Precipitation Behavior of W-Rich Phases in a High W-Containing Ni-Based Superalloys K416B
Received date: 2020-05-27
Revised date: 2020-09-01
Online published: 2020-11-04
Supported by
National Natural Science Foundation of China(51971214);Talents Program of Chinese Academy of Sciences(51771191);Innovation Science Foundation from Innovation Academy for Light-Duty Gas Turbine, Chinese Academy of Sciences(CXYJJ20-QN-02)
The high temperature strength of Ni-based cast superalloys can be significantly improved by adding tungsten (W), a solid solution strengthening element. Hence, superalloys with high W content have been developed as key materials for the preparation of aircraft engine blades. However, the high segregation coefficient of W results in inconsistent composition and microstructure during the solidification process, which can be difficult to eliminate via heat treatment leading to deteriorated mechanical properties. The Ni-based superalloy K416B contains approximately 16.5%W (mass fraction) and exhibits a high tendency to precipitate W-rich phases, such as the α-W and M6C phases, which not only consume a large amount of W in the matrix but also reduce the solid solution strengthening ability of the alloy. W-rich precipitates also become the origin and propagation paths of cracks during stress-rupture testing. Much research on high W-containing, Ni-based superalloys has focused on the effects of W content on W-rich phase formation and mechanical properties. However, the roles of casting temperature and cooling rate on the formation of the W-rich phase are still unclear. In this work, five groups of K416B alloy test bars with the same composition were prepared with different processes. Three casting temperatures were chosen, and the cooling rate was controlled by burying sand in the thick shell and single shell, respectively. The relationship between the precipitation behavior of the W-rich phase in the K416B alloy and casting temperature, and solidification rate under different casting processes were analyzed using SEM and EDS. When the casting temperature is lowered from 1500°C to 1450°C, the grain size is significantly reduced. Results show massive α-W phases in the residual eutectic of the alloy at different casting temperatures, and the morphology of the α-W phase show few differences. The larger M6C phase in the alloy exists with residual eutectic, and the small M6C phase is embedded at the edge of the residual eutectic. At a high solidification rate, the precipitation of the W-rich phase is inhibited, which is primarily manifested by the decreased number and size of the W-rich phase in the alloy. When casting high W-containing Ni-based superalloys, choosing an appropriate casting temperature and adopting an appropriate heat preservation system to accelerate the cooling rate during solidification will affect the precipitation and transformation of W-rich phases, and optimize the properties of the alloy.
Key words: Ni-based superalloy; W-rich phase; α-W; M6C; cooling rate
Yuping ZHU , SHENG Naicheng , Jun XIE , Zhenjiang WANG , Shuling XUN , Jinjiang YU , Jinguo LI , Lin YANG , Guichen HOU , Yizhou ZHOU , Xiaofeng SUN . Precipitation Behavior of W-Rich Phases in a High W-Containing Ni-Based Superalloys K416B[J]. Acta Metall Sin, 2021 , 57(2) : 215 -223 . DOI: 10.11900/0412.1961.2020.00180
