Investigations on the Accelerated Creep Testing of Alumina-Forming Austenitic Stainless Steel

  • Tian LIU ,
  • Rui LUO ,
  • Xiaonong CHENG ,
  • Qi ZHENG ,
  • Leli CHEN ,
  • Qian WANG
Expand
  • School of Materials Science and Engineering, Jiangsu University, Zhenjiang 212013, China

Received date: 2020-03-19

  Revised date: 2020-05-19

  Online published: 2020-08-21

Supported by

China Postdoctoral Science Foundation(2019M661738);Jiangsu Provincial Key Research and Development Program(BE2017127);Natural Science Foundation of the Jiangsu Higher Education Institutions of China(19KJB430001)

Abstract

The heat transfer component is a major component of a nuclear power plant, the safety and service life of which are determined based on the long-term creep performance of the heat-transfer pipe material. Several long-term creep tests are usually required to determine the creep life of the heat-transfer pipe materials, which considerably restrict the evaluation efficiency of the material service performance. The objective of this study is to investigate the feasibility of accelerated creep test (ACT) to reduce the time required for evaluating the creep properties of materials. A alumina-forming austenitic (AFA) stainless steel was prepared, and the ACT was performed on a Gleeble thermal simulator. Based on the ACT developed and realized on the Gleeble thermal simulator, damage accumulation was realized by applying elastic-plastic tensile and compressive strains on the ACT specimen to simulate the accelerated changes in the microstructure of the alloy that can be usually observed during a conventional creep test (CT). The average stress with respect to all the cyclic stress relaxation stages in the ACT was considered to be the initial stress of the conventional CT, and a creep fracture test was conducted on the alloy sample. Results revealed that the ACT accelerated the microstructure evolution of the precipitated phases, dislocations, twins, and so on in a short time. Nevertheless, the repeated generation and annihilation of a large number of dislocations in the AFA alloy during the ACT provided the nucleation point and reduced the driving force associated with the nucleation of the precipitated second phase, including the Laves phase. In addition, the cyclic strain applied during the ACT will reduce the strengthening effect of the nanoscale deformation twins in the AFA alloy, resulting in differences in the evaluation effect. Thus, ACT is useful for the efficient evaluation of the creep properties of materials; however, the optimal range of test parameters must be further investigated.

Cite this article

Tian LIU , Rui LUO , Xiaonong CHENG , Qi ZHENG , Leli CHEN , Qian WANG . Investigations on the Accelerated Creep Testing of Alumina-Forming Austenitic Stainless Steel[J]. Acta Metall Sin, 2020 , 56(11) : 1452 -1462 . DOI: 10.11900/0412.1961.2020.00088

