Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy
Received date: 2020-07-23
Revised date: 2020-10-30
Online published: 2020-11-16
Supported by
National Key Research and Development Program of China(2016YFE0111400)
To improve the properties of Ti-Ni shape memory alloys (SMAs), a third element can be added to them and assisted by a heat treatment process. After the Ni-rich Ti-Ni SMAs are doped with a small amount of Zr, the parent phase of the alloy is observed to exhibit enhanced stability; further, the alloys exhibit improved yield strength, elongation, and memory performance. The effects of the composition and annealing processes on the phase transformation behaviors and mechanical properties of the Ti-Ni-Zr SMAs have been studied; however, the microstructure, tensile properties, and shape memory behaviors of the aged Ti-Ni-Zr SMAs remain to be investigated. In this work, a Ni-rich Ti-50.8Ni-0.1Zr alloy could be obtained by doping the Ti-Ni alloys with 0.1%Zr (atomic fraction). The effects of the ageing processes on the microstructure, tensile properties, and shape memory behaviors of the alloy were investigated through TEM and tensile tests. The Ti3Ni4 precipitates in the Ti-50.8Ni-0.1Zr alloy samples aged at 300, 400, and 500oC exhibit morphologies of fine particles, lenticular particles, and long strips, respectively. The effect of ageing temperature on the morphology, size, and dispersion of precipitates is greater than that of the ageing time. The alloy exhibited enhanced strength but reduced ductility after the ageing treatment. With the increasing ageing time (tag), the tensile strength (Rm) increased and the percentage elongation (A) decreased when considering the alloy sample aged at 300oC. In case of the alloy sample aged at 400oC, Rm initially increased and subsequently decreased, whereas A initially decreased and subsequently increased. The alloy sample aged at 500oC exhibited a reduced Rm but an enhanced A. The alloy samples aged at 300oC for 1-50 h or at 400oC for 1 h exhibited superelasticity, whereas those aged at 400oC for 5-50 h or 500oC for 1-50 h exhibited the shape memory effect. In the alloy samples aged at 300oC, higher tag values resulted in enhanced energy dissipation and lower critical stress values for stress-induced martensite transformation. Alloy ageing at 400oC or 500oC resulted in lower critical stress values for martensite reorientation and lower energy dissipation.
Junjie YE , Zhirong HE , Kungang ZHANG , Yuqing DU . Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy[J]. Acta Metall Sin, 2021 , 57(6) : 717 -724 . DOI: 10.11900/0412.1961.2020.00276
| 1 | Jin M J, Song Y W, Wang X D, et al. Ultrahigh damping capacity achieved by modulating R phase in Ti49.2Ni50.8 shape memory alloy wires [J]. Scr. Mater., 2020, 183: 102 |
| 2 | Zheng Y, Dong Y, Li Y H. Resilience and life-cycle performance of smart bridges with shape memory alloy (SMA)-cable-based bearings [J]. Constr. Build. Mater., 2018, 158: 389 |
| 3 | Azadpour F, Maghsoudi A A. Experimental and analytical investigation of continuous RC beams strengthened by SMA strands under cyclic loading [J]. Constr. Build. Mater., 2020, 239: 117730 |
| 4 | Jani J M, Leary M, Subic A, et al. A review of shape memory alloy research, applications and opportunities [J]. Mater. Des., 2014, 56: 1078 |
| 5 | Soother D K, Daudpoto J, Chowdhry B S. Challenges for practical applications of shape memory alloy actuators [J]. Mater. Res. Express, 2020, 7: 073001 |
| 6 | Sun L, Huang W M, Ding Z, et al. Stimulus-responsive shape memory materials: A review [J]. Mater. Des., 2012, 33: 577 |
| 7 | Shariat B S, Meng Q L, Mahmud A S, et al. Functionally graded shape memory alloys: Design, fabrication and experimental evaluation [J]. Mater. Des., 2017, 124: 225 |
| 8 | He Z R, Zhou J E, Miyazaki S. Relationship between transformation behaviors and Ni content in solution-aged Ti-Ni alloys [J]. Acta Metall. Sin., 2003, 39: 617 |
| 8 | 贺志荣, 周敬恩, 宫崎修一. 固溶时效态Ti-Ni合金相变行为与Ni含量的关系 [J]. 金属学报, 2003, 39: 617 |
| 9 | He Z R, Wang F, Wang Y S, et al. Effects of V and Cr on transformation and deformation characteristics of Ti-Ni superelastic alloy [J]. Acta Metall. Sin., 2007, 43: 1293 |
| 9 | 贺志荣, 王 芳, 王永善等. V和Cr对Ti-Ni超弹性合金相变和形变特性的影响 [J]. 金属学报, 2007, 43: 1293 |
