Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain
Received date: 2020-06-23
Revised date: 2020-09-12
Online published: 2020-10-29
Supported by
National Natural Science Foundation of China(51461024)
It is difficult to form the precipitated phase of duplex stainless steel (DSS) with low nickel content, and a low Cr content of 18.7% (mass fraction) during hot working. However, the stability of the austenite phase changes by substituting Mn for Ni, which can increase the difference between the softening mechanisms of the two phases under high temperature and deformation conditions. Under a temperature and strain rate of 1123-1423 K and 0.1-10 s-1, respectively, the large thermal compression deformation behavior (70%) of 18.7Cr-1.0Ni-5.8Mn-0.2N DSS was investigated. The thermal deformation microstructures were analyzed by OM, SEM, and EBSD. The results show that the dynamic recrystallization (DRX) of the ferrite phase mainly occurred at a lower deformation temperature of 1123 K, and that the degree of grain refinement increased, and the degree of grain inhomogeneity decreased with an increase in strain rate. The strain rate was observed to have a large impact on the ferrite phase DRX, while the austenite phase DRX was more sensitive to deformation temperature. The ferrite phase underwent continuous dynamic recrystallization (CDRX) with the transition from low-angle to high-angle grain boundaries under deformation at 1223 K and 10 s-1, while the austenite phase was dominated by discontinuous dynamic recrystallization (DDRX) deformed at 1323 K and 0.1 s-1. DDRX can be easily induced by increasing the temperature at a low strain rate, while CDRX can be induced at a higher strain rate. The crystal orientation of the austenite phase is mainly characterized by the recrystallization texture of the (001) and (111) planes at higher temperatures and lower strain rates. In the ferrite phase, there is a competitive relationship between the recrystallization texture of the (001) and (111) planes. The critical stress (strain) was obtained by data fitting and its relationship with the peak stress (strain) was determined. As the strain increased, the flow instability domain of hot compression decreased, and the stability zone gradually moved toward higher temperature and strain rate. Furthermore, the optimum hot working conditions, 1323-1423 K and 0.01-6.05 s-1, were obtained.
Ke NI , Yinhui YANG , Jianchun CAO , Liuhang WANG , Zehui LIU , Hao QIAN . Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. Acta Metall Sin, 2021 , 57(2) : 224 -236 . DOI: 10.11900/0412.1961.2020.00218
| 1 | Yang Y H, Qian H, Su Y S. Effect of Mn addition on deformation behaviour of 23% Cr low nickel duplex stainless steel [J]. Mater. Charact., 2018, 145: 606 |
| 2 | Gao F, Liu Z Y, Wang G D. Hot deformation behavior of high-purified 17% Cr ferritic stainless steel [J]. J. Northeastern Univ. (Nat. Sci.), 2011, 32: 1406 |
| 2 | 高 飞, 刘振宇, 王国栋. 高纯Cr17铁素体不锈钢的热变形行为 [J]. 东北大学学报(自然科学版), 2011, 32: 1406 |
| 3 | Momeni A, Kazemi S, Ebrahimi G, et al. Dynamic recrystallization and precipitation in high manganese austenitic stainless steel during hot compression [J]. Int. J. Min. Metall. Mater, 2014, 21: 36 |
| 4 | Gourdet S, Montheillet F. An experimental study of the recrystallization mechanism during hot deformation of aluminium [J]. Mater. Sci. Eng., 2000, A283: 274 |
| 5 | McQueen H J, Blum W. Dynamic recovery: Sufficient mechanism in the hot deformation of Al (<99.99) [J]. Mater. Sci. Eng., 2000, A290: 95 |
| 6 | Eghbali B, Abdollah-Zadeh A, Beladi H, et al. Characterization on ferrite microstructure evolution during large strain warm torsion testing of plain low carbon steel [J]. Mater. Sci. Eng., 2006, A435: 499 |
| 7 | Eghbali B, Abdollah-Zadeh A, Hodgson P D. Dynamic softening of ferrite during large strain warm deformation of a plain-carbon steel [J]. Mater. Sci. Eng., 2007, A462: 259 |
| 8 | Eghbali B. Microstructural characterization of a warm-deformed microalloyed steel [J]. Mater. Charact., 2008, 59: 473 |
| 9 | Abdollah-Zadeh A, Eghbali B. Mechanism of ferrite grain refinement during warm deformation of a low carbon Nb-microalloyed steel [J]. Mater. Sci. Eng., 2007, A457: 219 |
| 10 | An F H, Sha Y H, Zuo L. Microstructural evolution of Fe-3%Si alloy during hot deformation [J]. J. Funct. Mater., 2010, 41: 1948 |
| 10 | 安丰辉, 沙玉辉, 左 良. Fe-3%Si合金热变形过程中的组织演变 [J]. 功能材料, 2010, 41: 1948 |
| 11 | Doherty R D, Hughes D A, Humphreys F J, et al. Current issues in recrystallization: A review [J] Mater. Sci. Eng., 1997, A238: 219 |
