Influence of White Spot Defects on Microstructure and Mechanical Property of the GH4586 Alloy

  • Haibing TAN ,
  • Shuo HUANG ,
  • Jing WANG ,
  • Shu LI ,
  • Changhong ZHU ,
  • Yan ZHONG ,
  • Shilin ZHONG ,
  • Aijie HE
Expand
  • 1 Sichuan Gas Turbine Establishment, Aero Engine Corporation of China, Chengdu 610500, China
    2 High Temperature Materials Research Division, Central Iron and Steel Research Institute, Beijing 100081, China

Received date: 2020-03-13

  Revised date: 2020-04-13

  Online published: 2020-06-12

Supported by

National Science and Technology Major Project(2017-VI-0015-0087);National Science and Technology Major Project(2017-VI-0018-0090)

Abstract

GH4586 is a nickel-based wrought superalloy developed by China, and features high Ti, W, Mo and low Al. However, it is easy to form whit spot (WP) defects within the disk components manufactured from the GH4586 ingot with a diameter of 508 mm produced by double vacuum melting method. In present work, the macro- and micro-structural characteristics, as well as the element distribution of WP defect were systematically studied. Special attention was focused on the effects of WP on mechanical properties. Hardness, tensile properties and fracture morphology of normal and defective areas were investigated for comparison. In addition, the formation mechanism and control method of WP defects were investigated based on the thermodynamic calculation and solidification simulation, respectively. In order to analyze its dendritic segregation and second phase precipitation in the solidification process, solidification phase diagram and thermodynamic equilibrium phase diagram of GH4586 alloy were calculated with JmatPro software. To study the forming mechanism of WP, the solidification process of vacuum introduction melting (VIM) GH4586 ingots was simulated with Procast software. Results show that the WP defects within GH4586 components are dendritic WP which exhibits dendritic pattern on the macro level. While on micro level, it is the precipitate clusters which consisted of MC carbides, M6C carbides and large incoherent γ′ phase. Due to the clusters' inherent rigid and fragile characteristics, the tensile strength and ductility of the alloy are significantly reduced. Therefore, the WP defects are harmful to the mechanical properties of the GH4586 disk significantly. The WP defects must be avoided during the forging process. Since excessive internal stress and shrinkage cavities form during the solidification process of large VIM GH4586 ingots, chips fall into molten pool easily if the VIM ingots are employed as vacuum arc remelting (VAR) electrode, and then give birth to WP defects within the final forging components. Therefore, it is the effective method for avoiding WP defects by improving the quality of VAR electrode and optimizing the VAR process.

Cite this article

Haibing TAN , Shuo HUANG , Jing WANG , Shu LI , Changhong ZHU , Yan ZHONG , Shilin ZHONG , Aijie HE . Influence of White Spot Defects on Microstructure and Mechanical Property of the GH4586 Alloy[J]. Acta Metall Sin, 2020 , 56(10) : 1411 -1422 . DOI: 10.11900/0412.1961.2020.00081

