Current Status and Challenges in Corrosion and Protection Strategies for Sintered NdFeB Magnets
Received date: 2020-08-17
Revised date: 2020-12-02
Online published: 2020-12-14
Supported by
National Natural Science Foundation of China(20571022);National Science and Technology Program(012BAE02B01);Anhui Key Research and Development Program(1804a09020068);Anhui Municipal Science and Technology Project(17030901063);Ministry of Major Science & Technology of Anhui(1301022080)
The susceptibility of sintered NdFeB to corrosion in harsh environments limits their wide variety of applications. Improved resistance to corrosion of NdFeB magnets and advancement of surface coatings are critical directions in permanent magnet material fields. Significant work has been undertaken on the development of long-life NdFeB magnets. However, comprehensive research of NdFeB corrosion, from process technology to fundamental theory, is lacking, mainly owing to the hysteresis in the study of the elementary works of corrosion and protection related to magnetism, and improving the quality and diversified market demands. This analysis covers recent research that has led to advances in anti-corrosion material technology for NdFeB magnets, including corrosion factors, contemporary methodologies from technology to fundamentals, the basic framework for surface protection and key techniques in the industry application. Finally, prospects and existing challenges in the field of corrosion and protection are reviewed, attempting to identify future developments and directions.
Key words: NdFeB; corrosion; coating; binary alloy technology; physical vapor deposition
Yucheng WU , Zhiqiang GAO , Guangqing XU , Jiaqin LIU , Haicheng XUAN , Youhao LIU , Xiaofei YI , Jingwu CHEN , Peide HAN . Current Status and Challenges in Corrosion and Protection Strategies for Sintered NdFeB Magnets[J]. Acta Metall Sin, 2021 , 57(2) : 171 -181 . DOI: 10.11900/0412.1961.2020.00308
| 1 | Jiang W, Shen L D, Wang K, et al. Study on Ni-Ni(S)-Ni(P) multilayer coating by friction-assisted jet electroplating on sintered NdFeB [J]. J. Alloys Compd., 2019, 787: 1089 |
| 2 | Zhang J X, Zhang T J, Cui K. Mechanism and prevention of NdFeB magnet corrosion [J]. Dev. Appl. Mater., 2001, 16(4): 38 |
| 2 | 张静贤, 张同俊, 崔 琨. NdFeB永磁材料腐蚀机理与防护 [J]. 材料开发与应用, 2001, 16(4): 38 |
| 3 | Liao X F, Zhang J S, Yu H Y, et al. Understanding the phase structure, magnetic properties and anti-corrosion behavior of melt-spun (La, Y)2Fe14B alloys [J]. J. Magn. Magn. Mater., 2019, 489: 165444 |
| 4 | Kong X W, Liu G Z, Zhao M J, et al. Research status of corrosion property of sintered NdFeB permanent magnet [J]. Chin. Rare Earths, 2013, 34(6): 69 |
| 4 | 孔祥薇, 刘国征, 赵明静等. 烧结NdFeB永磁体的腐蚀性研究现状 [J]. 稀土, 2013, 34(6): 69 |
| 5 | Li H Y, Hao Z Z, Liu Y H, et al. Research progress on corrosion mechanism and surface protection technology of sintered NdFeB permanent magnets [J]. Min. Metall. Eng., 2016, 36(6): 118 |
