Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors

  • Jiaying YU ,
  • Hua WANG ,
  • Weisen ZHENG ,
  • Yanlin HE ,
  • Yurui WU ,
  • Lin LI
Expand
  • 1.School of Materials Science and Engineering, Shanghai University, Shanghai 200444, China
    2.Saic Motor Corporation Limited Passenger Vehicle Co. , Shanghai 201804, China

Received date: 2019-10-21

  Revised date: 2020-01-12

  Online published: 2020-02-26

Supported by

National Key Research and Development Program of China(2017YFB0304402)

Abstract

Hot-dip galvanizing is the most economical way to improve the corrosion resistance of advanced high strength automobile steel. With the high trend of developing of automobile steel towards light-weight and high-strength, the contents of Si, Mn, Al alloy elements in steel increase accordingly. These alloy elements would be selectively oxidized during hot-dip galvanizing process, which affect in turn the wettability of steel surface and form different interface microstructures. However, its effect on the mechanical behavior of steel has never been known as clear as desired. Base on this point, the thermodynamics of the surface oxide and its effect on the interface microstructure of three high-strength automobile steels were studied after the same hot-dip galvanizing treatment as well as their tensile fracture behavior under different deformation conditions was in situ analyzed. Combined with the microstructure analysis and thermodynamic calculation, it can be concluded that different compositions of steel would produce different kinds of oxide on its surface. When Mn2SiO4 and SiO2 were formed as thermodynamic stable phases, it was difficult to form a continuous Fe2Al5Zn0.4 inhibition layer at the interface, zinc liquid could penetrate into the iron substrate and then form the brittle phase ζ-FeZn13, where the crack was easily to be obtained and expanded to the substrate, resulting in the decrease of mechanical properties. When MnO and Mn2SiO4 with a small amount were formed as thermodynamic stable phase, the Fe2Al5Zn0.4 inhibition layer can be obtained. Under the tensile stress, this crack generated at the interface and extended to the zinc layer. So, the fracture of the experimental steel was mainly resulted from the failure of substrate. When MnO and FeO were formed as metastable phase, Fe, as formed by aluminothermic reduction during hot-dip galvanizing, would reacted with zinc liquid to form Γ-Fe11Zn40 phase in the zinc layer. The crack generated under the tensile stress and expanded in the zinc layer. Since the unreduced MnO layer at the interface exhibited a higher bonding strength with substrate, tensile fracture of the experimental steel was caused by the failure of substrate.

Cite this article

Jiaying YU , Hua WANG , Weisen ZHENG , Yanlin HE , Yurui WU , Lin LI . Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors[J]. Acta Metall Sin, 2020 , 56(6) : 863 -873 . DOI: 10.11900/0412.1961.2019.00352

