Effect of Laser Process Parameters on the Microstructure and Properties of TiC Reinforced Co-Based Alloy Laser Cladding Layer
Received date: 2019-12-18
Revised date: 2020-03-09
Online published: 2020-03-31
Supported by
Scientific and Technological Research Project of Liaoning Provincial Department of Education(L201705)
The severe wear and uneven wear will happen on the surface of ductile cast iron such as the traction wheel of elevator, in the long-term working under the serious wear and impact conditions. Laser cladding can be applied to reinforce its surface, which can improve the properties and life of the cladded components, save materials and manufacturing cost and raise the economic efficiency, but as to the surface of different materials, especially the ductile cast iron, the alloy powder and process parameters for laser cladding need to be chosen carefully by the experimental studies because of the rapid melting and solidification, the difference of thermo-physical properties between the laser cladding layer and the matrix, the laser absorption of the cladding layer and matrix and so on. In this work, laser cladding is employed to fabricate Co-based composite coatings reinforced by TiC particles by a 6 kW CO2 laser. The effects of the technical parameters of laser on the composition, phase and microhardness of the laser cladding layer are investigated by OM, SEM, EDS, XRD and microhardness tester, with the emphases of analyzing the changes of the distribution, morphology and size of TiC in the laser cladding layer. It is shown by the results that the cladding layer is mainly composed of γ-Co, TiC/(Ti, W)C1-x, Cr-Ni-Fe-C and a small amount of Cr7C3 phase, and its microstructure changed from the fine dendrite crystal near the cast iron matrix to the equiaxed dendrite in the middle then to the fine dendrite crystal near the surface of laser cladding layer with the dispersed distribution of TiC at the root or tip of secondary dendrite arm, even at the branch of primary dendrite arm. The number of dendrite and the dendrite arm spacing both increase in the microstructure of the laser cladding layer and the morphology of TiC is transformed from the smooth circular shape to the irregular polygon shape, and its content obviously increases with the particle size of TiC decreasing and its distribution more uniform, when the laser power is decreased from 3.6 kW to 3.2 kW or the scanning rate increased from 350 mm/min to 410 mm/min. The growth of the primary dendrite or secondary dendrite can be inhibited by the precipitation of TiC after its dissolution in the melt pool of laser cladding. In this experiment, the hardness at the surface of laser cladding layer gradually increases with the decrease of laser power or the increase of scanning rate, in which the maximal microhardness is 1246.6 HV0.2, up to increasing by 5 times of the matrix.
Wenhui TONG , Xinyuan ZHANG , Weixuan LI , Yukun LIU , Yan LI , Xuming GUO . Effect of Laser Process Parameters on the Microstructure and Properties of TiC Reinforced Co-Based Alloy Laser Cladding Layer[J]. Acta Metall Sin, 2020 , 56(9) : 1265 -1274 . DOI: 10.11900/0412.1961.2019.00438
| [1] | Fang G R, Wang Y Z. The birth, application, tendency of technologh development—The one of the most important technology progresses of the material science of the 20th century [J]. Modern Cast Iron, 2000, (1): 3 |
| [1] | (房贵如, 王云昭. 现代球墨铸铁的诞生、应用及技术发展趋势—20世纪材料科学最重大的技术进展之一 [J]. 现代铸铁, 2000, (1): 3) |
| [2] | Sharifitabar M, Khaki J V, Sabzevar M H. Microstructure and wear resistance of in-situ TiC-Al2O3 particles reinforced Fe-based coatings produced by gas tungsten arc cladding [J]. Surf. Coat. Technol., 2016, 285: 47 |
| [3] | Xu J Y, Zou B L, Tao S Y, et al. Fabrication and properties of Al2O3-TiB2-TiC/Al metal matrix composite coatings by atmospheric plasma spraying of SHS powders [J]. J. Alloys Compd., 2016, 672: 251 |
| [4] | Nurminen J, Nakki J, Vuoristo P. Microstructure and properties of hard and wear resistant MMC coatings deposited by laser cladding [J]. Int. J. Refract. Met. Hard Mater., 2009, 27: 472 |
| [5] | Taillon G, Pougoum F, Lavigne S, et al. Cavitation erosion mechanisms in stainless steels and in composite metal-ceramic HVOF coatings [J]. Wear, 2016, 364-365: 201 |
| [6] | Su H J, Wei K C, Guo W, et al. New development of laser rapid forming and its application in high performance materials processing [J]. Chin. J. Nonferrous Met., 2013, 23: 1567 |
| [6] | (苏海军, 尉凯晨, 郭 伟等. 激光快速成形技术新进展及其在高性能材料加工中的应用 [J]. 中国有色金属学报, 2013, 23: 1567) |
| [7] | Lee C, Park H K, Yoo J, et al. Residual stress and crack initiation in laser clad composite layer with Co-based alloy and WC + NiCr [J]. Appl. Surf. Sci., 2015, 345: 286 |
