Microstructures and Mechanical Properties of TA15 Titanium Alloy and Graphene Reinforced TA15 Composites Prepared by Spark Plasma Sintering
Received date: 2020-05-29
Revised date: 2020-08-17
Online published: 2020-08-28
Supported by
National Natural Science Foundation of China(51674093)
Titanium alloys and titanium-based composites are widely used in the field of aerospace owing to their advantages such as low density and high specific strength. Graphene has been found to significantly improve the mechanical properties of metal matrix composites at a lower content due to high modulus, fracture strength, and specific surface area. To achieve excellent mechanical properties, TA15 titanium alloy was fabricated via spark plasma sintering (SPS), and the effects of sintering temperature, sintering time, and sintering pressure on the densification, microstructure, and mechanical properties of the obtained alloys were investigated. The results indicate that the sintering parameters exert trivial effect on the phase composition of the sintered TA15 titanium alloy. The microstructure of the sintered alloy is mainly determined by the sintering temperature, and the prolonged sintering time will cause microstructure coarsening. Meanwhile, the sintering pressure does not have obvious effect on the sintered microstructure. Furthermore, higher sintering temperature, longer sintering time, and accurate increase in sintering pressure contribute to the densification process of TA15 titanium alloy. At room and high temperatures, the comprehensive mechanical properties exhibited by the sintered TA15 titanium alloy are determined by density and microstructure. The dense TA15 titanium alloy can be fabricated via SPS under the sintering conditions of 900oC, 50 MPa, and 5 min. Such alloy exhibits optimally comprehensive mechanical properties at room and high temperatures. Additionally, 0.5% (mass fraction) graphene reinforced TA15 composites were fabricated by SPS under the sintering conditions of 900oC, 50 MPa, and 7 min. When compared with TA15 titanium alloy, the compression yield strength and ultimate compressive strength of composites have significantly improved at room and high temperatures.
Zhangqian LIN , Wei ZHENG , Hao LI , Dongjun WANG . Microstructures and Mechanical Properties of TA15 Titanium Alloy and Graphene Reinforced TA15 Composites Prepared by Spark Plasma Sintering[J]. Acta Metall Sin, 2021 , 57(1) : 111 -120 . DOI: 10.11900/0412.1961.2020.00186
| 1 | Khanna N, Davim J P. Design-of-experiments application in machining titanium alloys for aerospace structural components [J]. Measurement, 2015, 61: 280 |
| 2 | Williams J C, Starke E A. Progress in structural materials for aerospace systems [J]. Acta Mater., 2003, 51: 5775 |
| 3 | Singh P, Pungotra H, Kalsi N S. On the characteristics of titanium alloys for the aircraft applications [J]. Mater. Today, 2017, 4: 8971 |
| 4 | Gao A, Hang R Q, Bai L, et al. Electrochemical surface engineering of titanium-based alloys for biomedical application [J]. Electrochim. Acta, 2018, 271: 699 |
| 5 | Leyens C, Peters M. Titanium and Titanium Alloys [M]. 2nd Ed., Weinheim: Wiley-VCH, 2003: 2 |
| 6 | Cheng C, Chen Z Y, Qin X S, et al. Microstructure, texture and mechanical property of TA32 titanium alloy thick plate [J]. Acta Metall. Sin., 2020, 56: 193 |
| 6 | 程 超, 陈志勇, 秦绪山等. TA32钛合金厚板的微观组织、织构与力学性能 [J]. 金属学报, 2020, 56: 193 |
| 7 | Xu Q D, Li K J, Cai Z P, et al. Effect of pulsed magnetic field on the microstructure of TC4 titanium alloy and its mechanism [J]. Acta Metall. Sin., 2019, 55: 489 |
| 7 | 许擎栋, 李克俭, 蔡志鹏等. 脉冲磁场对TC4钛合金微观结构的影响及其机理探究 [J]. 金属学报, 2019, 55: 489 |
| 8 | Zhu S, Yang H, Guo L G, et al. Effect of cooling rate on microstructure evolution during α/β heat treatment of TA15 titanium alloy [J]. Mater. Charact., 2012, 70: 101 |
| 9 | Sun Y, Luo G Q, Zhang J, et al. Phase transition, microstructure and mechanical properties of TC4 titanium alloy prepared by plasma activated sintering [J]. J. Alloys Compd., 2018, 741: 918 |
| 10 | Lütjering G. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys [J]. Mater. Sci. Eng., 1998, A243: 32 |
| 11 | Sun Q J, Xie X. Microstructure and mechanical properties of TA15 alloy after thermo-mechanical processing [J]. Mater. Sci. Eng., 2018, A724: 493 |
| 12 | Kinloch I A, Suhr J, Lou J, et al. Composites with carbon nanotubes and graphene: An outlook [J]. Science, 2018, 362: 547 |
| 13 | Santosh M V, Suresh K R, Aithal S K. Mechanical characterization and microstructure analysis of Al C355.0 by sand casting, die casting and centrifugal casting techniques [J]. Mater. Today, 2017, 4: 10987 |
