Research paper

The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation

  • Jinliang WANG ,
  • Chenchong WANG ,
  • Minghao HUANG ,
  • Jun HU ,
  • Wei XU
Expand
  • State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
XU Wei, professor, Tel: (024)83680246, E-mail: xuwei@ral.neu.edu.cn

Received date: 2020-08-06

  Revised date: 2020-09-30

  Online published: 2020-11-16

Supported by

National Natural Science Foundation of China(U1808208);National Key Research and Development Program of China(2017YFB0703001)

Abstract

Pre-deformation with low strain can effectively control the thermal stability of metastable austenite. Till now, research has mainly focused on the effect of pre-deformation on martensitic transformation at one or more temperatures. However, research is still lacking on the effect of pre-deformation on the temperature at which martensite is formed (Ms), the final martensite content, and the transformational kinetics during continuous cooling. Furthermore, the mechanism underlying how pre-deformation affects martensitic transformation has not been reported. In this work, the influence rule and the corresponding effect of pre-deformation with low strain on martensitic transformation induced by temperature under continuous cooling from 300 K to 4 K was studied with 321 stainless steel samples by using the quasi-in-situ observation technique. The results show that Ms and the final amount of martensite increased under pre-deformation with low strain, and the martensitic transformation during continuous cooling was simultaneously accelerated. The quasi-in-situ observation demonstrated that the slip bands introduced by pre-deformation effectively provided nucleation sites for ε-martensite transformation. Accordingly, the formed ε-martensite increased the number of α'-martensite nucleation sites during continuous cooling, and finally promoted α'-martensite transformation. This builds on the theory proposed by other researchers that the dislocation defects introduced by pre-deformation directly provide the nucleation sites for α'-martensite transformation, and thus, promote martensitic transformation. In addition, by analyzing the nucleation behavior and nucleation priority at slip band defects, it is shown that the nucleation behavior of slip bands introduced by the pre-deformation was similar to that of faulted austenite induced by temperature. However, it is worth noting that the slip bands introduced by pre-deformation had a relatively higher nucleation priority. The crystallography of α'-martensite in the pre-deformed samples was analyzed, and it was found that the slip bands effectively changed the variant selection of α'-martensite so that the texture of α'-martensite was modified. This study advances the existing theory of martensitic transformation and provides theoretical guidance for the proactive control of temperature-induced martensitic transformation.

Cite this article

Jinliang WANG , Chenchong WANG , Minghao HUANG , Jun HU , Wei XU . The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. Acta Metall Sin, 2021 , 57(5) : 575 -585 . DOI: 10.11900/0412.1961.2020.00292

