Research paper

Mechanical and Electrical Properties of Cu-W Composites with Micro-Oriented Structures

  • Ying HAN ,
  • Hongshuang WANG ,
  • Yundong CAO ,
  • Yuejun AN ,
  • Guoqi TAN ,
  • Shujun LI ,
  • Zengqian LIU ,
  • Zhefeng ZHANG
Expand
  • 1.School of Electrical Engineering, Shenyang University of Technology, Shenyang 110870, China
    2.Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
HAN Ying, associate professor, Tel: 13478250188, E-mail: hany_dq@sut.edu.cn.

Received date: 2020-09-24

  Revised date: 2020-12-27

  Online published: 2021-02-05

Supported by

National Natural Science Foundation of China(51977132);Natural Science Foundation of Liaoning Province(2019-MS-249);Liaoning Province Science and Technology Major Special Project(2019JH1/10100016)

Abstract

Cu-W composites that combine the merits of Cu and W show good electric and heat conductivity, resistance to arc erosion, and high strength, etc., and are good candidates for electric contact materials. Until now, several methods, including the high-temperature liquid phase sintering method and the hot-pressure sintering method, have been developed to fabricate Cu-W composites. However, these methods may cause an uneven distribution of constituents in the material and a relatively low density and poor electric conductivity of the material. In this study, a Cu-W composite with micro-oriented W lamellas was prepared by the infiltration method, and the mechanical and electrical properties were investigated and compared with a commercial Cu-W composite. The results showed that the compressive strength of the studied Cu-W composite with micro-oriented W lamellas was between 300 and 1100 MPa when the W content was between 50% and 90% (mass fraction). The compressive strength of the studied composites presented obvious anisotropy, and the strength along the direction parallel to the W lamellas was higher than that perpendicular to the W lamellas. Compared with commercial Cu-W composites with disordered W frameworks, composites with micro-oriented W lamellas exhibit a higher electrical conductivity and compressive strength along the W lamellar direction, which is mainly related to the regular arrangement of the two phases of Cu and W in the composites. The studied composite is expected to be used as an electrical contact material to significantly improve the effect of electric contracts and prolong their service life while reducing the mass of the components and energy consumption.

Cite this article

Ying HAN , Hongshuang WANG , Yundong CAO , Yuejun AN , Guoqi TAN , Shujun LI , Zengqian LIU , Zhefeng ZHANG . Mechanical and Electrical Properties of Cu-W Composites with Micro-Oriented Structures[J]. Acta Metall Sin, 2021 , 57(8) : 1009 -1016 . DOI: 10.11900/0412.1961.2020.00387

