Research paper

Hydrogen Embrittlement Behavior of a Vacuum-Carburized Gear Steel

  • Na XIAO ,
  • Weijun HUI ,
  • Yongjian ZHANG ,
  • Xiaoli ZHAO
Expand
  • School of Mechanical, Electronic and Control Engineering, Beijing Jiaotong University, Beijing 100044, China
HUI Weijun, professor, Tel: (010)51685461, E-mail: wjhui@bjtu.edu.cn

Received date: 2020-09-11

  Revised date: 2020-12-08

  Online published: 2021-01-27

Supported by

Major Basic Research of National Security of China(61328301)

Abstract

Carburized gear steel has a high-hardness case layer with excellent wear and fatigue resistance and a low-hardness core with high toughness. Such different microstructures imply different susceptibilities to hydrogen embrittlement (HE). However, a few or no studies have explored the HE behavior of carburized gear steel. Herein, the HE behavior of a vacuum-carburized gear steel 20Cr2Ni4A was investigated via an electrochemical hydrogen-charging and slow strain rate tensile test. For comparison, another group of specimens was prepared by a conventional quenched and tempered (QT) treatment. The volume fraction of retained austenite was significantly higher in the case layer of the carburized specimen (13.8%) than in the core and the QT specimen (4.6%). The retained austenite in the case layer showed a mainly irregular block-type morphology with wide size distribution. The room-temperature diffusible hydrogen content in the hydrogen-charged carburized specimen were almost identical to the QT specimen but the nondiffusible hydrogen content was significantly higher in the former than in the latter. Meanwhile, the hydrogen diffusion coefficient was notably lower in the hydrogen-charged carburized specimen than that in the QT sepcimen because the former retained higher fractions of austenite and cementite. The QT specimen exhibited superior strength and ductility. After hydrogen charging, the strength of the QT specimen remained almost unchanged but the total elongation notably decreased, causing the HE index (HEI), as evidenced using the relative total elongation loss, being 54.3%. Relative to the QT specimen, the carburized specimen achieved a higher tensile strength (increase by 34.6%) but a much lower ductility (total elongation and reduction of area reductions by 66.5% and 92.4%, respectively). The carburized specimen underwent premature brittle fracture before yielding, indicating susceptibility to HE. In fact, the HEI was as high as 90.9%. Mixed intergranular and quasi-cleavage fractures were observed in the surface embrittled region of the hydrogen-charged QT specimen. This region roughly corresponded to the maximum hydrogen diffusion distance. Meanwhile, the hydrogen-charged carburized specimen exhibited an embrittled internal-surface region with a certain width of intergranular fracture, and a long crack had propagated along the circumferential direction near the effective case depth. The microstructure, strength level, and residual stress are thought to mainly explain the abovementioned differences between the carburized and QT specimens.

Cite this article

Na XIAO , Weijun HUI , Yongjian ZHANG , Xiaoli ZHAO . Hydrogen Embrittlement Behavior of a Vacuum-Carburized Gear Steel[J]. Acta Metall Sin, 2021 , 57(8) : 977 -988 . DOI: 10.11900/0412.1961.2020.00363

