Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy

  • Liang ZHU ,
  • Mingxing GUO ,
  • Bo YUAN ,
  • Linzhong ZHUANG ,
  • Jishan ZHANG
Expand
  • 1. State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China
    2. Beijing Laboratory of Metallic Materials and Processing for Modern Transportation, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2019-11-11

  Revised date: 2020-01-14

  Online published: 2020-03-09

Supported by

National Key Research and Development Program of China(2016YFB0300801);National Natural Science Foundation of China(51871029);National Natural Science Foundation of China(51571023);National Natural Science Foundation of China(51301016);Government Guided Program-Intergovernmental Bilateral Innovation Cooperation Project(BZ2019019)

Abstract

In order to reduce the weight of car body, Al-Mg-Si-Cu alloys have been widely studied and used to produce outer body panels of automobiles due to their favorable high-strength-to-weight ratio, recyclability and good formability. Moreover, the strength of Al-Mg-Si-Cu series alloys can be enhanced by bake hardening treatment. However, their formability and final strengths still need to be further improved compared to steels, which are the major obstacles to wide-scale application of Al alloys in the automotive fields. In this work, the effect of ageing routes on the precipitation behavior of Al-Mg-Si-Cu-Zn alloy with high Mg/Si ratio was systematically studied by DSC, TEM, tensile and hardness tests. The results show that the precipitation activation energies of the β″ phase formed in the non-isothermal ageing processes of the as-quenched and pre-aged alloys are 80.1 kJ/mol and 64.5 kJ/mol, respectively; both the different age hardening rates and microstructure evolution behaviors can be also observed during their isothermal ageing processes, such as, the age hardening rate of as-quenched alloy is much higher, but the peak hardness and strength values of the alloy treated by the two routes were basically the same. However, the elongation and strain hardening rate of the pre-aged alloy in the peak ageing state, and the hardness reduction rate in the over-ageing state are all much higher. In addition, a large number of complex solute clusters can be formed during pre-ageing, which will further grow in high temperature isothermal ageing process, but the sizes of precipitates formed in the under-ageing, peak-ageing and over-ageing states all show a multi-scale characteristics; in comparison, this feature cannot be found in the precipitates formed in the as-quenched alloy aged in the different conditions. The ageing routes cannot change the precipitation sequence of the alloy, but give a significant influence on the nucleation and growth rates of precipitates. As a consequence, a schematic diagram of nucleation and growth process of precipitates in the alloy with ageing routes is proposed.

Cite this article

Liang ZHU , Mingxing GUO , Bo YUAN , Linzhong ZHUANG , Jishan ZHANG . Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy[J]. Acta Metall Sin, 2020 , 56(7) : 997 -1006 . DOI: 10.11900/0412.1961.2019.00386

