Research paper

Precipitation Strengthening Model of AA 7055 Aluminium Alloy

  • Junzhou CHEN ,
  • Liangxing LV ,
  • Liang ZHEN ,
  • Shenglong DAI
Expand
  • 1.AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
    2.Beijing Engineering Research Center of Advanced Aluminum Alloys and Applications, Beijing 100095, China
    3.School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China

Received date: 2020-08-26

  Revised date: 2020-09-30

  Online published: 2020-11-16

Abstract

AA 7055 aluminium alloy has been widely applied in aviation and aerospace applications, especially after T7751 heat treatment, owing to its excellent properties, such as high strength and good stress corrosion and fatigue resistances. For 7XXX aluminium alloys, aging hardening is the main strengthening mechanism, and the hardening effect is determined by the microstructural features of precipitates including morphology, composition, volume fraction, nucleation density, and size distribution. To further improve the property of alloy and expand the breadth of applications, establishing a precise predictive model regarding strength performance associated with the precipitates is necessary. In this work, based on the quantitative results of the precipitates obtained using small angle X-ray scattering techniques, the strengthening models of AA 7055 Al alloys aged at 120 and 160oC were investigated. Precipitation kinetics show that at the early stages of aging, the evolution of radius and the half thickness of plate-like precipitates are both linear with t1/2 (t means the aging time). Conversely, at the later stages of aging, they are linear with t1/3. The evolution of the volume fraction of the precipitates follows a JMA (Johnson-Mehl-Avrami)-type equation. Strength contributions from both GPI zones and η' precipitates are considered. Moreover, strengthening modeling considered both the modulus and coherency strain strengthening mechanisms of these two kinds of precipitates that had been built for the AA 7055 Al alloy aged at 120 and 160oC. Therefore, yield strength during aging can be predicted.

Cite this article

Junzhou CHEN , Liangxing LV , Liang ZHEN , Shenglong DAI . Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. Acta Metall Sin, 2021 , 57(3) : 353 -362 . DOI: 10.11900/0412.1961.2020.00328