| 5 | 李红英, 郝壮志, 刘宇晖等. 烧结NdFeB永磁材料腐蚀机理与表面防护技术研究进展 [J]. 矿冶工程, 2016, 36(6): 118 |
| 6 | Yan F Y, Zhao C Y, Zhang L. Advances in protective technology on NdFeB permanent magnetic material [J]. Plat. Finish., 2012, 34(8): 22 |
| 6 | 严芬英, 赵春英, 张 琳. 钕铁硼永磁材料表面防护技术的研究进展 [J]. 电镀与精饰, 2012, 34(8): 22 |
| 7 | Liu W, Hou J. Production status and prospect of NdFeB magnet electroplating [J]. Plat. Finish., 2012, 34(4): 20 |
| 7 | 刘 伟, 侯 进. 钕铁硼电镀技术生产现状与展望 [J]. 电镀与精饰, 2012, 34(4): 20 |
| 8 | Wang E S. The anti-corrosion technology of NdFeB chemical conversion coating [J]. Plat. Finish., 2013, 35(12): 13 |
| 8 | 王恩生. 钕铁硼化学转化膜防腐蚀技术 [J]. 电镀与精饰, 2013, 35(12): 13 |
| 9 | Hu F, Xu W, Dai M J, et al. Research progress on physical vapor deposition and related process of NdFeB magnets [J]. Mater. Rev., 2014, 28(3): 20 |
| 9 | 胡 芳, 许 伟, 代明江等. 钕铁硼永磁材料物理气相沉积技术及相关工艺的研究进展 [J]. 材料导报, 2014, 28(3): 20 |
| 10 | Chen X P, Zhao D L, Li Y, et al. The development of electroplating process and equipment on NdFeB permanent magnet materials [J]. Met. Funct. Mater., 2015, 22(5): 32 |
| 10 | 陈小平, 赵栋梁, 李 勇等. 钕铁硼永磁材料电镀工艺与装备的发展 [J]. 金属功能材料, 2015, 22(5): 32 |
| 11 | Peng N, Wang X D, Chen X P, et al. Study on surface protection for NdFeB permanent magnet alloy [J]. Hot Work. Technol., 2016, 45(4): 6 |
| 11 | 彭 楠, 王向东, 陈小平等. 钕铁硼永磁体的表面防护技术研究 [J]. 热加工工艺, 2016, 45(4): 6 |
| 12 | Liu W Q, Yue M, Zhang J X, et al. Intrinsic corrosion characteristic of sintered NdFeB permanent magnets [J]. Powder Metall. Technol., 2006, 24: 195 |
| 12 | 刘卫强, 岳 明, 张久兴等. 烧结NdFeB永磁合金本征腐蚀特性研究进展 [J]. 粉末冶金技术, 2006, 24: 195 |
| 13 | Yan G L, McGuiness P J, Farr J P G, et al. Environmental degradation of NdFeB magnets [J]. J. Alloys Compd., 2009, 478: 188 |
| 14 | Wu Y P, Zhu M G, Shi X N, et al. Corrosion research of (Ce15Nd85)30FebalB1M sintered magnet in hydrothermal environment [J]. J. Chin. Soc. Rare Earth, 2016, 34: 171 |
| 14 | 吴亚萍, 朱明刚, 石晓宁等. (Ce15Nd85)30FebalB1M永磁体湿热条件下的腐蚀性研究 [J]. 中国稀土学报, 2016, 34: 171 |
| 15 | Wu Y P, Zhu M G, Shi X N, et al. Study on the diversity of corrosion products of (Ce20Nd80)31FebalB1M magnet [J]. Powder Metall. Ind., 2017, 27(5): 36 |
| 15 | 吴亚萍, 朱明刚, 石晓宁等. (Ce20Nd80)31FebalB1M磁体腐蚀产物多样性的研究 [J]. 粉末冶金工业, 2017, 27(5): 36 |
| 16 | Liu W Q, Yue M, Zhang D T, et al. Corrosion behavior of conventional and spark plasma-sintered Nd-Fe-B permanent magnets in different solutions [J]. Corrosion, 2009, 65: 501 |
| 17 | Liu W Q, Yue M, Zhang J X, et al. The effect of Nd-rich phase for sintered NdFeB corrosion resistance [J]. Rare Met. Mater. Eng., 2007, 36: 1066 |
| 17 | 刘卫强, 岳 明, 张久兴等. 富钕相对烧结NdFeB磁体耐腐蚀性的影响 [J]. 稀有金属材料与工程, 2007, 36: 1066 |
| 18 | Cui J, Kramer M, Zhou L, et al. Current progress and future challenges in rare-earth-free permanent magnets [J]. Acta Mater., 2018, 158: 118 |
| 19 | Li J J, An G H, Guo C J, et al. Accelerated corrosion behavior of sintered NdFeB magnets in HAST climate [J]. J. Chin. Soc. Rare Earths, 2016, 34: 555 |
