Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal
Received date: 2019-11-15
Revised date: 2019-12-14
Online published: 2020-01-08
Supported by
National Natural Science Foundation of China(U1860206);National Natural Science Foundation of China(51874023);National Natural Science Foundation of China(51601011);Fundamental Research Funds for the Central Universities(FRF-TP-18-003B1);Recruitment Program of Global Experts
Non-metallic inclusions generally reduce the properties of steels, such as reducing transverse mechanical properties, initiating cracks, reducing fatigue life and inducing corrosion. Reducing the number and changing the morphology of inclusions can significantly improve the performance of steels. Therefore, inclusion removal and its morphology control in steel have always been the focus issue. Although the bottom-blown argon, electromagnetic stirring and filtration can remove inclusions to a certain extent, these methods are difficult to effectively remove inclusions smaller than 20 μm in size and cannot effectively control the morphology of the inclusions. Recently, electric current has become a new method for inclusion removal and morphology control. This article briefly reviews the hazards of inclusions and their control methods, and reviews the effects of current on the removal, orientation and morphological evolution of inclusions in metal melts in detail, and introduces three mechanisms of current-controlled inclusion separation: electrophoresis, electrical free energy driving and electromagnetic repulsion. Electrophoresis theory believes that inclusions in the melt are charged, and they migrate parallel to the direction of the current under the action of the electric field force. While the electrical free energy driving and electromagnetic repulsion hold that inclusions migrate perpendicular to the direction of the current. The current waveforms significantly affect the removal efficiency of inclusions. Compared with direct current and alternating current, the pulsed electric current has a stronger ability to remove inclusions, especially pulsed electric current can effectively separate inclusions with a size larger than 5 μm in the molten steel. In addition, the pulse current can not only control the orientation and morphology of the inclusions, but also affect the morphology of the bubbles; the inclusions tend to be refined, spheroidized and arranged parallel to the current under the action of the pulse current. Finally, the research status of current-controlled inclusion separation is summarized, and future research trends are analyzed. At the same time, the application and prospect of pulsed current in anti-clogging of submerged entry nozzle was also analyzed. Due to the low energy consumption, excellent inclusion removal efficiency and easy process equipment, pulsed current separation technique is expected to become a new technology for removing inclusions and suppressing nozzle blockage in the future.
ZHANG Xinfang , YAN Longge . Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal[J]. Acta Metall Sin, 2020 , 56(3) : 257 -277 . DOI: 10.11900/0412.1961.2019.00391
