Phase Field Simulations of the Sintering Process of UO2

  • Zhengyang SUN ,
  • Chao YANG ,
  • Wenbo LIU
Expand
  • 1 School of Nuclear Science and Technology, Xi‘an Jiaotong University, Xi'an 710049,China
    2 Shaanxi Key Laboratory of Advanced Nuclear Energy and Technology, Shaanxi Engineering Research Center of Advanced Nuclear Energy, Xi’an Jiaotong University, Xi’an 710049, China
    3 Advanced Research Institute of Multidisciplinary Science, Beijing Institute of Technology, Beijing 100081, China

Received date: 2019-12-19

  Revised date: 2020-02-24

  Online published: 2020-03-09

Supported by

National Natural Science Foundation of China(11705137);China Postdoctoral Science Foundation(2019M663738);China Postdoctoral Science Foundation(2018T111053);State Key Laboratory of New Ceramic and Fine Processing, Tsinghua University(KF201713);Innovative Scientific Program of CNNC

Abstract

UO2 is widely used as fuel in various nuclear reactors, and the sintering of UO2 ceramic powder under high temperature is one of the most important processes during the preparation of UO2 fuel. However, sintering is a very complicated process which is controlled by many simultaneous mechanisms. The phase field method was used to simulate the sintering process of UO2 ceramic powder in the present work. In the modified phase field model, the influence of three anisotropic diffusion mechanisms, including surface diffusion, grain boundary diffusion and lattice diffusion, on the microstructure evolution during sintering was considered, and the effect of the interface energy between different ceramic particles on the sintering morphology was also considered. Based on the experimental conditions and thermodynamic parameters, the sintering process of UO2 ceramic powder at 2000 K was simulated. The simulation results showed that the initial morphology of the ceramic powder affects the sintering kinetics; large grains grow more easily, and small grains disappear at the last stage of sintering; the GB diffusion mechanism is the dominant mechanism during the sintering; the equilibrium dihedral angle between GB and phase boundaries can be strongly affected by the GB energy. In addition, the sintering process of the polycrystalline UO2 ceramic powder was also simulated, and the simulation results were in good agreement with the experimental results.

Cite this article

Zhengyang SUN , Chao YANG , Wenbo LIU . Phase Field Simulations of the Sintering Process of UO2[J]. Acta Metall Sin, 2020 , 56(9) : 1295 -1303 . DOI: 10.11900/0412.1961.2019.00440

