Study on Computational Prediction About Microstructure and Hardness of Q345 Steel Welded Joint Based on SH-CCT Diagram
Received date: 2020-09-18
Revised date: 2020-10-18
Online published: 2021-02-01
Supported by
National Natural Science Foundation of China(51875063)
Q345 steel is a low-alloy high-strength steel that is widely used in production. As the solid-state phase transition of Q345 steel is very sensitive to temperature, the microstructure and hardness of joints fabricated with this steel are difficult to predict. Therefore, studying the welding metallurgy, residual welding stress, and welding deformation of Q345 steel joints is essential for improving the safety and service life of Q345 welding structures. In this study, the microstructure and distribution of hardness of a Q345-steel tungsten-inert-gas welded and re-melted joint were calculated using four models encoded in the general finite element software, ABAQUS, and FORTRAN language. Three models were based on only one of three welding continuous-cooling transformation curves of the simulated heat-affected zone (SH-CCT) of Q345 steel, with peak temperatures of 1300, 1100, and 900oC (hereafter denoted as SH-CCT1300, SH-CCT1100, and SH-CCT900, respectively). The final model was based on the associated diagram consisting of these curves SH-CCT diagram above. Comparing the simulation and experimental results, the capabilities and accuracies of the prediction methods based on the different models were investigated. The microstructural calculations of the single SH-CCT diagram agreed with the experimental results only in the local heat-affected zone (HAZ) and largely deviated in the other areas. In the model based on SH-CCT900, the relative error of the ferrite volume fraction in the inter-critically HAZ (ICHAZ) was 7.7%. In the model based on SH-CCT1100, the relative errors of the ferrite, bainite, and martensite volume fractions in the fine-grained HAZ (FGHAZ) were 11.3%, 17.3%, and 15.5%, respectively. In the model based on SH-CCT1300, the relative error of the martensite volume fraction in the coarse-grained HAZ (CGHAZ) was 29.6%. In contrast, the microstructural calculations of the associated SH-CCT diagram agreed with the experimental results over the whole HAZ. The results showed that models based on the single SH-CCT diagrams met the tested hardness only in several narrow areas of the HAZ, but the hardness computed by the model, based on the associated diagram, was consistent with the tested hardness, with absolute differences ranging from 0 to 14 HV. The calculated microstructure and hardness in the fusion zone (FZ) greatly deviated from the test results in all the four models, indicating that predictions in the FZ require an accurate SH-CCT diagram of the FZ. In practical welding processes, the corresponding single SH-CCT diagram can adequately predict the microstructure and hardness during the phase transition of one HAZ area (such as the CGHAZ).
Long HU , Yifeng WANG , Suo LI , Chaohua ZHANG , Dean DENG . Study on Computational Prediction About Microstructure and Hardness of Q345 Steel Welded Joint Based on SH-CCT Diagram[J]. Acta Metall Sin, 2021 , 57(8) : 1073 -1086 . DOI: 10.11900/0412.1961.2020.00371
| 1 | Shi G, Shi Y J, Ban H Y. High-Strength Steel and Structure [M]. Beijing: China Architecture & Building Press, 2014: 1 |
| 1 | 施 刚, 石永久, 班慧勇. 高强度钢材钢结构 [M]. 北京: 中国建筑工业出版社, 2014: 1 |
| 2 | Liu H J, Yan J C, Wei Y H. Welding Metallurgy and Weldability [M]. Beijing: China Machine Press, 2007: 1 |