References

[1] Yamamoto Y, Brady M P, Lu Z P, et al. Creep-resistant, Al2O3-forming austenitic stainless steels [J]. Science, 2007, 316: 433
[2] Yamamoto Y, Takeyama M, Lu Z P, et al. Alloying effects on creep and oxidation resistance of austenitic stainless steel alloys employing intermetallic precipitates [J]. Intermetallics, 2008, 16: 453
[3] Nie S H, Chen Y, Ren X, et al. Corrosion of alumina-forming austenitic steel Fe-20Ni-14Cr-3Al-0.6Nb-0.1Ti in supercritical water [J]. J. Nucl. Mater., 2010, 399: 231
[4] Bei H, Yamamoto Y, Brady M P, et al. Aging effects on the mechanical properties of alumina-forming austenitic stainless steels [J]. Mater. Sci. Eng., 2010, A527: 2079
[5] Leitner H, Schober M, Schnitzer R. Splitting phenomenon in the precipitation evolution in an Fe-Ni-Al-Ti-Cr stainless steel [J]. Acta Mater., 2010, 58: 1261
[6] Iseda A, Okada H, Semba H, et al. Long term creep properties and microstructure of SUPER304H, TP347HFG and HR3C for A-USC boilers [J]. Energy Mater., 2007, 2: 199
[7] Kim W G, Yoon S N, Ryu W S. Application and standard error analysis of the parametric methods for predicting the creep life of type 316LN SS [J]. Key. Eng. Mater., 2005, 297-300: 2272
[8] Hart R V. Assessment of remaining creep life using accelerated stress-rupture tests [J]. Met. Technol., 1976, 3: 1
[9] Penny R K, Marriott D L. Design for Creep [M]. London: Chapman & Hall, 1995: 40
[10] Sims C T, Stoloff N S, Hagel W C. Superalloys II [M]. New York: John Wiley & Sons, 1987: 1
[11] Yuan C, Guo J T, Yang H C. Cyclic creep behavior of directionally solidified nickel-base superalloy DZ17G [J]. Acta Metall. Sin., 1999, 35: 942
[11] (袁 超, 郭建亭, 杨洪才. 定向凝固镍基高温合金DZ17G的循环蠕变行为 [J]. 金属学报, 1999, 35: 942)
[12] Nechache A, Bouzid A H. The effect of cylinder and hub creep on the load relaxation in bolted flanged joints [J]. J. Pressure Vessel Technol., 2008, 130: 031211
[13] Gjestland H, Nussbaum G, Regazzoni G, et al. Stress-relaxation and creep behaviour of some rapidly solidified magnesium alloys [J]. Mater. Sci. Eng., 1991, A134: 1197
[14] Zhou Y M, Zhao Z P, Li H L. The microstructure and stress ralaxation property of 12%Cr steel [J]. Mater. Mech. Eng., 1992, 16: 27
[14] (周晔明, 赵中平, 李感琳. 12%Cr钢的组织与应力松弛性能 [J]. 机械工程材料, 1992, 16: 27)
[15] Mandziej S T, Vyrostkova A, Solar M. Accelerated creep testing of new creep-resisting weld metals [J]. Weld. World, 2010, 54: R160
[16] Mandziej S T. Accelerated microstructure transformation caused by thermal-mechanical fatigue [J]. Mater. Sci. Forum, 2012, 706-709: 871
[17] Kasl J, Jandová D, Mandziej S T, et al. Comparison of results of accelerated and conventional creep tests of dissimilar weld joint of steels FB2 and F [J]. Mater. Sci. Forum, 2017, 891: 322
[18] Mandziej S T, Vyrostková A. Evolution of Cr-Mo-V weld metal microstructure during creep testing—Part 1: P91 material [J]. Weld. World, 2008, 52: 3
[19] Auburtin P, Wang T, Cockcroft S L, et al. Freckle formation and freckle criterion in superalloy castings [J]. Metall. Mater. Trans., 2000, 31A: 801
[20] Cadek J. Creep in Metallic Materials [M]. Amsterdam: Elsevier, 1988: 33
[21] Zurob H S, Hutchinson C R, Brechet Y, et al. Modeling recrystallization of microalloyed austenite: Effect of coupling recovery, precipitation and recrystallization [J]. Acta Mater., 2002, 50: 3077
[22] Heilmaier M, Reppich B. Creep lifetime prediction of oxide-dispersion-strengthened nickel-base superalloys: A micromechanically based approach [J]. Metall. Mater. Trans., 1996, 27A: 3861
[23] Wang W Z, Buhl P, Klenk A, et al. Influence of high-temperature dwell time on creep-fatigue behavior in a 1000 MW steam turbine rotor [J]. Eng. Fract. Mech., 2016, 166: 1
[24] Zhou D Q, Xu X Q, Mao H H, et al. Plastic flow behaviour in an alumina-forming austenitic stainless steel at elevated temperatures [J]. Mater. Sci. Eng., 2014, A594: 246
[25] Ueji R, Tsuchida N, Terada D, et al. Tensile properties and twinning behavior of high manganese austenitic steel with fine-grained structure [J]. Scr. Mater., 2008, 59: 963
[26] Brady M P, Yamamoto Y, Muralidharan G, et al. Deployment of alumina forming austenitic (AFA) stainless steel [R]. Oak Ridge:Oak Ridge National Laboratory, 2013: 28
[27] Rodney D. Molecular dynamics simulation of screw dislocations interacting with interstitial frank loops in a model FCC crystal [J]. Acta Mater., 2004, 52: 607
[28] Lv X Z, Zhang J X. Core structure of a <100> interfacial superdislocations in a nickel-base superalloy during high-temperature and low-stress creep [J]. Mater. Sci. Eng., 2017, A683: 9
[29] Brager H R, Straalsund J L. Frank loop development in neutron-irradiated cold-worked type 316 stainless steel [J]. J. Nucl. Mater., 1973, 47: 105
[30] Karaman I, Sehitoglu H, Gall K, et al. On the deformation mechanisms in single crystal hadfield manganese steels [J]. Scr. Mater., 1998, 38: 1009
[31] Broek D. Elementary Engineering Fracture Mechanics [M]. Netherlands: Springer, 1982: 56
Outlines

/