Research Progress on the Interface Design and Interface Response of Irradiation Resistant Metal-Based Nanostructured Materials

  • Yue LIU ,
  • Pengzheng TANG ,
  • Kunming YANG ,
  • Yiming SHEN ,
  • Zhongguang WU ,
  • Tongxiang FAN
Expand
  • 1.State Key Laboratory of Metal Matrix Composites, Shanghai Jiao Tong University, Shanghai 200240, China
    2.Shanghai Academy of Spaceflight Technology, Shanghai 201109, China

Received date: 2020-05-21

  Revised date: 2020-06-25

  Online published: 2020-08-27

Supported by

National Natural Science Foundation of China(51901129);National Key Research and Development Program of China(2017YFB0703101)

Abstract

High-energy particle irradiation can often cause microstructure damage, resulting in different types of defects in metal-based structured materials. These irradiation-induced defects can accumulate and evolve, leading to the deformation and reduction of the structural integrity of the materials. Finally, this causes the degradation of the mechanical and physical properties of the aforementioned materials. These defects can be shielded, absorbed, and annihilated by introducing interfaces in materials, alleviating the radiation damage. In the previous two decades, metal-based nanostructured materials have attracted considerable attention in designing irradiation-resistant materials because of its high density of internal interfaces. This review aims to investigate the effect of the interface microstructure and energy on strengthening the irradiation resistance of metal-based nanostructured materials, with special emphasis on the interface responses of low- and high-energy interfaces. Furthermore, this review provides the theoretical and scientific foundation for optimizing the interface structure design and exhibits delicate balance between the interface microstructure, interface energy, interface stability, and irradiation resistance. In addition, the recent research progress on irradiation-resistant carbon-/metal-based nanostructured materials that consider such interface characteristics is reviewed in detail. Finally, the prospect of future irradiation-resistant metal-based nanostructured material development is discussed.

Cite this article

Yue LIU , Pengzheng TANG , Kunming YANG , Yiming SHEN , Zhongguang WU , Tongxiang FAN . Research Progress on the Interface Design and Interface Response of Irradiation Resistant Metal-Based Nanostructured Materials[J]. Acta Metall Sin, 2021 , 57(2) : 150 -170 . DOI: 10.11900/0412.1961.2020.00169