| 14 | Hodbe G A, Shinde B R. Design and simulation of LM 25 sand casting for defect minimization [J]. Mater. Today, 2018, 5: 4489 |
| 15 | Azevedo J M C, Serrenho A C, Allwood J M. Energy and material efficiency of steel powder metallurgy [J]. Powder Technol., 2018, 328: 329 |
| 16 | Patil O M, Khedkar N N, Sachit T S, et al. A review on effect of powder metallurgy process on mechanical and tribological properties of hybrid nano composites [J]. Mater. Today, 2018, 5: 5802 |
| 17 | Sluzalec A. Stochastic characteristics of powder metallurgy processing [J]. Appl. Math. Model., 2015, 39: 7303 |
| 18 | Li X P, Yan M, Imai H, et al. The critical role of heating rate in enabling the removal of surface oxide films during spark plasma sintering of Al-based bulk metallic glass powder [J]. J. Non-Cryst. Solids, 2013, 375: 95 |
| 19 | Bonifacio C S, Holland T B, van Benthem K. Evidence of surface cleaning during electric field assisted sintering [J]. Scr. Mater., 2013, 69: 769 |
| 20 | Zhang Z H, Liu Z F, Lu J F, et al. The sintering mechanism in spark plasma sintering—Proof of the occurrence of spark discharge [J]. Scr. Mater., 2014, 81: 56 |
| 21 | Ceja-Cárdenas L, Lemus-Ruíz J, Jaramillo-Vigueras D, et al. Spark plasma sintering of α-Si3N4 ceramics with Al2O3 and Y2O3 as additives and its morphology transformation [J]. J. Alloys Compd., 2010, 501: 345 |
| 22 | Wang D J, Li H, Wang X S, et al. The microstructure evolution and mechanical properties of TiBw/TA15 composite with network structure prepared by rapid current assisted sintering [J]. Metals, 2019, 9: 540 |
| 23 | Feng H B, Jia D C, Zhou Y. Spark plasma sintering reaction synthesized TiB reinforced titanium matrix composites [J]. Composites, 2005, 36A: 558 |
| 24 | Wang D J, Yuan H, Qiang J M. The microstructure evolution, mechanical properties and densification mechanism of TiAl-based alloys prepared by spark plasma sintering [J]. Metals, 2017, 7: 201 |
| 25 | Asl M S, Namini A S, Motallebzadeh A, et al. Effects of sintering temperature on microstructure and mechanical properties of spark plasma sintered titanium [J]. Mater. Chem. Phys., 2018, 203: 266 |
| 26 | Miklaszewski A, Garbiec D, Niespodziana K. Sintering behavior and microstructure evolution in cp-titanium processed by spark plasma sintering [J]. Adv. Powder Technol., 2018, 29: 50 |
| 27 | Falodun O E, Obadele B A, Oke S R, et al. Effect of sintering parameters on densification and microstructural evolution of nano-sized titanium nitride reinforced titanium alloys [J]. J. Alloys Compd., 2018, 736: 202 |
| 28 | Zhang F M, Wang J, Liu T F, et al. Enhanced mechanical properties of few-layer graphene reinforced titanium alloy matrix nanocomposites with a network architecture [J]. Mater. Des., 2020, 186: 108330 |
| 29 | Zhao Y, Guo H Z, Shi Z F, et al. Microstructure evolution of TA15 titanium alloy subjected to equal channel angular pressing and subsequent annealing at various temperatures [J]. J. Mater. Process. Technol., 2011, 211: 1364 |
| 30 | Sun Z C, Yang H, Han G J, et al. A numerical model based on internal-state-variable method for the microstructure evolution during hot-working process of TA15 titanium alloy [J]. Mater. Sci. Eng., 2010, A527: 3464 |
| 31 | Fan X G, Yang H, Yan S L, et al. Mechanism and kinetics of static globularization in TA15 titanium alloy with transformed structure [J]. J. Alloys Compd., 2012, 533: 1 |
| 32 | Chen H, Mi G B, Li P J, et al. Effects of graphene oxide on microstructure and mechanical properties of 600oC high temperature titanium alloy [J]. J. Mater. Eng., 2019, 47(9): 38 |
| 32 | 陈 航, 弭光宝, 李培杰等. 氧化石墨烯对600℃高温钛合金微观组织和力学性能的影响 [J]. 材料工程, 2019, 47(9): 38 |
| 33 | Cao H C, Liang Y L. The microstructures and mechanical properties of graphene-reinforced titanium matrix composites [J]. J. Alloys Compd., 2020, 812: 152057 |
| 34 | Dong L L, Chen W G, Deng N, et al. A novel fabrication of graphene by chemical reaction with a green reductant [J]. Chem. Eng. J., 2016, 306: 754 |
| 35 | Mu X N, Zhang H M, Cai H N, et al. Microstructure evolution and superior tensile properties of low content graphene nanoplatelets reinforced pure Ti matrix composites [J]. Mater. Sci. Eng., 2017, A687: 164 |
| 36 | Nagae T, Yokota M, Nose M, et al. Effects of pulse current on an aluminum powder oxide layer during pulse current pressure sintering [J]. Mater. Trans., 2002, 43: 1390 |
| 37 | Liu R F, Wang W X, Chen H S, et al. Densification of pure magnesium by spark plasma sintering-discussion of sintering mechanism [J]. Adv. Powder Technol., 2019, 30: 2649 |
/
| 〈 |
|
〉 |