Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process

  • Zijie DU ,
  • Wenyuan LI ,
  • Jianrong LIU ,
  • Hongbo SUO ,
  • Qingjiang WANG
Expand
  • 1 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3 Qingdao JointX Intelligent Manufacturing Limited, Qingdao 266109, China

Received date: 2020-04-01

  Revised date: 2020-05-07

  Online published: 2020-06-17

Abstract

TC4-DT alloy is developed based on TC4 alloy, with medium strength and high damage-tolerance, showing a great promise to be widely used in aerospace field. However, the traditional method to fabricate large and complicated parts has the problems of hot working difficulty, long processing cycle, low "buy-to-fly" ratio and high-cost. Additive manufacturing (AM) technology is a good alternative and has been used to manufacture titanium parts since year 2006. Compared to other AM technologies, cold metal transfer mode wire and arc additive manufacturing (CMT WAAM), as a kind of gas metal arc welding (GMAW) technology, has several advantages like simple structure, good spatial accessibility and high efficiency. In this study, a TC4-DT deposit was fabricated by CMT WAAM method. The macrostructure and microstructure, texture, and tensile properties in the overlapping zone and ordinary deposition zone were investigated and compared. The bottom of the ordinary deposition zone consisted of columnar and equiaxed prior β grains, and in higher zone the coarse equiaxed prior β grains were in the majority. The microstructure of the ordinary deposition zone was mainly characterized by basketweave α phase platelets. Microstructure of both sides of the overlapping line was characterized by a mixture of fine basketweave, lamellar and coarse basketweave α phase due to temperature gradient. Transformed α texture from {001}β//Z silk texture existed in different zones, and the texture of overlapping zone was complicated due to the complexity of heat dissipation conditions, including transformed α texture and other complicated texture. EBSD results showed that there was a strong <0001>α //X texture at the overlapping line, resulting in low Schmid factors for both prismatic slip and basal slip at the overlapping line, hindering the slip of dislocation. Combined with the Hall-Petch relationship, it was concluded that the prior β grain boundary and the overlapping line were main factors affecting the uniformity of mechanical properties. The average effective dislocation slip distances in different zones had the following relationship: overlapping zone<bottom of the ordinary deposition zone<top of the ordinary deposition zone, leading to different yield strengths in different zones of the ordinary deposition zone.

Cite this article

Zijie DU , Wenyuan LI , Jianrong LIU , Hongbo SUO , Qingjiang WANG . Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process[J]. Acta Metall Sin, 2020 , 56(12) : 1667 -1680 . DOI: 10.11900/0412.1961.2020.00104