| 19 | 李家节, 安桂焕, 郭诚君等. 烧结NdFeB磁体高温高压高湿加速腐蚀行为研究 [J]. 中国稀土学报, 2016, 34: 555 |
| 20 | Nan H Y, Zhu L Q, Liu H C, et al. Protection of NdFeB magnets by corrosion resistance phytic acid conversion film [J]. App. Surf. Sci., 2015, 355: 1215 |
| 21 | Zhou L J, Pei W L, Guo X L, et al. Corrosion behavior of low cost sintered Nd-Fe-B magnet containing element Ce [J]. J. Mater. Metall., 2015, 14: 217 |
| 21 | 周丽娟, 裴文利, 郭小莲等. 含Ce烧结Nd-Fe-B磁体的腐蚀行为 [J]. 材料与冶金学报, 2015, 14: 217 |
| 22 | Zheng J W, Du Z Y, Jiang M Y, et al. Corrosion behavior of Nd-Fe-B sintered magnets at remanence state [J]. Rare Met. Mater. Eng., 2008, 37: 1369 |
| 22 | 郑精武, 都周云, 蒋梅燕等. 烧结钕铁硼在剩磁状态下的腐蚀研究 [J]. 稀有金属材料与工程, 2008, 37: 1369 |
| 23 | Jiang L Q, Zheng J W. Corrosion behavior of sintered NdFeB magnets in various acid solution [J]. Rare Met. Mater. Eng., 2006, 35: 340 |
| 23 | 姜力强, 郑精武. 烧结钕铁硼在各种酸介质中的腐蚀研究 [J]. 稀有金属材料与工程, 2006, 35: 340 |
| 24 | Xu J L, Huang Z X, Luo J M, et al. Corrosion behavior of sintered NdFeB magnets in different acidic solutions [J]. Rare Met. Mater. Eng., 2015, 44: 786 |
| 25 | Ding X, Xue L F, Ding K H, et al. Corrosion behavior of the sintered Nd-Fe-B permanent magnets in different acid solutions [J]. J. Cent. South Univ. (Sci. Technol.), 2016, 47: 1105 |
| 25 | 丁 霞, 薛龙飞, 丁开鸿等. 烧结钕铁硼永磁合金在不同酸溶液中的腐蚀行为 [J]. 中南大学学报(自然科学版), 2016, 47: 1105 |
| 26 | Sueptitz R, Uhlemann M, Gebert A, et al. Corrosion, passivation and breakdown of passivity of neodymium [J]. Corros. Sci., 2010, 52: 886 |
| 27 | Liu H, Fu S, Fu Q Q, et al. Research status of medical NdFeB implantation surface modification [J]. Prog. Mod. Biomed., 2019, 19: 175 |
| 27 | 刘 豪, 付 珊, 付琴琴等. 医用钕铁硼体内植入表面改性研究现状 [J]. 现代生物医学进展, 2019, 19: 175 |
| 28 | Tang Z, Wu J Y, Chen X. In vitro study of the corrosiveness resistance property of NdFeB magnet with different coatings [J]. J. Pract. Stomatol., 2013, 29: 195 |
| 28 | 唐 镇, 吴建勇, 陈 溪. 不同镀膜钕铁硼磁体抗腐蚀性的体外实验研究 [J]. 实用口腔医学杂志, 2013, 29: 195 |
| 29 | Tian B Y, Liu H, Fu S, et al. In vitro study on corrosion resistance of different surface modified [J]. China Med. Dev., 2019, 34(3): 5 |
| 29 | 田波彦, 刘 豪, 付 珊等. 不同表面改性钕铁硼磁体抗胃液腐蚀的体外研究 [J]. 中国医疗设备, 2019, 34(3): 5 |
| 30 | Tian B Y, Liu H, Fu S, et al. In vitro study on the bile corrosion resistance of NdFeB magnets with different coatings [J]. Prog. Mod. Biomed., 2019, 19: 1006 |
| 30 | 田波彦, 刘豪, 付珊等. 不同镀层钕铁硼磁体抗胆汁腐蚀的体外研究 [J]. 现代生物医学进展, 2019, 19: 1006 |
| 31 | Costa I, Oliveira M C L, de Melo H G, et al. The effect of the magnetic field on the corrosion behavior of Nd-Fe-B permanent magnets [J]. J. Magn. Magn. Mater., 2004, 278: 348 |
| 32 | Sueptitz R, Tschulik K, Uhlemann M, et al. Effect of magnetization state on the corrosion behaviour of NdFeB permanent magnets [J]. Corros. Sci., 2011, 53: 2843 |
| 33 | Yan G L, Williams A J, Farr J P G, et al. The effect of density on the corrosion of NdFeB magnets [J]. J. Alloys Compd., 1999, 292: 266 |