References

1 Xiao N, Hui W J, Zhang Y J, et al. High cycle fatigue behavior of a low carbon alloy steel: The influence of vacuum carburizing treatment [J]. Eng. Fail. Anal., 2020, 109: 104215
2 Zhao M H, Han X C, Wang G, et al. Determination of the mechanical properties of surface-modified layer of 18CrNiMo7-6 steel alloys after carburizing heat treatment [J]. Int. J. Mech. Sci., 2018, 148: 84
3 Yan G W, Yu Q Z. Analysis of the delayed fracture of heavy-duty automobile gear [J]. J. Zhejiang Metall., 2017, (2): 38
3 严国卫, 余其中. 重载汽车齿轮延迟断裂原因分析 [J]. 浙江冶金, 2017, (2): 38
4 Jia H Y, Li Y L, Gong X Y, et al. Carburization and hydrogen embrittlement of 20CrMnMo steel center block [J]. Heat Treat. Met., 2002, 27(8): 57
4 贾厚雨, 李忆莲, 宫心勇等. 20CrMnMo钢中心楔块的渗碳与氢脆 [J]. 金属热处理, 2002, 27(8): 57
5 Xiao X, Long Y Q, Tan Z D. Hydrogen embrittlement in carburizing and its remedies [J]. Corros. Prot., 2000, 21: 469
5 肖 鑫, 龙有前, 谭正德. 渗碳齿轮氢脆及其解决方法 [J]. 腐蚀与防护, 2000, 21: 469
6 Straffelini G, Versari L. Brittle intergranular fracture of a thread: The role of a carburizing treatment [J]. Eng. Fail. Anal., 2009, 16: 1448
7 L'Hostis B, Minfray C, Frégonèse M, et al. Influence of lubricant formulation on rolling contact fatigue of gears-interaction of lubricant additives with fatigue cracks [J]. Wear, 2017, 382-383: 113
8 Kinami T. Carbo-nitrided steel with excellent rolling contact fatigue strength duo to hydrogen embrittlement [J]. Daiki Steel Mak., 2014, 85: 127
8 木南俊哉. 水素脆性型転動疲労強度に優れた浸炭窒化鋼 [J]. 電気製鋼, 2014, 85: 127
9 Li J X, Wang W, Zhou Y, et al. A review of research status of hydrogen embrittlement for automotive advanced high-strength steels [J]. Acta Metall. Sin., 2020, 56: 444
9 李金许, 王 伟, 周 耀等. 汽车用先进高强钢的氢脆研究进展 [J]. 金属学报, 2020, 56: 444
10 Dwivedi S K, Vishwakarma M. Hydrogen embrittlement in different materials: A review [J]. Int. J. Hydrogen Energy, 2018, 43: 21603
11 Zhang Y J, Hui W J, Zhao X L, et al. Effects of hot stamping and tempering on hydrogen embrittlement of a low-carbon boron-alloyed steel [J]. Materials, 2018, 11: 2507
12 Wang Y F, Hu S Y, Li Y, et al. Improved hydrogen embrittlement resistance after quenching-tempering treatment for a Cr-Mo-V high strength steel [J]. Int. J. Hydrogen Energy, 2019, 44: 29017
13 Li X F, Zhang J, Shen S C, et al. Effect of tempering temperature and inclusions on hydrogen-assisted fracture behaviors of a low alloy steel [J]. Mater. Sci. Eng., 2017, A682: 359
14 Zhang C L, Liu Y Z, Jiang C, et al. Effects of niobium and vanadium on hydrogen-induced delayed fracture in high strength spring steel [J]. J. Iron Steel Res. Int., 2011, 18: 49
15 Zhang Y J, Hui W J, Dong H. Hydrogen induced delayed fracture behavior of a low-carbon Mn-B type ultra-high strength steel sheet after hot stamping [J]. Acta Metall. Sin., 2013, 49: 1153
15 张永健, 惠卫军, 董 瀚. 一种低碳Mn-B系超高强度钢板热成形后的氢致延迟断裂行为 [J]. 金属学报, 2013, 49: 1153
16 Zhao X L, Zhang Y J, Shao C W, et al. Hydrogen embrittlement of intercritically annealed cold-rolled 0.1C-5Mn steel [J]. Acta Metall. Sin., 2018, 54: 1031
16 赵晓丽, 张永健, 邵成伟等. 两相区退火处理冷轧0.1C-5Mn中锰钢的氢脆敏感性 [J]. 金属学报, 2018, 54: 1031
17 Xiao N, Hui W J, Zhang Y J, et al. High-cycle fatigue behavior of vacuum-carburized 20Cr2Ni4 steel with different case depths [J]. J. Mater. Eng. Perform., 2019, 28: 3413
18 Bhadeshia H K D H. Prevention of hydrogen embrittlement in steels [J]. ISIJ Int., 2016, 56: 24
19 Jiang Y, Wu Q, Wang Y F, et al. Suppression of hydrogen absorption into 304L austenitic stainless steel by surface low temperature gas carburizing treatment [J]. Int. J. Hydrogen Energy, 2019, 44: 24054
20 Li Y, Li W, Zhu X, et al. Mechanism of improved hydrogen embrittlement resistance of low-temperature plasma carburised stainless steel [J]. Surf. Eng., 2018, 34: 189
21 Michler T. Influence of plasma nitriding on hydrogen environment embrittlement of 1.4301 austenitic stainless steel [J]. Surf. Coat. Technol., 2008, 202: 1688
22 Chu W Y, Qiao L J, Li J X, et al. Hydrogen Embrittlement and Stress Corrosion Cracking [M]. Beijing: Science Press, 2013: 94
22 褚武扬, 乔利杰, 李金许等. 氢脆和应力腐蚀 [M]. 北京: 科学出版社, 2013: 94
23 Zhang Y J, Hui W J, Zhao X L, et al. Effect of reverted austenite fraction on hydrogen embrittlement of TRIP-aided medium Mn steel (0.1C-5Mn) [J]. Eng. Fail. Anal., 2019, 97: 605
24 Carneiro Filho C J, Mansur M B, Modenesi P J, et al. The effect of hydrogen release at room temperature on the ductility of steel wire rods for pre-stressed concrete [J]. Mater. Sci. Eng., 2010, A527: 4947
25 Wang J J, Hui W J, Xie Z Q, et al. Hydrogen embrittlement of a cold-rolled Al-containing medium-Mn steel: Effect of pre-strain [J]. Int. J. Hydrogen Energy, 2020, 45: 22080
26 Hui W J, Zhang H X, Zhang Y J, et al. Effect of nickel on hydrogen embrittlement behavior of medium-carbon high strength steels [J]. Mater. Sci. Eng., 2016, A674: 615
27 Chiang J, Lawrence B, Boyd J D, et al. Effect of microstructure on retained austenite stability and work hardening of TRIP steels [J]. Mater. Sci. Eng., 2011, A528: 4516
28 Han J, Nam J H, Lee Y K. The mechanism of hydrogen embrittlement in intercritically annealed medium Mn TRIP steel [J]. Acta Mater., 2016, 113: 1
Outlines

/