Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model
Received date: 2020-08-05
Revised date: 2020-12-10
Online published: 2021-01-13
Supported by
National Natural Science Foundation of China(U1960109);Key Program for the Innovation and Entrepreneurship Support Plan for Returning Overseas Chinese Scholars in Anhui Province
Cluster dynamics is a mesoscopic modeling technique describing the various kinetic stages of homogeneous precipitation by the same set of rate equations. However, when the simulated cluster size continuously increases, it easily causes an enormous computational workload, and the use of a particle-size-grouping method is often necessary to solve this problem. In this study, an ungrouped cluster dynamics model and certain existing grouping methods are reviewed. Next, a new grouping method with an assumed logarithmically-linear distribution of cluster number densities inside each group size is proposed. Comparing the results of all grouped models with the exact solution of the ungrouped model for simulating aluminum-scandium (Al3Sc) precipitation in the Al-0.18%Sc (atomic fraction) alloy at 300oC, the new grouping method was able to reduce computational costs considerably keeping enough total and local accuracies. Moreover, the reasonable agreements of the mean radii and size distributions as functions of time between experiments and simulations were obtained, demonstrating the ability of the new grouping method in modeling large-scale precipitation kinetics.
Kun XU , Haichuan WANG , Hui KONG , Zhaoyang WU , Zhan ZHANG . Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model[J]. Acta Metall Sin, 2021 , 57(6) : 822 -830 . DOI: 10.11900/0412.1961.2020.00289
| 1 | Mathon M H, Barbu A, Dunstetter F, et al. Experimental study and modelling of copper precipitation under electron irradiation in dilute FeCu binary alloys [J]. J. Nucl. Mater., 1997, 245: 224 |
| 2 | Christien F, Barbu A. Modelling of copper precipitation in iron during thermal aging and irradiation [J]. J. Nucl. Mater., 2004, 324: 90 |
| 3 | Clouet E, Barbu A, Laé L, et al. Precipitation kinetics of Al3Zr and Al3Sc in aluminum alloys modeled with cluster dynamics [J]. Acta Meter., 2005, 53: 2313 |
| 4 | Lepinoux L. Modelling precipitation in binary alloys by cluster dynamics [J]. Acta Mater., 2009, 57: 1086 |
| 5 | Ke H B, Wells P, Edmondson P D, et al. Thermodynamic and kinetic modeling of Mn-Ni-Si precipitates in low-Cu reactor pressure vessel steels [J]. Acta Mater., 2017, 138: 10 |
| 6 | Kiritani M. Analysis of the clustering process of supersaturated lattice vacancies [J]. J. Phys. Soc. Jpn., 1973, 35: 95 |
| 7 | Koiwa M. On the validity of the grouping method—Comments on “analysis of the clustering process of supersaturated lattice vacancies”–[J]. J. Phys. Soc. Jpn., 1974, 37: 1532 |
| 8 | Golubov S I, Ovcharenko A M, Barashev A V, et al. Grouping method for the approximate solution of a kinetic equation describing the evolution of point-defect clusters [J]. Philos. Mag., 2001, 81A: 643 |
| 9 | Ovcharenko A M, Golubov S I, Woo C H, et al. GMIC++: Grouping method in C++: An efficient method to solve large number of Master equations [J]. Comput. Phys. Commun., 2003, 152: 208 |