References

1 Zhou T P, Wang C Y, Wang C, et al. Austenite stability and deformation-induced transformation mechanism in cold-rolled medium-Mn steel [J]. Mater. Sci. Eng., 2020, A798: 140147
2 He B B, Pan S, Huang M X. Extra work hardening in room-temperature quenching and partitioning medium Mn steel enabled by intercritical annealing [J]. Mater. Sci. Eng., 2020, A797: 140106
3 de Knijf D D, Petrov R, F?jer C, et al. Effect of fresh martensite on the stability of retained austenite in quenching and partitioning steel [J]. Mater. Sci. Eng., 2014, A615: 107
4 Xiong X C, Chen B, Huang M X, et al. The effect of morphology on the stability of retained austenite in a quenched and partitioned steel [J]. Scr. Mater., 2013, 68: 321
5 Speer J, Matlock D K, De Cooman B C, et al. Carbon partitioning into austenite after martensite transformation [J]. Acta Mater., 2003, 51: 2611
6 Yang G, Huang C X, Wu S D, et al. Strain-induced martensitic transformation in 304L austenitic stainless steel under ECAP deformation [J]. Acta Metall. Sin., 2009, 45: 906
6 杨 钢, 黄崇湘, 吴世丁等. ECAP变形下304L奥氏体不锈钢的形变诱导马氏体相变 [J]. 金属学报, 2009, 45: 906
7 Yang F, Luo H W, Dong H. Effects of intercritical annealing temperature on the tensile behavior of cold rolled 7Mn steel and the constitutive modeling [J]. Acta Metall. Sin., 2018, 54: 859
7 阳 锋, 罗海文, 董 瀚. 退火温度对冷轧7Mn钢拉伸行为的影响及模拟研究 [J]. 金属学报, 2018, 54: 859
8 Shao C W, Hui W J, Zhang Y J, et al. Microstructure and mechanical properties of a novel cold rolled medium-Mn steel with superior strength and ductility [J]. Acta Metall. Sin., 2019, 55: 191
8 邵成伟, 惠卫军, 张永健等. 一种新型高强度高塑性冷轧中锰钢的组织和力学性能 [J]. 金属学报, 2019, 55: 191
9 van der Zwaag S, Zhao L, Kruijver S O, et al. Thermal and mechanical stability of retained austenite in aluminum-containing multiphase TRIP steels [J]. ISIJ Int., 2002, 42: 1565
10 Garrison Jr W M, Brooks J A. The thermal and mechanical stability of austenite in the low carbon martensitic steel PH 13-8 [J]. Mater. Sci. Eng., 1991, A149: 65
11 Xu W, Huang M H, Wang J L, et al. Review: Relations between metastable austenite and fatigue behavior of steels [J]. Acta Metall. Sin., 2020, 56: 459
11 徐 伟, 黄明浩, 王金亮等. 综述: 钢中亚稳奥氏体组织与疲劳性能关系 [J]. 金属学报, 2020, 56: 459
12 van Bohemen S M C, Sietsma J. Effect of composition on kinetics of athermal martensite formation in plain carbon steels [J]. Mater. Sci. Technol., 2009, 25: 1009
13 Seo E J, Cho L, Estrin Y, et al. Microstructure-mechanical properties relationships for quenching and partitioning (Q&P) processed steel [J]. Acta Mater., 2016, 113: 124
14 Chen S, Wang C C, Shan L Y, et al. Revealing the conditions of bainitic transformation in quenching and partitioning steels [J]. Metall. Mater. Trans., 2019, 50A: 4037
15 Song C H, Yu H, Li L L, et al. The stability of retained austenite at different locations during straining of I&Q&P steel [J]. Mater. Sci. Eng., 2016, A670: 326
16 Le Houillier R, Bégin G, Dubé A. A study of the peculiarities of austenite during the formation of bainite [J]. Metall. Trans., 1971, 2: 2645
17 Brofman P J, Ansell G S. On the effect of fine grain size on the Ms temperature in Fe-27Ni-0.025C alloys [J]. Metall. Trans., 1983, 14A: 1929
18 Yang H S, Bhadeshia H K D H. Austenite grain size and the martensite-start temperature [J]. Scr. Mater., 2009, 60: 493
19 Fiedler H C, Averbach B L, Cohen M. Effect of deformation on the martensitic transformation in stainless steels [J]. Trans. ASM, 1955, 47: 267
20 Breedis J F. Influence of dislocation substructure on the martensitic transformation in stainless steel [J]. Acta Metall., 1965, 13: 239
21 Lagneborgj R. The martensite transformation in 18%Cr-8%Ni steels [J]. Acta Metall., 1964, 12: 823
22 Strife J R, Carr M J, Ansell G S. The effect of austenite prestrain above the Md temperature on the martensitic transformation in Fe-Ni-Cr-C alloys [J]. Metall. Trans., 1977, 8A: 1471
23 Thadhani N N, Meyers M A. Kinetics of isothermal martensitic transformation [J]. Prog. Mater. Sci., 1986, 30: 1
24 Pati S R, Cohen M. Kinetics of isothermal martensitic transformations in an iron-nickel-manganese alloy [J]. Acta Metall., 1971, 19: 1327
25 Olson G B, Cohen M. A general mechanism of martensitic nucleation: Part I. General concepts and the FCC→HCP transformation [J]. Metall. Trans., 1976, 7A: 1897
