Microstruture and Properties of Ti/TNTZO Multi-Layered Material by Direct Laser Deposition
Received date: 2020-07-13
Revised date: 2020-08-03
Online published: 2020-09-16
Supported by
National Natural Science Foundation of China(51871152)
Commercially pure titanium (CP-Ti) is a human-implant metal material commonly used for cardiovascular scaffolds and dental implants in the medical field. This is because CP-Ti has better biocompatibility and corrosion resistance compared to other alloys such as titanium-aluminum-vanadium alloy (Ti-6Al-4V). However, the low strength properties of CP-Ti have limited its wider application (e.g., load-bearing components). On the contrary, Novel β titanium alloys possess higher strength and lower elastic modulus, which has led to the consideration of Ti-Nb based alloys for biomedical applications, while also taking into consideration their biocompatibility and other mechanical properties. Recently, laminated metal composites (LMCs) have attracted a lot of attention due to the excellent properties of the constituent alloys. Direct laser deposition (DLD) is an additive manufacturing technology that can be potentially used to manufacture LMCs. In this work, the DLD process was used to manufacture Ti/TNTZO LMC, and CP-Ti and TNTZO alloy powders were the raw materials. Subsequently, the microstructure, phase composition, mechanical properties, and in vitro bioactivity of the Ti/TNTZO LMCs were analyzed. The results demonstrated that high-density, crack-free Ti/TNTZO can be fabricated using the DLD process. Ti/TNTZO is mainly composed of α/α' and β phases. Transmitted Kikuchi diffraction maps showed the presence of α" martensite, but due to its low content, there were no relevant peaks in the X-ray powder diffraction spectra. The hardness of the Ti region in the Ti/TNTZO increased due to the diffusion of alloy elements and refinement of the structure formed as a result of a faster cooling rate. However, for the TNTZO region, the hardness also increased due to the martensite transformation caused by the dilution of β-stabilizing elements compared with the TNTZO manufactured using the DLD process. In comparison with the CP-Ti and TNTZO made using the DLD process, the microstructure of the Ti/TNTZO multilayered materials was significantly different. The microstructure of Ti layers had coarse columnar grains and fine α/α' plates, and there was acicular martensite at the subgrain boundary of the TNTZO layers. As a result of the alloy elements diffusion, transition layer with a size of approximately 50 μm was found between the Ti layer and TNTZO layer. The tensile test results also showed that the multilayered materials have high yield strength and ultimate tensile strength. However, the presence of acicular martensite at the interface reduces the plasticity of the materials. Additionally, the Ti/TNTZO multilayered materials showed good ability to induce apatite formation after soaking in simulated body fluid for 14 d. Therefore, the results of this study showed that the Ti/TNTZO multilayered composites fabricated using the DLD process have potential application in the biomedical field.
Key words: multi-layered material; direct laser deposition; TNTZO; dual-phase Ti alloy; implant
Ting ZHANG , Zhongjie LI , Hao XU , Anping DONG , Dafan DU , Hui XING , Donghong WANG , Baode SUN . Microstruture and Properties of Ti/TNTZO Multi-Layered Material by Direct Laser Deposition[J]. Acta Metall Sin, 2021 , 57(6) : 757 -766 . DOI: 10.11900/0412.1961.2020.00255