| [1] | Murakami Y, Kodama S, Konuma S. Quantitative evaluation of effects of non-metallic inclusions on fatigue strength of high strength steels. I: Basic fatigue mechanism and evaluation of correlation between the fatigue fracture stress and the size and location of non-metallic inclusions [J]. Int. J. Fatigue, 1989, 11: 291 |
| [2] | Jin T Y, Liu Z Y, Cheng Y F. Effect of non-metallic inclusions on hydrogen-induced cracking of API5L X100 steel [J]. Int. J. Hydrogen Energy, 2010, 35: 8014 |
| [3] | Moghaddam S M, Sadeghi F, Paulson K, et al. Effect of non-metallic inclusions on butterfly wing initiation, crack formation, and spall geometry in bearing steels [J]. Int. J. Fatigue, 2015, 80: 203 |
| [4] | Liu H B, Liu J H, Michelic S K, et al. Characterization and analysis of non-metallic inclusions in low-carbon Fe-Mn-Si-Al TWIP steels [J]. Steel Res. Int., 2016, 87: 1723 |
| [5] | Guan J, Wang L Q, Zhang C W, et al. E?ects of non-metallic inclusions on the crack propagation in bearing steel [J]. Tribol. Int., 2017, 106: 123 |
| [6] | Krewerth D, Lippmann T, Weidner A, et al. Influence of non-metallic inclusions on fatigue life in the very high cycle fatigue regime [J]. Int. J. Fatigue, 2016, 84: 40 |
| [7] | Kim S T, Jeon S H, Lee I S, et al. Effects of rare earth metals addition on the resistance to pitting corrosion of super duplex stainless steel—Part 1 [J]. Corros. Sci., 2010, 52: 1897 |
| [8] | Shibaeva T V, Laurinavichyute V K, Tsirlina G A, et al. The effect of microstructure and non-metallic inclusions on corrosion behavior of low carbon steel in chloride containing solutions [J]. Corros. Sci., 2014, 80: 299 |
| [9] | Shim J H, Cho Y W, Chung S H, et al. Nucleation of intragranular ferrite at Ti2O3 particle in low carbon steel [J]. Acta Mater., 1999, 47: 2751 |
| [10] | Madariaga I, Gutiérrez I. Role of the particle-matrix interface on the nucleation of acicular ferrite in a medium carbon microalloyed steel [J]. Acta Mater., 1999, 47: 951 |
| [11] | Wang L Z, Yang S F, Li J S, et al. Effect of Mg addition on the refinement and homogenized distribution of inclusions in steel with different Al contents [J]. Metall. Mater. Trans., 2017, 48B: 805 |
| [12] | Birat J P. Impact of steelmaking and casting technologies on processing and properties of steel [J]. Ironmaking Steelmaking, 2001, 28: 152 |
| [13] | Bertrand C, Molinero J, Landa S, et al. Metallurgy of plastic inclusions to improve fatigue life of engineering steels [J]. Ironmaking Steelmaking, 2003, 30: 165 |
| [14] | Zheng X F, Hayes P C, Lee H G. Particle removal from liquid phase using fine gas bubbles [J]. ISIJ Int., 1997, 37: 1091 |
| [15] | Weidner A, Krewerth D, Witschel B, et al. Microstructure of non-metallic inclusions identified in cast steel 42CrMo4 after metal melt filtration by novel foam filters [J]. Steel Res. Int., 2016, 87: 1038 |
| [16] | Miki Y, Kitaoka H, Sakuraya T, et al. Mechanism for separating inclusions from molten steel stirred with a rotating electro-magnetic field [J]. ISIJ Int., 1992, 32: 142 |
| [17] | Liu X, Wang L M. Effects of rare earth addition on the inclusions and mechanical properties of 2205 duplex stainless steel [J]. Adv. Mater., 2012, 503: 463 |
| [18] | Wilson W G, Heaslip L J, Sommerville I D. Rare earth additions in continuously cast steel [J]. JOM, 1985, 37(9): 36 |
| [19] | Pan F, Zhang J, Chen H L, et al. Effects of rare earth metals on steel microstructures [J]. Materials, 2016, 9: 417 |
