In the recent years, lightweight and high-strength structural materials have gained much attention in engineering applications. Carbon nanotube (CNT)-reinforced Al (CNT/Al) composites are promising structural materials owing to the good mechanical properties and high reinforcing efficiency of CNTs. Previous studies on these composites mainly focused on fabricating CNT-reinforced low-strength or medium-high-strength Al alloys (such as pure Al, or 2xxx series or 6xxx series Al alloys) composites via various dispersion methods. However, only few studies investigated composites with super-high-strength Al alloys as the matrices. In the present work, CNT/7055Al composites with CNT volume fractions of 0%, 1%, and 3% were prepared by high-energy ball milling combined with powder metallurgy. The CNT distribution, grain structure, interface, and mechanical properties of the CNT/7055Al composite were investigated using OM, SEM, TEM, and tensile tests. The strengthening mechanism and anisotropy of the composite were analyzed. The results indicated that the composite had a bimodal grain structure consisting of CNT-free coarse grain zones and CNT-enriched ultrafine grain zones. CNTs were well dispersed in the ultrafine grain zones of the Al matrix, and the CNT/Al interface was clean. There were only few reaction products at the interface. The tensile strength of the 3%CNT/7055Al composite reached 816 MPa, but the elongation was only 0.5%. Grain refinement and Orowan strengthening were the main strengthening mechanisms of the CNT/7055Al composite. Because of the load transfer efficiency of CNTs and a coarse grain band structure, the composite exhibited stronger anisotropy than the matrix alloy. The tensile properties of the CNT/7055Al composite normal to the extrusion direction were weaker than those in the extrusion direction.
Sheng BI , Zechen LI , Haixia SUN , Baoyong SONG , Zhenyu LIU , Bolv XIAO , Zongyi MA . Microstructure and Mechanical Properties of Carbon Nanotubes-Reinforced 7055Al Composites Fabricated by High-Energy Ball Milling and Powder Metallurgy Processing[J]. Acta Metall Sin, 2021 , 57(1) : 71 -81 . DOI: 10.11900/0412.1961.2020.00238
| 1 | Wang C, Wang B B, Wang D, et al. High-speed friction stir welding of SiCp/Al-Mg-Si-Cu composite [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 32: 677 |
| 2 | Ma K, Zhang X X, Wang D, et al. Optimization and simulation of deformation parameters of SiC/2009Al composites [J]. Acta Metall. Sin., 2019, 55: 1329 |
| 2 | 马 凯, 张星星, 王 东等. SiC/2009Al复合材料的变形加工参数的优化仿真研究 [J]. 金属学报, 2019, 55: 1329 |
| 3 | Ma G N, Wang D, Liu Z Y, et al. Effect of hot pressing temperature on microstructure and tensile properties of SiC/Al-Zn-Mg-Cu composites [J]. Acta Metall. Sin., 2019, 55: 1319 |
| 3 | 马国楠, 王 东, 刘振宇等. 热压烧结温度对SiC/Al-Zn-Mg-Cu复合材料微观结构与力学性能的影响 [J]. 金属学报, 2019, 55: 1319 |
| 4 | Zhou L, Cui C, Wang Q Z, et al. Constitutive equation and model validation for a 31 vol.% B4Cp/6061Al composite during hot compression [J]. J. Mater. Sci. Technol., 2018, 34: 1730 |
| 5 | Li J C, Zhang X X, Geng L. Improving graphene distribution and mechanical properties of GNP/Al composites by cold drawing [J]. Mater. Des., 2018, 144: 159 |
| 6 | Zheng Z, Zhang X X, Li J C, et al. Achieving homogeneous distribution of high-content graphene in aluminum alloys via high-temperature cumulative shear deformation [J]. Mater. Des., 2020, 193: 108796 |
