Influence of Manufacturing Parameters on the Properties of Electron Beam Melted Ti-Ni Alloy
Received date: 2019-11-29
Revised date: 2020-02-28
Online published: 2020-03-11
Supported by
Strategic Priority Research Program of the Chinese Academy of Sciences(XDA22010103)
Electron beam melting (EBM) is one of the additive manufacturing technologies which can be used to fabricate the complex structure and shape samples. Until now, there are few literatures published about the properties of Ti-Ni samples produced by EBM. In this work, the influence of two important manufacturing parameters of focus offset (FO) and speed function (SF) on the density, phase content and transformation behavior, microstructure and mechanical properties was investigated for the equiatomic Ti-Ni shape memory alloy fabricated by EBM used DSC, XRD, SEM, TEM and electronic universal testing machine. The results showed that all the Ti-Ni samples had a high relative density beyond than 97% for fabricated by different combinations of FO and SF in the selected range. The corresponding phase transformation temperatures for all the Ti-Ni samples fabricated by EBM were higher than the pre-alloyed Ti-Ni powder, due to the effect of evaporation of Ni element higher than that of the formation of Ni-rich Ti2Ni phase during the quickly melting and solidification process. On the other hand, the EBM manufacturing parameters of FO and SF had limited influence on the phase contents, phase transformation temperatures and Vickers hardness. Due to the feature of the EBM fabricating method, the different types of defects would be introduced in the Ti-Ni solid samples. Though all the samples had similar high relative density, the performance of the compression behavior were shown great difference, and the crack defect had the larger effect than the gas and lack-of fusion porosities on the compression fracture stress and strain.
Dechun REN , Huibo ZHANG , Xiaodong ZHAO , Fuyu WANG , Wentao HOU , Shaogang WANG , Shujun LI , Wei JIN , Rui YANG . Influence of Manufacturing Parameters on the Properties of Electron Beam Melted Ti-Ni Alloy[J]. Acta Metall Sin, 2020 , 56(8) : 1103 -1112 . DOI: 10.11900/0412.1961.2019.00410
| [1] | Jiang H C, Rong L J. Releasing behavior of Ni in porous NiTi shape memory alloy [J]. Acta Metall. Sin., 2008, 44: 198 |
| [1] | (姜海昌, 戎利建. 多孔NiTi形状记忆合金中Ni的释放行为 [J]. 金属学报, 2008, 44: 198) |
| [2] | He Z R, Wu P Z, Liu K K, et al. Microstructure, phase transformation and shape memory behavior of chilled Ti-47Ni alloy ribbons [J]. Acta Metall. Sin., 2018, 54: 1157 |
| [2] | (贺志荣, 吴佩泽, 刘康凯等. 激冷Ti-47Ni合金薄带的组织、相变和形状记忆行为 [J]. 金属学报, 2018, 54: 1157) |
| [3] | Liu X P, Jin W, Meng C G, et al. Effect of cold deformation on the transformation behaviors of TiNi film [J]. Acta Metall. Sin., 2001, 37: 589 |
| [3] | (刘晓鹏, 金 伟, 孟长功等. 预变形对TiNi薄膜相变行为的影响 [J]. 金属学报, 2001, 37: 589) |
| [4] | Elahinia M H, Hashemi M, Tabesh M, et al. Manufacturing and processing of NiTi implants: A review [J]. Prog. Mater. Sci., 2012, 57: 911 |
| [5] | Liu L J, Li S J, Wang H L, et al. Microstructure, defects and mechanical behavior of beta-type titanium porous structures manufactured by electron beam melting and selective laser melting [J]. Acta Mater., 2016, 113: 56 |
| [6] | Zhao X L, Li S J, Zhang M, et al. Comparison of the microstructures and mechanical properties of Ti-6Al-4V fabricated by selective laser melting and electron beam melting [J]. Mater. Des., 2016, 95: 21 |
| [7] | Ren D C, Li S J, Wang H, et al. Fatigue behavior of Ti-6Al-4V cellular structures fabricated by additive manufacturing technique [J]. J. Mater. Sci. Technol., 2019, 35: 285 |