| 34 | Zhou L, Liu T, Zhang X, et al. Facters affecting corrosion weight loss of sintered NdFeB magnets and improvement in corrosion resistance [J]. J. Magn. Mater. Dev., 2018, 49(4): 10 |
| 34 | 周 磊, 刘 涛, 张 昕等. 烧结钕铁硼磁体腐蚀失重的影响因素及耐蚀性改进 [J]. 磁性材料及器件, 2018, 49(4): 10 |
| 35 | Wang Z X, Pei K, Zhang J J, et al. Correlation between the microstructure and magnetic configuration in coarse-grain inhibited hot-deformed Nd-Fe-B magnets [J]. Acta Mater., 2019, 167: 103 |
| 36 | Zhang P, Hu M J, Ke H B, et al. Tuning grain boundary fine structure in Nd65Ni35-added Nd-Fe-B based magnets [J]. J. Magn. Magn. Mater., 2018, 465: 246 |
| 37 | Tan C L, Bao D X, Yan M. Sintered Nd-Fe-B magnets for high temperatures [J]. Mater. Rev., 2005, 19(4): 97 |
| 37 | 谭春林, 包大新, 严 密. 高工作温度烧结钕铁硼磁体的研究现状 [J]. 材料导报, 2005, 19(4): 97 |
| 38 | El-Moneim A A, Gebert A, Uhlemann M, et al. The influence of Co and Ga additions on the corrosion behavior of nanocrystalline NdFeB magnets [J]. Corros. Sci., 2002, 44: 1857 |
| 39 | Li J J, Huang X Y, Zeng L L, et al. Tuning magnetic properties, thermal stability and microstructure of NdFeB magnets with diffusing Pr-Zn films [J]. J. Mater. Sci. Technol., 2020, 41: 81 |
| 40 | Chen H, Yang X, Sun L, et al. Effects of Ag on the magnetic and mechanical properties of sintered NdFeB permanent magnets [J]. J. Magn. Magn. Mater., 2019, 485: 49 |
| 41 | Liu W Q, Zha S S, Yue M, et al. Research progress of sintered Nd-Fe-B permanent magnets with high coercivity [J]. J. Beijing Univ. Technol., 2017, 43: 1569 |
| 41 | 刘卫强, 查善顺, 岳 明等. 高矫顽力烧结钕铁硼永磁研究进展 [J]. 北京工业大学学报, 2017, 43: 1569 |
| 42 | Zhang P, Ma T Y, Liang L P, et al. Influence of Ta intergranular addition on microstructure and corrosion resistance of Nd-Dy-Fe-B sintered magnets [J]. J. Alloys Compd., 2014, 593: 137 |
| 43 | Yu L Q, Huang C C, Yuan Y F. Effect of Nd, Dy content on magnetic properties and corrosion resistance of NdFeB [J]. Powder Metall. Ind., 2008, 18(6): 19 |
| 43 | 于濂清, 黄翠翠, 袁永锋. Nd, Dy含量对高磁能积烧结NdFeB磁性能和耐蚀性影响 [J]. 粉末冶金工业, 2008, 18(6): 19 |
| 44 | Xie Z F, Zhang S M, Gao H Q. Effects on addition of Dy and Nb on microstructure and properties of sintered NdFeB magnets [J]. Chin. Rare Earths, 2013, 34(3): 36 |
| 44 | 谢泽峰, 张时茂, 高海强. 添加Dy、Nb对烧结NdFeB磁体结构与性能的影响 [J]. 稀土, 2013, 34(3): 36 |
| 45 | Li J, Zhou L, Liu T, et al. Progress of grain boundary diffusion technique with Dy for sintered Nd-Fe-B magnet [J]. Chin. Rare Earths, 2013, 34(3): 86 |
| 45 | 李 建, 周 磊, 刘 涛等. 烧结钕铁硼晶界扩散Dy工艺进展 [J]. 稀土, 2013, 34(3): 86 |
| 46 | Liu X L, Wang X J, Liang L P, et al. Rapid coercivity increment of Nd-Fe-B sintered magnets by Dy69Ni31 grain boundary restructuring [J]. J. Magn. Magn. Mater., 2014, 370: 76 |
| 47 | Liu X L, Zhang Y J, Zhang P, et al. Microstructure evolution of Dy69Ni31-added Nd-Fe-B sintered magnets during annealing [J]. J. Magn. Magn. Mater., 2019, 486: 165260 |