| 10 | Bozzolo G, Noebe R D, Mosca H O. Site preference of ternary alloying additions to NiTi: Fe, Pt, Pd, Au, Al, Cu, Zr and Hf [J]. J. Alloys Compd., 2005, 389: 80 |
| 11 | Yuan Z S, Lin D Z, Cui Y, et al. Research progress on the phase transformation behavior, microstructure and property of NiTi based high temperature shape memory alloys [J]. Rare Met. Mater. Eng., 2018, 47: 2269 |
| 11 | 袁志山, 吝德智, 崔 跃等. NiTi基高温记忆合金相变行为与组织性能研究进展 [J]. 稀有金属材料与工程, 2018, 47: 2269 |
| 12 | He Z R, Wang F, Zhou J E. Effect of Ni content and heat treatment on phase transformation and deformation behavior of Ti-Ni shape memory alloys [J]. Heat Treat. Met, 2006, 31(9): 17 |
| 12 | 贺志荣, 王 芳, 周敬恩. Ni含量和热处理对Ti-Ni形状记忆合金相变和形变行为的影响 [J]. 金属热处理, 2006, 31(9): 17 |
| 13 | Wang H Z. Microstructure and strain recovery characteristic of proton irradiated NiTi alloys [D]. Harbin: Harbin Institute of Technology, 2019 |
| 13 | 王海振. 质子辐照NiTi合金的微观组织结构与应变恢复特性 [D]. 哈尔滨: 哈尔滨工业大学, 2019 |
| 14 | Frenzel J, George E P, Dlouhy A, et al. Influence of Ni on martensitic phase transformations in NiTi shape memory alloys [J]. Acta Mater., 2010, 58: 3444 |
| 15 | Tong Y X, Liu J T, Chen F, et al. Effect of aging on martensitic transformation and superelasticity of TiNiCr shape memory alloy [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2598 |
| 16 | He Z R, Wang F. Effect of heat treatment on transformation behavior of low-temperature superelasticity alloy Ti-50.8Ni-0.3Cr [J]. Acta Metall. Sin., 2010, 46: 329 |
| 16 | 贺志荣, 王 芳. 热处理对Ti-Ni-Cr低温超弹性合金相变行为的影响 [J]. 金属学报, 2010, 46: 329 |
| 17 | Feng Z W, Qian D F, Gao B D, et al. Research on properties of TiNiZr shape memory alloys [J]. Chin. J. Rare Met., 2001, 25: 47 |
| 17 | 冯昭伟, 千东范, 高宝东等. TiNiZr形状记忆合金的性能研究 [J]. 稀有金属, 2001, 25: 47 |
| 18 | Feng Z W, Cui Y, Shang Z Y, et al. Development of NiTiZr high temperature shape memory alloys [J]. Mater. Rev., 2016, 30: 616 |
| 18 | 冯昭伟, 崔 跃, 尚再艳等. 镍钛锆高温形状记忆合金的研究进展 [J]. 材料导报, 2016, 30: 616 |
| 19 | Yi X Y, Wang H Z, Sun B, et al. The crystallization process, microstructure, martensitic transformation and mechanical properties of Ti-Ni-Zr alloy ribbons [J]. J. Alloys Compd., 2019, 778: 542 |
| 20 | Li Q Q, Ma Y H, Li Y. Microstructure, phase transformation and shape memory properties of Ni-Ti-Zr alloys [J]. Foundry, 2019, 68: 1204 |
| 20 | 李启泉, 马悦辉, 李 岩. Ni-Ti-Zr合金组织、相变与形状记忆性能 [J]. 铸造, 2019, 68: 1204 |
| 21 | Malykhin S V, Kondratenko V V, АKopylets I, et al. Structure and phase formation features of Ti-Zr-Ni quasicrystalline films under heating [J]. J. Nano-Electron. Phys., 2019, 11: 03009 |
| 22 | Atli K C. The effect of tensile deformation on the damping capacity of NiTi shape memory alloy [J]. J. Alloys Compd., 2016, 679: 260 |
| 23 | Yi X Y, Gao W H, Wang H Z, et al. Dependence of aging parameters on precipitation behavior, martensitic transformation and mechanical properties of the aged Ni-Ti alloy under super high pressure [J]. Mater. Sci. Eng., 2018, A736: 354 |
| 24 | Holec D, Bojda O, Dlouhy A. Ni4Ti3 precipitate structures in Ni-rich NiTi shape memory alloys [J]. Mater. Sci. Eng., 2006, A481-482: 462 |
| 25 | Santamarta R, Arróyave R, Pons J, et al. TEM study of structural and microstructural characteristics of a precipitate phase in Ni-rich Ni-Ti-Hf and Ni-Ti-Zr shape memory alloys [J]. Acta Mater., 2013, 61: 6191 |
| 26 | Wang Q, He Z R, Shao D W. Effects of Solution annealing and aging on tensile property and microstructure of Ti-Ni-Cr shape memory alloy [J]. Rare Met. Mater. Eng., 2012, 41: 1191 |
| 26 | 王 启, 贺志荣, 邵大伟. 固溶-时效处理对Ti-Ni-Cr形状记忆合金拉伸性能和显微组织的影响 [J]. 稀有金属材料与工程, 2012, 41: 1191 |
| 27 | Sandu A M, Tsuchiya K, Tabuchi M, et al. Microstructural evolution during isothermal aging in Ni-Rich Ti-Zr-Ni shape memory alloys [J]. Mater. Trans., 2007, 48: 432 |
| 28 | Sandu A, Tsuchiya K, Yamamoto S, et al. Effect of aging on microstructure and martensitic transformation in Ti-Zr-Ni shape memory alloys [J]. Mater. Sci. Forum, 2007, 539-543: 3163 |
| 29 | Chang B C, Shaw J A, Iadicola M A. Thermodynamics of shape memory alloy wire: Modeling, experiments, and application [J]. Continuum Mech. Thermodyn., 2006, 18: 83 |
| 30 | Chumlyakov Y I, Kireeva I V, Karaman I, et al. Orientational dependence of shape memory effects and superelasticity in CoNiGa, NiMnGa, CoNiAl, FeNiCoTi, and TiNi single crystals [J]. Russ. Phys. J., 2004, 47: 893 |
/
| 〈 |
|
〉 |