Corrosion Behaviors and Mechanisms of ODS Steel Exposed to Static Pb-Bi Eutectic at 600 and 700 ℃
Received date: 2020-01-21
Revised date: 2020-04-16
Online published: 2020-06-03
Supported by
Nuclear Power Technology Innovation Center Project of Nuclear Power Institute of China(HDLCXZX-2019-HD-15-01);National Natural Science Foundation of China(U1832206);"Excellent Scholar Funding" initialed by Institute of Metal Research, Chinese Academy of Science(JY7A7A111A1)
With good neutron properties, anti-irradiation performances, heat transfer properties and inherent safety characteristics, liquid lead or Pb-Bi eutectic (LBE) has been a primary candidate coolant for accelerator driven system and advanced nuclear reactors. However, corrosion of structural materials is a critical challenge in the use of liquid lead and LBE in high temperature nuclear reactors. Therefore, research on corrosion compatibility of structural materials with LBE at elevated temperatures is of great significance. In this work, the long-term corrosion experiments in static LBE for a oxide dispersion strengthened (ODS) steel were carried out at 600 and 700 ℃. The temperature effects on different corrosion behaviors were studied by the analyses of XRD, SEM and EDS, and the underlying mechanisms were clarified. After exposing to LBE at 600 ℃ for up to 2000 h, a typical double-layer oxide scale with the thickness of about 10 μm was formed on the surface of ODS steel, which was composed of outer layers of Pb-Fe-O and Fe3O4 and inner layer of Fe-Cr-Al spinal. In addition, a thin Al-rich layer was also formed under the inner layer. Due to the protective effect of the relatively dense inner layer and the Al-rich layer, ODS steel showed excellent resistance to LBE corrosion at 600 ℃ with a significantly lower corrosion rate. On the contrary, when exposed to LBE at 700 ℃ , the structure and thickness of the oxide scale formed on the surface of the ODS steel were obviously different. After exposure for 100 h, a dense protective Al2O3 oxide layer with a thickness of about 500 nm was formed, greatly reducing the corrosion rate. With the corrosion time prolonging to 500 h at 700 ℃, most of Al2O3 layer was still remained. However, a few of nodular-like oxides were formed originated from local weak areas, which broken off the continuity of protective Al2O3 and led to deeper corrosion by LBE.
Feiyang BAO , Yanfen LI , Guangquan WANG , Jiarong ZHANG , Wei YAN , Quanqiang SHI , Yiyin SHAN , Ke YANG , Bin XU , Danrong SONG , Mingyu YAN , Xuedong WEI . Corrosion Behaviors and Mechanisms of ODS Steel Exposed to Static Pb-Bi Eutectic at 600 and 700 ℃[J]. Acta Metall Sin, 2020 , 56(10) : 1366 -1376 . DOI: 10.11900/0412.1961.2020.00035
| [1] | Lorusso P, Bassini S, Del Nevo A, et al. GEN-IV LFR development: Status & perspectives [J]. Prog. Nucl. Energy, 2018, 105: 318 |
| [2] | Fiori F, Zhou Z. A study on the Chinese nuclear energy options and the role of ADS reactor in the Chinese nuclear expansion [J]. Prog. Nucl. Energy, 2016, 91: 159 |
| [3] | Zhang J S. A review of steel corrosion by liquid lead and lead-bismuth [J]. Corros. Sci., 2009, 51: 1207 |
| [4] | Ballinger R G, Lim J. An overview of corrosion issues for the design and operation of high-temperature lead- and lead-bismuth-cooled reactor systems [J]. Nucl. Technol., 2004, 147: 418 |
| [5] | Zhang J S, Li N. Review of the studies on fundamental issues in LBE corrosion [J]. J. Nucl. Mater., 2008, 373: 351 |