| 7 | Qian D, Wagner G J, Liu W K, et al. Mechanics of carbon nanotubes [J]. Appl. Mech. Rev., 2002, 55: 495 |
| 8 | Liu Z Y, Xiao B L, Wang W G, et al. Effect of carbon nanotube orientation on mechanical properties and thermal expansion coefficient of carbon nanotube-reinforced aluminum matrix composites [J]. Acta Metall. Sin. (Engl. Lett.), 2014, 27: 901 |
| 9 | Zhao K, Liu Z Y, Xiao B Y, et al. Friction stir welding of carbon nanotubes reinforced Al-Cu-Mg alloy composite plates [J]. J. Mater. Sci. Technol., 2017, 33: 1004 |
| 10 | Yu Z Y, Tan Z Q, Fan G L, et al. Effect of interfacial reaction on Young??s modulus in CNT/Al nanocomposite: A quantitative analysis [J]. Mater. Charact., 2018, 137: 84 |
| 11 | Esawi A M K, Morsi K, Sayed A, et al. Effect of carbon nanotube (CNT) content on the mechanical properties of CNT-reinforced aluminium composites [J]. Compos. Sci. Technol., 2010, 70: 2237 |
| 12 | Jafari M, Abbasi M H, Enayati M H, et al. Mechanical properties of nanostructured Al2024-MWCNT composite prepared by optimized mechanical milling and hot pressing methods [J]. Adv. Powder Technol., 2012, 23: 205 |
| 13 | Jiang L, Li Z Q, Fan G L, et al. The use of flake powder metallurgy to produce carbon nanotube (CNT)/aluminum composites with a homogenous CNT distribution [J]. Carbon, 2012, 50: 1993 |
| 14 | Yang X D, Zou T C, Shi C S, et al. Effect of carbon nanotube (CNT) content on the properties of in-situ synthesis CNT reinforced Al composites [J]. Mater. Sci. Eng., 2016, A660: 11 |
| 15 | Nam D H, Cha S I, Lim B K, et al. Synergistic strengthening by load transfer mechanism and grain refinement of CNT/Al-Cu composites [J]. Carbon, 2012, 50: 2417 |
| 16 | Liu Z Y, Zhao K, Xiao B L, et al. Fabrication of CNT/Al composites with low damage to CNTs by a novel solution-assisted wet mixing combined with powder metallurgy processing [J]. Mater. Des., 2016, 97: 424 |
| 17 | Zhao K, Liu Z Y, Xiao B L, et al. Origin of insignificant strengthening effect of CNTs in T6-treated CNT/6061Al composites [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 134 |
| 18 | Liu Z Y, Xiao B L, Wang W G, et al. Analysis of carbon nanotube shortening and composite strengthening in carbon nanotube/aluminum composites fabricated by multi-pass friction stir processing [J]. Carbon, 2014, 69: 264 |
| 19 | Xu R, Tan Z Q, Xiong D B, et al. Balanced strength and ductility in CNT/Al composites achieved by flake powder metallurgy via shift-speed ball milling [J]. Composites, 2017, 96A: 57 |
| 20 | Liu X Q, Li C J, Eckert J, et al. Microstructure evolution and mechanical properties of carbon nanotubes reinforced Al matrix composites [J]. Mater. Charact., 2017, 133: 122 |
| 21 | Zhang X X, Zhang J F, Liu Z Y, et al. Microscopic stresses in carbon nanotube reinforced aluminum matrix composites determined by in-situ neutron diffraction [J]. J. Mater. Sci. Technol., 2020, 54: 58 |
| 22 | Liu Z Y, Xiao B L, Wang W G, et al. Modelling of carbon nanotube dispersion and strengthening mechanisms in Al matrix composites prepared by high energy ball milling-powder metallurgy method [J]. Composites, 2017, 94A: 189 |
| 23 | Liu Z Y, Xu S J, Xiao B L, et al. Effect of ball-milling time on mechanical properties of carbon nanotubes reinforced aluminum matrix composites [J]. Composites, 2012, 43A: 2161 |