References

[1] Wang C Y, Yang J, Chang Y, et al. Development trend and challenge of advanced high strength automobile steels [J]. Iron Steel, 2019, 54(2): 1
[1] 王存宇, 杨 洁, 常 颖等. 先进高强度汽车钢的发展趋势与挑战 [J]. 钢铁, 2019, 54(2): 1
[2] Wang A H, Zhu J F. Development trend of substituting hot-biq galvanized sheet for electro-galvanized sheet [J]. Res. Iron Steel, 2007, 35(6): 53
[2] 王爱华, 朱久发. 国内外热镀锌板取代电镀锌板的发展趋势 [J]. 钢铁研究, 2007, 35(6): 53
[3] Miyata M, Fushiwaki Y, Suzuki Y, et al. Effect of Si/Mn ratio on galvannealing behavior of Si-addied steel [J]. ISIJ Int., 2018, 58: 1600
[4] Blumenau M, Norden M, Friedel F, et al. Reactive wetting during hot-dip galvanizing of high manganese alloyed steel [J]. Surf. Coat. Technol., 2011, 205: 3319
[5] Bellhouse E M, McDermid J R. Selective oxidation and reactive wetting of 1.0 pct Si-0.5 pct Al and 1.5 pct Si TRIP-assisted steels [J]. Metall. Mater. Trans., 2010, 41A: 1539
[6] Bellhouse E M, Mertens A I M, McDermid J R. Development of the surface structure of TRIP steels prior to hot-dip galvanizing [J]. Mater. Sci. Eng., 2007, A463: 147
[7] Park S J, Hwang B, Lee K H, et al. Microstructure and tensile behavior of duplex low-density steel containing 5 mass% aluminum [J]. Scr. Mater., 2013, 68: 365
[8] Gupta A K, Kumar D A. Formability of galvanized interstitial-free steel sheets [J]. J. Mater. Process. Technol, 2006, 172: 225
[9] Liu H C, Li F, Shi W, et al. Characterization of hot-dip galvanized coating on dual phase steels [J]. Surf. Coat. Technol., 2011, 205: 3535
[10] Cho L, Lee S J, Kim M S, et al. Influence of gas atmosphere dew point on the selective oxidation and the reactive wetting during hot dip galvanizing of CMnSi TRIP steel [J]. Metall. Mater. Trans., 2013, 44A: 362
[11] Gong Y F, Kim H S, De Cooman B C. Formation of surface and subsurface oxides during ferritic, intercritical and austenitic annealing of CMnSi TRIP steel [J]. ISIJ Int., 2008, 48: 1745
[12] Lee S K, Kim J S, Choi J W, et al. Effects of dew point on selective oxidation of TRIP steels containing Si, Mn, and B [J]. Met. Mater. Int., 2011, 17: 251
[13] Lins V D F C, Madeira L, Vilela J M C, et al. Selective oxidation of dual phase steel after annealing at different dew points [J]. Appl. Surf. Sci., 2011, 257: 5871
[14] Suzuki Y, Yamashita T, Sugimoto Y, et al. Thermodynamic analysis of selective oxidation behavior of Si and Mn-added steel during recrystallization annealing [J]. ISIJ Int., 2009, 49: 564
[15] Huin D, Flauder P, Leblond J B. Numerical simulation of internal oxidation of steels during annealing treatments [J]. Oxid. Met., 2005, 64: 131
[16] Bellhouse E M, Mcdermid J R. Selective oxidation and reactive wetting during hot-dip galvanizing of a 1.0 pct Al-0.5 pct Si TRIP-assisted steel [J]. Metall. Mater. Trans., 2012, 43A: 2426
[17] Bellhouse E M, Mcdermid J R. Analysis of the Fe-Zn interface of galvanized high Al-low Si TRIP steels [J]. Mater. Sci. Eng., 2008, A491: 39
[18] Bellhouse E M, McDermid J R. Selective oxidation and reactive wetting during galvanizing of a CMnAl TRIP-assisted steel [J]. Metall. Mater. Trans., 2011, 42A: 2753
[19] Wang K K, Hsu C W, Chang L W, et al. Role of Al in Zn bath on the formation of the inhibition layer during hot-dip galvanizing for a 1.2Si-1.5Mn transformation-induced plasticity steel [J]. Appl. Surf. Sci., 2013, 285: 458
[20] Li F, Liu H, Shi W, et al. Hot dip galvanizing behavior of advanced high strength steel [J]. Mater. Corros., 2012, 63: 396
[21] Jeong T K, Jung G, Lee K, et al. Selective oxidation of Al rich Fe-Mn-Al-C low density steels [J]. Mater. Sci. Technol., 2014, 30: 1805
[22] Song G M, Sloof W G. Effect of alloying element segregation on the work of adhesion of metallic coating on metallic substrate: Application to zinc coatings on steel substrates [J]. Surf. Coat. Technol., 2011, 205: 4632
[23] Marder A R. The metallurgy of zinc-coated steel [J]. Prog. Mater. Sci., 2000, 45: 191
[24] Okamoto N L, Kashioka D, Inomoto M, et al. Compression deformability of Γ and ζ Fe-Zn intermetallics to mitigate detachment of brittle intermetallic coating of galvannealed steels [J]. Scr. Mater., 2013, 69: 307
[25] Song G M, Vystavel T, van der Pers N, et al. Relation between microstructure and adhesion of hot dip galvanized zinc coatings on dual phase steel [J]. Acta Mater., 2012, 60: 2973
Outlines

/