References

1 Zinkle S J, Was G S. Materials challenges in nuclear energy [J]. Acta Mater., 2013, 61: 735
2 Chu S, Majumdar A. Opportunities and challenges for a sustainable energy future [J]. Nature, 2012, 488: 294
3 Zinkle S J, Busby J T. Structural materials for fission & fusion energy [J]. Mater. Today, 2009, 12: 12
4 Odette G R, Alinger M J, Wirth B D. Recent developments in irradiation-resistant steels [J]. Annu. Rev. Mater. Res., 2008, 38: 471
5 Was G S. Fundamentals of Radiation Materials Science: Metals and Alloys [M]. New York: Springer, 2007: 827
6 Zinkle S J, Snead L L. Designing radiation resistance in materials for fusion energy [J]. Annu. Rev. Mater. Res., 2014, 44: 241
7 Odette G R, Alinger M J, Wirth B D. Recent developments in irradiation-resistant steels [J]. Annu. Rev. Mater. Res., 2008, 38: 471
8 Bai X M, Voter A F, Hoagland R G, et al. Efficient annealing of radiation damage near grain boundaries via interstitial emission [J]. Science, 2010, 327: 1631
9 Cheng G M, Xu W Z, Wang Y Q, et al. Grain size effect on radiation tolerance of nanocrystalline Mo [J]. Scr. Mater., 2016, 123: 90
10 Yu K Y, Sun C, Chen Y, et al. Superior tolerance of Ag/Ni multilayers against Kr ion irradiation: An in situ study [J]. Philos. Mag., 2013, 93: 3547
11 Han W Z, Demkowicz M J, Mara N A, et al. Design of radiation tolerant materials via interface engineering [J]. Adv. Mater., 2013, 25: 6975
12 Fu E G, Caro M, Zepeda-Ruiz L A, et al. Surface effects on the radiation response of nanoporous Au foams [J]. Appl. Phys. Lett., 2012, 101: 191607
13 Han W Z, Demkowicz M J, Fu E G, et al. Effect of grain boundary character on sink efficiency [J]. Acta Mater., 2012, 60: 6341
14 Gao J, Liu Z J, Wan F R. Limited effect of twin boundaries on radiation damage [J]. Acta Metall. Sin. (Engl. Lett.), 2016, 29: 72
15 Mao S M, Shu S P, Zhou J, et al. Quantitative comparison of sink efficiency of Cu-Nb, Cu-V and Cu-Ni interfaces for point defects [J]. Acta Mater., 2015, 82: 328
16 Vattré A J, Abdolrahim N, Kolluri K, et al. Computational design of patterned interfaces using reduced order models [J]. Sci. Rep., 2014, 4: 6231
17 Beyerlein I J, Demkowicz M J, Misra A, et al. Defect-interface interactions [J]. Prog. Mater. Sci., 2015, 74: 125
18 Vetterick G A, Gruber J, Suri P K, et al. Achieving radiation tolerance through non-equilibrium grain boundary structures [J]. Sci. Rep., 2017, 7: 12275
19 Qin W J, Ren F, Doerner R P, et al. Nanochannel structures in W enhance radiation tolerance [J]. Acta Mater., 2018, 153: 147
20 Fan C, Li J, Fan Z, et al. In situ studies on the irradiation-induced twin boundary-defect interactions in Cu [J]. Metall. Mater. Trans., 2017, 48A: 5172
21 Tang X Z, Guo Y F, Fan Y, et al. Interstitial emission at grain boundary in nanolayered alpha-Fe [J]. Acta Mater., 2016, 105: 147
22 Bufford D, Wang H, Zhang X. High strength, epitaxial nanotwinned Ag films [J]. Acta Mater., 2011, 59: 93
23 Hodge A M, Furnish T A, Shute C J, et al. Twin stability in highly nanotwinned Cu under compression, torsion and tension [J]. Scr. Mater., 2012, 66: 872
24 Demkowicz M J, Anderoglu O, Zhang X H, et al. The influence of 3 twin boundaries on the formation of radiation-induced defect clusters in nanotwinned Cu [J]. J. Mater. Res., 2011, 26: 1666
25 Yu K Y, Bufford D, Sun C, et al. Removal of stacking-fault tetrahedra by twin boundaries in nanotwinned metals [J]. Nat. Commun., 2013, 4: 1377
26 Li J, Yu K Y, Chen Y, et al. In situ study of defect migration kinetics and self-healing of twin boundaries in heavy ion irradiated nanotwinned metals [J]. Nano Lett., 2015, 15: 2922
27 Wang Y M, Sansoz F, Lagrange T, et al. Defective twin boundaries in nanotwinned metals [J]. Nat. Mater., 2013, 12: 697
28 Jiao S Y, Kulkarni Y. Radiation tolerance of nanotwinned metals—An atomistic perspective [J]. Comp. Mater. Sci., 2018, 142: 290
29 Jin Z H, Gumbsch P, Albe K, et al. Interactions between non-screw lattice dislocations and coherent twin boundaries in face-centered cubic metals [J]. Acta Mater., 2008, 56: 1126
30 Wang J, Huang H. Novel deformation mechanism of twinned nanowires [J]. Appl. Phys. Lett., 2006, 88: 203112.
31 Li N, Wang J, Misra A, et al. Twinning dislocation multiplication at a coherent twin boundary [J]. Acta Mater., 2011, 59: 5989
