Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel

  • Hongwei ZHOU ,
  • Fengmei BAI ,
  • Lei YANG ,
  • Yan CHEN ,
  • Junfei FANG ,
  • Liqiang ZHANG ,
  • Hailong YI ,
  • Yizhu HE
Expand
  • 1. Key Laboratory of Green Fabrication and Surface Technology of Advanced Metal Materials, Ministry of Education, Anhui University of Technology, Maanshan 243032, China
    2. School of Materials Science and Engineering, Anhui University of Technology, Maanshan 243032, China
    3. School of Metallurgical Engineering, Anhui University of Technology, Maanshan 243032, China
    4. State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China

Received date: 2019-09-04

  Revised date: 2019-11-19

  Online published: 2020-03-13

Supported by

Joint Fund of National Natural Science Foundation of China(U1760108);National Natural Science Foundation of China(51674079);National Natural Science Foundation of China(51874001);Natural Science Foundation of Anhui Provincial Education Department(KJ2018A0062);Natural Science Foundation of Anhui Provincial Education Department(KJ2019A0059)

Abstract

The low-cycle fatigue (LCF) behavior of 1100 MPa grade tempered high strength steel under symmetrical strain control conditions was studied at the strain amplitude ranges of 0.4%~1.2% in this work. The LCF properties of quenching and tempering high strength steel were examined by means of OM, SEM and TEM. The microstructure changes, fracture morphology, crack propagation characteristics and inclusion morphology were studied in detail. The results show that the cyclic hardening and cyclic softening depend on strain amplitude. At the low strain amplitude of 0.4%, rapid cyclic hardening occurs in initial 10 cyc, and then the stress remains almost unchanged until the sample breaks. While at the strain amplitude ranges of 0.5%~1.2%, the cyclic hardening reaches a peak at the first few cycles, followed by the remarkable cyclic softening until the sample fails. The cyclic softening is mainly due to the recovery of some martensite lath under low-cycle fatigue loading and the decrease of dislocation density in the laths. 1100 MPa grade high-strength steel is found to obey LCF Manson-Coffin relationship. The high-strength steel has excellent LCF performance for two main reasons, which is related with the shape and size of inclusions. One is that the shape of the inclusion is nearly circular, and the diameter is 2~5 μm, which is lower than the critical dimension of the inclusions causing fatigue crack initiation. The crack is initiated on the surface of the sample. This increases fatigue crack initiation life. The other one is that the original austenite grain boundary, the martensite packet/block boundary and the inclusions or cavities can induce the crack deflection, reducing the crack propagation rate and increasing fatigue crack propagation life.

Cite this article

Hongwei ZHOU , Fengmei BAI , Lei YANG , Yan CHEN , Junfei FANG , Liqiang ZHANG , Hailong YI , Yizhu HE . Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. Acta Metall Sin, 2020 , 56(7) : 937 -948 . DOI: 10.11900/0412.1961.2019.00291

