Fracture Location Shift of Dissimilar Metal Welds Under Coupled Thermal-Stress Effect
Received date: 2020-05-06
Revised date: 2020-07-21
Online published: 2020-09-08
Supported by
National Natural Science Foundation of China(51775300);National Natural Science Foundation of China(51901113)
Dissimilar metal welds (DMWs) between high-Cr martensitic heat-resistant steels and nickel-based alloys with nickel-based filler metals are widely used in fossil-fired power plants. Reports of premature failures of DMW joints have attracted considerable attention as such occurrences in the field can lead to significant economic loss and safety issues. Moreover, a comprehensive understanding of the high-temperature performance of new types of DMWs is lacking. In this work, creep tests were conducted over a stress range of 140~260 MPa at of 600 and 620 ℃. A shift in the fracture location with variations in stress was observed, with three typical failure modes. At high stress levels (240~260 MPa), the DMW fractured in the base metal (BM) of martensitic steel, accompanied by a large degree of plastic deformation. At intermediate stress levels (200~240 MPa), the DMW fractured in the fine-grained heat-affected zone (FGHAZ) and the inter-critical heat-affected zone (ICHAZ), with creep cavities around coarsened carbides, indicating a typical type IV crack. At low stress levels (140~200 MPa), the DMW fractured in a mixed mode involving three stages. First, a crack initiated at the interface between the nickel-based weld metal and the martensitic steel, which was attributed to the interaction between the oxidation behavior of the martensitic steels and the thermal stress arising from the mismatch in the coefficients of thermal expansion. Second, the crack deflected into the FGHAZ/ICHAZ and developed into a type IV crack mode. Finally, the crack propagated into the adjacent BM, featuring significant plastic deformation. In addition, in the stress-LMP (Larson-Miller parameter) plot, the creep life at a relatively low stress level was shorter than that predicted by linear extrapolation of the data obtained at a high stress level, indicating a premature failure tendency at low stress. This premature failure tendency can be attributed to microstructure degradation in HAZs and preferential oxidation at the interface at low stress levels.
Kejian LI , Yu ZHANG , Zhipeng CAI . Fracture Location Shift of Dissimilar Metal Welds Under Coupled Thermal-Stress Effect[J]. Acta Metall Sin, 2020 , 56(11) : 1463 -1473 . DOI: 10.11900/0412.1961.2020.00140
| [1] | Bhaduri A K, Venkadesan S, Rodriguez P, et al. Transition metal joints for steam generators—An overview [J]. Int . J. Press. Vessels Pip., 1994, 58: 251 |
| [2] | DuPont J N. Microstructural evolution and high temperature failure of ferritic to austenitic dissimilar welds [J]. Int. Mater. Rev., 2012, 57: 208 |
| [3] | Parker J D, Stratford G C. Review of factors affecting condition assessment of nickel based transition joints [J]. Sci. Technol. Weld. Joining, 1999, 4: 29 |
| [4] | Dooley R B, Stephenson G G, Tinkler M J, et al. Ontario Hydro experience with dissimilar metal welds in boiler tubing [J]. Weld. J., 1982, 61(suppl.): 45S |
| [5] | Parameswaran P, Laha K. Role of microstructure on creep rupture behaviour of similar and dissimilar joints of modified 9Cr-1Mo steel [J]. Procedia Eng., 2013, 55: 438 |
| [6] | Shin K Y, Lee J W, Han J M, et al. Transition of creep damage region in dissimilar welds between Inconel 740H Ni-based superalloy and P92 ferritic/martensitic steel [J]. Mater. Charact., 2018, 139: 144 |