| 2 | 刘会杰, 闫久春, 魏艳红. 焊接冶金与焊接性 [M]. 北京: 机械工业出版社, 2007: 1 |
| 3 | Masao T. Determining the strength of welded joints—Knowing the characteristics of welding and utilizing inspection technology for quality control [J]. J. Jpn. Weld. Soc., 2012, 15: 21 |
| 3 | 豊田政男. 溶接継手の強度を決めるもの—溶接の特徴を知り、品質管理に検査技術を活かす [J]. 日本溶接学会誌, 2012, 15: 21 |
| 4 | Huang J H. Principles of Welding Metallurgy [M]. Beijing: China Machine Press, 2015: 205 |
| 4 | 黄继华. 焊接冶金原理 [M]. 北京: 机械工业出版社, 2015: 205 |
| 5 | Li Y J, Wang J. Analysis and Countermeasures of Celding Defects [M]. 2nd Ed., Beijing: Chemical Industry Press, 2014: 1 |
| 5 | 李亚江, 王 娟. 焊接缺陷分析与对策 [M], 第2版, 北京: 化学工业出版社, 2014: 1 |
| 6 | Sista S, Yang Z, Debroy T. Three-dimensional monte carlo simulation of grain growth in the heat-affected zone of a 2.25Cr-1Mo steel weld [J]. Metall. Mater. Trans., 2000, 31B: 529 |
| 7 | Wu M W, Xiong S M. Microstructure simulation of high pressure die cast magnesium alloy based on modified CA method [J]. Acta Metall. Sin., 2010, 46: 1534 |
| 7 | 吴孟武, 熊守美. 基于改进CA方法的压铸镁合金微观组织模拟 [J]. 金属学报, 2010, 46: 1534 |
| 8 | Yu J, Xu Q Y, Cui K, et al. Numerical simulation of microstructure evolution based on a modified Ca method [J]. Acta Metall. Sin., 2007, 43: 731 |
| 8 | 于 靖, 许庆彦, 崔 锴等. 基于一种改进CA模型的微观组织模拟 [J]. 金属学报, 2007, 43: 731 |
| 9 | Chen M J, Lv W, Huang Z X, et al. Application and development of microstructure simulation in welding research [J]. Electr. Weld. Mach., 2019, 49(2): 68 |
| 9 | 陈满骄, 吕 威, 黄作勋等. 微观组织模拟在焊接研究中的应用与发展 [J]. 电焊机, 2019, 49(2): 68 |
| 10 | Zheng W J, He Y M, Yang J G, et al. Influence of the crystal orientation of epitaxial solidification on the linear instability dynamic during the solidification of welding pool [J]. J. Mech. Eng., 2018, 54(2): 62 |
| 10 | 郑文健, 贺艳明, 杨建国等. 焊接熔池凝固过程联生结晶晶体学取向对线性不稳定动力学的影响 [J]. 机械工程学报, 2018, 54(2): 62 |
| 11 | Song K J. Modeling of microstructure in TIG welding heat affected zone and study on mechanical constitutive relation for TA15 alloy [D]. Harbin: Harbin Institute of Technology, 2014 |
| 11 | 宋奎晶. TA15钛合金TIG焊热影响区组织模拟及力学本构关系研究 [D]. 哈尔滨: 哈尔滨工业大学, 2014 |
| 12 | Cheon J, Na S J. Prediction of welding residual stress with real-time phase transformation by CFD thermal analysis [J]. Int. J. Mech. Sci., 2017, 131-132: 37 |
| 13 | Deng D A, Zhang Y B, Li S, et al. Influence of solid-state phase transformation on residual stress in P92 steel welded joint [J]. Acta Metall. Sin., 2016, 52: 394 |
| 13 | 邓德安, 张彦斌, 李 索等. 固态相变对P92钢焊接接头残余应力的影响 [J]. 金属学报, 2016, 52: 394 |
| 14 | Deng D A, Ren S D, Li S, et al. Influence of multi-thermal cycle and constraint condition on residual stress in P92 steel weldment [J]. Acta Metall. Sin., 2017, 53: 1532 |
| 14 | 邓德安, 任森栋, 李 索等. 多重热循环和约束条件对P92钢焊接残余应力的影响 [J]. 金属学报, 2017, 53: 1532 |
| 15 | Xavier C R, Delgado Junior H G, Castro J A, et al. Numerical predictions for the thermal history, microstructure and hardness distributions at the HAZ during welding of low alloy steels [J]. Mater. Res., 2016, 19: 520 |
| 16 | Kang S H, Im Y T. Finite element investigation of multi-phase transformation within carburized carbon steel [J]. J. Mater. Process. Technol., 2007, 183: 241 |
| 17 | Han L Z, Gu J F, Pan J S. Metallographic Atlas of SA508 Gr.3 Steel for Nuclear Power Heavy Forging [M]. Shanghai: Shanghai Jiao Tong University Press, 2016: 24 |
| 17 | 韩利战, 顾剑锋, 潘健生. 核电大型锻件SA508 Gr.3钢金相图谱 [M]. 上海: 上海交通大学出版社, 2016: 24 |
| 18 | Eshraghi-Kakhki M, Kermanpur A, Golozar M A. Three-dimensional simulation of quenching process of plain carbon steel gears incorporating phase transformations [J]. Mater. Sci. Technol., 2012, 28: 197 |
