Research paper

Effect of Superheat on Integral Morphology Characteristics of Solidification Structure and Permeability in Bearing Steel Billet

  • Jianghai CAO ,
  • Zibing HOU ,
  • Zhongao GUO ,
  • Dongwei GUO ,
  • Ping TANG
Expand
  • 1.College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China
    2.Chongqing Key Laboratory of Vanadium-Titanium Metallurgy and New Materials, Chongqing University, Chongqing, 400044, China
HOU Zibing, associate professor, Tel: (023)65105202, E-mail: houzibing@cqu.edu.cn

Received date: 2020-07-22

  Revised date: 2020-10-12

  Online published: 2020-10-30

Supported by

United Funds between National Natural Science Foundation and Baowu Steel Group Corporation Limited of China(U1860101);Chongqing Fundamental Research and Cutting-Edge Technology Funds(cstc2017jcyjAX0019)

Abstract

As a typical bearing steel, GCr15 steel tends to solidify over a wide temperature range during casting because of its high carbon content. The size of the mushy zone is relatively large, causing macrosegregation and porosity defects in bearing steel. The morphology of the solidification structure plays an important role in governing macrosegregation severity. Solidification structures have conventionally been characterized by measuring the primary or secondary dendrite arm spacing in a dendritic network, but these measures do not adequately describe the branched appearance of secondary and tertiary arms. In this work, fractal dimension and specific surface area have been introduced, and the solidification structure integral morphology characteristics of different locations in the continuous casting billet of GCr15 bearing steel have been quantitatively investigated. Then, the permeability of the interdendritic channels were calculated based on fractal dimension and specific surface area. The size of the billets was 220 mm × 220 mm, and the sampling location was in the cross section of the billet. Two superheats (20 and 35oC) were considered for studying the integral characteristics of the solidification structure. First, fractal dimension can describe the self-similar complexity of the solidification structure, and specific surface area can describe dendritic coarsening. Second, it was determined that the fractal dimension was larger and the specific surface area was smaller at 35oC superheat compared with 20oC superheat. This indicates that the self-similar complexity of dendrites is larger, and the dendrite coarsening is more significant at high superheating. Finally, the permeability in the equiaxed grain zone calculated using fractal dimension and specific surface area is lower at 20oC superheat. The smaller the permeability, the greater the flow resistance of the liquid, which is more conducive to the control of the macrosegregation defects. In addition, to effectively restrain the formation of macrosegregation defects at high superheat, the cooling rate in the equiaxed grains zone should increase by adjusting the process parameters under isothermal solidification conditions.

Cite this article

Jianghai CAO , Zibing HOU , Zhongao GUO , Dongwei GUO , Ping TANG . Effect of Superheat on Integral Morphology Characteristics of Solidification Structure and Permeability in Bearing Steel Billet[J]. Acta Metall Sin, 2021 , 57(5) : 586 -594 . DOI: 10.11900/0412.1961.2020.00274