26 Olson G B, Cohen M. A general mechanism of martensitic nucleation: Part II. FCC→BCC and other martensitic transformations [J]. Metall. Trans., 1976, 7A: 1905
27 Tian Y, Lin S, Ko J Y P, et al. Micromechanics and microstructure evolution during in situ uniaxial tensile loading of TRIP-assisted duplex stainless steels [J]. Mater. Sci. Eng., 2018, A734: 281
28 Olson G B, Cohen M. Stress-assisted isothermal martensitic transformation: Application to TRIP steels [J]. Metall. Trans., 1982, 13A: 1907
29 Lecroisey F, Pineau A. Martensitic transformations induced by plastic deformation in the Fe-Ni-Cr-C system [J]. Metall. Mater. Trans., 1972, 3B: 391
30 Murr L E, Staudhammer K P, Hecker S S. Effects of strain state and strain rate on deformation-induced transformation in 304 stainless steel: Part II. Microstructural study [J]. Metall. Trans., 1982, 13A: 627
31 Wang J L, Xi X H, Li Y, et al. New insights on nucleation and transformation process in temperature-induced martensitic transformation [J]. Mater. Charact., 2019, 151: 267
32 Wang J L, Huang M H, Xi X H, et al. Characteristics of nucleation and transformation sequence in deformation-induced martensitic transformation [J]. Mater. Charact., 2020, 163: 110234
33 Tian Y, Lienert U, Borgenstam A, et al. Martensite formation during incremental cooling of Fe-Cr-Ni alloys: An in-situ bulk X-ray study of the grain-averaged and single-grain behavior [J]. Scr. Mater. 2017, 136: 124
34 Kitahara H, Ueji R, Tsuji N, et al. Crystallographic features of lath martensite in low-carbon steel [J]. Acta Mater., 2006, 54: 1279
35 Jafarian H, Borhani E, Shibata A, et al. Variant selection of martensite transformation from ultrafine-grained austenite in Fe-Ni-C alloy [J]. J. Alloys Compd., 2013, 577: S668
36 Chiba T, Miyamoto G, Furuhara T. Variant selection of lenticular martensite by ausforming [J]. Scr. Mater., 2012, 67: 324
37 Tian Y, Borgenstam A, Hedstr?m P. Comparing the deformation-induced martensitic transformation with the athermal martensitic transformation in Fe-Cr-Ni alloys [J]. J. Alloys Compd., 2018, 766: 131
38 Swarr T, Krauss G. The effect of structure on the deformation of as-quenched and tempered martensite in an Fe-0.2 pct C alloy [J]. Metall. Trans., 1976, 7A: 41
39 Inoue T, Matsuda S, Okamura Y, et al. The fracture of a low carbon tempered martensite [J]. Trans. Japan Inst. Met., 1970, 11: 36
40 Kelly P M. The martensite transformation in steels with low stacking fault energy [J]. Acta Metall., 1965, 13: 635
41 Morito S, Tanaka H, Konishi R, et al. The morphology and crystallography of lath martensite in Fe-C alloys [J]. Acta Mater., 2003, 51: 1789
42 Schramm R E, Reed R P. Stacking fault energies of seven commercial austenitic stainless steels [J]. Metall. Trans., 1975, 6A: 1345
43 Cohen M, Olson G B. Martensitic nucleation and the role of the nucleation defect [J]. Suppl. Trans. JIM, 1976, 17: 93
44 Kaufman L, Cohen M. Thermodynamics and kinetics of martensitic transformations [J]. Prog. Met. Phys., 1958, 7: 165
45 Gu Q, van Humbeeck J, Delaey L. Review on the martensitic transformation and shape memory effect in Fe-Mn-Si alloys [J]. J. Phys. IV, 1994, 4: 135
46 Hoshino Y, Nakamura S, Ishikawa N, et al. In-situ observation of partial dislocation motion during γε transformation in a Fe-Mn-Si Shape memory alloy [J]. Mater. Trans., JIM, 1992, 33: 253
47 Shimizu K, Oka M, Wayman C M. The association of martensite platelets with austenite stacking faults in an Fe-8Cr-1C alloy [J]. Acta Metall., 1970, 18: 1005
48 Sato A, Kasuga H, Mori T. Effect of external stress on the γεα martensitic transformation examined by a double tensile deformation [J]. Acta Metall., 1980, 28: 1223
49 Li X, Chen L Q, Zhao Y, et al. Influence of manganese content on ε-/α′-martensitic transformation and tensile properties of low-C high-Mn TRIP steels [J]. Mater. Des., 2018, 142: 190
50 Masumura T, Nakada N, Tsuchiyama T, et al. The difference in thermal and mechanical stabilities of austenite between carbon- and nitrogen-added metastable austenitic stainless steels [J]. Acta Mater., 2015, 84: 330
51 Pisarik S T, van Aken D C. Crystallographic orientation of the εα′ martensitic (athermal) transformation in a FeMnAlSi steel [J]. Metall. Mater. Trans., 2014, 45A: 3173
Outlines

/