| [8] | Wang C C, Tan X P, Liu E J, et al. Process parameter optimization and mechanical properties for additively manufactured stainless steel 316L parts by selective electron beam melting [J]. Mater. Des., 2018, 147: 157 |
| [9] | Wang P, Sin W J, Nai M L S, et al. Effects of processing parameters on surface roughness of additive manufactured Ti-6Al-4V via electron beam melting [J]. Materials, 2017, 10: 1121 |
| [10] | Zhang L C, Liu Y J, Li S J, et al. Additive manufacturing of titanium alloys by electron beam melting: A review [J]. Adv. Eng. Mater., 2018, 20: 1700842 |
| [11] | Pushilina N, Syrtanov M, Kashkarov E, et al. Influence of manufacturing parameters on microstructure and hydrogen sorption behavior of electron beam melted titanium Ti-6Al-4V alloy [J]. Materials, 2018, 11: 763 |
| [12] | Saedi S, Turabi A S, Andani M T, et al. The influence of heat treatment on the thermomechanical response of Ni-rich NiTi alloys manufactured by selective laser melting [J]. J. Alloys Compd., 2016, 677: 204 |
| [13] | Ma J, Franco B, Tapia G, et al. Spatial control of functional response in 4D-Printed active metallic structures [J]. Sci. Rep., 2017, 7: 46707 |
| [14] | Moghaddam N S, Saghaian S E, Amerinatanzi A, et al. Anisotropic tensile and actuation properties of NiTi fabricated with selective laser melting [J]. Mater. Sci. Eng., 2018, A724: 220 |
| [15] | Habijan T, Haberland C, Meier H, et al. The biocompatibility of dense and porous nickel-titanium produced by selective laser melting [J]. Mater. Sci. Eng., 2013, C33: 419 |
| [16] | Li S, Hassanin H, Attallah M M, et al. The development of TiNi-based negative Poisson's ratio structure using selective laser melting [J]. Acta Mater., 2016, 105: 75 |
| [17] | Ren D C, Zhang H B, Liu Y J, et al. Microstructure and properties of equiatomic Ti-Ni alloy fabricated by selective laser melting [J]. Mater. Sci. Eng., 2020, A771: 138586 |
| [18] | Hayat M D, Chen G, Khan S, et al. Physical and tensile properties of NiTi alloy by selective electron beam melting [J]. Key Eng. Mater., 2018, 770: 148 |
| [19] | Schwerdtfeger J, Singer R F, K?rner C. In situ flaw detection by IR-imaging during electron beam melting [J]. Rapid Prototyp. J., 2012, 18: 259 |
| [20] | Al-Bermani S S. An investigation into microstructure and microstructural control of additive layer manufactured Ti-6Al-4V by electron beam melting [D]. Sheffield: University of Sheffield, 2011 |
| [21] | Cheng B, Price S, Lydon J, et al. On process temperature in powder-bed electron beam additive manufacturing: Model development and validation [J]. J. Manuf. Sci. Eng., 2014, 136: 061018 |
| [22] | Price S, Cheng B, Lydon J, et al. On process temperature in powder-bed electron beam additive manufacturing: Process parameter effects [J]. J. Manuf. Sci. Eng., 2014, 136: 061019 |
| [23] | Attar H, Calin M, Zhang L C, et al. Manufacture by selective laser melting and mechanical behavior of commercially pure titanium [J]. Mater. Sci. Eng., 2014, A593: 170 |
| [24] | Liu Y J, Liu Z, Jiang Y, et al. Gradient in microstructure and mechanical property of selective laser melted AlSi10Mg [J]. J. Alloys Compd., 2018, 735: 1414 |
| [25] | Krishna B V, Bose S, Bandyopadhyay A. Laser processing of net-shape NiTi shape memory alloy [J]. Metall. Mater. Trans., 2007, 38A: 1096 |
| [26] | Gong H J, Rafi K, Gu H F, et al. Influence of defects on mechanical properties of Ti-6Al-4 V components produced by selective laser melting and electron beam melting [J]. Mater. Des., 2015, 86: 545 |
| [27] | Li Y T. The study on defect formation in laser additive manufacturing titanium alloy [D]. Dalian: Dalian University of Technology, 2017 |
| [27] | (李永涛. 钛合金激光增材制造缺陷研究 [D]. 大连: 大连理工大学, 2017) |
/
| 〈 |
|
〉 |