An Investigation of Interface Bonding Strength of Bimetal Plate Based on the Optimization of Asymmetric Double Cantilever Beam Model
Received date: 2020-04-10
Revised date: 2020-07-23
Online published: 2020-09-30
Supported by
Basic and Applied Basic Research Fund for Guangdong Province(2019B1515120070);Special Funds for Science and Technology Innovation of Shunde Graduate School of University of Science and Technology Beijing(BK-19BE009)
The bimetal sheet products obtained by the incremental forming are gradually gaining popularity because of their excellent properties. The forming process of the bimetal sheets is more complicated than that of the single metal sheet because it involves a complex interface between the two metal sheets. The bonding strength of the interface is an important parameter for evaluating the bonding properties of a bimetal sheet. However, if the required bonding strength is higher than the strength of the substrate, appropriate strength is difficult to achieve using only experimental methods. An improved analytical method to calculate the interface bonding strength has been proposed based on the widely used interface model of an asymmetric double cantilever beam. This improved analytical method considers the plasticity of the interface. The interface bonding strength of the explosively welded T2/A1050 copper-aluminum bimetal sheet has been assessed using the improved method, and its interface bonding strength has been found to reach 208 MPa. This bonding strength has been used in a finite element model for the forming process of the bimetal sheet. The correctness of the method has been verified by comparing the analytical results with the experimental data. Furthermore, the influence of interface bonding strength on the maximum forming depth has been explored, and it has been found that the maximum forming depth increased by 210% when the interface bonding strength increased by 38%. Moreover, a three-dimensional model including a tool, the Cu-Al bimetal sheet, and a cohesive element between the two metal sheets has been suggested for investigating the bulge defect of the forming part. The bonding strength of the interface obtained above has again been utilized in the finite element analysis. The impacts of different reductions and tool diameters on the bulge defect of the forming part have systematically been discussed. The results show that bulge defect decreased by 57% when the reduction decreased from 2.0 mm to 0.5 mm, and the bulge defect decreased by 38% when the tool diameter increased from 10 mm to 22 mm. Optimized parameters have been suggested to effectively reduce the bulge defect by 53%.
Qin QIN , Cheng LI , Liu HE , Chenlong YE , Yong ZANG . An Investigation of Interface Bonding Strength of Bimetal Plate Based on the Optimization of Asymmetric Double Cantilever Beam Model[J]. Acta Metall Sin, 2020 , 56(12) : 1617 -1628 . DOI: 10.11900/0412.1961.2020.00114
| [1] | Zhang Y X, Yang C H. Recent developments in finite element analysis for laminated composite plates [J]. Compos. Struct., 2009, 88: 147 |
| [2] | Chen X Z. Review of laminar composite metal material manufacturing technique [J]. Nonferrous Met. Mater. Eng., 2017, 38: 63 |
| [2] | (陈兴章. 层状金属复合材料技术创新及发展趋势综述 [J]. 有色金属材料与工程, 2017, 38: 63) |
| [3] | Xiong J, Ma L, Pan S, et al. Shear and bending performance of carbon fiber composite sandwich panels with pyramidal truss cores [J]. Acta Mater., 2012, 60: 1455 |
| [4] | Lü Z Y. Research on interfacial bonding strength of asynchronous rolled copper/aluminum composite plate [J]. J. Plast. Eng., 2019, 26(4): 93 |
| [4] | (吕震宇. 异步轧制铜/铝复合板界面结合强度研究 [J]. 塑性工程学报, 2019, 26(4): 93) |
| [5] | Zhou J J, Pang Y H, Su X L, et al. Development of manufacturing technology for layer-metal composite plate [J]. Mater. Rev., 2005, 19: 220 |
| [5] | (周俊杰, 庞玉华, 苏晓莉等. 金属层状复合技术的研究现状与发展 [J]. 材料导报, 2005, 19: 220) |
| [6] | Qiu B, Xing S M, Dong Q. Characterization of interfacial bonding strength of particles reinforced metal matrix composites: Theory model, finite element simulation and experimental test [J]. Mater. Rev., 2019, 33: 862 |
| [6] | (邱 博, 邢书明, 董 琦. 颗粒增强金属基复合材料界面结合强度的表征: 理论模型、有限元模拟和实验测试 [J]. 材料导报, 2019, 33: 862) |
| [7] | Muralidharan N, Chockalingam K, Dinaharan I, et al. Microstructure and mechanical behavior of AA2024 aluminum matrix composites reinforced with in situ synthesized ZrB2 particles [J]. J. Alloys?Compd., 2018, 735: 2167 |
