) diamond/Al composite for electronic packaging substrates. By SEM, EPMA, and XRD techniques to investigate the fracture morphology and interface structure of the composite, the influence of diamond particle sizes (90, 106, 124, and 210 μm) on the thermophysical properties of diamond/Al composite was studied. The results showed that with the increase of a diamond particle size, the density of a composite material increased first and then sharply decreased and attained the optimal value when the diamond particle size was 106 μm. No harmful intermetallic Al4C3 was generated at the interface of the composite material. Coefficient of thermal expansion (αc) of the composite material increases slightly with increase in diamond particle sizes and remains relatively stable. The Kerner model can accurately simulate the αc of the diamond/Al composite. Thermal conductivity (λ) is also affected by diamond particle sizes and interface behaviors, and the trend of change in λ with the size of the diamond particles follows a similar trend to that between the density of composites and the particle size. The diamond/Al composite with diamond particle size of 106 μm has the best overall performance, relative density and αc attained 97.12% and 12.4 × 10-6 K-1, respectively. λ is 153.1 W/(m·K), meeting 69.31% of the Maxwell-Eucken model prediction value. The airtightness value meets the military standard for this type of an electronic packaging material.

Cite this article

Hongyu ZHOU , Minrui RAN , Yaqiang LI , Weidong ZHANG , Junyou LIU , Wenyue ZHENG . Effect of Diamond Particle Size on the Thermal Properties of Diamond/Al Composites for Packaging Substrate[J]. Acta Metall Sin, 2021 , 57(7) : 937 -947 . DOI: 10.11900/0412.1961.2020.00393