References

[1] An T B, Tian Z L, Shan J G, et al. Effect of the temperature of post weld heat treatment on microstructure and performance of weld metal for 1000 MPa grade high strength steel [J]. J. Mech. Eng., 2015, 51(4): 40
[1] (安同邦, 田志凌, 单际国等. 后热温度对1000 MPa级高强钢焊缝组织与性能的影响 [J]. 机械工程学报, 2015, 51(4): 40)
[2] Zhu B, Liu Z, Wang Y A, et al. Application of a model for quenching and partitioning in hot stamping of high-strength steel [J]. Metall. Mater. Trans., 2018, 49A: 1304
[3] Xie Z J, Fang Y P, Han G, et al. Structure-property relationship in a 960 MPa grade ultrahigh strength low carbon niobium-vanadium microalloyed steel: The significance of high frequency induction tempering [J]. Mater. Sci. Eng., 2014, A618: 112
[4] Fang J F, Xu Z L, Si S H, et al. Microstructure transformation characteristic of CGHAZ of Q1100 high-strength steel at different cooling rates [J]. Mater. Mech. Eng., 2017, 41(1): 107
[4] (方俊飞, 徐震霖, 斯松华等. 不同冷速下Q1100高强钢焊接热影响区粗晶区的组织转变特征 [J]. 机械工程材料, 2017, 41(1): 107)
[5] Zhang Y J. Low cycle fatigue characteristic of 10CrNiMo high-strength steel [J]. J. Univ. Sci. Technol. Beijing, 2011, 33(1): 22
[5] (张亚军. 10CrNiMo高强钢的低周疲劳特性 [J]. 北京科技大学学报, 2011, 33(1): 22)
[6] Sowards J W, Pfeif E A, Connolly M J, et al. Low-cycle fatigue behavior of fiber-laser welded, corrosion-resistant, high-strength low alloy sheet steel [J]. Mater. Des., 2017, 121: 393
[7] Branco R, Costa J D, Antunes F V. Low-cycle fatigue behaviour of 34CrNiMo6 high strength steel [J]. Theor. Appl. Fract. Mec., 2012, 58: 28
[8] Jiang Q M, Zhang X Q, Chen L Q, et al. SH-CCT Diagram, microstructures and properties of heat-affected zone in a 1000 MPa grade extra high-strength steel [J]. J. Iron Steel. Res., 2014, 26(1):47
[8] (蒋庆梅, 张小强, 陈礼清等. 1000 MPa级超高强钢的SH-CCT曲线及其热影响区的组织和性能 [J]. 钢铁研究学报, 2014, 26(1):47)
[9] Pang J C, Li S X, Wang Z G, et al. General relation between tensile strength and fatigue strength of metallic materials [J]. Mater. Sci. Eng., 2013, A564: 331
[10] Wang X S, Liang F, Zeng Y P, et al. SEM in situ observations to the effects of inclusions on initiation and propagation of the low cyclic fatigue crack in super strength steel [J]. Acta Metall. Sin., 2005, 41: 1272
[10] (王习术, 梁 锋, 曾燕屏等. 夹杂物对超高强度钢低周疲劳裂纹萌生及扩展影响的原位观测 [J]. 金属学报, 2005, 41: 1272)
[11] Li S X. Effects of inclusions on very high cycle fatigue properties of high strength steels [J]. Int. Mater. Rev., 2012, 57: 92
[12] Song S W, Lee J H, Lee H J, et al. Enhancing high-cycle fatigue properties of cold-drawn Fe-Mn-C TWIP steels [J]. Int. J. Fatigue, 2016, 85: 57
[13] Zhou H W, He Y Z, Zhang H, et al. Influence of dynamic strain aging pre-treatment on the low-cycle fatigue behavior of modified 9Cr-1Mo steel [J]. Int. J. Fatigue, 2013, 47: 83
[14] Ye D Y, Matsuoka S, Nagashima N, et al. The low-cycle fatigue, deformation and final fracture behaviour of an austenitic stainless steel [J]. Mater. Sci. Eng., 2006, A415: 104
[15] Bai F M, Zhou H W, Liu X H, et al. Masing behavior and microstructural change of quenched and tempered high-strength steel under low cycle fatigue [J]. Acta. Metall. Sin. (Engl. Lett.), 2019, 32: 1346
[16] Chakraborti P C, Mitra M K. Room temperature low cycle fatigue behaviour of two high strength lamellar duplex ferrite-martensite (DFM) steels [J]. Int. J. Fatigue, 2005, 27: 511
[17] Verma P, Srinivas N C S, Singh S R, et al. Low cycle fatigue behavior of modified 9Cr-1Mo steel at room temperature [J]. Mater. Sci. Eng., 2016, A652: 30
[18] Chauhan A, Hoffmann J, Litvinov D, et al. High-temperature low-cycle fatigue behavior of a 9Cr-ODS steel: Part 1-Pure fatigue, microstructure evolution and damage characteristics [J]. Mater. Sci. Eng., 2017, A707: 207
[19] Chauhan A, Litvinov D, Aktaa J. Deformation and damage mechanisms of a bimodal 12Cr-ODS steel under high-temperature cyclic loading [J]. Int. J. Fatigue, 2016, 93: 1