References

[1] Zhang B J, Zhao G P, Jiao L Y, et al. Influence of hot working process on microstructures of superalloy GH4586 [J]. Acta Metall. Sin., 2005, 41: 351
[1] (张北江, 赵光普, 焦兰英等. 热加工工艺对GH4586合金微观组织的影响 [J]. 金属学报, 2005, 41: 351)
[2] Wang L, Wang S, Song X, et al. Effects of precipitated phases on the crack propagation behaviour of a Ni-based superalloy [J]. Int. J. Fatigue, 2014, 62: 210
[3] Wang S, Wang L, Liu Y, et al. Effect of long-term aging on the fatigue crack growth rate of a nickel-based superalloy [J]. Mater. Sci. Eng., 2011, A528: 2110
[4] Fecht H, Furrer D. Processing of nickel-base superalloys for turbine engine disc applications [J]. Adv. Eng. Mater., 2000, 2: 777
[5] Du J H, Lv X D, Dong J X, et al. Research progress of wrought superalloys in China [J]. Acta Metall. Sin., 2019, 55: 1115
[5] (杜金辉, 吕旭东, 董建新等. 国内变形高温合金研制进展 [J]. 金属学报, 2019, 55: 1115)
[6] Xu G H, Jiao L Y, Zhang B J, et al. Effect of cooling rate after solid solution on microstructure and tensile properties of GH4586 superalloy at 850 ℃ [J]. Trans. Mater. Heat Treat., 2006, 27: 47
[6] (胥国华, 焦兰英, 张北江等. 固溶冷却速度对GH4586合金组织及850 ℃拉伸性能的影响 [J]. 材料热处理学报, 2006, 27: 47)
[7] Zhong Z Y, Zhuang J Y. Development of several important problems on producing technologies of wrought superalloy [J]. J. Iron Steel Res., 2003, 15(7): 1
[7] (仲增墉, 庄景云. 变形高温合金生产工艺中几个重要问题的研究和进展 [J]. 钢铁研究学报, 2003, 15(7): 1)
[8] Liu Q M, Huang S Z, Chen Y L, et al. Investigation on the abnormal corrosion spots of GH4169G alloy parts [J]. Gas Turb. Exp. Res., 2019, 32: 52
[8] (刘巧沐, 黄顺洲, 陈玉龙等. GH4169G合金零件异常腐蚀区缺陷分析 [J]. 燃气涡轮试验与研究, 2019, 32: 52)
[9] Reed R C. The Superalloys Fundamentals and Applications [M]. New York: Cambridge University Press, 2006: 222
[10] Jackman L A, Maurer G E, Widge S. White spots in superalloys [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale, PA: TMS, 1994: 153
[11] Zhang B J, Huang S, Zhang W Y, et al. Recent development of nickel-based disc alloys and corresponding cast-wrought processing techniques [J]. Acta Metall. Sin., 2019, 55: 1095
[11] (张北江, 黄 烁, 张文云等. 变形高温合金盘材及其制备技术研究进展 [J]. 金属学报, 2019, 55: 1095)
[12] Huang Q Y, Li H K. Superalloy [M]. Beijing: Metallurgical Industry Press, 2000: 186
[12] (黄乾尧, 李汉康. 高温合金 [M]. 北京: 冶金工业出版社, 2000: 186)
[13] Scarfo J P, Wolski K, Gros V, et al. Powerplant group chairman's factual report [R]. Washington: National Transportation Safety Board, 2017
[14] Damkroger B K, Kelley J B, Schlienger M E, et al. The influence of VAR processes and parameters on white spot formation in alloy 718 [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale, PA: TMS, 1994: 125
[15] Grignard J F, Soller A, Jourdan J, et al. On the formation of white-spot defects in a superalloy VAR ingot [J]. Adv. Eng. Mater., 2011, 13: 563
[16] Li L H, Dong J X, Zhang M C, et al. Integrated simulation of the forging process for GH4738 alloy turbine disk and its application [J]. Acta Metall. Sin., 2014, 50: 821
[16] (李林翰, 董建新, 张麦仓等. GH4738合金涡轮盘锻造过程的集成式模拟及应用 [J]. 金属学报, 2014, 50: 821)
[17] Samuelsson E, Domingue J A, Maurer G E. Characterizing solute-lean defects in superalloys [J]. JOM, 1990, 42(8): 27
[18] Wang Z X, Huang S, Zhang B J, et al. Study on freckle of a high-alloyed GH4065 nickel base wrought superalloy [J]. Acta Metall. Sin., 2019, 55: 417
[18] (王资兴, 黄 烁, 张北江等. 高合金化GH4065镍基变形高温合金点状偏析研究 [J]. 金属学报, 2019, 55: 417)
[19] Dong J X, Li A, Zhang M C. Thermodynamic simulation of precipitations in GH586 superalloy [J]. J. Mater. Eng., 2003, (9): 7
[19] (董建新, 李 昂, 张麦仓. GH586高温合金析出相的热力学模拟计算 [J]. 材料工程, 2003, (9): 7)
[20] Zhuang J Y, Du J H, Deng Q, et al. Wrought Superalloy GH4169 [M]. Beijing: Metallurgical Industry Press, 2006: 19
[20] (庄景云, 杜金辉, 邓 群等. 变形高温合金GH4169 [M]. 北京: 冶金工业出版社, 2006: 19)
[21] Jones R M F, Jackman L A. The structural evolution of superalloy ingots during hot working [J]. JOM, 1999, 51(1): 27
[22] Moyer J M, Jackman L A, Adasczik C B, et al. Advances in triple melting superalloys 718, 706, and 720 [A]. Superalloys 718, 625, 706 and Various Derivatives [C]. Warrendale, PA: TMS, 1994: 39
[23] Dong J X, Li L H, Li R Y, et al. Effect of extent of homogenization on the hot deformation recrystallization of superalloy ingot in cogging process [J]. Acta Metall. Sin., 2015, 51: 1207
[23] (董建新, 李林翰, 李浩宇等. 高温合金铸锭均匀化程度对开坯热变形的再结晶影响 [J]. 金属学报, 2015, 51: 1207)
[24] Xie S S, Yang H C, Wang Z X, et al. Effects of grain-boundary carbides on high-temperature strength in the superalloy GH586 [J]. J. Northeast. Univ. (Nat. Sci.), 1998, 19: 577
[24] (谢世殊, 杨洪才, 王志兴等. GH586合金的晶界碳化物高温强化 [J]. 东北大学学报(自然科学版), 1998, 19: 577)
[25] Van Den Avyle J A, Brooks J A, Powell A C. Reducing defects in remelting processes for high-performance alloys [J]. JOM, 1998, 50(3): 22
[26] Zhang B J, Zhao G P, Zhang W Y, et al. Investigation of high performance disc alloy GH4065 and associated advanced processing techniques [J]. Acta Metall. Sin., 2015, 51: 1227
[26] (张北江, 赵光普, 张文云等. 高性能涡轮盘材料GH4065及其先进制备技术研究 [J]. 金属学报, 2015, 51: 1227)
[27] Crozet C, Devaux A, Forestier R, et al. Effect of ingot size on microstructure and properties of the new advanced AD730TM superalloy [A]. Superalloys 2016: Proceedings of the 13th Intenational Symposium of Superalloys [C]. Warrendale, PA: TMS, 2016: 437
Outlines

/