32 Chen Y X, Fu E G, Yu K Y, et al. Enhanced radiation tolerance in immiscible Cu/Fe multilayers with coherent and incoherent layer interfaces [J]. J. Mater. Res., 2015, 30: 1300
33 Fu E G, Misra A, Wang H, et al. Interface enabled defects reduction in helium ion irradiated Cu/V nanolayers [J]. J. Nucl. Mater., 2010, 407: 178
34 Chen Y, Liu Y, Fu E G, et al. Unusual size-dependent strengthening mechanisms in helium ion-irradiated immiscible coherent Cu/Co nanolayers [J]. Acta Mater., 2015, 84: 393
35 Heinisch H L, Gao F, Kurtz R J. The effects of interfaces on radiation damage production in layered metal composites [J]. J. Nucl. Mater., 2004, 329-333: 924
36 Wang J, Misra A, Hirth J P. Shear response of ??3 {112} twin boundaries in face-centered-cubic metals [J]. Phys. Rev., 2011, 83B: 064106
37 Yu K Y, Bufford D, Khatkhatay F, et al. In situ studies of irradiation-induced twin boundary migration in nanotwinned Ag [J]. Scr. Mater., 2013, 69: 385
38 Chen Y, Yu K Y, Liu Y, et al. Damage-tolerant nanotwinned metals with nanovoids under radiation environments [J]. Nat. Commun., 2015, 6: 7036
39 Li N, Wang J, Wang Y Q, et al. Incoherent twin boundary migration induced by ion irradiation in Cu [J]. J. Appl. Phys., 2013, 113: 023508
40 Borovikov V, Mendelev M I, King A H. Effects of solutes on the thermal stability of nanotwinned materials [J]. Philos. Mag., 2014, 94: 2875
41 Zhu H Y, Liu S, Liu Z R, et al. Tailoring the stability of {101ˉ2} twins in magnesium with solute segregation at the twin boundary and strain path control [J]. Comp. Mater. Sci., 2018, 152: 113
42 Fan C C, Xie D Y, Li J, et al. 9R phase enabled superior radiation stability of nanotwinned Cu alloys via in situ radiation at elevated temperature [J]. Acta Mater., 2019, 167: 248
43 Li J, Xie D Y, Xue S, et al. Superior twin stability and radiation resistance of nanotwinned Ag solid solution alloy [J]. Acta Mater., 2018, 151: 395
44 Tschopp M A, Solanki K N, Gao F, et al. Probing grain boundary sink strength at the nanoscale: Energetics and length scales of vacancy and interstitial absorption by grain boundaries in α-Fe [J]. Phys. Rev., 2012, 85B: 064108
45 Barr C M, Barnard L, Nathaniel J E, et al. Grain boundary character dependence of radiation-induced segregation in a model Ni-Cr alloy [J]. J. Mater. Res., 2015, 30: 1290
46 Jiang C, Swaminathan N, Deng J, et al. Effect of grain boundary stresses on sink strength [J]. Mater. Res. Lett., 2014, 2: 100
47 El-Atwani O, Nathaniel J E, Leff A C, et al. The role of grain size in He bubble formation: Implications for swelling resistance [J]. J. Nucl. Mater., 2017, 484: 236
48 Sun C, Zheng S, Wei C C, et al. Superior radiation-resistant nanoengineered austenitic 304L stainless steel for applications in extreme radiation environments [J]. Sci. Rep., 2015, 5: 7801
49 Samaras M, Derlet P M, Van Swygenhoven H, et al. Radiation damage near grain boundaries [J]. Philos. Mag., 2003, 83: 3599
50 Xu J, Liu J B, Li S N, et al. Self-healing properties of nanocrystalline materials: A first-principles analysis of the role of grain boundaries [J]. Phys. Chem. Chem. Phys., 2016, 18: 17930
51 Sun C, Song M, Yu K Y, et al. In situ evidence of defect cluster absorption by grain boundaries in Kr ion irradiated nanocrystalline Ni [J]. Metall. Mater. Trans., 2013, 44A: 1966
52 Liu L L, Tang Z, Xiao W, et al. Self-healing mechanism of irradiation defects near Σ=11(113) grain boundary in copper [J]. Mater. Lett., 2013, 109: 221
53 Di C, Wang J, Chen T Y, et al. Defect annihilation at grain boundaries in alpha-Fe [J]. Sci. Rep., 2013, 3: 1450
54 Kirchheim R. Grain coarsening inhibited by solute segregation [J]. Acta Mater., 2002, 50: 413
55 Koch C C, Scattergood R O, Darling K A, et al. Stabilization of nanocrystalline grain sizes by solute additions [J]. J. Mater. Sci., 2008, 43: 7264
56 Liu F, Kirchheim R. Nano-scale grain growth inhibited by reducing grain boundary energy through solute segregation [J]. J. Cryst. Growth, 2004, 264: 385
57 Darling K A, Kecskes L J, Atwater M, et al. Thermal stability of nanocrystalline nickel with yttrium additions [J]. J. Mater. Res., 2013, 28: 1813
58 Du C C, Jin S B, Fang Y, et al. Ultrastrong nanocrystalline steel with exceptional thermal stability and radiation tolerance [J]. Nat. Commun., 2018, 9: 5389
59 Fang Y, Ge W, Yang T F, et al. Radiation tolerance of La-doped nanocrystalline steel under heavy-ion irradiation at different temperatures [J]. Nanotechnology, 2018, 29: 494001