| [20] | Zhang L F, Liu Y, Zhang Y, et al. Transient evolution of nonmetallic inclusions during calcium treatment of molten steel [J]. Metall. Mater. Trans., 2018, 49B: 1841 |
| [21] | Kusano Y, Kawauchi Y, Wajima M, et al. Calcium treatment technologies for special steel bars and wire rods [J]. ISIJ Int., 1996, 36(Suppl): S77 |
| [22] | Kojola N, Ekerot S, Andersson M, et al. Pilot plant study of nozzle clogging mechanisms during casting of REM treated stainless steels [J]. Ironmaking Steelmaking, 2013, 38: 1 |
| [23] | Zhang L F. Several important scientific research points of non-metallic inclusions in steel [J]. Steelmaking, 2016, 32(4): 1 |
| [23] | 张立峰. 钢中非金属夹杂物几个需要深入研究的课题 [J]. 炼钢, 2016, 32(4): 1 |
| [24] | da Costa e Silva A L V. Non-metallic inclusions in steels—Origin and control [J]. J. Mater. Res. Technol., 2018, 7: 283 |
| [25] | Misra A K. A novel solidification technique of metals and alloys: Under the influence of applied potential [J]. Metall. Trans., 1985, 16A: 1354 |
| [26] | Nakada M, Shiohara Y, Flemings M C. Modification of solidification structures by pulse electric discharging [J]. ISIJ Int., 1990, 30: 27 |
| [27] | Wang X L, Dai W B, Ma C W, et al. Effect of electric current direction on recrystallization rate and texture of a Cu-Zn alloy [J]. J. Mater. Res., 2013, 28: 1378 |
| [28] | Conrad H, White J, Cao W D, et al. Effect of electric current pulses on fatigue characteristics of polycrystalline copper [J]. Mater. Sci. Eng., 1991, A145: 1 |
| [29] | Liu X B, Zhang X F. An ultrafast performance regeneration of aged stainless steel by pulsed electric current [J]. Scr. Mater., 2018, 153: 86 |
| [30] | Gao J Y, Liu X B, Zhou H F, et al. Modification of corrosion resistance of the plain carbon steels by pulsed electric current [J]. Acta Metall. Sin. (Engl. Lett., 2018, 31: 1233 |
| [31] | Conrad H. Thermally activated plastic flow of metals and ceramics with an electric field or current [J]. Mater. Sci. Eng., 2002, A322: 100 |
| [32] | Leenov D, Kolin A. Theory of electromagnetophoresis. I. Magnetohydrodynamic forces experienced by spherical and symmetrically oriented cylindrical particles [J]. J. Chem. Phys., 1954, 22: 683 |
| [33] | Kolin A. An electromagnetokinetic phenomenon involving migration of neutral particles [J]. Science, 1953, 117: 134 |
| [34] | Taniguchi S, Brimacombe J K. Application of pinch force to the separation of inclusion particles from liquid steel [J]. ISIJ Int., 1994, 34: 722 |
| [35] | Zhong Y B, Ren Z M, Deng K, et al. Formation and control of turbulent in metal melts purified by alternating magnetic field [J]. Chin. J. Nonferrous Met., 2001, 11: 541 |
| [35] | 钟云波, 任忠鸣, 邓 康等. 交变磁场净化金属液时金属液紊流的形成及其控制 [J]. 中国有色金属学报, 2001, 11: 541 |
| [36] | Liu Z Y, Yu J K, Yuan L, et al. Research progress of effects of external electric current on inclusions in molten steel [J]. China Metall., 2018, 28(4): 7 |
| [36] | 刘朝阳, 于景坤, 袁 磊等. 外加电流对钢中夹杂物影响的研究进展 [J]. 中国冶金, 2018, 28(4): 7 |
| [37] | Liang C L, Lin K L. The microstructure and property variations of metals induced by electric current treatment: A review [J]. Mater. Charact., 2018, 145: 545 |
| [38] | Zhang B W, Ren Z M, Deng K, et al. Effects of direct current on electromagnetic purification for liquid metals [J]. Chin. J. Computat. Phys., 2002, 19: 527 |