| [8] | Kim Y K, Hong S I. Influence of interface structure and stress distribution on fracture and mechanical performance of STS439/Al1050/STS304 clad composite [J]. Mater. Sci. Eng., 2019, A749: 35 |
| [9] | Abbasi M, Salehi M T, Taheri A K. An investigation on cold roll welding of copper to aluminum using electrical resistivity [J]. Z. Metallkd., 2001, 92: 423 |
| [10] | Wang T H, Sidhar H, Mishra R S, et al. Evaluation of intermetallic compound layer at aluminum/steel interface joined by friction stir scribe technology [J]. Mater. Des., 2019, 174: 107795 |
| [11] | Zhang Z L. Theoretical and experimental study on the Iosipescu shear test method [J]. J. Aeronaut. Mater., 1996, 16(1): 55 |
| [11] | (张子龙. 复合材料面内剪切Iosipescue方法分析及试验研究 [J]. 航空材料学报, 1996, 16(1): 55) |
| [12] | You J H, Lutz W, Gerger H, et al. Fiber push-out study of a copper matrix composite with an engineered interface: Experiments and cohesive element simulation [J]. Int. J. Solids Struct., 2009, 46: 4277 |
| [13] | Nishikawa M, Okabe T, Takeda N. Determination of interface properties from experiments on the fragmentation process in single-fiber composites [J]. Mater. Sci. Eng., 2008, A480: 549 |
| [14] | Nishikawa M, Okabe T, Hemmi K, et al. Micromechanical modeling of the microbond test to quantify the interfacial properties of fiber-reinforced composites [J]. Int. J. Solids Struct., 2008, 45: 4098 |
| [15] | Ni L H. Interface and performance analysis of explosively welded Cu-Al bimetallic composite [D]. Zhenjiang: Jiangsu University of Science and Technology, 2015 |
| [15] | (倪梁华. 铜铝爆炸复合材料界面及性能分析 [D]. 镇江: 江苏科技大学, 2015) |
| [16] | Qu H P. Study on semi-analytical solution for thermoelastic composite laminated plate [D]. Tianjin: Civil Aviation University of China, 2018 |
| [16] | (屈鹤鹏. 复合材料层合板热弹性问题半解析法研究 [D]. 天津: 中国民航大学, 2018) |
| [17] | Dvorak G J, Laws N. Analysis of progressive matrix cracking in composite laminates II. First ply failure [J]. J. Compos. Mater., 1987, 21: 309 |
| [18] | Dvorak G J, Laws N, Hejazi M. Analysis of progressive matrix cracking in composite laminates I. Tthermoelastic properties of a ply with cracks [J]. J. Compos. Mater., 1985, 19: 216 |
| [19] | Reedy E D, Guess T R. Butt joint tensile strength: Interface corner stress intensity factor prediction [J]. J. Adhes. Sci. Technol., 1995, 9: 237 |
| [20] | Adams R. Structural Adhesive Joints in Engineering [M]. Netherlands: Springer, 1984: 1 |
| [21] | Dunn M L, Suwito W, Cunningham S. Fracture initiation at sharp notches: Correlation using critical stress intensities [J]. Int. J. Solids Struct., 1997, 34: 3873 |
| [22] | Maimí P, Camanho P P, Mayugo J A, et al. A continuum damage model for composite laminates: Part I—Constitutive model [J]. Mech. Mater., 2007, 39: 897 |
| [23] | Maimí P, Camanho P P, Mayugo J A, et al. A continuum damage model for composite laminates: Part II—Computational implementation and validation [J]. Mech. Mater., 2007, 39: 909 |
| [24] | Xiao F, Hui C Y, Kramer E J. Analysis of a mixed mode fracture specimen: The asymmetric double cantilever beam [J]. J. Mater. Sci., 1993, 28: 5620 |
| [25] | Bennati S, Fisicaro P, Valvo P S. An enhanced beam-theory model of the mixed-mode bending (MMB) test—Part I: Literature review and mechanical model [J]. Meccanica, 2013, 48: 443 |
| [26] | Bennati S, Fisicaro P, Valvo P S. An enhanced beam-theory model of the mixed-mode bending (MMB) test—Part II: Applications and results [J]. Meccanica, 2013, 48: 465 |
| [27] | Bennati S, Colleluori M, Corigliano D, et al. An enhanced beam-theory model of the asymmetric double cantilever beam (ADCB) test for composite laminates [J]. Compos. Sci. Technol., 2009, 69: 1735 |
| [28] | Hua X G, Li H G, Lu Y, et al. Interlaminar fracture toughness of GLARE laminates based on asymmetric double cantilever beam (ADCB) [J]. Composites, 2019, 163B: 175 |
| [29] | Williams J G. Fracture mechanics of anisotropic materials [J]. Compos. Mater. Ser., 1989, 6: 3 |
| [30] | Honarpisheh M, Jobedar M M, Alinaghian I. Multi-response optimization on single-point incremental forming of hyperbolic shape Al-1050/Cu bimetal using response surface methodology [J]. Int. J. Adv. Manuf. Technol., 2018, 96: 3069 |
| [31] | Bennati S, Valvo P S. Delamination growth in composite plates under compressive fatigue loads [J]. Compos. Sci. Technol., 2006, 66: 248 |
| [32] | Li X Q. Diffusion thickness and heat transfer performance of Cu-Al composite pate under service condions [D]. Shenyang: Shenyang University of Technology, 2019 |
| [32] | (李雪琪. 服役条件下铜铝复合板的扩散层厚度及传热性能 [D]. 沈阳: 沈阳工业大学, 2019) |
/
| 〈 |
|
〉 |