References

1 Suh D, Moon C M, Kim D, et al. Ultrahigh thermal conductivity of interface materials by silver-functionalized carbon nanotube phonon conduits [J]. Adv. Mater., 2016, 28: 7220
2 Li T, Li J Q, Wang W G, et al. A discussion on the main factors affecting thermal conductivity of carbon/metal matrix composites [J]. Mater. Rev., 2018, 32: 2640
2 李 通, 李金权, 王文广等. 影响碳/金属复合材料导热性能的主要因素探讨 [J]. 材料导报, 2018, 32: 2640
3 Zhang D, Yuan M Y, Tan Z Q, et al. Progress in interface modification and nanoscale study of diamond/Cu composites [J]. Acta Metall. Sin., 2018, 54: 1158
3 张 荻, 苑孟颖, 谭占秋等. 金刚石/Cu复合界面导热改性及其纳米化研究进展 [J]. 金属学报, 2018, 54: 1158
4 Janicki M, Napieralski A. Modelling electronic circuit radiation cooling using analytical thermal model [J]. Microelectron. J., 2000, 31: 781
5 Ma R L, Peng C Q, Wang R C, et al. Research progress of diamond/aluminum composites for electronic packaging [J]. Chin. J. Nonferrous Met., 2014, 24: 689
5 马如龙, 彭超群, 王日初等. 电子封装用diamond/Al复合材料研究进展 [J]. 中国有色金属学报, 2014, 24: 689
6 Liu X Y, Wang W G, Wang D, et al. Effect of nanometer TiC coated diamond on the strength and thermal conductivity of diamond/Al composites [J]. Mater. Chem. Phys., 2016, 182: 256
7 Zhang L, Wei Q P, An J J, et al. Construction of 3D interconnected diamond networks in Al-matrix composite for high-efficiency thermal management [J]. Chem. Eng. J., 2020, 380: 122551
8 Chu K, Jia C C, Liang X B, et al. Effect of particle size on the microstructure and thermal conductivity of Al/diamond composites prepared by spark plasma sintering [J]. Rare Met., 2009, 28: 646
9 Tan Z Q, Chen Z Z, Fan G L, et al. Effect of particle size on the thermal and mechanical properties of aluminum composites reinforced with SiC and diamond [J]. Mater. Des., 2016, 90: 845
10 Kwon H, Leparoux M, Heintz J M, et al. Fabrication of single crystalline diamond reinforced aluminum matrix composite by powder metallurgy route [J]. Met. Mater. Int., 2011, 17: 755
11 Zhang W X, Xu S S, Wang Y Z, et al. Diamond/Ti3AlC2 composite prepared by spark plasma sintering [J]. Superhard Mater. Eng., 2017, 29(1): 11
11 张旺玺, 徐世帅, 王艳芝等. 放电等离子烧结制备金刚石/钛铝碳复合材料 [J]. 超硬材料工程, 2017, 29(1): 11
12 Mizuuchi K, Inoue K, Agari Y, et al. Bimodal and monomodal diamond particle effect on the thermal properties of diamond-particle-dispersed Al-matrix composite fabricated by SPS [J]. Microelectron. Reliab., 2014, 54: 2463
13 Sun Y H, Zhang C, He L K, et al. Enhanced bending strength and thermal conductivity in diamond/Al composites with B4C coating [J]. Sci. Rep., 2018, 8: 11104
14 Ji G, Tan Z Q, Lu Y G, et al. Heterogeneous interfacial chemical nature and bonds in a W-coated diamond/Al composite [J]. Mater. Charact., 2016, 112: 129
15 Che Z F, Li J W, Wang Q X, et al. The formation of atomic-level interfacial layer and its effect on thermal conductivity of W-coated diamond particles reinforced Al matrix composites [J]. Composites, 2018, 107A: 164
16 Yang W L, Sang J Q, Zhou L P, et al. Overcoming selective interfacial bonding and enhancing thermal conductivity of diamond/aluminum composite by an ion bombardment pretreatment [J]. Diam. Relat. Mater., 2018, 81: 127
17 Ma S D, Zhao N Q, Shi C S, et al. Mo2C coating on diamond: Different effects on thermal conductivity of diamond/Al and diamond/Cu composites [J]. Appl. Surf. Sci., 2017, 402: 372
18 Wang P P, Xiu Z Y, Jiang L T, et al. Enhanced thermal conductivity and flexural properties in squeeze casted diamond/aluminum composites by processing control [J]. Mater. Des., 2015, 88: 1347
19 Liang X B, Jia C C, Chu K, et al. Thermal conductivity and microstructure of Al/diamond composites with Ti-coated diamond particles consolidated by spark plasma sintering [J]. J. Compos. Mater., 2012, 46: 1127
20 Tan Z Q, Li Z Q, Fan G L, et al. Fabrication of diamond aluminium composites by vacuum hot: Pressing process optimization and thermal properties [J]. Composites, 2013, 47B: 173
21 Xin L, Tian X, Yang W S, et al. Enhanced stability of the diamond/Al composites by W coatings prepared by the magnetron sputtering method [J]. J. Alloys Compd., 2018, 763: 305
22 Li N, Wang L H, Dai J J, et al. Interfacial products and thermal conductivity of diamond/Al composites reinforced with ZrC-coated diamond particles [J]. Diam. Relat. Mater., 2019, 100: 107565
23 Zhou H Y, Liu X, Yin Z, et al. The fabrication of functional gradient hypereutectic Al-Si composites by liquid-solid separation technology [J]. J. Alloys Compd., 2018, 763: 49
24 Zhou H Y, Yin Y L, Shi Z L, et al. The fabrication of Al-diamond composites for heat dissipation by liquid-solid separation technology [J]. J. Mater. Sci.: Mater. Electron., 2017, 28: 721
25 Zhou H Y, Yin Y L, Wu C J, et al. Microstructures and properties of diamond/Al composites prepared by liquid-solid separation technology [J]. Chin. J. Nonferrous. Met., 2017, 27: 1855
25 周洪宇, 尹衍利, 吴春京等. 液固分离法制备金刚石/铝封装材料的组织与性能 [J]. 中国有色金属学报, 2017, 27: 1855
26 Yamamoto Y, Imai T, Tanabe K, et al. The measurement of thermal properties of diamond [J]. Diam. Relat. Mater., 1997, 6: 1057
27 Yang W L, Peng K, Zhou L P, et al. Finite element simulation and experimental investigation on thermal conductivity of diamond/aluminium composites with imperfect interface [J]. Comput. Mater. Sci., 2014, 83: 375
28 Ren S B, He X B, Qu X H, et al. Effect of Mg and Si in the aluminum on the thermo-mechanical properties of pressureless infiltrated SiCp/Al composites [J]. Compos. Sci. Technol., 2007, 67: 2103
29 Yin S, Cizek J, Chen C Y, et al. Metallurgical bonding between metal matrix and core-shelled reinforcements in cold sprayed composite coating [J]. Scr. Mater., 2020, 177: 49
30 Tan Z Q, Li Z Q, Xiong D B, et al. A predictive model for interfacial thermal conductance in surface metallized diamond aluminum matrix composites [J]. Mater. Des., 2014, 55: 257
31 Yan Y W, Geng L. Effects of particle size on the thermal expansion behavior of SiCp/Al composites [J]. J. Mater. Sci., 2007, 42: 6433
32 Geiger A L, Jackson M. Low-expansion MMC's boost avionics [J]. Adv. Mater. Process., 1989, 136: 23
33 Turner P S. Thermal-expansion stress in reinforced plastics [J]. J. Res. Nat. Bur. Stand., 1946, 37: 250
34 Kerner E H. The elastic and thermo-elastic properties of composite media [J]. Proc. Phys. Soc., 1956, 69B: 808
35 Edtmaier C, Segl J, Koos R, et al. Characterization of interfacial bonding strength at Al(Si)/diamond interfaces by neutron diffraction: Effect of diamond surface termination and processing conditions [J]. Diam. Relat. Mater., 2020, 106: 107842
36 Vetterli M, Tavangar R, Weber L, et al. Influence of the elastic properties of the phases on the coefficient of thermal expansion of a metal matrix composite [J]. Scr. Mater., 2011, 64: 153
37 Fan T X, Liu Y, Yang K M, et al. Recent progress on interfacial structure optimization and their influencing mechanism of carbon reinforced metal matrix composites [J]. Acta Metall. Sin., 2019, 55: 16
37 范同祥, 刘 悦, 杨昆明等. 碳/金属复合材料界面结构优化及界面作用机制的研究进展 [J]. 金属学报, 2019, 55: 16
38 Yang W S, Chen G Q, Wang P P, et al. Enhanced thermal conductivity in diamond/Aluminum composites with tungsten coatings on diamond particles prepared by magnetron sputtering method [J]. J. Alloys Compd., 2017, 726: 623
39 Monje I E, Louis E, Molina J M. On critical aspects of infiltrated Al/diamond composites for thermal management: Diamond quality versus processing conditions [J]. Composites, 2014, 67A: 70
40 Caccia M, Rodríguez A, Narciso J. Diamond surface modification to enhance interfacial thermal conductivity in Al/diamond composites [J]. JOM, 2014, 66: 920
41 Maxwell J C. A Treatise on Electricity and Magnetism [M]. Oxford: Oxford University Press, 1937: 1
42 Tavangar R, Molina J M, Weber L. Assessing predictive schemes for thermal conductivity against diamond-reinforced silver matrix composites at intermediate phase contrast [J]. Scr. Mater., 2007, 56: 357
Outlines

/