| 48 | Zhou B B, Li X B, Liang X L, et al. Improvement of the magnetic property, thermal stability and corrosion resistance of the sintered Nd-Fe-B magnets with Dy80Al20 addition [J]. J. Magn. Magn. Mater., 2017, 429: 257 |
| 49 | Liang L P, Ma T Y, Zhang P, et al. Effects of Dy71.5Fe28.5 intergranular addition on the microstructure and the corrosion resistance of Nd-Fe-B sintered magnets [J]. J. Magn. Magn. Mater., 2015, 384: 133 |
| 50 | Zeng L L, Li J J, Huang X Y, et al. Thermal stability and corrosion resistance of sintered Nd-Fe-B magnets with intergranular addition of Dy80Fe13Ga7 [J]. Chin. J. Rare Met., 2019, 43: 779 |
| 50 | 曾亮亮, 李家节, 黄祥云等. 晶界添加Dy80Fe13Ga7对烧结钕铁硼热稳定性和耐腐蚀性的影响 [J]. 稀有金属, 2019, 43: 779 |
| 51 | Liang L P, Ma T Y, Zhang P, et al. Coercivity enhancement of NdFeB sintered magnets by low melting point Dy32.5Fe62Cu5.5 alloy modification [J]. J. Magn. Magn. Mater., 2014, 355: 131 |
| 52 | Fan X D, Ding G F, Chen K, et al. Whole process metallurgical behavior of the high-abundance rare-earth elements LRE (La, Ce and Y) and the magnetic performance of Nd0.75LRE0.25-Fe-B sintered magnets [J]. Acta Mater., 2018, 154: 343 |
| 53 | Binnemans K, Jones P T, Blanpain B, et al. Recycling of rare earths: A critical review [J]. J Clean. Prod., 2013, 51: 1 |
| 54 | Lei W K, Zeng Q W, Hu X J, et al. Research status and prospect of high abundant rare earth of permanent magnetic materials [J]. Nonferrous Met. Sci. Eng., 2017, 8(5): 1 |
| 54 | 雷伟凯, 曾庆文, 胡贤君等. 高丰度稀土永磁材料的研究现状与展望 [J]. 有色金属科学与工程, 2017, 8(5): 1 |
| 55 | Kim A S, Camp F E. High performance NdFeB magnets (invited) [J]. J. Appl. Phys., 1996, 79: 5035 |
| 56 | Liu W Q, Sun C, Yue M, et al. Improvement of coercivity and corrosion resistance of Nd-Fe-B sintered magnets by doping aluminium nano-particles [J]. J. Rare Earths, 2013, 31: 65 |
| 57 | Sun C, Liu W Q, Sun H, et al. Improvement of coercivity and corrosion resistance of Nd-Fe-B sintered magnets with Cu nano-particles doping [J]. J. Mater. Sci. Technol., 2012, 28: 927 |
| 58 | Zhang P, Ma T Y, Liang L P, et al. Improvement of corrosion resistance of Cu and Nb co-added Nd-Fe-B sintered magnets [J]. Mater. Chem. Phys., 2014, 147: 982 |
| 59 | Wu Y R, Ni J J, Ma T Y, et al. Corrosion resistance of Nd-Fe-B sintered magnets with intergranular addition of Cu60Zn40 powders [J]. Physica, 2010, 405B: 3303 |
| 60 | Yan M, Ni J J, Ma T Y, et al. Corrosion behavior of Al100-xCux (15≤x≤45) doped Nd-Fe-B magnets [J]. Mater. Chem. Phys., 2011, 126: 195 |
| 61 | Zeng H X, Wang Q X, Zhang J S, et al. Grain boundary diffusion treatment of sintered NdFeB magnets by low cost La-Al-Cu alloys with various Al/Cu ratios [J]. J. Magn. Magn. Mater., 2019, 490: 165498 |
| 62 | Ni J J, Zhou S T, Jia Z F, et al. Improvement of corrosion resistance in Nd-Fe-B sintered magnets by intergranular additions of Sn [J]. J. Alloys Compd., 2014, 588: 558 |