| [7] | Xu L Y, Wang Y F, Jing H Y, et al. Deformation mechanism and microstructure evolution of T92/S30432 dissimilar welded joint during creep [J]. J. Mater. Eng. Perform., 2016, 25: 3960 |
| [8] | Parker J D, Stratford G C. Characterisation of microstructures in nickel based transition joints [J]. J. Mater. Sci., 2000, 35: 4099 |
| [9] | Nicholson R D. Effect of aging on interfacial structures of nickel-based transition joints [J]. Met. Technol., 1984, 11: 115 |
| [10] | Laha K, Chandravathi K S, Parameswaran P, et al. A comparison of creep rupture strength of ferritic/austenitic dissimilar weld joints of different grades of Cr-Mo ferritic steels [J]. Metall. Mater. Trans., 2012, 43A: 1174 |
| [11] | Parker J D, Stratford G C. The high-temperature performance of nickel-based transition joints-Ⅱ. Fracture behaviour [J]. Mater. Sci. Eng., 2001, A299: 174 |
| [12] | Nicholson R D. Creep rupture properties of nickel-base transition joints after long-term service [J]. Mater. Sci. Technol., 1986, 2: 686 |
| [13] | Klueh R L, King J F. Austenitic stainless steel-ferritic steel weld joint failures [J]. Weld. J., 1982, 61(suppl.): 302S |
| [14] | Matsunaga T, Hongo H, Tabuchi M. Interfacial failure in dissimilar weld joint of high boron 9% chromium steel and nickel-based alloy under high-temperature creep condition [J]. Mater. Sci. Eng., 2017, A695: 302 |
| [15] | Gittos M F, Gooch T G. The interface below stainless steel and nickel-alloy claddings [J]. Weld. J., 1992, 71(suppl.): 461S |
| [16] | Sireesha M, Albert S K, Sundaresan S. Thermal cycling of transition joints between modified 9Cr-1Mo steel and alloy 800 for steam generator application [J]. Int . J. Press. Vessels Pip., 2002, 79: 819 |
| [17] | Williams J A, Parker J D. Effect of thermal cycling on creep behaviour of 2.25Cr-1Mo/type 316 steel dissimilar metal welds [J]. Mater. Sci. Technol., 1994, 10: 915 |
| [18] | Friedmann V, Siegele D. Damage behaviour of nickel-based transition welds under cyclic thermomechanical loading [J]. Mater. High Temp., 2010, 27: 35 |
| [19] | Mayr P, Schlacher C, Siefert J A, et al. Microstructural features, mechanical properties and high temperature failures of ferritic to ferritic dissimilar welds [J]. Int. Mater. Rev., 2019, 64: 1 |
| [20] | Laha K, Chandravathi K S, Parameswaran P, et al. Characterization of microstructures across the heat-affected zone of the modified 9Cr-1Mo weld joint to understand its role in promoting type Ⅳ cracking [J]. Metall. Mater. Trans., 2007, 38A: 58 |
| [21] | Wang X, Pan Q G, Tao Y S, et al. Type Ⅳ creep rupture characteristics of P92 steel weldment [J]. Acta Metall. Sin., 2012, 48: 427 |
| [21] | (王 学, 潘乾刚, 陶永顺等. P92钢焊接接头Ⅳ型蠕变断裂特性 [J]. 金属学报, 2012, 48: 427) |
| [22] | Abson D J, Rothwell J S. Review of type Ⅳ cracking of weldments in 9-12%Cr creep strength enhanced ferritic steels [J]. Int. Mater. Rev., 2013, 58: 437 |
| [23] | Liu Y, Tsukamoto S, Shirane T, et al. Formation mechanism of type IV failure in high Cr ferritic heat-resistant steel-welded joint [J]. Metall. Mater. Trans., 2013, 44A: 4626 |
| [24] | Tabuchi M, Hongo H, Abe F. Creep strength of dissimilar welded joints using high B-9Cr steel for advanced USC boiler [J]. Metall. Mater. Trans., 2014, 45A: 5068 |
| [25] | Wright I G, Dooley R B. A review of the oxidation behaviour of structural alloys in steam [J]. Int. Mater. Rev., 2010, 55: 129 |
/
| 〈 |
|
〉 |