Research paper

Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon

  • Xiang HU ,
  • Jiacheng GE ,
  • Sinan LIU ,
  • Shu FU ,
  • Zhenduo WU ,
  • Tao FENG ,
  • Dong LIU ,
  • Xunli WANG ,
  • Si LAN
Expand
  • 1.Herbert Gleiter Institute of Nanoscience, School of Materials Science and Engineering/Herbert Gleiter Institute, Nanjing University of Science and Technology, Nanjing 210094, China
    2.Department of Physics, City University of Hong Kong, Hong Kong 999077, China
    3.Applied Physics Centre of Neutron Scattering, Dongguan University of Hong Kong Research Institute, Dongguan 523808, China
    4.School of Energy and Power Engineering, Nanjing University of Science and Technology, Nanjing 210094, China
LAN Si, professor, Tel: 18115156168, E-mail: lansi@njust.edu.cn

Received date: 2020-10-26

  Revised date: 2020-12-02

  Online published: 2020-12-18

Supported by

National Natural Science Foundation of China(51871120);Natural Science Foundation of Jiangsu Province-Outstanding Youth Fund Project(BK20200019)

Abstract

The functional groups in traditional energetic materials typically contain C, N, and O. These elements are usually unstable and sensitive to external stimuli. Moreover, the chemicals used during the preparation process of traditional energetic materials are toxic and pose many safety and environmental issues. As one of the metastable materials, high-energy-state amorphous alloys are potential candidates for new energetic materials with high combustion heat, low ignition temperature, non-toxicity, and improved safety. In this work, the combustion mechanism of Fe-based amorphous ribbons with an anomalous exothermic phenomenon was systematically studied using in situ synchrotron X-ray diffraction, differential scanning calorimetry, thermogravimetric analysis, and X-ray photoelectron spectroscopy. Experimental results show that compared to Fe-Nb-B-Y amorphous alloys with normal thermophysical and combustion behaviors, (Fe0.72B0.24Nb0.04)95.5Y4.5 amorphous ribbons with anomalous exothermic phenomena possess low ignition temperature and self-propagating combustion behavior due to the catalysis of the rapid crystallization exothermic process. The anomalous exothermic phenomenon and associated liquid-liquid phase transitions can cause rapid crystallization at elevated temperatures during heating, followed by multi-step oxidation. On the other hand, it was possible to significantly reduce the activation energy of high-temperature oxidation. The liquid-liquid phase transition can lower the energy barrier of the oxidation reaction. In this way, the oxidation reaction at high temperatures can be promoted. The results suggest that the liquid-liquid phase transition has an “induced activation” effect on the combustion of Fe-based amorphous alloys.

Cite this article

Xiang HU , Jiacheng GE , Sinan LIU , Shu FU , Zhenduo WU , Tao FENG , Dong LIU , Xunli WANG , Si LAN . Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. Acta Metall Sin, 2021 , 57(4) : 542 -552 . DOI: 10.11900/0412.1961.2020.00420