60 El-Atwani O, Li N, Li M, et al. Outstanding radiation resistance of tungsten-based high-entropy alloys [J]. Sci. Adv., 2019, 5: eaav2002
61 Barnes R S, Redding G B, Cottrbll A H. The observation of vacancy sources in metals [J]. Philos. Mag., 1958, 3A: 97
62 Chen D, Li N, Yuryev D, et al. Imaging the in-plane distribution of helium precipitates at a Cu/V interface [J]. Mater. Res. Lett., 2017, 5: 335
63 Misra A, Demkowicz M J, Zhang X, et al. The radiation damage tolerance of ultra-high strength nanolayered composites [J]. JOM, 2007, 59(9): 62
64 Demkowicz M J, Hoagland R G, Hirth J P. Interface structure and radiation damage resistance in Cu-Nb multilayer nanocomposites [J]. Phys. Rev. Lett., 2008, 100: 136102
65 Shao S, Wang J, Misra A, et al. Spiral patterns of dislocations at nodes in (111) semi-coherent FCC interfaces [J]. Sci. Rep., 2013, 3: 2448
66 Vattré A J, Demkowicz M J. Determining the Burgers vectors and elastic strain energies of interface dislocation arrays using anisotropic elasticity theory [J]. Acta Mater., 2013, 61: 5172
67 Hirth J P, Pond R C, Hoagland R G, et al. Interface defects, reference spaces and the Frank-Bilby equation [J]. Prog. Mater. Sci., 2013, 58: 749
68 Vattré A, Jourdan T, Ding H, et al. Non-random walk diffusion enhances the sink strength of semicoherent interfaces [J]. Nat. Commun., 2016, 7: 10424
69 Reed D J. A review of recent theoretical developments in the understanding of the migration of helium in metals and its interaction with lattice defects [J]. Rad. Eff., 1977, 31: 129
70 McPhie M G, Capolungo L, Dunn A Y, et al. Interfacial trapping mechanism of He in Cu-Nb multilayer materials [J]. J. Nucl. Mater., 2013, 437: 222
71 H?chbauer T, Misra A, Hattar K, et al. Influence of interfaces on the storage of ion-implanted He in multilayered metallic composites [J]. J. Appl. Phys., 2005, 98: 123516
72 Lach T G, Ekiz E H, Averback R S, et al. Role of interfaces on the trapping of He in 2D and 3D Cu-Nb nanocomposites [J]. J. Nucl. Mater., 2015, 466: 36
73 Demkowicz M J, Bhattacharyya D, Usov I, et al. The effect of excess atomic volume on He bubble formation at fcc-bcc interfaces [J]. Appl. Phys. Lett., 2010, 97: 161903
74 Demkowicz M J, Misra A, Caro A. The role of interface structure in controlling high helium concentrations [J]. Curr. Opin. Solid State Mater. Sci., 2012, 16: 101
75 Bollmann W. O-lattice calculation of an F.C.C.-B.C.C. interface [J]. Phys. Status Solidi, 1974, 21A: 543
76 Yuryev D V, Demkowicz M J. Computational design of solid-state interfaces using O-lattice theory: An application to mitigating helium-induced damage [J]. Appl. Phys. Lett., 2014, 105: 221601
77 Yang L X, Zheng S J, Zhou Y T, et al. Effects of He radiation on cavity distribution and hardness of bulk nanolayered Cu-Nb composites [J]. J. Nucl. Mater., 2017, 487: 311
78 Chen D, Li N, Yuryev D, et al. Self-organization of helium precipitates into elongated channels within metal nanolayers [J]. Sci. Adv., 2017, 3: eaao2710
79 So K P, Chen D, Kushima A, et al. Dispersion of carbon nanotubes in aluminum improves radiation resistance [J]. Nano Energy, 2016, 22: 319
80 Wang X S, Li Q Q, Xie J, et al. Fabrication of ultralong and electrically uniform single-walled carbon nanotubes on clean substrates [J]. Nano Lett., 2009, 9: 3137
81 González R I, Valencia F, Mella J, et al. Metal-nanotube composites as radiation resistant materials [J]. Appl. Phys. Lett., 2016, 109: 033108
82 Si S Y, Li W Q, Zhao X L, et al. Significant radiation tolerance and moderate reduction in thermal transport of a tungsten nanofilm by inserting monolayer graphene [J]. Adv. Mater., 2017, 29: 1604623
83 Kim Y, Baek J, Kim S, et al. Radiation resistant vanadium-graphene nanolayered composite [J]. Sci. Rep., 2016, 6: 24785
84 Huang H, Tang X B, Chen F D, et al. Radiation damage resistance and interface stability of copper-graphene nanolayered composite [J]. J. Nucl. Mater., 2015, 460: 16
85 Yang T L, Yang L, Liu H, et al. Ab initio study of stability and migration of point defects in copper-graphene layered composite [J]. J. Alloys Compd., 2017, 692: 49
86 Huang H, Tang X B, Chen F D, et al. Graphene damage effects on radiation-resistance and configuration of copper-graphene nanocomposite under irradiation: A molecular dynamics study [J]. Sci. Rep., 2016, 6: 39391
Outlines

/