References

1 Pickering E J. Macrosegregation in steel ingots: The applicability of modelling and characterisation techniques [J]. ISIJ Int., 2013, 53: 935
2 Choudhary S K, Ganguly S. Morphology and segregation in continuously cast high carbon steel billets [J]. ISIJ Int., 2007, 47: 1759
3 Mayer F, Wu M, Ludwig A. On the formation of centreline segregation in continuous slab casting of steel due to bulging and/or feeding [J]. Steel Res. Int., 2010, 81: 660
4 Flemings M C. Our understanding of macrosegregation: Past and present [J]. ISIJ Int., 2000, 40: 833
5 Zhong X T, Rowenhorst D J, Beladi H, et al. The five-parameter grain boundary curvature distribution in an austenitic and ferritic steel [J]. Acta Mater., 2017, 123: 136
6 Bisang U, Bilgram J H. The fractal dimension of xenon dendrites [J]. J. Cryst. Growth, 1996, 166: 207
7 González-Cinca R, Ramírez-Piscina L. Numerical study of the shape and integral parameters of a dendrite [J]. Phys. Rev., 2004, 70E: 051612
8 Mandelbrot B B. The Fractal Geometry of Nature [M]. New York: Freeman Press, 1982: 206
9 Mandelbrot B B. How long is the coast of Britain? Statistical self-similarity and fractional dimension [J]. Science, 1967, 156: 636
10 Zaiser M, Bay K, H?hner P. Fractal analysis of deformation-induced dislocation patterns [J]. Acta Mater., 1999, 47: 2463
11 Chang Q, Chen D L, Ru H Q, et al. Three-dimensional fractal analysis of fracture surfaces in titanium-iron particulate reinforced hydroxyapatite composites: Relationship between fracture toughness and fractal dimension [J]. J. Mater. Sci., 2011, 46: 6118
12 Kobayashi S, Maruyama T, Tsurekawa S, et al. Grain boundary engineering based on fractal analysis for control of segregation-induced intergranular brittle fracture in polycrystalline nickel [J]. Acta Mater., 2012, 60: 6200
13 Long Q Y, Wen Y H, Zhu Z, et al. Sierpinski fractal description of the martensitic transformation [J]. Philos. Mag., 1993, 68A: 885
14 Hou Z B, Cao J H, Chang Y, et al. Morphology characteristics of carbon segregation in die steel billet by ESR based on fractal dimension [J]. Acta Metall. Sin., 2017, 53: 769
14 侯自兵, 曹江海, 常 毅等. 基于分形维数的模具钢电渣重熔铸坯碳偏析形貌特征研究 [J]. 金属学报, 2017, 53: 769
15 Yang A M, Xiong Y H, Liu L. Fractal characteristics of dendrite and cellular structure in nickel-based superalloy at intermediate cooling rate [J]. Sci. Technol. Adv. Mater., 2001, 2: 101
16 Ishida H, Natsume Y, Ohsasa K. Characterization of dendrite morphology for evaluating interdendritic fluidity based on phase-field simulation [J]. ISIJ Int., 2009, 49: 37
17 Cao J H, Hou Z B, Guo D W, et al. Morphology characteristics of solidification structure in high-carbon steel billet based on fractal theory [J]. J. Mater. Sci., 2019, 54: 12851
18 Cao J H, Hou Z B, Guo D W, et al. Fractal morphology characteristics of solidification structure in electroslag remelting billet of die steel by ESR [J]. J. Iron Steel Res., 2019, 31: 286
18 曹江海, 侯自兵, 郭东伟等. 模具钢电渣重熔铸坯凝固组织形貌的分形特征 [J]. 钢铁研究学报, 2019, 31: 286
19 Hou Z B, Jiang F, Cheng G G. Solidification structure and compactness degree of central equiaxed grain zone in continuous casting billet using cellular automaton-finite element method [J]. ISIJ Int., 2012, 52: 1301
20 Dubuc B, Quiniou J, Roques-Carmes C, et al. Evaluating the fractal dimension of profiles [J]. Phys. Rev., 1989, 39A: 1500
21 Genau A L, Freedman A C, Ratke L. Effect of solidification conditions on fractal dimension of dendrites [J]. J. Cryst. Growth, 2013, 363: 49
22 Kasperovich G, Genau A, Ratke L. Mushy zone coarsening in an AlCu30 alloy accelerated by a rotating magnetic field [J]. Metall. Mater. Trans., 2011, 42A: 1657
23 Wang W, Hou Z B, Chang Y, et al. Effect of superheat on quality of central equiaxed grain zone of continuously cast bearing steel billet based on two-dimensional segregation ratio [J]. J. Iron Steel Res. Int., 2018, 25: 9
24 Zhu M F, Xing L K, Fang H, et al. Progresses in dendrite coarsening during solidification of alloys [J]. Acta Metall. Sin., 2018, 54: 789
24 朱鸣芳, 邢丽科, 方 辉等. 合金凝固枝晶粗化的研究进展 [J]. 金属学报, 2018, 54: 789
25 Tiller W A, Jackson K A, Rutter J W, et al. The redistribution of solute atoms during the solidification of metals [J]. Acta Metall., 1953, 1: 428
26 Aritaka E, Esaka H, Shinozuka K. Mechanism for complex morphology due to mechanical vibration [J]. ISIJ Int., 2016, 56: 1413
27 Whisler N J, Kattamis T Z. Dendritic coarsening during solidification [J]. J. Cryst. Growth, 1972, 15: 20
28 Marsh S P, Glicksman M E. Overview of geometric effects on coarsening of mushy zones [J]. Metall. Mater. Trans., 1996, 27A: 557
29 Hu H Q. Principle of Metal Solidification [M]. 2nd Ed., Beijing: Mechanical Industry Press, 2000: 210
29 胡汉起. 金属凝固原理 [M]. 第2版,北京: 机械工业出版社, 2000: 210
30 Carman P C. Flow of Gases Through Porous Media [M]. London: Butterworth Scientific Publications, 1956: 10
31 Khajeh E, Maijer D M. Physical and numerical characterization of the near-eutectic permeability of aluminum-copper alloys [J]. Acta Mater., 2010, 58: 6334
32 Sun Z, Logé R E, Bernacki M. 3D finite element model of semi-solid permeability in an equiaxed granular structure [J]. Comput. Mater. Sci., 2010, 49: 158
Outlines

/