References

1 Williams J C, Starke Jr E A. Progress in structural materials for aerospace systems [J]. Acta Mater., 2003, 51: 5775
2 Deschamps A, Livet F, Bréchet Y. Influence of predeformation on ageing in an Al-Zn-Mg alloy-I. Microstructure evolution and mechanical properties [J]. Acta Mater., 1998, 47: 281
3 Liu J. Advanced aluminium and hybrid aerostructures for future aircraft [J]. Mater. Sci. Forum, 2006, 519-521: 1233
4 Cong F G, Zhao G, Tian N, et al. Research progress and development trend of strengthening-toughening of ultra-high strength 7XXX aluminum alloy [J]. Light Alloy Fabr. Technol., 2012, 40(10): 23
4 丛福官, 赵 刚, 田 妮等. 7XXX系超高强铝合金的强韧化研究进展及发展趋势 [J]. 轻合金加工技术, 2012, 40(10): 23
5 Du Z W, Sun Z M, Shao B L, et al. Quantitative evaluation of precipitates in an Al-Zn-Mg-Cu alloy after isothermal aging [J]. Mater. Charact., 2006, 56: 121
6 Deschamps A, Bréchet Y. Influence of predeformation and ageing of an Al-Zn-Mg alloy-II. Modeling of precipitation kinetics and yield stress [J]. Acta Mater., 1998, 47: 293
7 Starink M J, Wang P, Sinclair I, et al. Microstructure and strengthening of Al-Li-Cu-Mg alloys and MMCS: II. Modelling of yield strength [J]. Acta Mater., 1999, 47: 3855
8 Starink M J, Wang S C. A model for the yield strength of overaged Al-Zn-Mg-Cu alloys [J]. Acta Mater., 2003, 51: 5131
9 Liu G, Zhang G J, Ding X D, et al. Modeling the strengthening response to aging process of heat-treatable aluminum alloys containing plate/disc- or rod/needle-shaped precipitates [J]. Mater. Sci. Eng., 2003, A344: 113
10 Chen J Z, Lv L X, Zhen L, et al. Quantitative characterization on the precipitation of AA 7055 Aluminum Alloy by SAXS [J]. Acta. Metall. Sin., 2017, 53: 897
10 陈军洲, 吕良星, 甄 良等. AA 7055铝合金时效析出过程的小角度X射线散射定量表征 [J]. 金属学报, 2017, 53: 897
11 Liu G. Modeling and experimental investigation into the mechanical properties of aged aluminum alloys containing multi-scaled second phase particles [D]. Xi'an: Xi'an Jiao Tong University, 2002
11 刘 刚. 含多尺度第二相时效铝合金力学性能的模型化与实验研究 [D]. 西安: 西安交通大学, 2002
12 Russell K C. Nucleation in solids: The induction and steady state effects [J]. Adv. Colloid Interface Sci., 1980, 13: 205
13 Werenskiold J C, Deschamps A, Bréchet Y. Characterization and modeling of precipitation kinetics in an Al-Zn-Mg alloy [J]. Mater. Sci. Eng., 2000, A293: 267
14 Horvay G, Cahn J W. Dendritic and spheroidal growth [J]. Acta Metall., 1961, 9: 695
15 Ferrante M, Doherty R D. Influence of interfacial properties on the kinetics of precipitation and precipitate coarsening in aluminium-silver alloys [J]. Acta Metall., 1979, 27: 1603
16 Davies C K L, Nash P, Stevens R N. The effect of volume fraction of precipitate on Ostwald ripening [J]. Acta Metall., 1980, 28: 179
17 Feng D. Physics of Metals. Volume II Phase Transition [M]. Beijing: Science Press, 1990: 150
17 冯 端. 金属物理学. 第二卷 相变 [M]. 北京: 科学出版社, 1990: 150
18 Shercliff H R, Ashby M F. A process model for age hardening of aluminium alloys-I. The model [J]. Acta Metall. Mater., 1990, 38: 1789
19 Du Z W. Precipitation and strengthening of 7000 serials and their Li containing aluminum alloys [D]. Beijing: Beihang University, 2005
19 杜志伟. Al-Zn-Mg-Cu及其含Li合金沉淀析出过程显微结构演化的研究 [D]. 北京: 北京航空航天大学, 2005
20 Berg L K, Gj?nnes J, Hansen V, et al. GP-zones in Al-Zn-Mg alloys and their role in artificial aging [J]. Acta Mater., 2001, 49: 3443
21 Sha G, Cerezo A. Early-stage precipitation in Al-Zn-Mg-Cu alloy (7050) [J]. Acta Mater., 2004, 52: 4503
22 Yang D Z. Dislocations and Strengthening Mechanisms of Metals [M]. Harbin: Harbin Institute of Technology Press, 1991: 178
22 杨德庄. 位错与金属强化机制 [M]. 哈尔滨: 哈尔滨工业大学出版社, 1991: 178
23 Zhu A W, Starke Jr E A. Strengthening effect of unshearable particles of finite size: A computer experimental study [J]. Acta Mater., 1999, 47: 3263
24 Chen J Z, Zhen L, Yang S J, et al. Investigation of precipitation behavior and related hardening in AA 7055 aluminum alloy [J]. Mater. Sci. Eng., 2009, A500: 34
25 Song M. Modeling the hardness and yield strength evolutions of aluminum alloy with rod/needle-shaped precipitates [J]. Mater. Sci. Eng., 2007, A443: 172
26 Seidenkranz T, Hegenbarth E. Single-crystal elastic constants of MgZn2 in the temperature range from 4.2 to 300 K [J]. Phys. Stat. Sol., 1976, 33A: 205
27 Spriano S, Doglione R, TextureBaricco M., hardening and mechanical anisotropy in AA8090-T851 plate [J]. Mater. Sci. Eng., 1998, A257: 134
Outlines

/