| [8] | Ma Q S, Li Y J, Wang J, et al. Investigation on core-eutectic structure in Ni60/WC composite coatings fabricated by wide-band laser cladding [J]. J. Alloys Compd., 2015, 645: 151 |
| [9] | Leunda J, Sanz C, Soriano C. Laser cladding strategies for producing WC reinforced NiCr coatings inside twin barrels [J]. Surf. Coat. Technol., 2016, 307: 720 |
| [10] | Xu X, Mi G Y, Xiong L D, et al. Morphologies, microstructures and properties of TiC particle reinforced Inconel 625 coatings obtained by laser cladding with wire [J]. J. Alloys Compd., 2018, 740: 16 |
| [11] | Diao Y H, Zhang K M. Microstructure and corrosion resistance of TC2 Ti alloy by laser cladding with Ti/TiC/TiB2 powders [J]. Appl. Surf. Sci., 2015, 352: 163 |
| [12] | Arias-González F, Del Val J, Comesana R, et al. Fiber laser cladding of nickel-based alloy on cast iron [J]. Appl. Surf. Sci., 2016, 374: 197 |
| [13] | Li Y J, Dong S Y, He P, et al. Microstructure characteristics and mechanical properties of new-type FeNiCr laser cladding alloy coating on nodular cast iron [J]. J. Mater. Process. Technol., 2019, 269: 163 |
| [14] | Yang P C, Song Y L, Liu Y H, et al. Effect of scanning speed on microstructure of laser cladding layer on nodular cast iron [J]. Surf. Technol., 2018, 47(9): 187 |
| [14] | (杨鹏聪, 宋雨来, 刘耀辉等. 扫描速度对球墨铸铁激光熔覆层组织的影响 [J]. 表面技术, 2018, 47(9): 187) |
| [15] | Xu N J, Lv J B, Sun T, et al. Process optimization and properties of laser cladding high vanadium high speed steel coatings on nodular cast iron [J]. Adv. Mater. Res., 2013, 712-715: 611 |
| [16] | Navas C, Conde A, Fernández B J, et al. Laser coatings to improve wear resistance of mould steel [J]. Surf. Coat. Technol., 2005, 194: 136 |
| [17] | Orthner H R, Tomasi R, Botta W J. Reaction sintering of titanium carbide and titanium silicide prepared by high-energy milling [J]. Mater. Sci. Eng., 2002, A336: 202 |
| [18] | Gu D D, Meng G B, Li C, et al. Selective laser melting of TiC/Ti bulk nanocomposites: Influence of nanoscale reinforcement [J]. Scr. Mater., 2012, 67: 185 |
| [19] | Lagos M A, Agote I, Atxaga G, et al. Fabrication and characterisation of titanium matrix composites obtained using a combination of self propagating high temperature synthesis and spark plasma sintering [J]. Mater. Sci. Eng., 2016, A655: 44 |
| [20] | Emamian A, Corbin S F, Khajepour A. Effect of laser cladding process parameters on clad quality and in-situ formed microstructure of Fe-TiC composite coatings [J]. Surf. Coat. Technol., 2010, 205: 2007 |
| [21] | Tong W H, Zhao Z L, Zhang X Y, et al. Microstructure and properties of TiC/Co-based alloy by laser cladding on the surface of nodular graphite cast iron [J]. Acta Metall. Sin., 2017, 53: 472 |
| [21] | (童文辉, 赵子龙, 张新元等. 球墨铸铁表面激光熔覆TiC/钴基合金组织和性能研究 [J]. 金属学报, 2017, 53: 472) |
| [22] | Zhang J, Qiu B, Zhao L Z. Latest developments of laser cladding technology [J]. Hot Work. Technol., 2011, 40(18): 116 |
| [22] | (张 坚, 邱 斌, 赵龙志. 激光熔覆技术研究进展 [J]. 热加工工艺, 2011, 40(18): 116) |
| [23] | Candel J J, Jimenez J A, Franconetti P, et al. Effect of laser irradiation on failure mechanism of TiCp reinforced titanium composite coating produced by laser cladding [J]. J. Mater. Process. Technol., 2014, 214: 2325 |
| [24] | Li Y J, Dong S Y, Yan S X, et al. Phase evolution of ductile iron during laser cladding processing [J]. Surf. Coat. Technol., 2018, 339: 37 |
| [25] | Kwon H, Suh C Y, Kim W. Preparation of a highly toughened (Ti, W)C-20Ni cermet through in situ formation of solid solution and WC whiskers [J]. Ceram. Int., 2015, 41: 4223 |
| [26] | Liang Y J, Che Y C. Handbook of Thermodynamics of Inorganic Materials [M]. Shenyang: Northeastern University Press, 1993: 45 |
| [26] | (梁英教, 车荫昌. 无机物热力学数据手册 [M]. 沈阳: 东北大学出版社, 1993: 45) |
| [27] | Zhang Z G, Liu X F, Bian X F. Thermodynamics and kinetic of forming TiC in Al-Ti-C system [J]. Acta Metall. Sin., 2000, 36: 1025 |
| [27] | (张作贵, 刘相法, 边秀房. Al-Ti-C系中TiC形成的热力学与动力学研究 [J]. 金属学报, 2000, 36: 1025) |
| [28] | Feng K Q, Yang Y, Shen B L. Study on the thermodynamics of high temperature chemical reaction of TiC/Fe composite synthesized by reaction-casting [J]. Hot Work. Technol., 2002, (6): 8 |
| [28] | (冯可芹, 杨 屹, 沈保罗. 反应铸造TiC/Fe复合材料过程中高温化学反应的热力学研究 [J]. 热加工工艺, 2002, (6): 8) |
| [29] | Hu H Q. Principle of Metal Solidification [M]. Beijing: Mechanical Industry Press, 2012: 142 |
| [29] | (胡汉起. 金属凝固原理 [M]. 北京: 机械工业出版社, 2012: 142) |
| [30] | Khalili A, Goodarzi M, Mojtahedi M, et al. Solidification microstructure of in-situ laser-synthesized Fe-TiC hard coating [J]. Surf. Coat. Technol., 2016, 307: 747 |
/
| 〈 |
|
〉 |