| 19 | Zhang Q, Xie J W, Gao Z Y, et al. A metallurgical phase transformation framework applied to SLM additive manufacturing processes [J]. Mater. Des., 2019, 166: 107618 |
| 20 | Ronda J, Oliver G J. Consistent thermo-mechano-metallurgical model of welded steel with unified approach to derivation of phase evolution laws and transformation-induced plasticity [J]. Comput. Meth. Appl. Mech. Eng., 2000, 189: 361 |
| 21 | Deng D A, Murakawa H. Finite element analysis of temperature field, microstructure and residual stress in multi-pass butt-welded 2.25Cr-1Mo steel pipes [J]. Comput. Mater. Sci., 2008, 43: 681 |
| 22 | den Uijl N J, Nishibata H, Smith S, et al. Prediction of post weld hardness of advanced high strength steels for automotive application using a dedicated carbon equivalent number [J]. Weld. World, 2008, 52: 18 |
| 23 | Zhou H, Zhang Q Y, Yi B, et al. Hardness prediction based on microstructure evolution and residual stress evaluation during high tensile thick plate butt welding [J]. Int. J. Naval Archit. Ocean Eng., 2020, 12: 146 |
| 24 | Deng D A, Kiyoshima S. Influence of annealing temperature on calculation accuracy of welding residual stress in a SUS304 stainless steel joint [J]. Acta Metall. Sin., 2014, 50: 626 |
| 24 | 邓德安, Kiyoshima S. 退火温度对SUS304不锈钢焊接残余应力计算精度的影响 [J]. 金属学报, 2014, 50: 626 |
| 25 | Yang S M, Tao W Q. Heat Transfer [M]. Beijing: Higher Education Press, 2006: 1 |
| 25 | 杨世铭, 陶文铨. 传热学 [M]. 北京: 高等教育出版社, 2006: 1 |
| 26 | Goldak J, Chakravarti A, Bibby M. A new finite element model for welding heat sources [J]. Metall. Trans., 1984, 15B: 299 |
| 27 | Lu S J, Wang H, Dai P Y, et al. Effect of creep on prediction accuracy and calculating efficiency of residual stress in post weld heat treatment [J]. Acta Metall. Sin., 2019, 55: 1581 |
| 27 | 逯世杰, 王 虎, 戴培元等. 蠕变对焊后热处理残余应力预测精度和计算效率的影响 [J]. 金属学报, 2019, 55: 1581 |
| 28 | Watt D F, Coon L, Bibby M, et al. An algorithm for modelling microstructural development in weld heat-affected zones (part a) reaction kinetics [J]. Acta Metall., 1988, 36: 3029 |
| 29 | Kang S H, Im Y T. Three-dimensional thermo-elastic-plastic finite element modeling of quenching process of plain-carbon steel in couple with phase transformation [J]. Int. J. Mech. Sci., 2007, 49: 423 |
| 30 | Fukumoto M, Yoshizaki M, Imataka H, et al. Three-dimensional FEM analysis of helical gear subjected to the carburized quenching process [J]. J. Soc. Mat. Sci., Japan, 2001, 50: 598 |
| 30 | 福本学, 吉崎正敏, 今高秀樹等. ヘリカルギアの浸炭焼入れ3次元シミュレーション [J]. 材料, 2001, 50: 598 |
| 31 | Deng D A. FEM prediction of welding residual stress and distortion in carbon steel considering phase transformation effects [J]. Mater. Des., 2009, 30: 359 |
| 32 | Song Y P, Liu G Q, Liu J T. et al. Prediction of microstructure distribution in quenched jominy specimen by maynier mathematic model [J]. Heat Treat. Met., 2006, 31(3): 93 |
| 32 | 宋月鹏, 刘国权, 刘建涛等. 基于梅尼尔模型端淬试样组织分布的预报预测 [J]. 金属热处理, 2006, 31(3): 93 |
| 33 | Song D L, Jiao S H. Validation of hardness prediction mathematic models [J].Mater. Mech. Eng., 2008, 32(003): 29 |
| 33 | 宋冬利,焦四海. 硬度预测模型的试验验证[J]. 机械工程材料, 2008, 32(003): 29 |
| 34 | Kasuya T, Hashiba Y. Carbon equivalent to assess hardenability of steel and prediction of HAZ hardness distribution [J]. Shinnittetsu Giho, 2006, 385: 48 |
| 35 | Zhang C H, Li S, Hu L, et al. Effects of pass arrangement on angular distortion, residual stresses and lamellar tearing tendency in thick-plate T-joints of low alloy steel [J]. J. Mater. Process. Technol., 2019, 274: 116293 |
/
| 〈 |
|
〉 |