| 12 | Dehghan-Manshadi A, Hodgson P D. Effect of δ-ferrite co-existence on hot deformation and recrystallization of austenite [J] J. Mater. Sci., 2008, 43: 6272 |
| 13 | Fan G W, Liu J, Han P D, et al. Hot ductility and microstructure in casted 2205 duplex stainless steels [J]. Mater. Sci. Eng., 2009, A515: 108 |
| 14 | Cizek P, Wynne B P. A mechanism of ferrite softening in a duplex stainless steel deformed in hot torsion [J]. Mater. Sci. Eng., 1997, A230: 88 |
| 15 | Fang Y L, Liu Z Y, Zhang W N, et al. Microstructure evolution of lean duplex stainless steel 2101 during hot deformation [J]. Acta Metall. Sin., 2010, 46: 641 |
| 15 | 方轶琉, 刘振宇, 张维娜等. 节约型双相不锈钢2101高温变形过程中微观组织演化 [J]. 金属学报, 2010, 46: 641 |
| 16 | Haghdadi N, Martin D, Hodgson P. Physically-based constitutive modelling of hot deformation behavior in a LDX 2101 duplex stainless steel [J]. Mater. Des., 2016, 106: 420 |
| 17 | Estrin Y, Mecking H. A unified phenomenological description of work hardening and creep based on one-parameter models [J]. Acta Metall., 1984, 32: 57 |
| 18 | Yan F H, Li S K, Wang M J, et al. Flow stress behavior of TB6 titanium alloy during hot compression deformation at elevated temperature [J]. Chin. J. Nonferrous Met., 2010, 20: 478 |
| 18 | 闫飞昊, 李士凯, 王美娇等. TB6合金热压缩流变应力行为 [J]. 中国有色金属学报, 2010, 20: 478 |
| 19 | Yamagata H, Ohuchida Y, Saito N, et al. Dynamic recrystallization and dynamic recovery of 99.99 mass% aluminum single crystal having [112] orientation [J]. J. Mater. Sci. Lett., 2001, 20: 1947 |
| 20 | Zhang M M. Influence of hot-deformation parameters on ferrite grain refinement of Cu-P-Cr-Ni-Mo dual-phase weathering steel [D]. Qinhuangdao: Yanshan University, 2015 |
| 20 | 张萌萌. 热变形参数对Cu-P-Cr-Ni-Mo双相耐候钢铁素体晶粒细化的影响 [D]. 秦皇岛: 燕山大学, 2015 |
| 21 | Belyakov A, Sakai T, Miura H, et al. Strain-induced submicrocrystalline grains developed in austenitic stainless steel under severe warm deformation [J]. Philos. Mag. Lett., 2000, 80: 711 |
| 22 | Chen F, Cui Z S, Chen S J. Recrystallization of 30Cr2Ni4MoV ultra-super-critical rotor steel during hot deformation. Part I: Dynamic recrystallization [J]. Mater. Sci. Eng., 2011, A528: 5073 |
| 23 | Abedi H R, Hanzaki A Z, Liu Z, et al. Continuous dynamic recrystallization in low density steel [J]. Mater. Des., 2017, 114: 55 |
| 24 | Gutierrez I, Castro F R, Urcola J J, et al. Static recrystallization kinetics of commercial purity aluminium after hot deformation within the steady state regime [J]. Mater. Sci. Eng., 1988, A102: 77 |
| 25 | Vandermeer R A, Jensen D J. Recrystallization in hot vs cold deformed commercial aluminum: A microstructure path comparison [J]. Acta Mater., 2003, 51: 3005 |
| 26 | Mejía I, Bedolla-Jacuinde A, Maldonado C, et al. Determination of the critical conditions for the initiation of dynamic recrystallization in boron microalloyed steels [J]. Mater. Sci. Eng., 2011, A528: 4133 |
| 27 | Chen M S, Lin Y C, Ma X S. The kinetics of dynamic recrystallization of 42CrMo steel [J]. Mater. Sci. Eng., 2012, A556: 260 |
| 28 | Deng Y H, Yang Y H, Cao J C, et al. Research on dynamic recrystallization behavior of 23Cr-2.2Ni-6.3Mn-0.26N low nickel type duplex stainless steel [J]. Acta Metall. Sin., 2019, 55: 445 |
| 28 | 邓亚辉, 杨银辉, 曹建春等. 23Cr-2.2Ni-6.3Mn-0.26N节Ni型双相不锈钢动态再结晶行为研究 [J]. 金属学报, 2019, 55: 445 |
| 29 | Chen L, Zhang Y J, Li F, et al. Modeling of dynamic recrystallization behavior of 21Cr-11Ni-N-RE lean austenitic heat-resistant steel during hot deformation [J]. Mater. Sci. Eng., 2016, A663: 119 |
| 30 | Wang Y M, Hamza A V, Ma E. Temperature-dependent strain rate sensitivity and activation volume of nanocrystalline Ni [J]. Acta Mater., 2006, 54: 2715 |
| 31 | Zhang C, Zhang L W, Shen W F, et al. Study on constitutive modeling and processing maps for hot deformation of medium carbon Cr-Ni-Mo alloyed steel [J]. Mater. Des., 2016, 90: 804 |
| 32 | Chen L, Si J Y, Liu S H, et al. Hot deformation behavior and hot processing map of extruded FGH4096 superalloy [J]. Mater. Rev., 2019, 33: 2047 |
| 32 | 陈 龙, 司家勇, 刘松浩等. 挤压态FGH4096合金的热变形行为及热加工图 [J]. 材料导报, 2019, 33: 2047 |
| 33 | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242 [J]. Metall. Trans., 1984, 15: 1883 |
| 34 | Han Y, Zou D N, Chen Z Y, et al. Investigation on hot deformation behavior of 00Cr23Ni4N duplex stainless steel under medium-high strain rates [J]. Mater. Charact., 2011, 62: 198 |
| 35 | Shi X Z, Du S W, Chen S M. Processing properties analysis of medium carbon steel based on hot processing map [J]. J. Iron Steel Res., 2019, 31: 31 |
| 35 | 师先哲, 杜诗文, 陈双梅. 基于热加工图的中碳钢加工性能分析 [J]. 钢铁研究学报, 2019, 31: 31 |
/
| 〈 |
|
〉 |