Effect of Deformation and Annealing Treatment on Microstructure Evolution of Fe47Mn30Co10Cr10B3 Dual-Phase High-Entropy Alloy

  • Yi LIU ,
  • Jian TU ,
  • Weihua YANG ,
  • Ruisen YIN ,
  • Li TAN ,
  • Can HUANG ,
  • Zhiming ZHOU
Expand
  • 1 College of Materials Science and Engineering, Chongqing University of Technology, Chongqing 400054, China
    2 Chongqing Municipal Key Laboratory of Institutions of Higher Education for Mould Technology, Chongqing University of Technology, Chongqing 400054, China
    3 College of Aerospace Engineering, Chongqing University, Chongqing 400044, China

Received date: 2020-05-11

  Revised date: 2020-07-31

  Online published: 2020-08-24

Supported by

Science and Technology Research Program of Chongqing Municipal Education Commission(KJQN201801139);China Postdoctoral Science Foundation Funded Project(2018M632250);Graduate Student Innovation Program of Chongqing University of Technology(ycx20192040)

Abstract

In recent years, non-equiatomic high-entropy alloy (HEA) has been proposed to explore the flexibility of its design rule, avoiding the strength-ductility tradeoff. For further progress, non-equiatomic HEAs doped with interstitial atoms are developed. Boron, an effective dopant in metallurgy, has been used due to the beneficial compositional effects on the interfaces of metallic materials. In this work, the effects of deformation and annealing treatments on the microstructural evolution of Fe47Mn30Co10Cr10B3 dual-phase HEAs were investigated via electron channeling contrast imaging (ECCI) and EBSD. The results show that there are three stages in the deformation mechanism with an increase in the deformation degree, which include the dominant dislocation slip in the fcc phase, joint deformation of the transformation-induced plasticity and dislocation slip, and activation of dislocation slip in the hcp phase. With an increase in the annealing holding time, the partial recrystallization transformed to complete recrystallization. Further, particles located in the grain boundary can effectively restrain grain growth, and in turn, exhibit the bimodal grain size. The amount of annealing twinning variants is influenced by the fcc grain orientation: grains with <101> orientation are prone to forming multiple twinning variants, whereas, grains with <111> and <100> orientations are prone to forming a single twinning variant. The amount of annealing twinning variants also affected the morphological characteristics of the single hcp variant; the absence of annealing twinning variant is ascribed to the formation of blocky hcp phases and the single annealing twinning variant is attributed to the formation of laminate hcp phase. Moreover, the number of hcp variants was affected by the fcc grain sizes; large-sized grains facilitated the formation of multiple hcp variants, whereas, small-sized grains facilitated the formation of the single hcp variant.

Cite this article

Yi LIU , Jian TU , Weihua YANG , Ruisen YIN , Li TAN , Can HUANG , Zhiming ZHOU . Effect of Deformation and Annealing Treatment on Microstructure Evolution of Fe47Mn30Co10Cr10B3 Dual-Phase High-Entropy Alloy[J]. Acta Metall Sin, 2020 , 56(12) : 1569 -1580 . DOI: 10.11900/0412.1961.2020.00154