| 63 | Yang Y, Li Z J, Lv S H, et al. Effect of MgO/Mg nanopowders added to grain boundary on magnetic properties and corrosion resistance of sintered Nd-Fe-B [J]. Rare Met. Mater. Eng., 2020, 49: 1366 |
| 63 | 杨 洋, 李志杰, 吕森浩等. 晶界添加MgO/Mg纳米粉对烧结钕铁硼磁性和抗腐蚀性的影响 [J]. 稀有金属材料与工程, 2020, 49: 1366 |
| 64 | Li Z J, Wang X E, Li J Y, et al. Effects of Mg nanopowders intergranular addition on the magnetic properties and corrosion resistance of sintered Nd-Fe-B [J]. J. Magn. Magn. Mater., 2017, 442: 62 |
| 65 | Fernengel W, Rodewald W, Blank R, et al. The influence of Co on the corrosion resistance of sintered Nd-Fe-B magnets [J]. J. Magn. Magn. Mater., 1999, 196-197: 288 |
| 66 | Zhang P, Ma T Y, Liang L P, et al. Improved corrosion resistance of low rare-earth Nd-Fe-B sintered magnets by Nd6Co13Cu grain boundary restructuring [J]. J. Magn. Magn. Mater., 2015, 379: 186 |
| 67 | Isotahdon E, Huttunen-Saarivirta E, Kuokkala V T, et al. Corrosion behaviour of sintered Nd-Fe-B magnets [J]. Mater. Chem. Phys., 2012, 135: 762 |
| 68 | Zhang P, Liang L P, Jin J Y, et al. Magnetic properties and corrosion resistance of Nd-Fe-B magnets with Nd64Co36 intergranular addition [J]. J. Alloys Compd., 2014, 616: 345 |
| 69 | Hu Z H, Liu G J, Wang H J. Effect of niobium on thermal stability and impact toughness of Nd-Fe-B magnets with ultra-high intrinsic coercivity [J]. J. Rare Earths, 2011, 29: 243 |
| 70 | Yu L Q, Wen Y H, Yan M. Effects of Dy and Nb on the magnetic properties and corrosion resistance of sintered NdFeB [J]. J. Magn. Magn. Mater., 2004, 283: 353 |
| 71 | Yu L Q, Zhong X L, Zhang Y P, et al. Production and corrosion resistance of NdFeBZr magnets with an improved response to thermal variations during sintering [J]. J. Magn. Magn. Mater., 2011, 323: 1152 |
| 72 | Liang L P, Ma T Y, Wu C, et al. Coercivity enhancement of Dy-free Nd-Fe-B sintered magnets by intergranular adding Ho63.4Fe36.6 alloy [J]. J. Magn. Magn. Mater., 2016, 397: 139 |
| 73 | Xu J L, Xiao Q F, Mei D D, et al. Microstructure, corrosion resistance and formation mechanism of alumina micro-arc oxidation coatings on sintered NdFeB permanent magnets [J]. Surf. Coat. Technol., 2017, 309: 621 |
| 74 | Xu J L, Xiao Q F, Mei D D, et al. Fabrication and properties of micro-arc oxidation coatings on sintered NdFeB permanent magnets [J]. Rare Met. Mater. Eng., 2018, 47: 1059 |
| 75 | Xu J L, Xiao Q F, Mei D D, et al. Preparation and characterization of amorphous SiO2 coatings deposited by mirco-arc oxidation on sintered NdFeB permanent magnets [J]. J. Magn. Magn. Mater., 2017, 426: 361 |
| 76 | Milo?ev I, Frankel G S. Review-conversion coatings based on zirconium and/or titanium [J]. J. Electrochem. Soc., 2018, 165: C127 |
| 77 | Huang T, Wang X D, Shi X N, et al. Progress in protection technologies of NdFeB permanent magnets [J]. J. Chin. Soc. Rare Earths, 2018, 36: 394 |
| 77 | 黄 涛, 王向东, 石晓宁等. 钕铁硼稀土永磁材料腐蚀防护技术的研究进展 [J]. 中国稀土学报, 2018, 36: 394 |
