Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel

  • Zhanyi XU ,
  • Yuhui SHA ,
  • Fang ZHANG ,
  • Huabing ZHANG ,
  • Guobao LI ,
  • Shuangjie CHU ,
  • Liang ZUO
Expand
  • 1 Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China
    2 Baoshan Iron & Steel Cooperation Limited, Shanghai 201900, China
    3 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2019-12-17

  Revised date: 2020-02-27

  Online published: 2020-03-09

Supported by

National Key Research and Development Program of China(2016YFB0300305);National Natural Science Foundation of China(51671049);National Natural Science Foundation of China(51931002)

Abstract

The key index of grain-oriented silicon steel is the sharpness of secondary recrystallization Goss ({110}<001>) texture, which is determined by the matrix grain size distribution, texture environment and inhibitor level. In the widely used low-temperature slab heating process in virtue of high efficiency and low-cost manufacturing, the instability of inhibitor and the enlarged matrix grain size distribution seriously restrict the occurrence of secondary recrystallization and the sharpness of Goss texture. The investigation on orientation selection behavior during abnormal grain growth can explore the potential routines to solve the problem. In this work, the evolution process of secondary recrystallization texture in grain-oriented silicon steel has been studied by both experiment and calculation. It is found that single Goss texture is finally obtained by means of continuous orientation selection during secondary recrystallization. The kinetic model for secondary recrystallization, introduced with orientation-dependent relative grain boundary energy coefficient, can describe quantitatively the difference in growth rate between Goss grains with various deviation angles and non-Goss grains. The combined effects of grain size distribution, grain boundary characteristic between Goss and matrix grains, together with inhibition force level on orientation selection behavior are analyzed. Accordingly, a multi-parameter matching method for promoting the advantage of Goss grains in orientation selection is proposed.

Cite this article

Zhanyi XU , Yuhui SHA , Fang ZHANG , Huabing ZHANG , Guobao LI , Shuangjie CHU , Liang ZUO . Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. Acta Metall Sin, 2020 , 56(8) : 1067 -1074 . DOI: 10.11900/0412.1961.2019.00435