| 1 | Zheng Y F, Wu Y H. Revolutionizing metallic biomaterials [J]. Acta Metall. Sin., 2017, 53: 257 |
| 1 | 郑玉峰, 吴远浩. 处在变革中的医用金属材料 [J]. 金属学报, 2017, 53: 257 |
| 2 | Niinomi M. Recent research and development in titanium alloys for biomedical applications and healthcare goods [J]. Sci. Technol. Adv. Mater., 2003, 4: 445 |
| 3 | Jacobs J J, Skipor A K, Patterson L M, et al. Metal release in patients who have had a primary total hip arthroplasty. A prospective, controlled, longitudinal study [J]. J. Bone Joint Surg., 1998, 80: 1447 |
| 4 | An B L, Li Z R, Diao X O, et al. In vitro and in vivo studies of ultrafine-grain Ti as dental implant material processed by ECAP [J]. Mater. Sci. Eng., 2016, C67: 34 |
| 5 | Geetha M, Singh A K, Asokamani R, et al. Ti based biomaterials, the ultimate choice for orthopaedic implants—A review [J]. Prog. Mater. Sci., 2009, 54: 397 |
| 6 | Wang Q, Han C J, Choma T, et al. Effect of Nb content on microstructure, property and in vitro apatite-forming capability of Ti-Nb alloys fabricated via selective laser melting [J]. Mater. Des., 2017, 126: 268 |
| 7 | Mareci D, Chelariu R, Gordin D M, et al. Comparative corrosion study of Ti-Ta alloys for dental applications [J]. Acta Biomater., 2009, 5: 3625 |
| 8 | Zhao X F, Niinomi M, Nakai M, et al. Beta type Ti-Mo alloys with changeable Young's modulus for spinal fixation applications [J]. Acta Biomater., 2012, 8: 1990 |
| 9 | Li Y C, Ding Y F, Munir K, et al. Novel β-Ti35Zr28Nb alloy scaffolds manufactured using selective laser melting for bone implant applications [J]. Acta Biomater., 2019, 87: 273 |
| 10 | Zhang J R, Zhang Y W, Hao Y L, et al. Plastic deformation behavior of biomedical Ti-24Nb-4Zr-8Sn single crystal alloy [J]. Acta Metall. Sin., 2017, 53: 1385 |
| 10 | 张金睿, 张晏玮, 郝玉琳等. 生物医用Ti-24Nb-4Zr-8Sn单晶合金塑性变形行为研究 [J]. 金属学报, 2017, 53: 1385 |
| 11 | Bai Y, Li S J, Hao Y L, et al. Electrochemical corrosion behavior of a new biomedical Ti-24Nb-4Zr-8Sn alloy in Hanks solution [J]. Acta Metall. Sin., 2012, 48: 76 |
| 11 | 白 芸, 李述军, 郝玉琳等. 新型医用Ti-24Nb-4Zr-8Sn合金在Hanks溶液中的电化学腐蚀行为研究 [J]. 金属学报, 2012, 48: 76 |
| 12 | Wang S P, Xu J. TiZrNbTaMo high-entropy alloy designed for orthopedic implants: As-cast microstructure and mechanical properties [J]. Mater. Sci. Eng., 2017, C73: 80 |
| 13 | Saito T, Furuta T, Hwang J H, et al. Multifunctional alloys obtained via a dislocation-free plastic deformation mechanism [J]. Science, 2003, 300: 464 |
| 14 | Tane M, Nakano T, Kuramoto S, et al. Low young's modulus in Ti-Nb-Ta-Zr-O alloys: Cold working and oxygen effects [J]. Acta Mater., 2011, 59: 6975 |
| 15 | Guo W Y, Sun J, Wu J S. Electrochemical and XPS studies of corrosion behavior of Ti-23Nb-0.7Ta-2Zr-O alloy in Ringer's solution [J]. Mater. Chem. Phys., 2009, 113: 816 |
| 16 | Li J S, Wang S Z, Mao Q Z, et al. Soft/hard copper/bronze laminates with superior mechanical properties [J]. Mater. Sci. Eng., 2019, A756: 213 |
| 17 | Putra N E, Mirzaali M J, Apachitei I, et al. Multi-material additive manufacturing technologies for Ti-, Mg-, and Fe-based biomaterials for bone substitution [J]. Acta Biomater., 2020, 109: 1 |
| 18 | Zhang K, Tian X, Bermingham M, et al. Effects of boron addition on microstructures and mechanical properties of Ti-6Al-4V manufactured by direct laser deposition [J]. Mater. Des., 2019, 184: 108191 |
| 19 | Lima D D, Mantri S A, Mikler C V, et al. Laser additive processing of a functionally graded internal fracture fixation plate [J]. Mater. Des., 2017, 130: 8 |
