Overview

Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property

  • Qingping CAO ,
  • Linbo LV ,
  • Xiaodong WANG ,
  • Jianzhong JIANG
Expand
  • International Center for New-Structured Materials (ICNSM), School of Materials Science and Engineering, Zhejiang University, Hangzhou 310027, China
CAO Qingping, professor, Tel: (0571)87951528, E-mail: caoqp@zju.edu.cn

Received date: 2020-10-29

  Revised date: 2021-01-25

  Online published: 2021-02-05

Supported by

National Key Research and Development Program of China(2016YFB0700201);National Natural Science Foundation of China(51871198)

Abstract

Metallic glass thin film (MGTF) is a new thin film material developed based on metallic glasses. It has excellent physical, chemical, and mechanical properties owing to its disordered atomic packing structure. Moreover, nanostructured MGTF can be synthesized by adjusting the process of physical vapor deposition to construct nanostructure interfaces and overcome the intrinsic brittleness of bulky metallic glasses. Recently, the rapid development of MGTF in various fields has attracted extensive attention and has become a new research hotspot. In this paper, by reviewing the influence of preparation parameters on the microstructure and properties of MGTF, and sample size effect. In this manner, research progress is analyzed and summarized, and research prospects are briefly proposed to provide reference for researchers engaged in the study of MGTF.

Cite this article

Qingping CAO , Linbo LV , Xiaodong WANG , Jianzhong JIANG . Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property[J]. Acta Metall Sin, 2021 , 57(4) : 473 -490 . DOI: 10.11900/0412.1961.2020.00430

