β solidifying γ-TiAl alloys are being considered for high-temperature application in the aerospace and automotive industries as high efficiency materials which can withstand temperatures up to 800 ℃ and owns attractively thermal and mechanical properties. Through thermos-mechanical process can obtain excellent alloy properties, such as high strength and better elongation. But it will cause anisotropy. Ti-43.5Al-4Nb-1Mo-0.1B alloy rectangular bar was prepared by isothermal hot canned extrusion process. The OM, SEM, XRD, TEM and tensile methods were used to study the microstructure and tensile properties of the rectangular rods in different states and locations. The results show that the extruded structure of the rectangular rods is relatively uniform and there is no significant difference in the microstructure at different locations. The extrusion deformation makes the orientation of the lamellar uniform, tending to be parallel to the extrusion direction; γ phase in the grain boundary exists in the three forms of graininess, bulk and strip; the β phase is shredded during extrusion and is elongated in a parallel extrusion direction. Under the TEM observation, lamellar at the edge of the bar was completely shredded, and lamellar at the core position was elongated after lamellar was broken. A large number of ω0 phases are generated in the β0 phase, and the phase relationship of the two follows: [
Xianfeng LIU , Dong LIU , Renci LIU , Yuyou CUI , Rui YANG . Microstructure and Tensile Properties of Ti-43.5Al-4Nb-1Mo-0.1B Alloy Processed by Hot Canned Extrusion[J]. Acta Metall Sin, 2020 , 56(7) : 979 -987 . DOI: 10.11900/0412.1961.2019.00388
| [1] | Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129 |
| [1] | (杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129) |
| [2] | Kim Y W, Kim S L. Advances in gammalloy materials-processes-application technology: successes, dilemmas, and future [J]. JOM, 2018, 70: 553 |
| [3] | Bewlay B P, Weimer M, Kelly T, et al. Intermetallic-based alloys science, technology, and applications [A]. Materials Research Society Symposia Proceedings [C]. Cambrige: Cambridge University Press, 2013: 49 |
| [4] | Bewlay B P, Nag S, Suzuki A, et al. TiAl alloys in commercial aircraft engines [J]. Mater. High Temp., 2016, 33: 549 |
| [5] | Habel U, Heutling F, Helm D, et al. Forged intermetallic γ-TiAl based alloy low pressure turbine blade in the geared turbofan [A]. Proceeding of the 13th World Conference on Titanium [C]. Warrendale: TMS, 2016: 1223 |
| [6] | Appel F, Clemens H, Fischer F D. Modeling concepts for intermetallic titanium aluminides [J]. Prog. Mater. Sci., 2016, 81: 55 |
| [7] | Lasalmonie A. Intermetallics: Why is it so difficult to introduce them in gas turbine engines? [J]. Intermetallics, 2006, 14: 1123 |
| [8] | Djanarthany S, Viala J C, Bouix J. An overview of monolithic titanium aluminides based on Ti3Al and TiAl [J]. Mater. Chem. Phys., 2001, 72: 301 |
| [9] | Appel F, Paul J D H, Oehring M. Gamma Titanium Aluminide Alloys: Science and Technology [M]. Weinheim, Germany: Wiley, 2011: 1 |
| [10] | Kim Y W. Ordered intermetallic alloys, part III: Gamma titanium aluminides [J]. JOM, 1994, 46(7): 30 |
| [11] | Huang S C, Chesnutt J C. Structural Applications of Intermetallic Compounds [M]. Chapter 4, New York: Wiley, 2000: 1 |
| [12] | Semiatin S L, Chesnutt J C, Austin C, et al. Structural Intermetallics [M]. Warrendale: TMS, 1997: 263 |