References

1 Qian B G, Geng H R, Guo Z Q, et al. Development and application of electrical contact materials [J]. Mater. Mech. Eng., 2004, 28(3): 7
1 钱宝光, 耿浩然, 郭忠全等. 电触头材料的研究进展与应用 [J]. 机械工程材料, 2004, 28(3): 7
2 Zheng Z, Zhou X L, Zhou Y H, et al. Effect of Ni on the microstructure and properties of O-containing Cu-W alloy [J]. Mater. Rev., 2015, 29: 505
2 郑 忠, 周晓龙, 周允红等. Ni元素对含O的Cu-W合金组织与性能的影响 [J]. 材料导报, 2015, 29: 505
3 German R M, Rabin B H. Enhanced sintering through second phase additions [J]. Powder Metall., 1985, 28: 7
4 Gu D D, Shen Y F. Microstructures of laser sintered micron/nano-sized Cu-W powder [J]. Acta Metall. Sin., 2009, 45: 113
4 顾冬冬, 沈以赴. 微/纳米Cu-W粉末激光烧结体的显微组织 [J]. 金属学报, 2009, 45: 113
5 Ma G N, Wang D, Liu Z Y, et al. Effect of hot pressing temperature on microstructure and tensile properties of SiC/Al-Zn-Mg-Cu composites [J]. Acta Metall. Sin., 2019, 55: 1319
5 马国楠, 王 东, 刘振宇等. 热压烧结温度对SiC/Al-Zn-Mg-Cu复合材料微观结构与力学性能的影响 [J]. 金属学报, 2019, 55: 1319
6 Zhu Z F, Wang X F, Liu H, et al. Synthesis of quasi-monodispersed SnO2 microspheres via microwave solvothermal method [J]. J. Inorg. Mater., 2012, 27: 311
6 朱振峰, 王小枫, 刘 辉等. 准单分散SnO2微球的微波溶剂热合成 [J]. 无机材料学报, 2012, 27: 311
7 Lin Z J, Sun X D, Liu S H, et al. Effect of SnO2 particle size on properties of Ag-SnO2 electrical contact materials prepared by the reductive precipitation method [J]. Adv. Mater. Res., 2014, 936: 459
8 Qiao X Q, Shen Q H, Zhang L J, et al. A novel method for the preparation of Ag/SnO2 electrical contact materials [J]. Rare Met. Mater. Eng., 2014, 43: 2614
9 Zhang Z, Zhu P X, Zhou S G. Research and development of laminated metal composite and electrode material [J]. Hot Work. Technol., 2014, 43(18): 21
9 张 喆, 竺培显, 周生刚. 金属层状复合材料及电极材料的研究进展 [J]. 热加工工艺, 2014, 43(18): 21
10 Ma X H. Research on tungsten copper contact material for high voltage switch [J]. Heilongjiang Sci. Technol. Inform., 2013, (14): 48
10 马晓红. 高压开关用钨铜触头材料研究 [J]. 黑龙江科技信息, 2013, (14): 48
11 German R G, Hens K F, Johnson J L. Powder metallurgy processing of thermal management materials for microelectronic applications [J]. Int. J. Powder Metall., 1994, 30: 205
12 Kan X Q, Ding J, Yu C, et al. Biomimetic synthesis of porous ZrC/C composite ceramic materials [J]. Mater. Rev., 2018, 32: 1602
12 阚小清, 丁 军, 余 超等. 仿生制备多孔ZrC/C复合陶瓷材料 [J]. 材料导报, 2018, 32: 1602
13 Zhuo L C, Zhao Z, Qin Z C, et al. Enhanced mechanical and arc erosion resistant properties by homogenously precipitated nanocrystalline fcc-Nb in the hierarchical W-Nb-Cu composite [J]. Composites, 2019, 161B: 336
14 Tan G Q, Zhang J, Zheng L, et al. Nature-inspired nacre-like composites combining human tooth-matching elasticity and hardness with exceptional damage tolerance [J]. Adv. Mater., 2019, 31: 1904603
15 Koyama M, Zhang Z, Wang M M, et al. Bone-like crack resistance in hierarchical metastable nanolaminate steels [J]. Science, 2017, 355: 1055
16 Zhang Y, Tan G Q, Jiao D, et al. Ice-templated porous tungsten and tungsten carbide inspired by natural wood [J]. J. Mater. Sci. Technol., 2020, 45: 187
17 Wang X R, Wei S Z, Pan K M, et al. Electrical conductivity models and theoretical value calculation of W-Cu alloy [J]. Rare Met. Mater. Eng., 2019, 48: 33
18 Rajagopal C, Satyam M. Studies on electrical conductivity of insulator-conductor composites [J]. J. Appl. Phys., 1978, 49: 5536
19 Medalia A I. Electrical conduction in carbon blackcomposites [J]. Rubber Chem. Technol., 1986, 59: 432
20 van Beek L K H, van Pul B I C F. Internal field emission in carbon black-loaded natural rubber vulcanizates [J]. J. Appl. Polym. Sci., 1962, 6: 651
21 Lei Z L, Qi C M, Meng Y X, et al. Double percolation phenomenon in electrical conductive composites and its application [J]. Polym. Bull., 2002, (3): 69
21 雷忠利, 戚长谋, 孟雅新等. 导电复合材料中的双逾渗行为及其应用 [J]. 高分子通报, 2002, (3): 69
22 Xiu S X, Zou J Y, He J J. Effect of micro-features on macro-properties of CuCr contact material [J]. High Voltage Appar., 2000, 36(3): 40
22 修士新, 邹积岩, 何俊佳. CuCr触头材料微观特性对其宏观性能的影响 [J]. 高压电器, 2000, 36(3): 40
23 Zhang Z W, Hou W L, Wang Y H, et al. Notice of retraction: Microstructure evolution of Ag/SnO2 electrical contact materials via severe plastic deformation [A]. Proceedings of the 2010 International Conference on Future Information Technology and Management Engineering [C]. Changzhou, China: IEEE, 2010: 214
24 Tsuji K, Inada H, Kojima K, et al. Manufacturing process and material characteristics of Ag-Ni contacts consisting of nickel-compounded particles [J]. J. Mater. Sci., 1992, 27: 1179
25 Lin Z J. Microstructure control and properties of Ag-SnO2 and Ag-Ni electrical contact materials [D]. Shenyang: Northeastern University, 2016
25 林智杰. Ag-SnO2和Ag-Ni电触头材料微结构调控与性能研究 [D]. 沈阳: 东北大学, 2016
26 Suresh S, Mortensen A. Functionally graded metals and metal-ceramic composites: Part 2 Thermomechanical behaviour [J]. Int. Mater. Rev., 1997, 42: 85
27 Gibson L J, Ashby M F. Cellular Solids: Structure and Properties [M]. 2nd Ed., Cambridge: Cambridge University Press, 1997: 58
28 Li S J, Xu Q S, Wang Z, et al. Influence of cell shape on mechanical properties of Ti-6Al-4V meshes fabricated by electron beam melting method [J]. Acta Biomater., 2014, 10: 4537
Outlines

/