References

1 Klement W, Willens R H, Duwez P. Non-crystalline structure in solidified gold-silicon alloys [J]. Nature, 1960, 187: 869
2 Bu Y, Bu X M, Lyu F C, et al. Full-color reflective filters in a large area with a wide-band tunable absorber deposited by one-step magnetron sputtering [J]. Adv. Opt. Mater., 2020, 8: 1901626
3 Oliver J N, Su Y C, Lu X N, et al. Bioactive glass coatings on metallic implants for biomedical applications [J]. Bioact. Mater., 2019, 4: 261
4 Latthe S S, Sutar R S, Bhosale A K, et al. Recent developments in air-trapped superhydrophobic and liquid-infused slippery surfaces for anti-icing application [J]. Prog. Org. Coat., 2019, 137: 105373
5 Schwarz R B, Johnson W L. Formation of an amorphous alloy by solid-state reaction of the pure polycrystalline metals [J]. Phys. Rev. Lett., 1983, 51: 415
6 Lee M L, Win K K, Gan C L, et al. Ultra-high-density phase-change storage using AlNiGd metallic glass thin film as recording layer [J]. Intermetallics, 2010, 18: 119
7 Chu J H, Lee J, Chang C C, et al. Antimicrobial characteristics in Cu-containing Zr-based thin film metallic glass [J]. Surf. Coat. Technol., 2014, 259: 87
8 Hayashi Y, Yamazaki H, Ono D, et al. Investigation of PdCuSi metallic glass film for hysteresis-free and fast response capacitive MEMS hydrogen sensors [J]. Int. J. Hydrog. Energy, 2018, 43: 9438
9 Pharr G M, Herbert E G, Gao Y F. The indentation size effect: A critical examination of experimental observations and mechanistic interpretations [J]. Ann. Rev. Mater. Res., 2010, 40: 271
10 Greer J R, Oliver W C, Nix W D. Size dependence of mechanical properties of gold at the micron scale in the absence of strain gradients [J]. Acta Mater., 2005, 53: 1821
11 Greer J R, De Hosson J T M. Plasticity in small-sized metallic systems: Intrinsic versus extrinsic size effect [J]. Prog. Mater. Sci., 2011, 56: 654
12 Guo H, Yan P F, Wang Y B, et al. Tensile ductility and necking of metallic glass [J]. Nat. Mater., 2007, 6: 735
13 Schuster B E, Wei Q, Hufnagel T C, et al. Size-independent strength and deformation mode in compression of a Pd-based metallic glass [J]. Acta Mater., 2008, 56: 5091
14 Dubach A, Raghavan R, L?ffler J F, et al. Micropillar compression studies on a bulk metallic glass in different structural states [J]. Scr. Mater., 2009, 60: 567
15 Volkert C A, Donohue A, Spaepen F. Effect of sample size on deformation in amorphous metals [J]. J. Appl. Phys., 2008, 103: 083539
16 Kumar G, Desai A, Schroers J. Bulk metallic glass: The smaller the better [J]. Adv. Mater., 2011, 23: 461
17 Ediger M D, Angell C A, Nagel S R. Supercooled liquids and glasses [J]. J. Phys. Chem., 1996, 100: 13200
18 Swallen S F, Kearns K L, Mapes M K, et al. Organic glasses with exceptional thermodynamic and kinetic stability [J]. Science, 2007, 315: 353
19 Yu H B, Luo Y S, Samwer K. Ultrastable metallic glass [J]. Adv. Mater., 2013, 25: 5904
20 Dawson K, Zhu L, Kopff L A, et al. Highly stable vapor-deposited glasses of four tris-naphthylbenzene isomers [J]. J. Phys. Chem. Lett., 2011, 2: 2683
21 Ediger M D, Harrowell P. Perspective: Supercooled liquids and glasses [J]. J. Chem. Phys., 2012, 137: 080901
22 Guo Y L, Morozov A, Schneider D, et al. Ultrastable nanostructured polymer glasses [J]. Nat. Mater., 2012, 11: 337
23 Liu S Y, Cao Q P, Yu Q, et al. Substrate temperature effect on growth behavior and microstructure-properties relationship in amorphous Ni-Nb thin films [J]. J. Non-Cryst. Solids, 2019, 510: 112
24 Mullins W W. The effect of thermal grooving on grain boundary motion [J]. Acta Metall., 1958, 6: 414
25 Liu S Y, Cao Q P, Qian X, et al. Effects of substrate temperature on structure, thermal stability and mechanical property of a Zr-based metallic glass thin film [J]. Thin Solid Films, 2015, 595: 17
26 Zeng F, Gao Y, Li L, et al. Elastic modulus and hardness of Cu-Ta amorphous films [J]. J. Alloys Compd., 2005, 389: 75
27 Kearns K L, Swallen S F, Ediger M D, et al. Influence of substrate temperature on the stability of glasses prepared by vapor deposition [J]. J. Chem. Phys., 2007, 127: 154702
28 Singh S, Ediger M D, de Pablo J J. Ultrastable glasses from in silico vapour deposition [J]. Nat. Mater., 2013, 12: 139
29 Yu H B, Tylinski M, Guiseppi-Elie A, et al. Suppression of β relaxation in vapor-deposited ultrastable glasses [J]. Phys. Rev. Lett., 2015, 115: 185501
30 Luo P, Cao C R, Zhu F, et al. Ultrastable metallic glasses formed on cold substrates [J]. Nat. Commun., 2018, 9: 1389
31 Chou H S, Huang J C, Chang L W. Mechanical properties of ZrCuTi thin film metallic glass with high content of immiscible tantalum [J]. Surf. Coat. Technol., 2010, 205: 587