| 20 | Schneider-Maunoury C, Weiss L, Perroud O, et al. An application of differential injection to fabricate functionally graded Ti-Nb alloys using DED-CLAD? process [J]. J. Mater. Process. Technol., 2019, 268: 171 |
| 21 | He B, Xing M, Yang G, et al. Effect of composition gradient on microstructure and properties of laser deposition TC4/TC11 interface [J]. Acta Metall. Sin., 2019, 55: 1251 |
| 21 | 何 波, 邢 盟, 杨 光, 等. 成分梯度对激光沉积制造TC4/TC11连接界面组织和性能的影响 [J]. 金属学报, 2019, 55: 1251 |
| 22 | Liu Y, Liang C P, Liu W S, et al. Dilution of Al and V through laser powder deposition enables a continuously compositionally Ti/Ti6Al4V graded structure [J]. J. Alloys Compd., 2018, 763: 376 |
| 23 | Xu H, Xing H, Dong A P, et al. Investigation of gum metal coating on Ti6Al4V plate by direct laser deposition [J]. Surf. Coat. Technol., 2019, 363: 161 |
| 24 | Zhao X, Song B, Fan W R, et al. Selective laser melting of carbon/AlSi10Mg composites: Microstructure, mechanical and electronical properties [J]. J. Alloys Compd., 2016, 665: 271 |
| 25 | Kasperovich G, Haubrich J, Gussone J, et al. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting [J]. Mater. Des., 2016, 105: 160 |
| 26 | Sun Y, Moroz A, Alrbaey K. Sliding wear characteristics and corrosion behaviour of selective laser melted 316L stainless steel [J]. J. Mater. Eng. Perform., 2014, 23: 518 |
| 27 | Meacock C, Vilar R. Laser powder microdeposition of CP2 titanium [J]. Mater. Des., 2008, 29: 353 |
| 28 | Attar H, Calin M, Zhang L C, et al. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium [J]. Mater. Sci. Eng., 2014, A593: 170 |
| 29 | Li X P, van Humbeeck J, Kruth J P. Selective laser melting of weak-textured commercially pure titanium with high strength and ductility: A study from laser power perspective [J]. Mater. Des., 2017, 116: 352 |
| 30 | Yamanaka K, Saito W, Mori M, et al. Preparation of weak-textured commercially pure titanium by electron beam melting [J]. Addit. Manuf., 2015, 8: 105 |
| 31 | Reichardt A, Dillon R P, Borgonia J P, et al. Development and characterization of Ti-6Al-4V to 304L stainless steel gradient components fabricated with laser deposition additive manufacturing [J]. Mater. Des., 2016, 104: 404 |
| 32 | Dinda G P, Dasgupta A K, Mazumder J. Laser aided direct metal deposition of Inconel 625 superalloy: Microstructural evolution and thermal stability [J]. Mater. Sci. Eng., 2009, A509: 98 |
| 33 | Yan H. Microstructure and interfacial characteristics of wear-resistant composite coatings on copper by laser cladding [D]. Wuhan: Huazhong University of Science and Technology, 2010 |
| 33 | 闫 华. 铜合金表面激光复合耐磨层及界面特性研究 [D]. 武汉: 华中科技大学, 2010 |
| 34 | Boyer R, Welsch G, Collings E W. Materials properties handbook: Titanium alloys [R]. Materials Park: ASM, 1994 |
| 35 | Wu X D, Yang G J, Ge P, et al. Inductions of β titanium alloy and solid state phase transition [J]. Titan. Ind. Prog., 2008, 25(5): 1 |
| 35 | 吴晓东, 杨冠军, 葛 鹏等. β钛合金及其固态相变的归纳 [J]. 钛工业进展, 2008, 25(5): 1 |
| 36 | Zhang T, Xu H, Li Z J, et al. Microstructure and properties of TC4/TNTZO multi-layered composite by direct laser deposition [J]. J. Mech. Behav. Biomed. Mater., 2020, 109: 103842 |
| 37 | Zhao D L, Han C J, Li J J, et al. In situ fabrication of a titanium-niobium alloy with tailored microstructures, enhanced mechanical properties and biocompatibility by using selective laser melting [J]. Mater. Sci. Eng., 2020, C111: 110784 |
| 38 | Behera R R, Hasan A, Sankar M R, et al. Laser cladding with HA and functionally graded TiO2-HA precursors on Ti-6Al-4V alloy for enhancing bioactivity and cyto-compatibility [J]. Surf. Coat. Technol., 2018, 352: 420 |
/
| 〈 |
|
〉 |