References

[1] Yin B Y. Ceramic Nuclear Fuel Process [M]. Harbin: Harbin Engineering University Press, 2016: 277
[1] (尹邦跃.陶瓷核燃料工艺 [M]. 哈尔滨: 哈尔滨工程大学出版社, 2016: 277)
[2] Zhou M S, Tian M B, Dai X J. Nuclear Materials and Application [M]. Beijing: Tsinghua University Press, 2017: 22
[2] (周明胜, 田民波, 戴兴建. 核材料与应用 [M]. 北京: 清华大学出版社, 2017: 22)
[3] Rahaman M N. Ceramic Processing and Sintering [M]. New York: Marcel Dekker, 1995: 446
[4] German R M. Sintering Theory and Practice [M]. New York: John Wiley&Sons Ltd., 1996: 1
[5] Burke J E, Turnbull D. Recrystallization and grain growth [J]. Prog. Metall. Phys., 1952, 3: 220
[6] Mullins W W. Two-dimension motion of idealized grain boundaries [J]. J. Appl. Phys., 1956, 27: 900
[7] Hillert M. On the theory of normal and abnormal grain growth [J]. Acta Metall., 1965, 13: 227
[8] Srolovitz D J, Anderson M P, Grest G S, et al. Computer-simulation of grain-growth—Ⅲ. Influence of a particle dispersion [J]. Acta Metall., 1984, 32: 1429
[9] Tikare V, Braginsky M, Olevsky E A. Numerical simulation of solid-state sintering: I, Sintering of three particles [J]. J. Am. Ceram. Soc., 2003, 86: 49
[10] Liu Y, Baudin T, Penelle R. Simulation of normal grain growth by cellular automata [J]. Scr. Mater., 1996, 34: 1679
[11] Svoboda J, Riedel H. Quasi-equilibrium sintering for coupled grain-boundary and surface diffusion [J]. Acta Metall. Mater., 1995, 43: 499
[12] Zhang W, Schneibel J H. The sintering of two particles by surface and grain boundary diffusion—A two-dimensional numerical study [J]. Acta Metall. Mater., 1995, 43: 4377
[13] Pan J, Cocks A C F. A numerical technique for the analysis of coupled surface and grain-boundary diffusion [J]. Acta Metall. Mater., 1995, 43: 1395
[14] Kundin J, Sohaib H, Schiedung R, et al. Phase-field modeling of pores and precipitates in polycrystalline system [J]. Modell. Simul. Mater. Sci. Eng., 2018, 26: 065003
[15] H?tzer J, Seiz M, Kellner M, et al. Phase-field simulation of solid state sintering [J]. Acta Mater., 2019, 164: 184
[16] Fan D, Chen L Q. Computer simulation of grain growth using a continuum field model [J]. Acta. Mater., 1997, 45: 611
[17] Chockalingam K, Kouznetsova V G, van der Sluis O, et al. 2D phase field modeling of sintering of silver nanoparticles [J]. Comput. Method Appl. Mech. Eng., 2016, 312: 492
[18] Wakai F, Brakke K A. Mechanics of sintering for coupled grain boundary and surface diffusion [J]. Acta Mater., 2011, 59: 5379
[19] Biswas S, Schwen D, Tomar V. Implementation of a phase field model for simulating evolution of two powder particles representing microstructural changes during sintering [J]. J. Mater. Sci., 2018, 53: 5799
[20] Cahn J W, Hilliard J E. Free energy of a nonuniform system. I. Interfacial free energy [J]. J. Chem. Phys., 1958, 28: 258
[21] Jing X N, Ni Y, He L H, et al. 2-D phase-field simulation of pore evolution in sintering ceramics [J]. J. Inorg. Mater., 2002, 17: 1078
[21] (景晓宁, 倪 勇, 何陵辉等. 陶瓷烧结过程孔隙演化的二维相场模拟 [J]. 无机材料学报, 2002, 17: 1078)
[22] Liu M Z, Zhang R J, Fang W, et al. Phase field simulation of sintering process in biphasic porous material [J]. Acta. Metall. Sin., 2012, 48: 1207
[22] (刘明治, 张瑞杰, 方 伟等. 相场法模拟两相多孔组织烧结 [J]. 金属学报, 2012, 48: 1207)
[23] Wang Y U. Computer modeling and simulation of solid-state sintering: A phase field approach [J]. Acta Mater., 2006, 54: 953
[24] Kumar V, Fang Z Z, Fife P C. Phase field simulations of grain growth during sintering of two unequal-sized particles [J]. Mater. Sci. Eng., 2010, A528: 254
[25] Gugenberger C, Spatschek R, Kassner K. Comparison of phase-field models for surface diffusion [J]. Phys. Rev., 2008, 78E: 016703
[26] Moelans N, Blanpain B, Wollants P. Quantitative analysis of grain boundary properties in a generalized phase field model for grain growth in anisotropic systems [J]. Phys. Rev., 2008, 78B: 024113
[27] Deng J. A phase field model of sintering with direction-dependent diffusion [J]. Mater. Trans., 2012, 53: 385
[28] Read W T, Shockley W. Dislocation models of crystal grain boundaries [J]. Phys. Rev., 1950, 78: 275
[29] Ahmed K, Yablinsky C A, Schulte A, et al. Phase field modeling of the effect of porosity on grain growth kinetics in polycrystalline ceramics [J]. Modell. Simul. Mater. Sci. Eng., 2013, 21: 065005
[30] Cahn J W. On spinodal decomposition [J]. Acta Metall., 1961, 9: 795
[31] Bourgeois L, Dehaudt P, Lemaignan C, et al. Pore migration in UO2 and grain growth kinetics [J]. J. Nucl. Mater., 2001, 295: 73
[32] Reynolds G L, Burton B. Grain-boundary diffusion in uranium dioxide: The correlation between sintering and creep and a reinterpretation of creep mechanism [J]. J. Nucl. Mater., 1979, 82: 22
[33] Allen S M, Cahn J W. A microscopic theory for antiphase boundary motion and its application to antiphase domain coarsening [J]. Acta Metall., 1979, 27: 1085
[34] Ahmed K, Pakarinen J, Allen T, et al. Phase field simulation of grain growth in porous uranium dioxide [J]. J. Nucl. Mater., 2014, 446: 90
[35] Ge L H, Subhash G, Baney R H, et al. Influence of processing parameters on thermal conductivity of uranium dioxide pellets prepared by spark plasma sintering [J]. J. Eur. Ceram. Soc., 2014, 34: 1791
[36] Ahmed K, Allen T, El-Azab A. Phase field modeling for grain growth in porous solids [J]. J. Mater. Sci., 2016, 51: 1261
[37] Riedel H, Svoboda J. A theoretical study of grain growth in porous solids during sintering [J]. Acta Metall. Mater., 1993, 41: 1929
[38] Smith C S. Grains, phases, and interfaces: An interpretation of microstructure [J]. Trans. Met. Soc. AIME., 1948, 175: 15
Outlines

/