References

[1] Li L, Sun J K, Meng X J. Application state and prospects for titanium alloys [J]. Titan. Ind. Prog., 2004, 21(5): 19
[1] (李 梁, 孙健科, 孟祥军. 钛合金的应用现状及发展前景 [J]. 钛工业进展, 2004, 21(5): 19)
[2] Zhang X Y, Zhao Y Q, Bai C G. Titanium Alloy and Its Application [M]. Beijing: Chemical Industry Press, 2005: 1
[2] (张喜燕, 赵永庆, 白晨光. 钛合金及应用 [M]. 北京: 化学工业出版社, 2005: 1)
[3] Feng B X, Mao X N, Yang G J, et al. Residual stress field and thermal relaxation behavior of shot-peened TC4-DT titanium alloy [J]. Mater. Sci. Eng., 2009, A512: 105
[4] Lu W, Shi Y W, Lei Y P, et al. Effect of electron beam welding on the microstructures and mechanical properties of thick TC4-DT alloy [J]. Mater. Des., 2012, 34: 509
[5] Peng X N, Guo H Z, Wang T, et al. Effects of β treatments on microstructures and mechanical properties of TC4-DT titanium alloy [J]. Mater. Sci. Eng., 2012, A533: 55
[6] Liu W. Study on microstructure and tensile properties of TC4-DT titanium alloy forgings [J]. Heavy Cast. Forg., 2018, (3): 38
[6] (刘 卫. TC4-DT钛合金锻件组织与拉伸性能研究 [J]. 大型铸锻件, 2018, (3): 38)
[7] Hong Q, Han D, Guo P, et al. Flow properties and microstructure evolution of TC4-DT alloy at high temperature [J]. Hot Working Technol., 2017, 46(7): 189
[7] (洪 权, 韩 栋, 郭 萍等. TC4-DT合金的高温流变特性及组织演变 [J]. 热加工工艺, 2017, 46(7): 189)
[8] Gong S L, Suo H B, Li H X. Development and application of metal additive manufacturing technology [J]. Aeronaut. Manuf. Technol., 2013, (13): 66
[8] (巩水利, 锁红波, 李怀学. 金属增材制造技术在航空领域的发展与应用 [J]. 航空制造技术, 2013, (13): 66)
[9] Liu S Y, Shin Y C. Additive manufacturing of Ti6Al4V alloy: A review [J]. Mater. Des., 2019, 164: 107552
[10] Li D C, Tian X Y, Wang Y X, et al. Developments of additive manufacturing technology [J]. Electromach. Mould, 2012, (suppl.1): 20
[10] (李涤尘, 田小永, 王永信等. 增材制造技术的发展 [J]. 电加工与模具, 2012, (增刊1): 20)
[11] Rodrigues T A, Duarte V, Miranda R M, et al. Current status and perspectives on wire and arc additive manufacturing (WAAM) [J]. Materials, 2019, 12: 1121
[12] Pan Z X, Ding D H, Wu B T, et al. Arc welding processes for additive manufacturing: A review [A]. Transactions on Intelligent Welding Manufacturing [C]. Singapore: Springer, 2018: 3
[13] Williams S W, Martina F, Addison A C, et al. Wire+arc additive manufacturing [J]. Mater. Sci. Technol., 2016, 32: 641
[14] Tian C L, Chen J L, Dong P, et al. Current state and future development of the wire arc additive manufacture technology abroad [J]. Aerosp. Manuf. Technol., 2015, (2): 57
[14] (田彩兰, 陈济轮, 董 鹏等. 国外电弧增材制造技术的研究现状及展望 [J]. 航天制造技术, 2015, (2): 57)
[15] Wang F D, Williams S, Rush M. Morphology investigation on direct current pulsed gas tungsten arc welded additive layer manufactured Ti6Al4V alloy [J]. Int. J. Adv. Manuf. Technol., 2011, 57: 597
[16] Wang B. Study on wire and arc additive manufacturing forming process of TC4 titanium alloy [D]. Shenyang: Shenyang Aerospace University, 2018
[16] (王 斌. TC4钛合金电弧熔丝沉积成形工艺研究 [D]. 沈阳: 沈阳航空航天大学, 2018)
[17] Baufeld B, Brandl E, van der Biest O. Wire based additive layer manufacturing: Comparison of microstructure and mechanical properties of Ti-6Al-4V components fabricated by laser-beam deposition and shaped metal deposition [J]. J. Mater. Process. Technol., 2011, 211: 1146
[18] Lin J J, Lv Y H, Liu Y X, et al. Microstructural evolution and mechanical property of Ti-6Al-4V wall deposited by continuous plasma arc additive manufacturing without post heat treatment [J]. J. Mech. Behav. Biomed. Mater., 2017, 69: 19
[19] He Z. Effect of ultrasonic impact on the properties of arc additive manufacturing of titanium alloy [D]. Wuhan: Huazhong University of Science and Technology, 2016
[19] (何 智. 超声冲击电弧增材制造钛合金零件的组织性能研究 [D]. 武汉: 华中科技大学, 2016)