32 Chen P S, Chen H W, Duh J G, et al. Characterization of mechanical properties and adhesion of Ta-Zr-Cu-Al-Ag thin film metallic glasses [J]. Surf. Coat. Technol., 2013, 231: 332
33 Obeydavi A, Shafyei A, Rezaeian A, et al. Microstructure, mechanical properties and corrosion performance of Fe44Cr15Mo14Co7C10B5-Si5 thin film metallic glass deposited by DC magnetron sputtering [J]. J. Non-Cryst. Solids, 2020, 527: 119718
34 Yanagitani T, Suzuki M. Significant shear mode softening in a c-axis tilt nanostructured hexagonal thin film induced by a self-shadowing effect [J]. Scr. Mater., 2013, 69: 724
35 Denis P, Liu S Y, Fecht H J. Growth mode transition in Au-based thin film metallic glasses [J]. Thin Solid Films, 2018, 665: 29
36 Thornton J A. Influence of apparatus geometry and deposition conditions on the structure and topography of thick sputtered coatings [J]. J. Vac. Sci. Technol., 1974, 11: 666
37 ?niadecki Z, Wang D, Ivanisenko Y, et al. Nanoscale morphology of Ni50Ti45Cu5 nanoglass [J]. Mater. Charact., 2016, 113: 26
38 Yao W, Cao Q P, Liu S Y, et al. Tailoring nanostructured Ni-Nb metallic glassy thin films by substrate temperature [J]. Acta Mater., 2020, 194: 13
39 Mayr S G, Samwer K. Tailoring the surface morphology of amorphous thin films by appropriately chosen deposition conditions [J]. J. Appl. Phys., 2002, 91: 2779
40 Bei H, George E P, Hay J L, et al. Influence of indenter tip geometry on elastic deformation during nanoindentation [J]. Phys. Rev. Lett., 2005, 95: 045501
41 Qian X, Cao Q P, Liu S Y, et al. Dependence of shear yield strain and shear transformation zone on the glass transition temperature in thin film metallic glasses [J]. J. Alloys Compd., 2015, 652: 191
42 Cao Q P, Sun L J, Wang C, et al. Effect of loading rate on creep behavior and shear transformation zone in amorphous alloy thin films, and its correlation with deformation mode transition [J]. Thin Solid Films, 2019, 681: 23
43 Wang C, Cao Q P, Feng T, et al. Indentation size effects of mechanical behavior and shear transformation zone in thin film metallic glasses [J]. Thin Solid Films, 2018, 646: 36
44 Ma C F, Li S, Huang P, et al. Size dependent hidden serration behaviors of shear banding in metallic glass thin films [J]. J. Non-Cryst. Solids, 2020, 534: 119953
45 Johnson W L, Samwer K. A universal criterion for plastic yielding of metallic glasses with a (T/Tg)2/3 temperature dependence [J]. Phys. Rev. Lett., 2005, 95: 195501
46 Jang D C, Greer J R. Transition from a strong-yet-brittle to a stronger-and-ductile state by size reduction of metallic glasses [J]. Nat. Mater., 2010, 9: 215
47 Jiang Q K, Liu P, Cao Q P, et al. The effect of size on the elastic strain limit in Ni60Nb40 glassy films [J]. Acta Mater., 2013, 61: 4689
48 Deng Q S, Cheng Y Q, Yue Y H, et al. Uniform tensile elongation in framed submicron metallic glass specimen in the limit of suppressed shear banding [J]. Acta Mater., 2011, 59: 6511
49 Jiang Q K, Liu P, Ma Y, et al. Super elastic strain limit in metallic glass films [J]. Sci. Rep., 2012, 2: 852
50 Ma Y, Cao Q P, Qu S X, et al. Stress-state-dependent deformation behavior in Ni-Nb metallic glassy film [J]. Acta Mater., 2012, 60: 4136
51 Wright T W, Ockendon H. A scaling law for the effect of inertia on the formation of adiabatic shear bands [J]. Int. J. Plast., 1996, 12: 927
52 Ashby M F, Greer A L. Metallic glasses as structural materials [J]. Scr. Mater., 2006, 54: 321
53 Zhang G P, Liu Y, Zhang B. Deformation behavior of free-standing Pd-based thin film metallic glass for micro electro mechanical systems applications [J]. Adv. Eng. Mater., 2005, 7: 606
54 Liu Y D, Hata S, Wada K, et al. Thermal, mechanical and electrical properties of Pd-based thin-film metallic glass [J]. Jpn. J. Appl. Phys., 2001, 40: 5382
55 Uchic M D, Dimiduk D M, Florando J N, et al. Exploring Specimen Size Effects in Plastic Deformation of Ni3(Al, Ta) [M]. MRS Online Proceeding Library, 2002, 753: 14.
56 Greer J R, Nix W D. Size dependence of mechanical properties of gold at the sub-micron scale [J]. Appl. Phys., 2005, 80A: 1625
57 Frick C P, Clark B G, Orso S, et al. Size effect on strength and strain hardening of small-scale [1 1 1] nickel compression pillars [J]. Mater. Sci. Eng., 2008, A489: 319
58 Liu Y H, Zhao F, Li Y L, et al. Deformation behavior of metallic glass thin films [J]. J. Appl. Phys., 2012, 112: 063504
59 Ghidelli M, Volland A, Blandin J J, et al. Exploring the mechanical size effects in Zr65Ni35 thin film metallic glasses [J]. J. Alloys Compd., 2014, 615(suppl.1): S90