References

[1] Ye Y F, Wang Q, Lu J, et al. High-entropy alloy: Challenges and prospects [J]. Mater. Today, 2016, 19: 349
[2] Tsai M H, Yeh J W. High-entropy alloys: A critical review [J]. Mater. Res. Lett., 2014, 2: 107
[3] Sharma A S, Yadav S, Biswas K, et al. High-entropy alloys and metallic nanocomposites: Processing challenges, microstructure development and property enhancement [J]. Mater. Sci. Eng., 2018, R131: 1
[4] Zhang W R, Liaw P K, Zhang Y. Science and technology in high-entropy alloys [J]. Sci. China Mater., 2018, 61: 2
[5] Otto F, Yang Y, Bei H, et al. Relative effects of enthalpy and entropy on the phase stability of equiatomic high-entropy alloys [J]. Acta Mater., 2013, 61: 2628
[6] Li Z M, Raabe D. Strong and ductile non-equiatomic high-entroy alloys: Design, processing, microstructure, and mechanical properties [J]. JOM, 2017, 69: 2099
[7] Pradeep K G, Tasan C C, Yao M J, et al. Non-equiatomic high entropy alloys: Approach towards rapid alloy screening and property-oriented design [J]. Mater. Sci. Eng., 2015, A648: 183
[8] Li Z M, Pradeep K G, Deng Y, et al. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off [J]. Nature, 2016, 534: 227
[9] Chang X J, Zeng M Q, Liu K L, et al. Phase engineering of high-entropy alloys [J]. Adv. Mater., 2020, 32: 1907226
[10] Sathiyamoorthi P, Kim H S. High-entropy alloys with heterogeneous microstructure: Processing and mechanical properties [J]. Prog. Mater. Sci., 2020: 100709
[11] Guo W Q, Su J, Lu W J, et al. Dislocation-induced breakthrough of strength and ductility trade-off in a non-equiatomic high-entropy alloy [J]. Acta Mater., 2020, 185: 45
[12] Jo Y H, Jung S, Choi W M, et al. Cryogenic strength improvement by utilizing room-temperature deformation twinning in a partially recrystallized VCrMnFeCoNi high-entropy alloy [J]. Nat. Commun., 2017, 8: 15719
[13] He Z F, Jia N, Ma D, et al. Joint contribution of transformation and twinning to the high strength-ductility combination of a FeMnCoCr high entropy alloy at cryogenic temperatures [J]. Mater. Sci. Eng., 2019, A759: 437
[14] Wei D X, Li X Q, Jiang J, et al. Novel Co-rich high performance twinning-induced plasticity (TWIP) and transformation-induced plasticity (TRIP) high-entropy alloys [J]. Scr. Mater., 2019, 165: 39
[15] Lv Z P, Jiang S H, He J Y, et al. Second phase strengthening in advanced metal materials [J]. Acta Metall. Sin., 2016, 52: 1183
[15] (吕昭平, 蒋虽合, 何骏阳等. 先进金属材料的第二相强化 [J]. 金属学报, 2016, 52: 1183)
[16] Lv Z P, Lei Z F, Huang H L, et al. Deformation behavior and toughening of high-rntropy alloys [J]. Acta Metall. Sin., 2018, 54: 1553
[16] (吕昭平, 雷智锋, 黄海龙等. 高熵合金的变形行为及强韧化 [J]. 金属学报, 2018, 54: 1553)
[17] Wang Z W, Baker I, Cai Z H, et al. The effect of interstitial carbon on the mechanical properties and dislocation substructure evolution in Fe40.4Ni11.3Mn34.8Al7.5Cr6 high entropy alloys [J]. Acta Mater., 2016, 120: 228
[18] Lei Z F, Wu Y, He J Y, et al. Snoek-type damping performance in strong and ductile high-entropy alloys [J]. Sci. Adv., 2020, 6: eaba7802
[19] Liu C T, White C L, Horton J A. Effect of boron on grain-boundaries in Ni3Al [J]. Acta Metall., 1985, 33: 213
[20] Raabe D, Herbig M, Sandl?bes S, et al. Grain boundary segregation engineering in metallic alloys: A pathway to the design of interfaces [J]. Curr. Opin. Solid State Mater. Sci., 2014, 18: 253
[21] Seol J B, Bae J W, Li Z M, et al. Boron doped ultrastrong and ductile high-entropy alloys [J]. Acta Mater., 2018, 151: 366
[22] Hansen N, Barlow C Y. Plastic deformation of metals and alloys [A]. Laughlin D E, Hono K. Physical Metallurgy II [M]. 5th Ed., Amsterdam: Elsevier Press, 2014: 1681
[23] Mahajan S, Green M L, Brasen D. A model for the FCC→HCP transformation, its applications, and experimental evidence [J]. Metall. Trans., 1977, 8A: 283
[24] Fujita H, Ueda S. Stacking faults and f.c.c. (γ)→h.c.p. (ε) transformation in 188-type stainless steel [J]. Acta Metall., 1972, 20: 759
[25] Raabe D. Physical Metallurgy [M]. 5th Ed., Oxford: Elsevier Press, 2014: 2291
[26] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena [M]. 2nd Ed., London: Elsevier Press, 2004: 121
[27] Humphreys F J. A unified theory of recovery, recrystallization and grain growth, based on the stability and growth of cellular microstructures—II. The effect of second-phase particles [J]. Acta Mater., 1997, 45: 5031
Outlines

/