References

[1] Hayakawa Y. Mechanism of secondary recrystallization of Goss grains in grain-oriented electrical steel [J]. Sci. Technol. Adv. Mater., 2017, 18: 480
[2] Xia Z S, Kang Y L, Wang Q L. Developments in the production of grain-oriented electrical steel [J]. J. Magn. Magn. Mater., 2008, 320: 3229
[3] Moses A J. Energy efficient electrical steels: Magnetic performance prediction and optimization [J]. Scr. Mater., 2012, 67: 560
[4] He C X, Yang F Y, Yan G C, et al. Effect of normalizing on textures of thin-gauge grain-oriented silicon steel [J]. Acta Metall. Sin., 2016, 52: 1063
[4] (何承绪, 杨富尧, 严国春等. 常化处理对薄规格取向硅钢织构的影响 [J]. 金属学报, 2016, 52: 1063)
[5] Chu S J, Yang Y J, He Z H, et al. Calculation of magnetostriction coefficient for laser-scribed grain-oriented silicon steel based on magnetic domain interaction [J]. Acta Metall. Sin., 2019, 55: 362
[5] (储双杰, 杨勇杰, 和正华等. 基于磁畴结构交互作用的激光刻痕取向硅钢磁致伸缩系数计算 [J]. 金属学报, 2019, 55: 362)
[6] Ushigami Y, Mizokami M, Fujikura M, et al. Recent development of low-loss grain-oriented silicon steel [J]. J. Magn. Magn. Mater., 2003, 254-255: 307
[7] Harase J, Shimizu R. Distribution of {110}<001> oriented grains in the primary recrystallized 3% Si-Fe alloy [J]. Trans. Jpn. Inst. Met., 1988, 29(5): 388
[8] Hayakawa Y, Szpunar J A, Palumbo G, et al. The role of grain boundary character distribution in Goss texture development in electrical steels [J]. J. Magn. Magn. Mater., 1996, 160: 143
[9] Rouag N, Vigna G, Penelle R. Evolution of local texture and grain boundary characteristics during secondary recrystallisation of Fe-3%Si sheets [J]. Acta Metall. Mater., 1990, 38: 1101
[10] Shimizu R, Harase J. Coincidence grain boundary and texture evolution in Fe-3%Si [J]. Acta Mater., 1989, 37: 1241
[11] Lin P, Palumbo G, Harase J, et al. Coincidence site lattice (CSL) grain boundaries and Goss texture development in Fe-3%Si alloy [J]. Acta Mater., 1996, 44: 4677
[12] Kumano T, Ushigami Y. Grain boundary characteristics of isolated grains in conventional grain oriented silicon steel [J]. ISIJ Int., 2007, 47: 890
[13] Hayakawa Y, Szpunar J A. The role of grain boundary character distribution in secondary recrystallization of electrical steels [J]. Acta Mater., 1997, 45: 1285
[14] Hayakawa Y, Szpunar J A. A new model of Goss texture development during secondary recrystallization of electrical steel [J]. Acta Mater., 1997, 45: 4713
[15] Rajmohan N, Szpunar J A, Hayakawa Y. A role of fractions of mobile grain boundaries in secondary recrystallization of Fe-Si steels [J]. Acta Mater., 1999, 47: 2999
[16] Rajmohan N, Szpunar J A, Hayakawa Y. Importance of fractions of highly mobile boundaries in abnormal growth of Goss grains [J]. Mater. Sci. Eng., 1999, A259: 8
[17] Rajmohan N, Szpunar J A. An analytical method for characterizing grain boundaries around growing Goss grains during secondary recrystallization [J]. Scr. Mater., 2001, 44: 2387
[18] Morawiec A. Grain misorientations in theories of abnormal grain growth in silicon steel [J]. Scr. Mater., 2000, 43: 275
[19] Morawiec A. On abnormal growth of Goss grains in grain-oriented silicon steel [J]. Scr. Mater., 2011, 64: 466
[20] Nakayama T, Ushigami Y. Modeling of secondary recrystallization in 3% silicon steels [J]. Mater. Sci. Forum, 1992, 94-96: 413
[21] Ushigami Y, Kawasaki K, Nakayama T, et al. Dynamic observation of the growth of secondary recrystallized grains of Fe-3%Si alloy utilizing synchrotron X-ray topography [J]. Mater. Sci. Forum, 1994, 157-162: 1081
[22] Ushigami Y. Theoretical analysis and computer simulation of secondary recrystallization in grain-oriented silicon steel [R]. Nippon Steel Technical Report No.102, 2013: 25
[23] Hillert M. On the theory of normal and abnormal grain growth [J]. Acta Metall., 1965, 13: 227
[24] Furtkamp M, Gottstein G, Molodov D A, et al. Grain boundary migration in Fe-3.5%Si bicrystals with [001] tilt boundaries [J]. Acta Mater., 1998, 46: 4103
[25] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena [M]. 2nd Ed., Amsterdam: Elsevier, 2004: 102
[26] Liu G T, Liu Z Q, Yang P, et al. Correlation between primary and secondary recrystallization texture components in low-temperature reheated grain-oriented silicon steel [J]. J. Iron Steel Res. Int., 2016, 23: 1234
[27] Yoshitomi Y, Ushigami Y, Harase J, et al. Coincidence grain boundary and role of primary recrystallized grain growth on secondary recrystallization texture evolution in Fe-3%Si alloy [J]. Acta Metall. Mater., 1994, 42: 2593
[28] Ko K J, Rollett A D, Hwang N M. Abnormal grain growth of Goss grains in Fe-3%Si steel driven by sub-boundary-enhanced solid-state wetting: Analysis by Monte Carlo simulation [J]. Acta Mater., 2010, 58: 4414
[29] Mao W M, Zhang M H, Yang P. Behaviors of normal grain growth in polycrystalline Fe-3%Si alloys [J]. Steel Res. Int., 2014, 85: 1215
Outlines

/