60 Apreutesei M, Esnouf C, Billard A, et al. Impact of local nanocrystallization on mechanical properties in the Zr-59 at.% Cu metallic glass thin film [J]. Mater. Des., 2016, 108: 8
61 Dalla Torre F H, Dubach A, Sch?llibaum J, et al. Shear striations and deformation kinetics in highly deformed Zr-based bulk metallic glasses [J]. Acta Mater., 2008, 56: 4635
62 Hata S, Yamauchi R, Sakurai J, et al. Behavior of joining interface between thin film metallic glass and silicon nitride at heating [J]. Mater. Sci. Eng., 2008, B148: 149
63 Chen D Z, Jang D, Guan K M, et al. Nanometallic glasses: Size reduction brings ductility, surface state drives its extent [J]. Nano Lett., 2013, 13: 4462
64 Tian L, Wang X L, Shan Z W. Mechanical behavior of micronanoscaled metallic glasses [J]. Mater. Res. Lett., 2016, 4: 63
65 Ye J C, Chu J P, Chen Y C, et al. Hardness, yield strength, and plastic flow in thin film metallic-glass [J]. J. Appl. Phys., 2012, 112: 053516
66 Magagnosc D J, Ehrbar R, Kumar G, et al. Tunable tensile ductility in metallic glasses [J]. Sci. Rep., 2013, 3: 1096
67 Yi J, Wang W H, Lewandowski J J. Sample size and preparation effects on the tensile ductility of Pd-based metallic glass nanowires [J]. Acta Mater., 2015, 87: 1
68 Luo J H, Wu F F, Huang J Y, et al. Superelongation and atomic chain formation in nanosized metallic glass [J]. Phys. Rev. Lett., 2010, 104: 215503
69 Ebner C, Rajagopalan J, Lekka C, et al. Electron beam induced rejuvenation in a metallic glass film during in-situ TEM tensile straining [J]. Acta Mater., 2019, 181: 148
70 Glushko O, Mühlbacher M, Gammer C, et al. Exceptional fracture resistance of ultrathin metallic glass films due to an intrinsic size effect [J]. Sci. Rep., 2019, 9: 8281
71 Leterrier Y, Médico L, Demarco F, et al. Mechanical integrity of transparent conductive oxide films for flexible polymer-based displays [J]. Thin Solid Films, 2004, 460: 156
72 Greer A L, Cheng Y Q, Ma E. Shear bands in metallic glasses [J]. Mater. Sci. Eng., 2013, R74(4): 71
73 Li Q K, Li M. Assessing the critical sizes for shear band formation in metallic glasses from molecular dynamics simulation [J]. Appl. Phys. Lett., 2007, 91: 231905
74 Cao Q P, Wang C, Bu K J, et al. The influence of glass transition temperature on the critical size for deformation mode transition in metallic glassy films [J]. Scr. Mater., 2014, 77: 64
75 Zhong C, Zhang H, Cao Q P, et al. The size-dependent non-localized deformation in a metallic alloy [J]. Scr. Mater., 2015, 101: 48
76 Chen C Q, Pei Y T, De Hosson J T M. Effects of size on the mechanical response of metallic glasses investigated through in situ TEM bending and compression experiments [J]. Acta Mater., 2010, 58: 189
77 Schuh C A, Lund A C, Nieh T G. New regime of homogeneous flow in the deformation map of metallic glasses: Elevated temperature nanoindentation experiments and mechanistic modeling [J]. Acta Mater., 2004, 52: 5879
78 McCarthy C T, Hussey M, Gilchrist M D. On the sharpness of straight edge blades in cutting soft solids: Part I—indentation experiments [J]. Eng. Fract. Mech., 2007, 74: 2205
79 Khan M M, Deen K M, Haider W. Combinatorial development and assessment of a Zr-based metallic glass for prospective biomedical applications [J]. J. Non-Cryst. Solids, 2019, 523: 119544
80 Tsai P H, Lin Y Z, Li J B, et al. Sharpness improvement of surgical blade by means of ZrCuAlAgSi metallic glass and metallic glass thin film coating [J]. Intermetallics, 2012, 31: 127
81 Cai C N, Zhang C, Sun Y S, et al. ZrCuFeAlAg thin film metallic glass for potential dental applications [J]. Intermetallics, 2017, 86: 80
82 Chu J P, Diyatmika W, Tseng Y J, et al. Coating cutting blades with thin-film metallic glass to enhance sharpness [J]. Sci. Rep., 2019, 9: 15558
83 Chen X W, Hong L, Xu Y F, et al. Ceramic pore channels with inducted carbon nanotubes for removing oil from water [J]. ACS Appl. Mater. Interfaces, 2012, 4: 1909
84 Ke J L, Huang C H, Chen Y H, et al. In vitro biocompatibility response of Ti-Zr-Si thin film metallic glasses [J]. Appl. Surf. Sci., 2014, 322: 41
85 Bouala G I N, Etiemble A, Der Loughian C, et al. Silver influence on the antibacterial activity of multi-functional Zr-Cu based thin film metallic glasses [J]. Surf. Coat. Technol., 2018, 343: 108
86 Chu J P, Yu C C, Tanatsugu Y, et al. Non-stick syringe needles: Beneficial effects of thin film metallic glass coating [J]. Sci. Rep., 2016, 6: 31847
87 Kassa S T, Hu C C, Liao Y C, et al. Thin film metallic glass as an effective coating for enhancing oil/water separation of electrospun polyacrylonitrile membrane [J]. Surf. Coat. Technol., 2019, 368: 33
Outlines

/