| [38] | 张邦文, 任忠鸣, 邓 康等. 直流电对金属液电磁净化的影响 [J]. 计算物理, 2002, 19: 527 |
| [39] | Zhang B W, Ren Z M, Zhong Y B, et al. Theoretical analysis on electromagnetic separation of inclusions from molten metal only by current [J]. J. Baotou Univ. Iron Steel Technol., 2002, 21: 228 |
| [39] | 张邦文, 任忠鸣, 钟云波等. 金属液单电流电磁净化的理论分析 [J]. 包头钢铁学院学报, 2002, 21: 228 |
| [40] | Sellier A. Migration of an insulating particle under the action of uniform ambient electric and magnetic fields. Part 2. Boundary formulation and ellipsoidal particles [J]. J. Fluid Mech., 2003, 488: 335 |
| [41] | Zhang L F, Wang S Q, Deng A P, et al. Application of electromagnetic (EM) separation technology to metal refining processes: A review [J]. Metall. Mater. Trans., 2014, 45B: 2153 |
| [42] | Paik Y H, Shin H C, Lee J M. Electrical charge of metal oxides in liquid metals [J]. Met. Mater., 1998, 4: 995 |
| [43] | Paik Y H, Yoon W J, Shin H C. Static electrification of solid oxide in liquid metal and electrical double layer at the interface [J]. J. Colloid Interface Sci., 2004, 269: 354 |
| [44] | Yang X, Zhou X L, Yu J K. Research on reducing nozzle clogging by controlling the electrical characteristics of SEN [A]. The 11th CSM Steel Congress——S02. Steelmaking and Continuous Casting [C]. Beijing: Metallurgical Industry Press, 2017: 251 |
| [44] | 杨 鑫, 周秀丽, 于景坤. 控制浸入式水口带电行为改善水口堵塞的研究 [A]. 第十一届中国钢铁年会论文集——S02.炼钢与连铸 [C]. 北京: 冶金工业出版社, 2017: 251 |
| [45] | Zhou X L. Clogging research of submerged nozzle used the pulse current [J]. Continuous Cast., 2017, 42(2): 27 |
| [45] | 周秀丽. 脉冲电流防水口堵塞的应用研究 [J]. 连铸, 2017, 42(2): 27 |
| [46] | Wang X L, Guo J D, Wang Y M, et al. Segregation of lead in Cu-Zn alloy under electric current pulses [J]. Appl. Phys. Lett., 2006, 89: 061910 |
| [47] | Dolinsky Y, Elperin T. Thermodynamics of nucleation in current-carrying conductors [J]. Phys. Rev., 1994, 50B: 52 |
| [48] | Qin R S, Bhowmik A. Computational thermodynamics in electric current metallurgy [J]. Mater. Sci. Technol., 2015, 31: 1560 |
| [49] | Zhang X F, Qin R S. Electric current-driven migration of electrically neutral particles in liquids [J]. Appl. Phys. Lett., 2014, 104: 114106 |
| [50] | Li W F. Study on purification process of aluminum melt electric flux [D]. Lanzhou: Lanzhou University of Technology, 2004 |
| [50] | 李文凤. 铝熔体电熔剂净化工艺的研究 [D]. 兰州: 兰州理工大学, 2004 |
| [51] | Bai S H, Yang G C, Zhou S R. The influence of elec-flux refining on the macrostructure of Al-4.5wt%Cu alloy [J]. Rere Met. Mater. Eng., 1996, 25(1): 41 |
| [51] | 白世鸿, 杨根仓, 周少荣. 电熔剂净化对Al-4.5wt%Cu合金宏观组织的影响 [J]. 稀有金属材料与工程, 1996, 25(1): 41 |
| [52] | Yan Y F, Li W W, Hao Y, et al. Influencing factors in molten aluminum treating by elec-flux process [J]. Nonferrous Met., 2005, 57(1): 39 |
| [52] | 阎峰云, 李文凤, 郝 远等. 电熔剂法净化处理铝熔体的影响因素 [J]. 有色金属, 2005, 57(1): 39 |
| [53] | Yan Y F, Hao Y, Huang X L, et al. Purification of molten aluminum by electro-flux [J]. Spec. Cast. Nonferrous Alloy, 2006, 26: 756 |
| [53] | 阎峰云, 郝 远, 黄秀玲等. 电熔剂法净化处理铝熔体的试验研究 [J]. 特种铸造及有色合金, 2006, 26: 756 |
| [54] | Zhong Y B, Ren Z M, Zhang B W, et al. Mechanism and efficiency of inclusion-removal in purifying molten metal by electro-flux method [J]. Chin. J. Nonferrous Met., 2004, 14: 1329 |