[20] Ji L, Lu J P, Tang S Y, et al. Research on mechanisms and controlling methods of macro defects in TC4 alloy fabricated by wire additive manufacturing [J]. Materials, 2018, 11: 1104
[21] Xu F D, Dhokia V, Colegrove P, et al. Realisation of a multi-sensor framework for process monitoring of the wire arc additive manufacturing in producing Ti-6Al-4V parts [J]. Int. J. Comput. Integr. Manuf., 2018, 31: 785
[22] Park S C, Choi B K. Tool-path planning for direction-parallel area milling [J]. Comput. Aided Des., 2000, 32: 17
[23] Rajan V T, Srinivasan V, Tarabanis K A. The optimal zigzag direction for filling a two-dimensional region [J]. Rapid Prototyping J., 2001, 7(5): 231
[24] Hu Z Q, Qin X P, Li Y F, et al. Multi-bead overlapping model with varying cross-section profile for robotic GMAW-based additive manufacturing [J]. J. Intell. Manuf., 2020, 31: 1133
[25] Zhang H T, Feng J C, Hu L L. Energy input and metal transfer behavior of CMT welding process [J]. Mater. Sci. Technol., 2012, 20(2): 128
[25] (张洪涛, 冯吉才, 胡乐亮. CMT能量输入特点与熔滴过渡行为 [J]. 材料科学与工艺, 2012, 20(2): 128)
[26] Liu Z. The microstructure and tensile behavior of TC4 titanium alloy produced via electron beam rapid manufacturing [D]. Hefei: University of Science and Technology of China, 2019
[26] (刘 征. 电子束熔丝成形TC4合金的组织和拉伸力学行为研究 [D]. 合肥: 中国科学技术大学, 2019)
[27] Suo H B. Microstructure and mechanical properties of Ti6Al4V produced by electron beam rapid manufacturing [D]. Wuhan: Huazhong University of Science and Technology, 2014
[27] (锁红波. 电子束快速成形TC4钛合金显微组织及力学性能研究 [D]. 武汉: 华中科技大学, 2014)
[28] Du Z J, Li W Y, Liu J R, et al. Microstructure and its CET prediction of TC4-DT by CMT mode wire and arc additive manufacturing [J]. Chin. J. Mater. Res., 2020, 34: 518
[28] (杜子杰, 李文渊, 刘建荣等. CMT成型TC4-DT合金组织及形成机理的CET模型预测 [J]. 材料研究学报, 2020, 34: 518)
[29] Zhao Z B. The crystallographic orientation of α phase in Ti60 alloy [D]. Beijing: University of Chinese Academy of Sciences, 2014
[29] (赵子博. Ti60合金中α相的晶体取向研究 [D]. 北京: 中国科学院大学, 2014)
[30] de Formanoir C, Michotte S, Rigo O, et al. Electron beam melted Ti-6Al-4V: Microstructure, texture and mechanical behavior of the as-built and heat-treated material [J]. Mater. Sci. Eng., 2016, A652: 105
[31] Paradkar A G, Kamat S V, Gogia A K, et al. On the validity of Hall-Petch equation for single-phase β Ti-Al-Nb alloys undergoing stress-induced martensitic transformation [J]. Mater. Sci. Eng., 2009, A520: 168
[32] Semiatin S L, Bieler T R. The effect of alpha platelet thickness on plastic flow during hot working of TI-6Al-4V with a transformed microstructure [J]. Acta Mater., 2001, 49: 3565
[33] Bridier F, Villechaise P, Mendez J. Analysis of the different slip systems activated by tension in a α/β titanium alloy in relation with local crystallographic orientation [J]. Acta Mater., 2005, 53: 555
[34] Li H, Boehlert C J, Bieler T R, et al. Examination of the distribution of the tensile deformation systems in tension and tension-creep of Ti-6Al-4V (wt.%) at 296 K and 728 K [J]. Philos. Mag., 2015, 95: 691
[35] Pilchak A L, Williams R E A, Williams J C. Crystallography of fatigue crack initiation and growth in fully lamellar Ti-6Al-4V [J]. Metall. Mater. Trans., 2010, 41A: 106
[36] Yu Y N. Fundamentals of Material Science [M]. 2nd Ed., Beijing: Higher Education Press, 2012: 350
[36] (余永宁. 材料科学基础 [M]. 第2版. 北京: 高等教育出版社, 2012: 350)
[37] Hu G X, Cai X. Fundamentals of Material Science [M]. Shanghai: Shanghai Jiao Tong University Press, 2000: 172
[37] (胡赓祥, 蔡 珣. 材料科学基础 [M]. 上海: 上海交通大学出版社, 2000: 172)
[38] Pan J S, Tong J M, Tian M B. Fundamentals of Material Science [M]. Beijing: Tsinghua University Press, 2011: 1
[38] (潘金生, 仝健民, 田民波. 材料科学基础 [M]. 北京: 清华大学出版社, 2011: 1)
Outlines

/