Ultrasonic Detection for Fiber Broken in Aero-Engine Integral Bladed Ring
Received date: 2019-12-23
Revised date: 2020-01-21
Online published: 2020-05-19
Supported by
National Natural Science Foundation of China(51605468);Technology Innovation Project of Function Development of Instrument and Equipment, Chinese Academy of Sciences(Y8M1734171);Natural Science Foundation of Liaoning Province(2019-MS-334)
The fiber fracture is a very dangerous defect in the aeroengine integral bladed rings which is manufactured by continuous SiC fibers-reinforced titanium alloy matrix composite (Ti-MMC). Currently the lack of an effective method for inspecting the fiber fracture seriously influences the quality control of the aeroengine integral bladed rings, therefore solving the problem of non-destructive testing for deep buried radial micro-cracks is an insurmountable barrier for the application of Ti-MMC integral bladed rings in aviation. In this work, based on the theory of ultrasonic head-waves, the refraction longitudinal waves with the proper angle generated by the creeping wave probe are propagated on the interface, which means the creeping wave with high energy is generated. The finite element simulation model of the creeping wave is established for inspecting the defect of SiC fibers breakage in Ti-MMC aero-engine bling structure. Based on the results of the finite element simulation, significant defect signal waves are generated in the water layer above the defect. After that, not only the ultrasonic propagation characteristics at the interface of multilayer media but also the diffraction phenomenon of the creeping wave when they encounter the broken wire defect are analyzed. And the detection signal amplitude is not only affected by the incident angle of the creeping probe but also is related to the thickness of titanium alloy. In order to receive the diffracted waves with high sensitivity, the assembled probe, which is composed by a creeping wave exciter (5 MHz, 20°) and an immersion focusing sensor (5 MHz, diameter 6 mm), is specially designed and manufactured according to the results of the finite element simulation. In addition, the artificial sample with the broken fiber is prepared and then tested by the ultrasonic C-scan testing system with the assembled probe. The results show that the three-layer broken wire defects (the crack height is about 0.42 mm) with different depths in the artificial sample can be detected successfully. The C-scan results can match the defect positions of the artificial sample which means this detection method is valid. This method is simple, economical and fast, and is expected to solve the problem of nondestructive testing for broken wire in the deep embedded fiber ring in the Ti-MMC aero-engine bling structure.
Yupeng WU , Bo ZHANG , Jingming LI , Shuangnan ZHANG , Ying WU , Yumin WANG , Guixi CAI . Ultrasonic Detection for Fiber Broken in Aero-Engine Integral Bladed Ring[J]. Acta Metall Sin, 2020 , 56(8) : 1175 -1184 . DOI: 10.11900/0412.1961.2019.00441
| [1] | Yang R, Shi N L, Wang Y M, et al. Recent progress in SiC fibre reinforced titanium matrix composites [J]. Titanium Ind. Prog., 2005, 22(5): 32 |
| [1] | (杨 锐, 石南林, 王玉敏等. SiC纤维增强钛基复合材料研究进展 [J]. 钛工业进展, 2005, 22(5): 32) |
| [2] | Wang Y M, Zhang G X, Zhang X, et al. Advances in SiC fiber reinforced titanium matrix composites [J]. Acta Metall. Sin., 2016, 52: 1153 |
| [2] | (王玉敏, 张国兴, 张 旭等. 连续SiC纤维增强钛基复合材料研究进展 [J]. 金属学报, 2016, 52: 1153) |
| [3] | Wang Y M, Xiao P, Shi N L, et al. SiC fibre reinforced titanium matrix composite: Interface evolution and component manufacturing [J]. Mater. China, 2010, 29(5): 9 |
| [3] | (王玉敏, 肖 鹏, 石南林等. SiC纤维增强钛基复合材料界面研究及构件研制 [J]. 中国材料进展, 2010, 29(5): 9) |
| [4] | Chang D J, Kao W H. SiC reinforced titanium corrugated structures for high temperature application [J]. Sampe J., 1998, 24: 13 |
| [5] | Wu H, Zhao Y Q, Ge P. The advanced design and manufacturing technology of the key component of titanium for aviation engine [J]. Mater. Rev., 2011, 25(7): 101 |
| [5] | (吴 欢, 赵永庆, 葛 鹏. 航空发动机用关键钛合金部件先进设计及制造技术 [J]. 材料导报, 2011, 25(7): 101) |
| [6] | Zhang G Q, Zhao M, Lu S, et al. Development of research on aeroengine bling structure [J]. Aeronaut. Manuf. Technol., 2003, (9): 50 |