[20] Marinelli M C, Alvarez-Armas I, Krupp U. Cyclic deformation mechanisms and microcracks behavior in high-strength bainitic steel [J]. Mater. Sci. Eng., 2017, A684: 254
[21] Kang J, Zhang F C, Long X Y, et al. Low cycle fatigue behavior in a medium-carbon carbide-free bainitic steel [J]. Mater. Sci. Eng., 2016, A66: 88
[22] Fran?ois D, Pineau A, Zaoui A. Mechanical Behaviour of Materials: Volume II: Fracture Mechanics and Damage [M]. 2nd Ed., London: Springer Dordrecht Heidelberg, 2013: 340
[23] Glode? S, Knez M, Jezernik N, et al. Fatigue and fracture behaviour of high strength steel S1100Q [J]. Eng. Fail. Anal., 2009, 16: 2348
[24] Wang J G, Yang S L, Wang H Y, et al. Low-cycle fatigue properties of 800 MPa-grade ultrafine-grained steel [J]. J. Univ. Sci. Technol. Beijing, 2005, 27(1): 75
[24] (王建国, 杨胜利, 王红缨等. 800 MPa级低合金高强度钢低周疲劳性能 [J]. 北京科技大学学报, 2005, 27(1): 75)
[25] Koh S K, Stephens R I. Mean stress effects on low cycle fatigue for a high strength steel [J]. Fatigue Fract. Eng. Mater. Struct., 1991, 14: 413
[26] Fang Y P, Xie Z J, Shang C J. Effect of induction tempering on carbide precipitation behavior and toughness of a 1000 MPa grade high strength low alloy steel [J]. Acta Metall. Sin., 2014, 50: 1413
[26] (房玉佩, 谢振家, 尚成嘉. 感应回火对1000 MPa级高强度低合金钢碳化物析出行为及韧性的影响 [J]. 金属学报, 2014, 50: 1413)
[27] Zhou H W, He Y Z, Cui M, et al. Dependence of dynamic strain ageing on strain amplitudes during the low-cycle fatigue of TP347H austenitic stainless steel at 550 ℃ [J]. Int. J. Fatigue, 2013, 56: 1
[28] Kruml T, Polák J. Fatigue cracks in Eurofer 97 steel: Part I. Nucleation and small crack growth kinetics [J]. J Nucl. Mater., 2011, 412: 2
[29] Man J, Vystavěl T, Weidner A, et al. Study of cyclic strain localization and fatigue crack initiation using FIB technique [J]. Int. J. Fatigue, 2012, 39: 44
[30] Man J, Klapetek P, Man O, et al. Extrusions and intrusions in fatigued metals. Part 2. AFM and EBSD study of the early growth of extrusions and intrusions in 316L steel fatigued at room temperature [J]. Philos. Mag., 2009, 89: 1337
[31] Chan K S. Roles of microstructure in fatigue crack initiation [J]. Int. J. Fatigue, 2010, 32: 1428
[32] Pan Q S, Zhou H F, Lu Q H, et al. History-independent cyclic response of nanotwinned metals [J]. Nature, 2017, 551: 214
[33] Koyama M, Zhang Z, Wang M M, et al. Bone-like crack resistance in hierarchical metastable nanolaminate steels [J]. Science, 2017, 355: 1055
[34] Abareshi M, Emadoddin E. Effect of retained austenite characteristics on fatigue behavior and tensile properties of transformation induced plasticity steel [J]. Mater. Des., 2011, 32: 5099
[35] Gui X L, Zhang B X, Gao G H, et al. Fatigue behavior of bainite/martensite multiphase high strength steel treated by quenching-partitioning-tempering process [J]. Acta Metall. Sin., 2016, 52: 1036
[35] (桂晓露, 张宝祥, 高古辉等. Q-P-T处理贝氏体/马氏体复相高强钢疲劳断裂特性研究 [J]. 金属学报, 2016, 52: 1036)
[36] Zhang Z, Hu Z F, Fan L K, et al. Low cycle fatigue behavior and cyclic softening of P92 ferritic-martensitic steel [J]. J. Iron Steel Res. Int., 2015, 22: 534
[37] Huang Z W, Yuan F H, Wang Z G, et al. Low cycle fatigue properties and fracture mechanisms of M38 nickel base superalloy at high temperature [J]. Acta Metall. Sin., 2007, 43: 1025
[37] (黄志伟, 袁福河, 王中光等. M38镍基高温合金高温低周疲劳性能及断裂机制 [J]. 金属学报, 2007, 43: 1025)
[38] Wei D Y, Gu J L, Fang H S, et al. Fatigue behavior on a 1500 MPa grade bainite/martensite duplex-phase high strength steel [J]. Acta Metall. Sin., 2003, 39: 734
[38] (韦东远, 顾家琳, 方鸿生等. 1500 MPa级贝氏体/马氏体复相高强钢的疲劳断裂特性 [J]. 金属学报, 2003, 39: 734)
[39] Hu D Y, Wang T, Ma Q H, et al. Effect of inclusions on low cycle fatigue lifetime in a powder metallurgy nickel-based superalloy FGH96 [J]. Int. J. Fatigue, 2019, 118: 237
Outlines

/