| [6] | Yeliseyeva O, Tsisar V, Benamati G. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb-Bi melt saturated by oxygen [J]. Corros. Sci., 2008, 50: 1672 |
| [7] | Schroer C, Wedemeyer O, Novotny J, et al. Selective leaching of nickel and chromium from type 316 austenitic steel in oxygen-containing lead-bismuth eutectic (LBE) [J]. Corros. Sci., 2014, 84: 113 |
| [8] | Martinelli L, Balbaud-Célérier F, Terlain A, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part I) [J]. Corros. Sci., 2008, 50: 2523 |
| [9] | Martinelli L, Balbaud-Célérier F, Terlain A, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy at 470 ℃ (Part II) [J]. Corros. Sci., 2008, 50: 2537 |
| [10] | Martinelli L, Balbaud-Célérier F, Picard G, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part III) [J]. Corros. Sci., 2008, 50: 2549 |
| [11] | Yang K, Yan W, Wang Z G, et al. Development of a novel structural material (SIMP steel) for nuclear equipment with balanced resistances to high temperature, radiation and liquid metal corrosion [J]. Acta Metall. Sin., 2016, 52: 1207 |
| [11] | (杨 柯, 严 伟, 王志光等. 核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展 [J]. 金属学报, 2016, 52: 1207) |
| [12] | Yamaki E, Ginestar K, Martinelli L. Dissolution mechanism of 316L in lead-bismuth eutectic at 500 ℃ [J]. Corros. Sci., 2011, 53: 3075 |
| [13] | Gong X, Marmy P, Volodin A, et al. Multiscale investigation of quasi-brittle fracture characteristics in a 9Cr-1Mo ferritic-martensitic steel embrittled by liquid lead-bismuth under low cycle fatigue [J]. Corros. Sci., 2016, 102: 137 |
| [14] | Sapundjiev D, van Dyck S, Bogaerts W. Liquid metal corrosion of T91 and A316L materials in Pb-Bi eutectic at temperatures 400-600 ℃ [J]. Corros. Sci., 2006, 48: 577 |
| [15] | Tsisar V, Yeliseyeva O. Oxidation of Armco-Fe and steels in oxygen saturated liquid lead [J]. Mater. High Temp., 2007, 24: 93 |
| [16] | Weisenburger A, Aoto K, Müller G, et al. Behaviour of chromium steels in liquid Pb-55.5Bi with changing oxygen content and temperature [J]. J. Nucl. Mater., 2006, 358: 69 |
| [17] | Wang J, Lu S P, Rong L J, et al. Effect of silicon on the oxidation resistance of 9wt.% Cr heat resistance steels in 550 ℃ lead-bismuth eutectic [J]. Corros. Sci., 2016, 111: 13 |
| [18] | Kurata Y, Futakawa M, Saito S. Comparison of the corrosion behavior of austenitic and ferritic/martensitic steels exposed to static liquid Pb-Bi at 450 and 550 ℃ [J]. J. Nucl. Mater., 2005, 343: 333 |
| [19] | Müller G, Heinzel A, Konys J, et al. Results of steel corrosion tests in flowing liquid Pb/Bi at 420-600 ℃ after 2000 h [J]. J. Nucl. Mater., 2002, 301: 40 |
| [20] | Del Giacco M, Weisenburger A, Müller G. Fretting of fuel cladding materials for Pb cooled fast reactors-Approach to long term prediction using fretting maps [J]. Nucl. Eng. Des., 2014, 280: 697 |
| [21] | Kelly J E. Generation IV international forum: A decade of progress through international cooperation [J]. Prog. Nucl. Energy, 2014, 77: 240 |
| [22] | Odette G R. On the status and prospects for nanostructured ferritic alloys for nuclear fission and fusion application with emphasis on the underlying science [J]. Scr. Mater., 2018, 143: 142 |
| [23] | Li Y F, Nagasaka T, Muroga T, et al. High-temperature mechanical properties and microstructure of 9Cr oxide dispersion strengthened steel compared with RAFMs [J]. Fusion Eng. Des., 2011, 86: 2495 |