| [54] | 钟云波, 任忠鸣, 张邦文等. 电熔剂去除金属熔体中夹杂物的机理及效率分析 [J]. 中国有色金属学报, 2004, 14: 1329 |
| [55] | Taniguchi S, Brimacombe J K. Numerical analysis on the separation of inclusion particles by pinch force from liquid steel flowing in a rectangular pipe [J]. Tetsu Hagané, 1994, 80: 312 |
| [55] | 谷口 尚司, Brimacombe J K. ピンチカによる矩形管内溶鋼流からの介在物除去の数値解析 [J]. 鉄と鋼, 1994, 80: 312 |
| [56] | Zhang B W, Ren Z M, Zhong Y B, et al. Theoretical investigation on by-only-current electromagnetic separation of inclusion from molten metals [J]. Acta Metall. Sin. (Engl. Lett., 2002, 15: 416 |
| [57] | Wu J X. Basic study of electromagnetic separation of inclusion particles only by current [D]. Shanghai: Shanghai University, 2004 |
| [57] | 吴加雄. 单电流电磁分离夹杂物的基础研究 [D]. 上海: 上海大学, 2004 |
| [58] | Afshar M R, Aboutalebi M R, Isac M, et al. Mathematical modeling of electromagnetic separation of inclusions from magnesium melt in a rectangular channel [J]. Mater. Lett., 2007, 61: 2045 |
| [59] | Wu J X, Ren Z M, Zhang B W, et al. Electromagnetic purification of aluminum alloy melt only by alternating current [J]. Chin. J. Nonferrous Met., 2004, 14: 354 |
| [59] | 吴加雄, 任忠鸣, 张邦文等. 交流电净化铝合金熔体 [J]. 中国有色金属学报, 2004, 14: 354 |
| [60] | Zhong Y B, Ren Z M, Deng K, et al. Analysis of formation of turbulent flow in molten metal being purified by traveling magnetic field [J]. Shanghai Nonferrous Met., 1999, 20: 5 |
| [60] | 钟云波, 任忠鸣, 邓 康等. 金属电磁净化技术中金属液流动的成因分析 [J]. 上海有色金属, 1999, 20: 5 |
| [61] | Makarov S, Ludwig R, Resnick J, et al. The effect of a short pulse of current on small particles in a conducting fluid [J]. J. Nondestruct. Eval., 1999, 18: 99 |
| [62] | Korovin V M. Pressure pulse induced by a pulsed electric current in a cylindrical liquid conductor [J]. Tech. Phys., 2005, 50: 815 |
| [63] | Guo J D, Wang X L, Dai W B. Microstructure evolution in metals induced by high density electric current pulses [J]. Mater. Sci. Technol., 2015, 31: 1545 |
| [64] | Liu Y. Investigation of removing inclusions in steel and/or controlling state of inclusions by applied electric fields [D]. Anshan: University of Science and Technology Liaoning, 2012 |
| [64] | 刘 洋. 外加电场去除钢中夹杂及其形态控制的研究 [D]. 鞍山: 辽宁科技大学, 2012 |
| [65] | Zhang X F, Lu W J, Qin R S. Removal of MnS inclusions in molten steel using electropulsing [J]. Scr. Mater., 2013, 69: 453 |
| [66] | Zhang X F, Qin R S. Separation of electrically neutral non-metallic inclusions from molten steel by pulsed electric current [J]. Mater. Sci. Technol., 2017, 33: 1399 |
| [67] | Zhang X F, Qin R S. Controlled motion of electrically neutral microparticles by pulsed direct current [J]. Sci. Rep., 2015, 5: 10162 |
| [68] | Zhang G Z, Yan L G, Zhang X F. Inclusion removal in molten magnesium by pulsed electric current [J]. ISIJ Int., 2020, in press |
| [69] | Du M C. The effect of current on inclusion and bubble in molten steel [D]. Shenyang: Northeastern University, 2013 |
| [69] | 杜明传. 电流对钢液中气泡和夹杂物的影响 [D]. 沈阳: 东北大学, 2013 |
| [70] | Shao X J, Wang X H, Wang W J, et al. In situ observation of MnS inclusion behavior in resulfurized free-cutting steel during heating [J]. Acta Metall. Sin., 2011, 47: 1210 |
| [70] | 邵肖静, 王新华, 王万军等. 加热过程中硫系易切削钢中MnS夹杂物行为的动态原位观察 [J]. 金属学报, 2011, 47: 1210 |