References

1 Baletto F, Ferrando R. Structural properties of nanoclusters: Energetic, thermodynamic, and kinetic effects [J]. Rev. Mod. Phys., 2005, 77: 371
2 Sikder A K, Sikder N. A review of advanced high performance, insensitive and thermally stable energetic materials emerging for military and space applications [J]. J. Hazard. Mater., 2004, 112: 1
3 Li G, Zhang C Y. Review of the molecular and crystal correlations on sensitivities of energetic materials [J]. J. Hazard. Mater., 2020, 398: 122910
4 Yu B S, Sun Y H, Bai H Y, et al. Highly energetic and flammable metallic glasses [J]. Sci. China Phys. Mech. Astron., 2020, 63: 276112
5 Badgujar D M, Talawar M B, Asthana S N, et al. Advances in science and technology of modern energetic materials: An overview [J]. J. Hazard. Mater., 2008, 151: 289
6 Trunov M A, Schoenitz M, Dreizin E L. Ignition of aluminum powders under different experimental conditions [J]. Propell. Explos. Pyrot., 2005, 30: 36
7 Yagodnikov D A, Ignatov A V, Gusachenko E I. Ignition and combustion of pyrotechnic compositions based on microsized and ultra-nanosized aluminum particles in a moist medium in a two-zone gas generator [J]. Combust. Explos. Shock Waves, 2017, 53: 15
8 Pan J, Wang Y X, Guo Q, et al. Extreme rejuvenation and softening in a bulk metallic glass [J]. Nat. Commun., 2018, 9: 560
9 Dreizin E L. Phase changes in metal combustion [J]. Prog. Energy Combust. Sci., 2000, 26: 57
10 Ge J C, He H Y, Zhou J, et al. In-situ scattering study of a liquid-liquid phase transition in Fe-B-Nb-Y supercooled liquids and its correlation with glass-forming ability [J]. J. Alloys Compd., 2019, 787: 831
11 Lan S, Ren Y, Wei X Y, et al. Hidden amorphous phase and reentrant supercooled liquid in Pd-Ni-P metallic glasses [J]. Nat. Commun., 2017, 8: 14679
12 Tanaka H. General view of a liquid-liquid phase transition [J]. Phys. Rev., 2000, 62E: 6968
13 Palmer J C, Martelli F, Liu Y, et al. Metastable liquid-liquid transition in a molecular model of water [J]. Nature, 2014, 510: 385
14 Shimizu R, Kobayashi M, Tanaka H. Evidence of liquid-liquid transition in triphenyl phosphite from time-resolved light scattering experiments [J]. Phys. Rev. Lett., 2014, 112: 125702
15 Zhou Z J, Hu X, You Z, et al. Oxy-fuel combustion characteristics and kinetic parameters of lignite coal from thermo-gravimetric data [J]. Thermochim. Acta, 2013, 553: 54
16 Fakhraai Z, Forrest J A. Measuring the surface dynamics of glassy polymers [J]. Science, 2008, 319: 600
17 K?k M V, Acar C. Kinetics of crude oil combustion [J]. J. Therm. Anal. Calorim., 2006, 83: 445
18 Lysenko E N, Surzhikov A P, Zhuravkov S P, et al. The oxidation kinetics study of ultrafine iron powders by thermogravimetric analysis [J]. J. Therm. Anal. Calorim., 2014, 115: 1447
19 Qi X W, Zhou J, Yue Z X, et al. Auto-combustion synthesis of nanocrystalline LaFeO3 [J]. Mater. Chem. Phys., 2003, 78: 25
20 Takacs L. Self-sustaining reactions induced by ball milling: An overview [J]. Int. J. Self-Propag. High-Temp. Synth., 2009, 18: 276
21 Takahashi M, Koshimura M, Abuzuka T. Phase diagram of amorphous and crystallized Fe-B alloy system [J]. Jpn. J. Appl. Phys., 1981, 20: 1821
22 Abrosimova G E, Aronin A S. Formation of metastable phases during crystallization of amorphous iron-based alloys [J]. Crystallogr. Rep., 2020, 65: 573
23 Grosvenor A P, Kobe B A, Biesinger M C, et al. Investigation of multiplet splitting of Fe 2p XPS spectra and bonding in iron compounds [J]. Surf. Interface Anal., 2004, 36: 1564
24 Yamashita T, Hayes P. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials [J]. Appl. Surf. Sci., 2008, 254: 2441
25 Kim K J, Moon D W, Lee S K, et al. Formation of a highly oriented FeO thin film by phase transition of Fe3O4 and Fe nanocrystallines [J]. Thin Solid Films, 2000, 360: 118
26 Li Y X, Claydon J S, Ahmad E, et al. XPS and XMCD study of Fe3O4 GaAs interface [J]. IEEE Trans. Magn., 2005, 41: 2808
27 Rydén M, Leion H, Mattisson T, et al. Combined oxides as oxygen-carrier material for chemical-looping with oxygen uncoupling [J]. Appl. Energy, 2014, 113: 1924
28 Zhang C, Wu Y, Liu L. Robust hydrophobic Fe-based amorphous coating by thermal spraying [J]. Appl. Phys. Lett., 2012, 101: 121603
29 Filonenko N Y, Babachenko O I, Kononenko G A. Influence of overheating and cooling rate on the structures and properties of alloys of the Fe-B system [J]. Mater. Sci., 2019, 55: 440
30 Otero T F, Santos F. Polythiophene oxidation: Rate coefficients, activation energy and conformational energies [J]. Electrochim. Acta, 2008, 53: 3166
31 Zhong Z Y, Highfield J, Lin M, et al. Insights into the oxidation and decomposition of CO on Au/α-Fe2O3 and on α-Fe2O3 by coupled TG-FTIR [J]. Langmuir, 2008, 24: 8576
32 Cao C R, Lu Y M, Bai H Y, et al. High surface mobility and fast surface enhanced crystallization of metallic glass [J]. Appl. Phys. Lett., 2015, 107: 141606
Outlines

/