Research paper

Effect of Ti on β Structural Stability and Mechanical Properties of Zr-Nb Binary Alloys

  • Mingkang WANG ,
  • Junhao YUAN ,
  • Yufeng LIU ,
  • Qing WANG ,
  • Chuang DONG ,
  • Zhongwei ZHANG
Expand
  • 1.Key Laboratory of Materials Modification by Laser, Ion and Electron Beams (Ministry of Education), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
    2.Science and Technology of Advanced Functional Composites Laboratory, Aerospace Research Institute of Materials and Processing Technology, Beijing 100076, China
    3.Institute of Advanced Structure Technology, Beijing Institute of Technology, Beijing 100081, China

Received date: 2020-04-20

  Revised date: 2020-08-25

  Online published: 2020-09-09

Supported by

National Key Research and Development Program of China(2017YFB0702401);National Natural Science Foundation of China(91860108);Natural Science Foundation of Liaoning Province of China(2019-KF-05-01)

Abstract

Metastable bcc β-Zr alloys generally have low elastic modulus, magnetic susceptibility, good mechanical properties, corrosion resistance, and biocompatibility, which are ascribed to co-alloying of multiple elements to enhance the structural stability of the bcc-β phase. This work systematically investigated the effects of Nb and Ti elements on the structural stability of the bcc-β phase and mechanical properties of Zr-Nb-Ti alloys. Various binary [Zr-Zr14](Zr, Nb)3 alloy compositions were designed by the cluster formula approach, based on which Ti was substituted for the base Zr to form ternary alloys. Alloy rods were prepared by the copper-mold suction-cast method with vacuum protection. The microstructure and mechanical properties of the alloys were characterized using XRD, OM, and TEM etc. The results show that the crystal structures of the Zr-Nb binary alloys could change from hcp-α to bcc-β with increasing Nb content, whereas, the ω-phase always coexists with the β-phase. An appropriate amount of Ti addition can significantly inhibit the precipitation of ω, resulting in the further improvement of the stability of the β-phase. The single β-[Ti-Zr14]Nb3 (Zr-17.37Nb-2.98Ti, mass fraction, %) ternary alloy exhibited not only a low elastic modulus of E=57 GPa but also a good tensile property with a high yield strength of σYS=557 MPa and an elongation of δ=15.5%.

Cite this article

Mingkang WANG , Junhao YUAN , Yufeng LIU , Qing WANG , Chuang DONG , Zhongwei ZHANG . Effect of Ti on β Structural Stability and Mechanical Properties of Zr-Nb Binary Alloys[J]. Acta Metall Sin, 2021 , 57(1) : 95 -102 . DOI: 10.11900/0412.1961.2020.00125