| 24 | Choi H J, Shin J H, Bae D H. The effect of milling conditions on microstructures and mechanical properties of Al/MWCNT composites [J]. Composites, 2012, 43A: 1061 |
| 25 | Esawi A M K, Morsi K, Sayed A, et al. Fabrication and properties of dispersed carbon nanotube-aluminum composites [J]. Mater. Sci. Eng., 2009, A508: 167 |
| 26 | Choi H J, Bae D H. Strengthening and toughening of aluminum by single-walled carbon nanotubes [J]. Mater. Sci. Eng., 2011, A528: 2412 |
| 27 | Liu Z Y, Ma K, Fan G H, et al. Enhancement of the strength-ductility relationship for carbon nanotube/Al-Cu-Mg nanocomposites by material parameter optimisation [J]. Carbon, 2020, 157: 602 |
| 28 | Chen M L, Fan G L, Tan Z Q, et al. Design of an efficient flake powder metallurgy route to fabricate CNT/6061Al composites [J]. Mater. Des., 2018, 142: 288 |
| 29 | Xu R, Tan Z Q, Fan G L, et al. High-strength CNT/Al-Zn-Mg-Cu composites with improved ductility achieved by flake powder metallurgy via elemental alloying [J]. Composites, 2018, 111A: 1 |
| 30 | Choi H, Shin J, Min B, et al. Reinforcing effects of carbon nanotubes in structural aluminum matrix nanocomposites [J]. J. Mater. Res., 2009, 24: 2610 |
| 31 | Li M J, Ma K K, Jiang L, et al. Synthesis and mechanical behavior of nanostructured Al 5083/n-TiB2 metal matrix composites [J]. Mater. Sci. Eng., 2016, A656: 241 |
| 32 | Chen K H, Liu H W, Zhang Z, et al. The improvement of constituent dissolution and mechanical properties of 7055 aluminum alloy by stepped heat treatments [J]. J. Mater. Process. Technol., 2003, 142: 190 |
| 33 | Williamson G K, Hall W H. X-Ray line broadening from filed aluminium and wolfram [J]. Acta Metall., 1953, 1: 22 |
| 34 | Zhao Y H, Liao X Z, Jin Z, et al. Microstructures and mechanical properties of ultrafine grained 7075 Al alloy processed by ECAP and their evolutions during annealing [J]. Acta Mater., 2004, 52: 4589 |
| 35 | Chen B, Shen J, Ye X, et al. Length effect of carbon nanotubes on the strengthening mechanisms in metal matrix composites [J]. Acta Mater., 2017, 140: 317 |
| 36 | Choi H J, Min B H, Shin J H, et al. Strengthening in nanostructured 2024 aluminum alloy and its composites containing carbon nanotubes [J]. Composites, 2011, 42A: 1438 |
| 37 | Fan X G, Jiang D M, Meng Q C, et al. The microstructural evolution of an Al-Zn-Mg-Cu alloy during homogenization [J]. Mater. Lett., 2006, 60: 1475 |
| 38 | Ci L J, Ryu Z, Jin-Phillipp N Y, et al. Investigation of the interfacial reaction between multi-walled carbon nanotubes and aluminum [J]. Acta Mater., 2006, 54: 5367 |
| 39 | Lipecka J, Andrzejczuk M, Lewandowska M, et al. Evaluation of thermal stability of ultrafine grained aluminium matrix composites reinforced with carbon nanotubes [J]. Compos. Sci. Technol., 2011, 71: 1881 |
| 40 | Liu Z Y, Xiao B L, Wang W G, et al. Elevated temperature tensile properties and thermal expansion of CNT/2009Al composites [J]. Compos. Sci. Technol., 2012, 72: 1826 |
| 41 | Kim W J, Lee S H. High-temperature deformation behavior of carbon nanotube (CNT)-reinforced aluminum composites and prediction of their high-temperature strength [J]. Composites, 2014, 67A: 308 |
| 42 | Chen J Z, Zhen L, Yang S J, et al. Investigation of precipitation behavior and related hardening in AA 7055 aluminum alloy [J]. Mater. Sci. Eng., 2009, A500: 34 |