| [71] | Wu M, Fang W, Chen R M, et al. Mechanical anisotropy and local ductility in transverse tensile deformation in hot rolled steels: The role of MnS inclusions [J]. Mater. Sci. Eng., 2019, A744: 324 |
| [72] | Dai W B, Yu J K, Du C M, et al. Refinement of inclusions in molten steel by electric current pulse [J]. Mater. Sci. Technol., 2015, 31: 1555 |
| [73] | Zhang X F, Lu W J, Qin R S. Morphology and distribution control of MnS inclusions in molten steel by electropulsing [J]. Mater. Res. Innov., 2014, 18: S4-244 |
| [74] | Zhang X F, Lu W J, Qin R S. Oriented sulphides induced by electric current in medium carbon steel [J]. Philos. Mag. Lett., 2015, 95: 101 |
| [75] | Yan J C, Li T, Shang Z Q, et al. Three-dimensional characterization of MnS inclusions in steel during rolling process [J]. Mater. Charact., 2019, 158: 109944 |
| [76] | Zhao Z C, Qin R S. Morphology and orientation selection of non-metallic inclusions in electrified molten metal [J]. Metall. Mater. Trans., 2017, 48B: 2781 |
| [77] | Qin R S. Electric-field-induced alignment of electrically neutral disk-like particles: Modelling and calculation [J]. Sci. Rep., 2017, 7: 8449 |
| [78] | Zhao Z C, Qin R S. Inclusion agglomeration in electrified molten metal: Thermodynamic consideration [J]. Mater. Sci. Technol., 2017, 33: 1404 |
| [79] | Yan L G, Zhang X F. Achieving the control of non-metallic inclusions morphology and orientation by electric current [J]. Steel Res. Int., 2019: 1900465 |
| [80] | Luo C H, St?hlberg U. An alternative way for evaluating the deformation of MnS inclusions in hot rolling of steel [J]. Scand. J. Met., 2002, 31: 184 |
| [81] | Andalib S, Hokmabad B V, Esmaeilzadeh E. Study of a single coarse bubble behavior in the presence of D.C. electric field [J]. Colloid Surf., 2013, 436A: 604 |
| [82] | Allen P H G, Karayiannis T G. Electrohydrodynamic enhancement of heat transfer and fluid flow [J]. Heat Recov. Syst. CHP, 1995, 15: 389 |
| [83] | Cho H J, Kang I S, Kweon Y C, et al. Numerical study of the behavior of a bubble attached to a tip in a nonuniform electric field [J]. Int. J. Multiphase Flow, 1998, 24: 479 |
| [84] | Herman C, Iacona E. Modeling of bubble detachment in reduced gravity under the influence of electric fields and experimental verification [J]. Heat Mass Transfer, 2004, 40: 943 |
| [85] | Rahmat A, Tofighi N, Yildiz M. Numerical simulation of the electrohydrodynamic effects on bubble rising using the SPH method [J]. Int. J. Heat Fluid Flow, 2016, 62: 313 |
| [86] | Siedel S, Cioulachtjian S, Robinson A J, et al. Lateral coalescence of bubbles in the presence of a DC electric field [J]. Int. Commun. Heat Mass Transfer, 2016, 76: 127 |
| [87] | Zhang X F, Qin R S. Exploring the particle reconfiguration in the metallic materials under the pulsed electric current [J]. Steel Res. Int., 2018, 89: 1800062 |
| [88] | Schulze H J. Hydrodynamics of bubble-mineral particle collisions [J]. Proc. Ext. Met. Rev., 1989, 5: 43 |
| [89] | Wang L H, Lee H G, Hayes P. Prediction of the optimum bubble size for inclusion removal from molten steel by flotation [J]. ISIJ Int., 1996, 36: 7 |
| [90] | Zhang L, Taniguchi S. Fundamentals of inclusion removal from liquid steel by bubble flotation [J]. Int. Mater. Rev., 2000, 45: 59 |