| 1 | Tang Z J, Guo T M, Fu Y, et al. Research present situation and the development prospect of nickel-based superalloy [J]. Met. World, 2014, (1): 36 |
| 1 | 唐中杰, 郭铁明, 付 迎等. 镍基高温合金的研究现状与发展前景 [J]. 金属世界, 2014, (1): 36 |
| 2 | Yabansu Y C, Iskakov A, Kapustina A, et al. Application of Gaussian process regression models for capturing the evolution of microstructure statistics in aging of nickel-based superalloys [J]. Acta Mater., 2019, 178: 45 |
| 3 | Zhang J, Lou L H. Basic research in development and applicationof cast superalloy [J]. Acta Metall. Sin., 2018, 54: 1637 |
| 3 | 张 健, 楼琅洪. 铸造高温合金研发中的应用基础研究 [J]. 金属学报, 2018, 54: 1637 |
| 4 | Reed R C. The Superalloys Fundamentals and Applications [M]. London: Cambridge University Press, 2006: 1 |
| 5 | Guo J T. Materials Science and Engineering for Superalloys [M]. Vol.1, Beijing: Science Press, 2008: 1 |
| 5 | 郭建亭. 高温合金材料学 [M]. 上册, 北京: 科学出版社, 2008: 1 |
| 6 | Yue Q Z, Liu L, Yang W C, et al. Research progress of creep behaviors in advanced Ni-based single crystal superalloys [J]. Mater. Rep., 2019, 33: 479 |
| 6 | 岳全召, 刘 林, 杨文超等. 先进镍基单晶高温合金蠕变行为的研究进展 [J]. 材料导报, 2019, 33: 479 |
| 7 | Wang Z Q. Key manufacturing technology of advanced aeroengine [J]. Aeron. Manuf. Technol., 2015, (22): 34 |
| 7 | 王增强. 先进航空发动机关键制造技术 [J]. 航空制造技术, 2015, (22): 34 |
| 8 | Sun F, Tong J Y, Feng Q, et al. Microstructural evolution and deformation features in gas turbine blades operated in-service [J]. J. Alloys Compd., 2015, 618: 728 |
| 9 | Kang B I, Han C H, Shin Y K, et al. Effects of boron and zirconium on grain boundary morphology and creep resistance in nickel-based superalloy [J]. J. Mater. Eng. Perform., 2019, 28: 7025 |
| 10 | Rai R K, Sahu J K, Jena P S M, et al. High temperature tensile deformation of a directionally solidified nickel base superalloy: Role of micro constituents [J]. Mater. Sci. Eng., 2017, A705: 189 |
| 11 | Huang B, Xiong W H, Zhang M, et al. Effect of W content in solid solution on properties and microstructure of (Ti, W)C-Ni3Al cermets [J]. J. Alloys Compd., 2016, 676: 142 |
| 12 | Guth S, Doll S, Lang K H. Influence of phase angle on lifetime, cyclic deformation and damage behavior of Mar-M247 LC under thermo-mechanical fatigue [J]. Mater. Sci. Eng., 2015, A642: 42 |
| 13 | Meyer A, Daenicke E, Horke K, et al. Metal injection moulding of nickel-based superalloy CM247LC [J]. Powder Metall., 2016, 59: 51 |
| 14 | Wang L N, Sun X F, Guan H R. Effect of melt heat treatment on MC carbide formation in nickel-based superalloy K465 [J]. Results Phys., 2017, 7: 2111 |
| 15 | Du B N, Yang J X, Cui C Y, et al. Effects of grain size on the high-cycle fatigue behavior of IN792 superalloy [J]. Mater. Des., 2015, 65: 57 |
| 16 | Raju S V, Oni A A, Godwal B K, et al. Effect of B and Cr on elastic strength and crystal structure of Ni3Al alloys under high pressure [J]. J. Alloys Compd., 2015, 619: 616 |
| 17 | Zhang B Q. The research on transient liquid phase bonding of Mar-M247 nickel-based superalloys [D]. Chongqing: Chongqing University, 2018 |
| 17 | 张邦强. Mar-M247镍基高温合金瞬时液相连接研究 [D]. 重庆: 重庆大学, 2018 |
| 18 | Zhou T J, Ding H S, Ma X P, et al. Microstructure and stress-rupture life of high W-content cast Ni-based superalloy after 100-1100oC thermal exposures [J]. Mater. Sci. Eng., 2018, A725: 299 |
| 19 | Yang J X, Li J G, Wang M, et al. Effects of heat treatment process on the microstructure and properties of a new cast nickel-based superalloy [J]. Acta Metall. Sin., 2012, 48: 654 |