| [24] | Song L L, Yang X Y, Zhao Y Y, et al. Si-containing 9Cr ODS steel designed for high temperature application in lead-cooled fast reactor [J]. J. Nucl. Mater., 2019, 519: 22 |
| [25] | Schroer C, Konys J, Furukawa T, et al. Oxidation behaviour of P122 and a 9Cr-2W ODS steel at 550 ℃ in oxygen-containing flowing lead-bismuth eutectic [J]. J. Nucl. Mater., 2010, 398: 109 |
| [26] | Hosemann P, Thau H T, Johnson A L, et al. Corrosion of ODS steels in lead-bismuth eutectic [J]. J. Nucl. Mater., 2008, 373: 246 |
| [27] | Hojna A, Hadraba H, Di Gabriele F, et al. Behaviour of pre-stressed T91 and ODS steels exposed to liquid lead-bismuth eutectic [J]. Corros. Sci., 2018, 131: 264 |
| [28] | Tsisar V P. Oxidation of ferritic steels dispersion strengthened with TiO2 and Y2O3 oxides in lead melt [J]. Mater. Sci., 2008, 44: 630 |
| [29] | Baker B W, Brewer L N. Evaluation of liquid metal embrittlement of oxide dispersion strengthened steel MA956 [J]. Microsc. Microanal., 2014, 20(S3): 1852 |
| [30] | Lim J, Nam H O, Hwang I S, et al. A study of early corrosion behaviors of FeCrAl alloys in liquid lead-bismuth eutectic environments [J]. J. Nucl. Mater., 2010, 407: 205 |
| [31] | Lim J, Hwang I S, Kim J H. Design of alumina forming FeCrAl steels for lead or lead-bismuth cooled fast reactors [J]. J. Nucl. Mater., 2013, 441: 650 |
| [32] | Jianu A, Fetzer R, Weisenburger A, et al. Stability domain of alumina thermally grown on Fe-Cr-Al-based model alloys and modified surface layers exposed to oxygen-containing molten Pb [J]. J. Nucl. Mater., 2016, 470: 68 |
| [33] | Short M P, Ballinger R G, H?nninen H E. Corrosion resistance of alloys F91 and Fe-12Cr-2Si in lead-bismuth eutectic up to 715 ℃ [J]. J. Nucl. Mater., 2013, 434: 259 |
| [34] | Li Y F, Yan W, Xu B, et al. Design and fabrication of a novel structural ODS material with resistances to corrosion and irradiation and high strength [P]. Chin Pat, 201911332252.3, 2019 |
| [34] | (李艳芬, 严 伟, 许 斌等. 一种耐腐蚀、抗辐照、高强度的超级ODS钢及制备方法 [P]. 中国专利,201911332252.3, 2019) |
| [35] | Li M S. High Temperature Corrosion of Metals [M]. Beijing: Metallurgical Industry Press, 2001: 5 |
| [35] | (李美栓. 金属的高温腐蚀 [M]. 北京: 冶金工业出版社, 2001: 5) |
| [36] | Shi Q Q, Liu J, Luan H, et al. Oxidation behavior of ferritic/martensitic steels in stagnant liquid LBE saturated by oxygen at 600 ℃ [J]. J. Nucl. Mater., 2015, 457: 135 |
| [37] | Martinelli L, Dufrenoy T, Jaakou K, et al. High temperature oxidation of Fe-9Cr-1Mo steel in stagnant liquid lead-bismuth at several temperatures and for different lead contents in the liquid alloy [J]. J. Nucl. Mater., 2008, 376: 282 |
| [38] | Yeliseyeva O, Tsisar V. Comparison of oxidation of ferritic-martensitic steel EP-823 and Armco-Fe in Pb melt saturated by oxygen [J]. J. Corros. Sci. Eng., 2004, 7: 37 |
| [39] | Gromov B F, Orlov Y I, Martynov P N, et al. Liquid Metal Systems [M]. Boston: Springer, 1995: 339 |
| [40] | Weisenburger A, Jianu A, Doyle S, et al. Oxide scales formed on Fe-Cr-Al-based model alloys exposed to oxygen containing molten lead [J]. J. Nucl. Mater., 2013, 437: 282 |
| [41] | Tomaszewicz P, Wallwork G R. Observations of nodule growth during the oxidation of pure binary iron-aluminum alloys [J]. Oxid. Met., 1983, 19: 165 |
| [42] | Zhang Z G, Niu Y. Effect of chromium on the oxidation of a Fe-10Al alloy at 1000 ℃ [J]. Mater. Sci. Forum, 2005, 475-479: 685 |
/
| 〈 |
|
〉 |