| 78 | Zhang P J, Cao Y J, Sun W, et al. Synthesis and corrosion resistance of CeO2/silane composite coatings on surface of sintered NdFeB magnet [J]. Trans. Mater. Heat Treat., 2020, 41(1): 123 |
| 78 | 张鹏杰, 曹玉杰, 孙 威等. 烧结钕铁硼磁体表面CeO2/硅烷复合涂层的制备及其耐蚀性能 [J]. 材料热处理学报, 2020, 41(1): 123 |
| 79 | Zaferani S H, Peikari M, Zaarei D, et al. Using silane films to produce an alternative for chromate conversion coatings [J]. Corrosion, 2013, 69: 372 |
| 80 | Gao Z Q, Zhang D W, Li X G, et al. Current status, opportunities and challenges in chemical conversion coatings for zinc [J]. Colloids Surf., 2018, 546A: 221 |
| 81 | Gao Z Q, Zhang D W, Liu Z Y, et al. Formation mechanisms of environmentally acceptable chemical conversion coatings for zinc: A review [J]. J. Coat. Technol. Res., 2019, 16: 1 |
| 82 | Zhang X, Sloof W G, Hovestad A, et al. Characterization of chromate conversion coatings on zinc using XPS and SKPFM [J]. Surf. Coat. Technol., 2005, 197: 168 |
| 83 | Ouyang Y B, Qiu R, Xiao Y M, et al. Magnetic fluid based on mussel inspired chemistry as corrosion-resistant coating of NdFeB magnetic material [J]. Chem. Eng. J., 2019, 368: 331 |
| 84 | He W T, Zhu L Q, Chen H N, et al. Electrophoretic deposition of graphene oxide as a corrosion inhibitor for sintered NdFeB [J]. Appl. Surf. Sci., 2013, 279: 416 |
| 85 | Zhang P J, Xu G Q, Liu J Q, et al. Effect of pretreating technologies on the adhesive strength and anticorrosion property of Zn coated NdFeB specimens [J]. Appl. Surf. Sci., 2016, 363: 499 |
| 86 | Li Y, Zhu L Q, Li W P, et al. Electrodeposition and properties of copper layer on NdFeB device [J]. J. Mater. Eng., 2017, 45(6): 55 |
| 86 | 李 悦, 朱立群, 李卫平等. 钕铁硼器件表面电沉积铜层及性能 [J]. 材料工程, 2017, 45(6): 55 |
| 87 | Chen J, Xu B J, Ling G P. Amorphous Al-Mn coating on NdFeB magnets: Electrodeposition from AlCl3-EMIC-MnCl2 ionic liquid and its corrosion behavior [J]. Mater. Chem. Phys., 2012, 134: 1067 |
| 88 | Ding J J, Xu B J, Ling G P. Al-Mn coating electrodeposited from ionic liquid on NdFeB magnet with high hardness and corrosion resistance [J]. Appl. Surf. Sci., 2014, 305: 309 |
| 89 | Luo C, Qiu X M, Ruan Y, et al. Effect of Bi addition on the corrosion resistance and mechanical properties of sintered NdFeB permanent magnet/steel soldered joints [J]. Mater. Sci. Eng., 2020, A792: 139832 |
| 90 | Zhang P J, Wu Y C, Cao Y J, et al. Effects of pretreatment technologies on structure and properties of Al coatings on sintered NdFeB substrates via vacuum evaporation [J]. China Surf. Eng., 2016, 29(4): 49 |
| 90 | 张鹏杰, 吴玉程, 曹玉杰等. 前处理工艺对NdFeB表面真空蒸镀Al薄膜结构及性能的影响 [J]. 中国表面工程, 2016, 29(4): 49 |
| 91 | Liu J Q, Cao Y J, Zhang P J, et al. Preparation and properties of Al coating on sintered NdFeB magnet surface via vacuum evaporations [J]. Trans. Mater. Heat Treat., 2017, 38(3): 159 |
| 91 | 刘家琴, 曹玉杰, 张鹏杰等. 钕铁硼表面真空蒸镀Al膜的制备及其性能 [J]. 材料热处理学报, 2017, 38(3): 159 |