References

[1] Hirsch J. Recent development in aluminium for automotive applications [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 1995
[2] Guo M X, Sha G, Cao L Y, et al. Enhanced bake-hardening response of an Al-Mg-Si-Cu alloy with Zn addition [J]. Mater. Chem. Phys., 2015, 162: 15
[3] Peng X Y, Guo M X, Wang X F, et al. Influence of particles with different sizes on microstructure, texture and mechanical properties of Al-Mg-Si-Cu series alloys [J]. Acta Metall. Sin., 2015, 51: 169
[3] (彭祥阳, 郭明星, 汪小锋等. 不同尺寸粒子对Al-Mg-Si-Cu系合金组织、织构和力学性能的影响 [J]. 金属学报, 2015, 51: 169)
[4] Li Y, Guo M X, Jiang N, et al. Precipitation behaviors and preparation of an advanced Al-0.93Mg-0.78Si-0.20Cu-3.00Zn alloy for automotive application [J]. Acta Metall. Sin., 2016, 52: 191
[4] (李 勇, 郭明星, 姜 宁等. 汽车用新型Al-0.93Mg-0.78Si-0.20Cu-3.00Zn合金的制备及其时效析出行为研究 [J]. 金属学报, 2016, 52: 191)
[5] Yuan B, Guo M X, Wu Y, et al. Influence of treatment pathways on the precipitation behaviors of Al-Mg-Si-Cu-(Zn)-Mn alloys [J]. J. Alloys Compd., 2019, 797: 26
[6] Guo M X, Zhang Y D, Yuan B, et al. Influence of aging pathways on the evolution of heterogeneous solute-rich features in peak-aged Al-Mg-Si-Cu alloy with a high Mg/Si ratio [J]. Philos. Mag. Lett., 2019, 99: 49
[7] Li G J, Guo M X, Du J Q, et al. Influence of precipitate-assisted nucleation on the microstructure and mechanical properties of Al-Mg-Si-Cu-Zn alloys [J]. Philos. Mag., 2019, 99: 1335
[8] Guo M X, Du J Q, Zheng C H, et al. Influence of Zn contents on precipitation and corrosion of Al-Mg-Si-Cu-Zn alloys for automotive applications [J]. J. Alloys Compd., 2019, 778: 256
[9] Jin S X, Ngai T, Zhang G W, et al. Precipitation strengthening mechanisms during natural ageing and subsequent artificial aging in an Al-Mg-Si-Cu alloy [J]. Mater. Sci. Eng., 2018, A724: 53
[10] Guo M X, Li G J, Zhang Y D, et al. Influence of Zn on the distribution and composition of heterogeneous solute-rich features in peak aged Al-Mg-Si-Cu alloys [J]. Scr. Mater., 2019, 159: 5
[11] Banhart J, Chang C S T, Liang Z Q, et al. Natural aging in Al-Mg-Si alloys—A process of unexpected complexity [J]. Adv. Eng. Mater., 2010, 12: 559
[12] Marioara C D, Andersen S J, Jansen J, et al. The influence of temperature and storage time at RT on nucleation of the β″ phase in a 6082 Al-Mg-Si alloy [J]. Acta Mater., 2003, 51: 789
[13] Pogatscher S, Kozeschnik E, Antrekowitsch H, et al. Process-controlled suppression of natural aging in an Al-Mg-Si alloy [J]. Scr. Mater., 2014, 89: 53
[14] Tao G H, Liu C H, Chen J H, et al. The influence of Mg/Si ratio on the negative natural aging effect in Al-Mg-Si-Cu alloys [J]. Mater. Sci. Eng., 2015, A642: 241
[15] Chang C S T, Wieler I, Wanderka N, et al. Positive effect of natural pre-ageing on precipitation hardening in Al-0.44at%Mg-0.38at%Si alloy [J]. Ultramicroscopy, 2009, 109: 585
[16] Pogatscher S, Antrekowitsch H, Werinos M, et al. Diffusion on demand to control precipitation aging: Application to Al-Mg-Si alloys [J]. Phys. Rev. Lett., 2014, 112: 225701
[17] Zhen L, Kang S B, Kim H W. Effect of natural aging and preaging on subsequent precipitation process of an AI-Mg-Si alloy with high excess silicon [J]. Mater. Sci. Technol., 1997, 13: 905
[18] Zandbergen M W, Cerezo A, Smith G D W. Study of precipitation in Al-Mg-Si Alloys by atom probe tomography II. Influence of Cu additions [J]. Acta Mater., 2015, 101: 149
[19] Weng Y Y, Jia Z H, Ding L P, et al. Clustering behavior during natural aging and artificial aging in Al-Mg-Si alloys with different Ag and Cu addition [J]. Mater. Sci. Eng., 2018, A732: 273
[20] Guo M X, Zhang Y D, Li G J, et al. Solute clustering in Al-Mg-Si-Cu-(Zn) alloys during aging [J]. J. Alloys Compd., 2019, 774: 347
[21] Liu M, Zhang X P, K?rner B, et al. Effect of Sn and In on the natural ageing kinetics of Al-Mg-Si alloys [J]. Materialia, 2019, 6: 100261
[22] Ding L P, He Y, Wen Z, et al. Optimization of the pre-aging treatment for an AA6022 alloy at various temperatures and holding times [J]. J. Alloys Compd., 2015, 647: 238
[23] Abid T, Boubertakh A, Hamamda S. Effect of pre-aging and maturing on the precipitation hardening of an Al-Mg-Si alloy [J]. J. Alloys Compd., 2010, 490: 166
[24] Murayama M, Hono K. Pre-precipitate clusters and precipitation processes in Al-Mg-Si Alloys [J]. Acta Mater., 1999, 47: 1537
[25] De Geuser F, Lefebvre W, Blavette D. 3D atom probe study of solute atoms clustering during natural ageing and pre-ageing of an Al-Mg-Si alloy [J]. Philos. Mag. Lett., 2006, 86: 227
[26] Lumley R. Fundamentals of Aluminium Metallurgy [M]. Cambridge: Woodhead Publishing Press, 2011: 307
[27] Zhang Q L, Luan X, Dhawan S, et al. Development of the post-form strength prediction model for a high-strength 6xxx aluminium alloy with pre-existing precipitates and residual dislocations [J]. Int. J. Plast., 2019, 119: 230
[28] Poole W J, Wang X, Lloyd D J, et al. The shearable-non-shearable transition in Al-Mg-Si-Cu precipitation hardening alloys: Implications on the distribution of slip, work hardening and fracture [J]. Philos. Mag., 2005, 85: 3113
[29] ? Ryen, Laukli H I, Holmedal B, et al. Large strain work hardening of aluminum alloys and the effect of mg in solid solution [J]. Metall. Mater. Trans., 2006, 37A: 2007
[30] Esteban-Manzanares G, Martínez E, Segurado J, et al. An atomistic investigation of the interaction of dislocations with Guinier-Preston zones in Al-Cu alloys [J]. Acta Mater., 2019, 162: 189
Outlines

/