| 10 | Liu C, He L, Zhai Y, et al. Evolution of small defect clusters in ion-irradiated 3C-SiC: Combined cluster dynamics modeling and experimental study [J]. Acta Mater., 2017, 125: 377 |
| 11 | Fell M, Murphy S M. The nucleation and growth of gas bubbles in irradiated metals [J]. J. Nucl. Mater., 1990, 172: 1 |
| 12 | Golubov S I, Stoller R E, Zinkle S J, et al. Kinetics of coarsening of helium bubbles during implantation and post-implantation annealing [J]. J. Nucl. Mater., 2007, 361: 149 |
| 13 | Kampmann R, Wagner R. Kinetics of precipitation in metastable binary alloys—Τheory and application to Cu-1.9at % Ti and Ni-14 at % Al [A]. Decomposition of Alloys: The Early Stages [C]. Oxford: Pergamon Press, 1984: 91 |
| 14 | Cahn R W, Haasen P, Kramer E J. Materials Science and Technology [M]. Weinheim: John Wiley & Sons Inc., 1991: 213 |
| 15 | Svoboda J, Fischer F D, Fratzl P, et al. Modelling of kinetics in multi-component multi-phase systems with spherical precipitates: I: Theory [J]. Mater. Sci. Eng., 2004, A385: 166 |
| 16 | Becker R, D?ring W. Kinetische behandlung der keimbildung in übers?ttigten d?mpfen [J]. Ann. Phys., 1935, 416: 719 |
| 17 | Zhang L F, Li Y L, Ren Y. Fundamentals of non-metallic inclusions in steel: part I. Control of unsteady casting and big inclusion; nucleation, motion, removal and capture of inclusions in molten steel [J]. Iron Steel, 2013, 48(11): 1 |
| 17 | 张立峰, 李燕龙, 任 英. 钢中非金属夹杂物的相关基础研究(I)——非稳态浇铸中的大颗粒夹杂物及夹杂物的形核、长大、运动、去除和捕捉 [J]. 钢铁, 2013, 48(11): 1 |
| 18 | Li Y G, Zhou W H, Huang L F, et al. Cluster dynamics modeling of accumulation and diffusion of helium in neutron irradiated tungsten [J]. J. Nucl. Mater., 2012, 431: 26 |
| 19 | Gao C. Cluster dynamics simulation of defect evolution in electron-irradiated BCC Fe and Fe-Cu dilute alloys [D]. Shanghai: Shanghai University, 2015 |
| 19 | 高 超. BCC铁和铁铜合金电子辐照缺陷演化的团簇动力学模拟 [D]. 上海: 上海大学, 2015 |
| 20 | Xu K, Thomas B G. Particle-size-grouping model of precipitation kinetics in microalloyed steels [J]. Metall. Mater. Trans., 2012, 43A: 1079 |
| 21 | Marquis E A, Seidman D N. Nanoscale structural evolution of Al3Sc precipitates in Al(Sc) alloys [J]. Acta Mater., 2001, 49: 1909 |
| 22 | Watanabe C, Kondo T, Monzen R. Coarsening of Al3Sc precipitates in an Al-0.28 wt pct Sc alloy [J]. Metall. Mater. Trans., 2004, 35A: 3003 |
| 23 | R?yset J, Ryum N. Kinetics and mechanisms of precipitation in an Al-0.2 wt.% Sc alloy [J]. Mater. Sci. Eng., 2005, A396: 409 |
| 24 | Fujikawa S I. Impurity diffusion of scandium in aluminium [J]. Defect Diffus. Forum., 1997, 143-147: 115 |
| 25 | Novotny G M, Ardell A J. Precipitation of Al3Sc in binary Al-Sc alloys [J]. Mater. Sci. Eng., 2001, A318: 144 |
| 26 | Iwamura S, Miura Y. Loss in coherency and coarsening behavior of Al3Sc precipitates [J]. Acta Mater., 2004, 52: 591 |
| 27 | Robson J D, Jones M J, Prangnell P B. Extension of the N-model to predict competing homogeneous and heterogeneous precipitation in Al-Sc alloys [J]. Acta Mater., 2003, 51: 1453 |
| 28 | Hyland R W. Homogeneous nucleation kinetics of Al3Sc in a dilute Al-Sc alloy [J]. Metall. Mater. Trans., 1992, 23A: 1947 |
| 29 | Zener C. Theory of growth of spherical precipitates from solid solution [J]. J. Appl. Phys., 1949, 20: 950 |