| [6] | (张国乾, 赵 明, 陆 山等. 航空发动机整体叶环结构的研究进展 [J]. 航空制造技术, 2003, (9): 50) |
| [7] | Favre J P, Vassel A, Laclau C. Testing of SiC/titanium composites by fragmentation and push-out tests: Comparison and discussion of test data [J]. Composites, 1994, 25: 482 |
| [8] | Kerans R J, Parthasarathy T A. Theoretical analysis of the fiber pullout and pushout tests [J]. J. Am. Ceram. Soc., 1991, 74: 1585 |
| [9] | Kong X, Wang Y M, Yang Q, et al. In situ detection of damage in the SiCf/Ti6242 composite during the thermomechanical fatigue test [J]. Rare Met. Mater. Eng., 2020, 49: 933 |
| [9] | (孔 旭, 王玉敏, 杨 青等. SiCf/Ti6242复合材料热机械疲劳损伤原位研究 [J]. 稀有金属材料与工程, 2020, 49: 933) |
| [10] | Ji X, Luo X, Yang Y Q, et al. Research progress of nondestructive testing for continuous fiber-reinforced metal-matrix composites [J]. Rare Met. Mater. Eng., 2013, 42(S2): 401 |
| [10] | (吉 幸, 罗 贤, 杨延清等. 连续纤维增强金属基复合材料无损检测研究进展 [J]. 稀有金属材料与工程, 2013, 42(增刊2): 401) |
| [11] | Waterbury M C, Karpur P, Matikas T E, et al. In situobservation of the single-fiber fragmentation process in metal-matrix composites by ultrasonic imaging [J]. Compos. Sci. Technol., 1994, 52: 261 |
| [12] | Park J M, Lee S I, Kwon O Y, et al. Comparison of nondestructive microfailure evaluation of fiber-optic bragg grating and acoustic emission piezoelectric sensors using fragmentation test [J]. Composites, 2003, 34A: 203 |
| [13] | Yancey R N, Baaklini G Y. Computed tomography evaluation of metal-matrix composites for aeropropulsion engine applications [J]. J. Eng. Gas Turbines Power., 1994, 116: 635 |
| [14] | Mueller B R, Lange A, Harward M, et al. Micro crack characterization of metal matrix composite by 3D refraction-computed-tomography [Z]. https://www.ndt.net/article/wcndt2004/pdf/materials_characterization/262_mueller.pdf |
| [15] | Hirano T, Usami K, Tanaka Y, et al. In situX-ray CT under tensile loading using synchrotron radiation [J]. J. Mater. Res., 1995, 10: 381 |
| [16] | Daryabor P, Safizadeh M S. Investigation of morphology techniques capability for the enhancement of ultrasonic C-scan images of composite patches [J]. Mater. Eval., 2019, 77: 203 |
| [17] | Cawley P. The rapid non-destructive inspection of large composite structures [J]. Composites, 1994, 25: 351 |
| [18] | Cai G X, Shen J Z, Sha G F, et al. The formation mechanism and characteristics of the delayed wave echoes in the slender piece by axial ultrasonic inspection [J]. Nondestruct. Test., 2018, 40(7): 1 |
| [18] | (蔡桂喜, 沈建中, 沙高峰等. 细长工件轴向超声检测中迟到波的形成机制及特性 [J]. 无损检测, 2018, 40(7): 1) |
| [19] | Leyens C, Kocian F, Hausmann J, et al. Materials and design concepts for high performance compressor components [J]. Aerosp. Sci. Technol., 2003, 7: 201 |
| [20] | Zhang X, Wang Y M, Lei J F, et al. The interfacial thermal stability and element diffusion mechanism of SiCf/TC17 composite [J]. Acta Metall. Sin., 2012, 48: 1306 |
| [20] | (张 旭, 王玉敏, 雷家峰等. SiCf/TC17复合材料界面热稳定性及元素扩散机理 [J]. 金属学报, 2012, 48: 1306) |
| [21] | Wang Y M, Fu Y C, Shi N L, et al. Effects of sputtering parameter on the microstructure of Ti-6Al-4V coating on SiC fibre [J]. Acta Metall. Sin, 2004, 40: 359 |
| [21] | (王玉敏, 符跃春, 石南林等. 溅射参量对SiC涂层Ti-6Al-4V显微组织的影响 [J]. 金属学报, 2004, 40: 359) |
| [22] | Zhang X, Yang Q, Wang Y M, et al. Room and elevated temperature tensile properties of SiCf/TC17 composite [A]. Proceedings of the 12th World Conference on Titanium [C]. Beijing: Science Press, 2011: 1545 |
| [23] | Heelan P A. On the theory of head waves [J]. Geophysics, 1953, 18: 871 |
| [24] | ISO. ISO 5577: 2017 Non-destructive testing—Ultrasonic testing—Vocabulary [S]. 2017 |
| [25] | Hojjati M H, Honarvar F. An investigation of the relationship between subsurface and head waves by finite element modeling [J]. Nondestr. Test. Eval., 2016, 31: 319 |
| [26] | Ferrand A, Darmon M, Chatillon S, et al. Modeling of ray paths of head waves on irregular interfaces in TOFD inspection for NDE [J]. Ultrasonics, 2014, 54: 1851 |
| [27] | Merazi-Meksen T, Kemmouche A, Boudraa M, et al. Sparse representations to replace TOFD images in non-destructive testing of materials [J]. J. Nondestr. Eval., 2017, 36: 67 |
/
| 〈 |
|
〉 |