| 43 | Mondal C, Mishra B, Jena P K, et al. Effect of heat treatment on the behavior of an AA7055 aluminum alloy during ballistic impact [J]. Int. J. Impact Eng., 2011, 38: 745 |
| 44 | Wang T, Yin Z M, Shen K, et al. Single-aging characteristics of 7055 aluminum alloy [J]. Trans. Nonferrous Met. Soc. China, 2007, 17: 548 |
| 45 | Hu T, Ma K, Topping T D, et al. Precipitation phenomena in an ultrafine-grained Al alloy [J]. Acta Mater., 2013, 61: 2163 |
| 46 | Sha G, Yao L, Liao X Z, et al. Segregation of solute elements at grain boundaries in an ultrafine grained Al-Zn-Mg-Cu alloy [J]. Ultramicroscopy, 2011, 111: 500 |
| 47 | Dresselhaus M S, Dresselhaus G, Saito R, et al. Raman spectroscopy of carbon nanotubes [J]. Phys. Rep., 2005, 409: 47 |
| 48 | Yan L P, Tan Z Q, Ji G, et al. A quantitative method to characterize the Al4C3-formed interfacial reaction: The case study of MWCNT/Al composites [J]. Mater. Charact., 2016, 112: 213 |
| 49 | He C, Zhao N, Shi C, et al. An approach to obtaining homogeneously dispersed carbon nanotubes in Al powders for preparing reinforced Al-matrix composites [J]. Adv. Mater., 2007, 19: 1128 |
| 50 | Liu Z Y, Xiao B L, Wang W G, et al. Tensile strength and electrical conductivity of carbon nanotube reinforced aluminum matrix composites fabricated by powder metallurgy combined with friction stir processing [J]. J. Mater. Sci. Technol., 2014, 30: 649 |
| 51 | Wei H, Li Z Q, Xiong D B, et al. Towards strong and stiff carbon nanotube-reinforced high-strength aluminum alloy composites through a microlaminated architecture design [J]. Scr. Mater., 2014, 75: 30 |
| 52 | Zhang Z W, Liu Z Y, Xiao B L, et al. High efficiency dispersal and strengthening of graphene reinforced aluminum alloy composites fabricated by powder metallurgy combined with friction stir processing [J]. Carbon, 2018, 135: 215 |
| 53 | Li S H, Chao C G. Effects of carbon fiber/Al interface on mechanical properties of carbon-fiber-reinforced aluminum-matrix composites [J]. Metall. Mater. Trans., 2004, 35A: 2153 |
| 54 | Liu Z Y, Wang L H, Zan Y N, et al. Enhancing strengthening efficiency of graphene nano-sheets in aluminum matrix composite by improving interface bonding [J]. Composites, 2020, 199B: 108268 |
| 55 | Li J C, Zhang X X, Geng L. Effect of heat treatment on interfacial bonding and strengthening efficiency of graphene in GNP/Al composites [J]. Composites, 2019, 121A: 487 |
| 56 | Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy [J]. Acta Mater., 2014, 62: 141 |
| 57 | Liu Z Y, Xiao B L, Wang W G, et al. Singly dispersed carbon nanotube/aluminum composites fabricated by powder metallurgy combined with friction stir processing [J]. Carbon, 2012, 50: 1843 |
| 58 | Nardone V C, Prewo K M. On the strength of discontinuous silicon carbide reinforced aluminum composites [J]. Scr. Mater., 1986, 20: 43 |
| 59 | English A T. Influence of mechanical fibering on anisotropy of strength and ductility [J]. JOM, 1965, 17(4): 395 |
| 60 | Nasiri-Abarbekoh H, Ekrami A, Ziaei-Moayyed A A, et al. Effects of rolling reduction on mechanical properties anisotropy of commercially pure titanium [J]. Mater. Des., 2012, 34: 268 |
| 61 | Shaji E M, Kalidindi S R, Doherty R D, et al. Fracture properties of multiphase alloy MP35N [J]. Mater. Sci. Eng., 2003, A349: 313 |
/
| 〈 |
|
〉 |