| 92 | Chen J, Yang H Y, Xu G Q, et al. Phosphating passivation of vacuum evaporated Al/NdFeB magnets boosting high anti-corrosion performances [J]. Surf. Coat. Technol., 2020, 339: 126115 |
| 93 | Tao L, Li H Q, Huang Y Q, et al. Structure and corrosion resistance of SiC thin film coated on NdFeB by magnetron sputtering [J]. J. Hefei Univ. Technol. (Nat. Sci.), 2015, 38: 1040 |
| 93 | 陶 磊, 李合琴, 黄依琴等. NdFeB磁控溅射SiC薄膜的结构及耐腐蚀性能 [J]. 合肥工业大学学报(自然科学版), 2015, 38: 1040 |
| 94 | Hu F, Dai M J, Lin S S, et al. Influences of cycles argon ion bombardment on structure and properties of Al films deposited by magnetron sputtering [J]. China Surf. Eng., 2015, 28(1): 49 |
| 94 | 胡 芳, 代明江, 林松盛等. 循环氩离子轰击对磁控溅射铝膜结构和性能的影响 [J]. 中国表面工程, 2015, 28(1): 49 |
| 95 | Mao S D, Yang H X, Song Z L, et al. Corrosion behaviour of sintered NdFeB deposited with an aluminium coating [J]. Corros. Sci., 2011, 53: 1887 |
| 96 | Zhang P J, Liu J Q, Xu G Q, et al. Anticorrosive property of Al coatings on sintered NdFeB substrates via plasma assisted physical vapor deposition method [J]. Surf. Coat. Technol., 2015, 282: 86 |
| 97 | Mao S D, Yang H X, Li J L, et al. Corrosion properties of aluminium coatings deposited on sintered NdFeB by ion-beam-assisted deposition [J]. Appl. Surf. Sci., 2011, 257: 5581 |
| 98 | Su Y A, Wan P S, Guo H M. Corrosion mechanism and surface protective technology of sintered Nd-Fe-Boron permanent magnetic material [J]. Mater. Rev., 2004, 18(S3): 257 |
| 98 | 苏永安, 万潘顺, 郭惠铭. 烧结钕铁硼永磁材料腐蚀机理与表面防护技术 [J]. 材料导报, 2004, 18(S3): 257 |
| 99 | Chaudhary V, Mantri S A, Ramanujan R V, et al. Additive manufacturing of magnetic materials [J]. Prog. Mater. Sci., 2020, 114: 100688 |
| 100 | Périgo E A, Jacimovic J, Ferré F G, et al. Additive manufacturing of magnetic materials [J]. Addit. Manuf., 2019, 30: 100870 |
| 101 | He J Z, Lin T, Shao H P, et al. 3D printing of NdFeB rare earth permanent magnet [J]. Chin. J. Rare Met., 2018, 42: 657 |
| 101 | 何建壮, 林 涛, 邵慧萍等. 稀土永磁钕铁硼材料的3D打印研究现状 [J]. 稀有金属, 2018, 42: 657 |
| 102 | Borkar T, Conteri R, Chen X, et al. Laser additive processing of functionally-graded Fe-Si-B-Cu-Nb soft magnetic materials [J]. Mater. Manuf. Process., 2017, 32: 1581 |
| 103 | Chaudhary V, Kumar Yadav N M S K, Mantri S A, et al. Additive manufacturing of functionally graded Co-Fe and Ni-Fe magnetic materials [J]. J. Alloys Compd., 2020, 823: 153817 |
| 104 | Mazeeva A K, Staritsyn M V, Bobyr V V, et al. Magnetic properties of Fe-Ni permalloy produced by selective laser melting [J]. J. Alloys Compd., 2020, 814: 152315 |
| 105 | Liu Z Q, Meyers M A, Zhang Z F, et al. Functional gradients and heterogeneities in biological materials: Design principles, functions, and bioinspired applications [J]. Prog. Mater. Sci., 2017, 88: 467 |
| 106 | Zhang C, Chen F, Huang Z F, et al. Additive manufacturing of functionally graded materials: A review [J]. Mater. Sci. Eng., 2019, A764: 138209 |
/
| 〈 |
|
〉 |