| [13] | Xie J X, Liu J A. Metal Extrusion: Fundamental and Technology [M]. Beijing: Metallurgical Industry Press, 2002: 8 |
| [13] | (谢建新, 刘建安. 金属挤压理论与技术 [M]. 北京: 冶金工业出版社, 2002: 8) |
| [14] | Liu D. Hot extrusion process, microstructure control and mechanical properties of γ-TiAl alloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2007 |
| [14] | (刘 冬. γ-TiAl热挤压成型工艺、组织控制及性能研究 [D]. 沈阳: 中国科学院金属研究所, 2007) |
| [15] | Liu R C. Microstructure evolution and mechanical properties of Ti-47Al-2Cr-2Nb-0.15B alloy processed by hot extrusion [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2013 |
| [15] | (刘仁慈. Ti-47Al-2Cr-2Nb-0.15B合金挤压变形组织演变及其力学性能研究 [D]. 沈阳: 中国科学院金属研究所, 2013) |
| [16] | Naka S. Structural Intermetallics [M]. Warrendale, PA: TMS, 1997: 313 |
| [17] | Kustner V, Oehring M, al AChatterjeeet. Gamma titanium aluminides 2003 [M]. Warrendale, PA: TMS, 2003: 89 |
| [18] | Imayev R M, Imayev V M, Khismatullin T G, et al. New approaches to designing alloys based on γ-TiAl+α2-Ti3Al phases [J]. Phys. Met. Metall., 2006, 102: 105 |
| [19] | Tetsui T, Shindo K, Kobayashi S, et al. A newly developed hot worked TiAl alloy for blades and structural components [J]. Scr. Mater., 2002, 47: 399 |
| [20] | Tetsui T, Shindo K, Kaji S, et al. Fabrication of TiAl components by means of hot forging and machining [J]. Intermetallics, 2005, 13: 971 |
| [21] | Clemens H, Chladil H F, Wallgram W, et al. In and ex situ investigations of the β-phase in a Nb and Mo containing γ-TiAl based alloy [J]. Intermetallics, 2008, 16: 828 |
| [22] | Clemens H, Boeck B, Wallgram W, et al. Experimental studies and hermodynamic simulations of phase transformations in Ti-(41-45)Al-4Nb-1Mo-0.1B alloys [A]. Materials Research Society Symposia Proceedings [C]. Warrendale, PA: MRS, 2009: 115 |
| [23] | Schwaighofer E, Clemens H, Mayer S, et al. Microstructural design and mechanical properties of a cast and heat-treated intermetallic multi-phase γ-TiAl based alloy [J]. Intermetallics, 2014, 44: 128 |
| [24] | Lin B C. Study on effect of surface condition and casting defects on mechanical properties of TiAl [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2018 |
| [24] | (林博超. 表面状态和铸造缺陷对TiAl力学性能影响研究 [D]. 沈阳: 中国科学院金属研究所, 2018) |
| [25] | Wang X, Liu R C, Cao R X, et al. Effect of cooling rate on boride and room temperature tensile properties of β-solidifying γ-TiAl alloys [J]. Acta Metall. Sin., 2019, 56: 203 |
| [25] | (王 希, 刘仁慈, 曹如心等. 冷却速率对β凝固γ-TiAl合金硼化物和室温拉伸性能的影响 [J]. 金属学报, 2019, 56: 203) |
| [26] | Liu R C, Wang Z, Liu D, et al. Microstructure and tensile properties of Ti-45.5Al-2Cr-2Nb-0.15B alloy processed by hot extrusion [J]. Acta Metall. Sin., 2013, 49: 641 |
| [26] | (刘仁慈, 王 震, 刘 冬等. Ti-45.5Al-2Cr-2Nb-0.15B合金热挤压组织与拉伸性能研究 [J]. 金属学报, 2013, 49: 641) |
| [27] | Zhang W J, Lorenz U, Appel F.Recovery, recrystallization and phase transformations during thermomechanical processing and treatment of TiAl-based alloys [J]. Acta Mater., 2000, 48: 2803 |
| [28] | Wallgram W, Schm?lzer T, Cha L M, et al. Technology and mechanical properties of advanced γ-TiAl based alloys [J]. Int. J. Mater. Res., 2009, 100: 8 |
| [29] | Stark A, Oehring M, Pyczak F, et al. In situ observation of various phase transformation paths in Nb-rich TiAl alloys during quenching with different rates [J]. Adv. Eng. Mater., 2011, 13: 700 |
| [30] | Maziasz P J, Liu C T. Development of ultrafine lamellar structures in two-phase γ-TiAl alloys [J]. Metall. Mater. Trans., 1998, 29A: 105 |
/
| 〈 |
|
〉 |