References

1 Yamamoto A, Honma R, Sumita M. Cytotoxicity evaluation of 43 metal salts using murine fibroblasts and osteoblastic cells [J]. J. Biomed. Mater. Res., 1998, 39: 331
2 Guo S F, Liu Z, Chan K C, et al. A plastic Ni-free Zr-based bulk metallic glass with high specific strength and good corrosion properties in simulated body fluid [J]. Mater. Lett., 2012, 84: 81
3 Mantripragada V P, Lecka-Czernik B, Ebraheim N A, et al. An overview of recent advances in designing orthopedic and craniofacial implants [J]. J. Biomed. Mater. Res., 2013, 101A: 3349
4 Li H F, Zhou F Y, Li L, et al. Design and development of novel MRI compatible zirconium-ruthenium alloys with ultralow magnetic susceptibility [J]. Sci. Rep., 2016, 6: 24414
5 Pêcheur D, Lefebvre F, Motta A T, et al. Effect of irradiation on the precipitate stability in Zr alloys [J]. J. Nucl. Mater., 1993, 205: 445
6 Geetha M, Singh A K, Asokamani R, et al. Ti based biomaterials, the ultimate choice for orthopaedic implants—A review [J]. Prog. Mater Sci., 2009, 54: 397
7 Li Y H, Yang C, Zhao H D, et al. New developments of Ti-based alloys for biomedical applications [J]. Materials, 2014, 7: 1709
8 Suyalatu, Nomura N, Oya K, et al. Microstructure and magnetic susceptibility of as-cast Zr-Mo alloys [J]. Acta Biomater., 2010, 6: 1033
9 Yang H L, Kano S, Matsukawa Y, et al. Study on recrystallization and correlated mechanical properties in Mo-modified Zr-Nb alloys [J]. Mater. Sci. Eng., 2016, A661: 9
10 ? Zuzjaková, Zeman P, Haviar S, et al. Thermal stability of structure, microstructure and enhanced properties of Zr-Ta-O films with a low and high Ta content [J]. Surf. Coat. Technol., 2018, 335: 95
11 Pang C, Wang Q, Zhang R Q, et al. β Zr-Nb-Ti-Mo-Sn alloys with low Young??s modulus and low magnetic susceptibility optimized via a cluster-plus-glue-atom model [J]. Mater. Sci. Eng., 2015, A626: 369
12 Cai S, Daymond M R, Khan A K, et al. Elastic and plastic properties of βZr at room temperature [J]. J. Nucl. Mater., 2009, 393: 67
13 Kondo R, Nomura N, Suyalatu, et al. Microstructure and mechanical properties of as-cast Zr-Nb alloys [J]. Acta Biomater., 2011, 7: 4278
14 Kondo R, Shimizu R, Nomura N, et al. Effect of cold rolling on the magnetic susceptibility of Zr-14Nb alloy [J]. Acta Biomater., 2013, 9: 5795
15 Dey G K, Tewari R, Banerjee S, et al. Formation of a shock deformation induced ω phase in Zr-20Nb alloy [J]. Acta Mater., 2004, 52: 5243
16 Srivastava D, Mukhopadhyay P, Banerjee S, et al. Morphology and substructure of lath martensites in dilute Zr-Nb alloys [J]. Mater. Sci. Eng., 2000, A288: 101
17 Ikeda M, Miyazaki T, Doi S, et al. Phase constitution and heat treatment behavior of Zr-Nb alloys [J]. Mater. Sci. Forum, 2007, 561: 1435
18 Dey G K, Tewari R, Banerjee S, et al. Formation of a shock deformation induced ω phase in Zr-20Nb alloy [J]. Acta Mater., 2004, 52: 5243
19 Banerjee S, Krishnan R. Martensitic transformation in zirconium-niobium alloys [J]. Acta Metall., 1971, 19: 1317
20 Dey G K, Singh R N, Tewari R, et al. Metastability of the β-phase in Zr-rich Zr-Nb alloys [J]. J. Nucl. Mater., 1995, 224: 146
21 Jiang B B, Wang Q, Wen D H, et al. Effects of Nb and Zr on structural stabilities of Ti-Mo-Sn-based alloys with low modulus [J]. Mater. Sci. Eng., 2017, A687: 1
22 Jiang B B, Wang Q, Li X N, et al. Structural stability of the metastable β-[(Mo0.5Sn0.5)-(Ti13Zr1)]Nb1 alloy with low Young's modulus at different states [J]. Metall. Mater. Trans., 2017, 48A: 3912
23 Pang C, Jiang B B, Shi Y, et al. Cluster-plus-glue-atom model and universal composition formulas [cluster](glue atom)x for BCC solid solution alloys [J]. J. Alloys Compd., 2015, 652: 63
24 Hong H L, Wang Q, Dong C, et al. Understanding the Cu-Zn brass alloys using a short-range-order cluster model: Significance of specific compositions of industrial alloys [J]. Sci. Rep., 2014, 4: 7065
25 Wang Q, Ji C J, Wang Y M, et al. β-Ti alloys with low Young??s moduli interpreted by cluster-plus-glue-atom model [J]. Metall. Mater. Trans., 2013, 44A: 1872
26 Weiss I, Semiatin S L. Thermomechanical processing of beta titanium alloys—An overview [J]. Mater. Sci. Eng., 1998, A243: 46
27 Wang Q, Dong C, Liaw P K. Structural stabilities of β-Ti alloys studied using a new Mo equivalent derived from [β/(α+β)] phase-boundary slopes [J]. Metall. Mater. Trans., 2015, 46A: 3440
28 Zhang J Y, Fan S, Hao Y L, et al. Influence of equiatomic Zr/Nb substitution on superelastic behavior of Ti-Nb-Zr alloy [J]. Mater. Sci. Eng., 2013, A563: 78
29 Bagaryatskiy Y A, Nosova G I. On the crystalline structure and the nature of the ω-phase in titanium alloys with chrome [J]. Fiz. Met. Metalloved., 1962, 13: 415
30 Sun F, Zhang J Y, Marteleur M, et al. Investigation of early stage deformation mechanisms in a metastable β titanium alloy showing combined twinning-induced plasticity and transformation-induced plasticity effects [J]. Acta Mater., 2013, 61: 6406
31 Ping D H, Mitarai Y, Yin F X. Microstructure and shape memory behavior of a Ti-30Nb-3Pd alloy [J]. Scr. Mater., 2005, 52: 1287
32 Banerjee S, Tewari R, Dey G K. Omega phase transformation-morphologies and mechanisms [J]. Z. Metallkd., 2006, 97: 963
Outlines

/