| 19 | 杨金侠, 李金国, 王 猛等. 热处理工艺对一种新型铸造镍基高温合金的组织和性能影响 [J]. 金属学报, 2012, 48: 654 |
| 20 | Yang Y H. Investigation of microstructure and mechanical properties of K416B alloy [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2012 |
| 20 | 杨彦红. K416B镍基高温合金组织和性能研究 [D]. 沈阳: 中国科学院金属研究所, 2012 |
| 21 | Xu Z F, Jiang L, Dong J S, et al. The effect of silicon on precipitation and decomposition behaviors of M6C carbide in a Ni-Mo-Cr superalloy [J]. J. Alloys Compd., 2015, 620: 197 |
| 22 | Zheng L. The effects of tantalum and ruthenium on the microstructures and properties of low chromium and high tungsten content cast nickel-base superalloys [D]. Xi􀆳an: Xi􀆳an University of Technology, 2004 |
| 22 | 郑 亮. Ta和Ru对低Cr高W铸造镍基高温合金组织及性能的影响 [D]. 西安: 西安理工大学, 2004 |
| 23 | Zheng L. Formation and transformation of α phase in Ta-containing low Cr and high W content cast Ni-base superalloys [J]. Chin. J. Nonferrous. Met., 2005, 15: 1566 |
| 23 | 郑 亮. 含Ta低Cr高W铸造镍基高温合金中α相的形成与转变 [J]. 中国有色金属学报, 2005, 15: 1566 |
| 24 | Wang W Y, Shang S L, Wang Y, et al. Impact of W on structural evolution and diffusivity of Ni-W melts: An ab initio molecular dynamics study [J]. J. Mater. Sci., 2015, 50: 1071 |
| 25 | Ma Y H, Zhao K, Yang F X, et al. Precipitation of α-W phase in nickel-based superalloy [J]. J. Chin. Electr. Microsc. Soc., 2005, 24: 297 |
| 25 | 马永会, 赵 锴, 杨飞雪等. 镍基高温合金中α-W相的析出 [J]. 电子显微学报, 2005, 24: 297 |
| 26 | Hu H Q. Principles of Metal Solidification [M]. 2nd Ed., Beijing: Mechanical Industry Press, 2000: 1 |
| 26 | 胡汉起. 金属凝固原理 [M]. 第2版,北京: 机械工业出版社, 2000: 1 |
| 27 | Xie J. Preparation technology, mechanical properties and application of K416B Ni-base superalloy [R]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2015 |
| 27 | 谢 君. K416B镍基合金的制备工艺和力学性能研究 [R]. 沈阳: 中国科学院金属研究所, 2015 |
| 28 | Ge H C, Yuan G Q, Peng C. Physical Chemistry [M]. Beijing: Higher Education Press, 2008: 1 |
| 28 | 葛华才, 袁高清, 彭 程. 物理化学 [M]. 北京: 高等教育出版社, 2008: 1 |
| 29 | Takamichi I, Roderick I L G, translated by Xian A P, Wang L W. The Physical Properties of Liquid Metals [M]. Beijing: Science Press, 2005: 1 |
| 29 | Takamichi I, Roderick I L G著, 冼爱平, 王连文译. 液态金属的物理性能 [M]. 北京: 科学出版社, 2005: 1 |
| 30 | Liang Z F, Pan Y T, Feng M Y, et al. Research on thermal properties of coal gangue [J]. Coal Technol., 2018, 37(10): 231 |
| 30 | 梁志峰, 潘永泰, 冯茂原等. 煤矸石的热物性研究 [J]. 煤炭技术, 2018, 37(10): 231 |
| 31 | Guo J T. Materials Science and Engineerning for Superalloy [M]. Vol.2, Beijing: Science Press, 2008: 1 |
| 31 | 郭建亭. 高温合金材料学 [M]. 中册, 北京: 科学出版社, 2008: 1 |
| 32 | Zhang A W, Zhang S, Liu F, et al. Effect of cooling rate on phosphorus segregation behavior and the corresponding precipitation of γ'' and γ' phases in IN718 alloy [J]. J. Mater. Sci. Technol., 2019, 35: 1485 |
| 33 | Gong L, Chen B, Zhang L, et al. Effect of cooling rate on microstructure, microsegregation and mechanical properties of cast Ni-based superalloy K417G [J]. J. Mater. Sci. Technol., 2018, 34: 811 |
| 34 | Hua H Y, Xie J, Shu D L, et al. Influence of W content on the microstructure of nickel base superalloy with high W content [J]. Acta Metall. Sin., 2020, 56: 161 |
| 34 | 华涵钰, 谢 君, 舒德龙等. W含量对一种高W镍基高温合金显微组织的影响 [J]. 金属学报, 2020, 56: 161 |
| 35 | Zhao H B, Feng W, Zhou T J. Distribution of primary M6C carbide in large nickel-based superalloy casting [J]. Found. Technol., 2017, 38: 1288 |
| 35 | 赵会彬, 冯 薇, 周同金. 大型镍基高温合金铸件中初生M6C碳化物的分布规律 [J]. 铸造技术, 2017, 38: 1288 |
/
| 〈 |
|
〉 |