| [91] | Zheng H G, Chen W Q, Liu Q, et al. Investigation on clogging of submerged entry nozzle during continuous casting Ti-bearing stainless steel [J]. J. Iron Steel Res. Int., 2005, 17(1): 14 |
| [91] | 郑宏光, 陈伟庆, 刘 青等. 含钛不锈钢连铸浸入式水口结瘤的研究 [J]. 钢铁研究学报, 2005, 17(1): 14 |
| [92] | Zhao L P, Wang Y, Wang H S. Current research status of tundish nozzle clogging [J]. Steelmaking, 2007, 22(3): 59 |
| [92] | 赵李平, 王 勇, 王鸿盛. 连铸中间包水口堵塞问题的研究现状 [J]. 炼钢, 2007, 22(3): 59 |
| [93] | Lavers J D, Kadar L. Application of electromagnetic forces to reduce tundish nozzle clogging [J]. Appl. Math. Modell., 2004, 28: 29 |
| [94] | Yaun F M, Wang X H, Zhang J M, et al. Numerical simulation of tundish nozzle clogging during continuous casting [J]. Acta Metall. Sin., 2006, 42: 1109 |
| [94] | 袁方明, 王新华, 张炯明等. 连铸中间包水口堵塞的数值模拟 [J]. 金属学报, 2006, 42: 1109 |
| [95] | Nakanishi K. Japanese state of the art continuous casting process [J]. ISIJ Int., 1996, 36(Suppl.1): S14 |
| [96] | Yang M L, Cheng C G, Li Y, et al. Development of control technology and clogging mechanism for tundish nozzle in continuous casting [J]. J. Iron Steel Res. Int., 2017, 29: 773 |
| [96] | 杨明磊, 程常桂, 李 阳等. 连铸中间包水口堵塞机理及控制技术的发展 [J]. 钢铁研究学报, 2017, 29: 773 |
| [97] | Yan Z G. Research and development of structures and materials of submerged entry nozzle for thin slab continuous casting [D]. Shenyang: Northeastern University, 2011 |
| [97] | 颜正国. 薄板坯浸入式水口结构及材质的开发研究 [D]. 沈阳: 东北大学, 2011 |
| [98] | Svensson J K S, Memarpour A, Ekerot S, et al. Studies of new coating materials to prevent clogging of submerged entry nozzle (SEN) during continuous casting of Al killed low carbon steels [J]. Ironmaking Steelmaking, 2017, 44: 117 |
| [99] | Holappa L, H?m?l?inen M, Liukkonen M, et al. Thermodynamic examination of inclusion modification and precipitation from calcium treatment to solidified steel [J]. Ironmaking Steelmaking, 2003, 30: 111 |
| [100] | Bai H, Thomas B G. Effects of clogging, argon injection, and continuous casting conditions on flow and air aspiration in submerged entry nozzles [J]. Metall. Mater. Trans., 2001, 32B: 707 |
| [101] | Tian C, Yu J K, Jin E D, et al. Effect of interfacial reaction behaviour on the clogging of SEN in the continuous casting of bearing steel containing rare earth elements [J]. J. Alloys Compd., 2019, 792: 1. |
| [102] | Liu Y B, Ge J G, Liu H L, et al. Analysis of ladle slide gate clogging in pouring RE steel [J]. Sci. Technol. Baotou Steel (Group) Corporat., 2000, 26(2): 50 |
| [102] | 刘越表, 葛建国, 刘宏玲等. 稀土钢水口堵塞的成因分析 [J]. 包钢科技, 2000, 26(2): 50 |
| [103] | Yang Y C, Luan Y K, Li D Z, et al. Effect of RE on inclusions in highly clean bearing steel [J]. Steelmaking, 2016, 32(4): 54 |
| [103] | 杨超云, 栾义坤, 李殿中等. 稀土元素对高洁净度轴承钢中夹杂物的影响研究 [J]. 炼钢, 2016, 32(4): 54 |
| [104] | Yao Y K. Exploitation of fluxes and research on mechanisms of nozzle blockage for continuous casting of RE steel [D]. Shenyang: Northeastern University, 2004 |
| [104] | 姚永宽. 稀土钢连铸粉剂开发及中间包水口结瘤机理研究 [D]. 沈阳: 东北大学, 2004 |
| [105] | Yang X, Yu J K, Liu Z Y, et al. The charged characteristics of the submerged entry nozzle used for continuous casting [J]. Ceram. Int., 2017, 43: 2881 |
| [106] | Yu J K, Yang X, Liu Z Y, et al. Anti-clogging of submerged entry nozzle through control of electrical characteristics [J]. Ceram. Int., 2017, 43: 13025 |
| [107] | Yang X, Liu Z Y, Yu J K. Anti-fouling of submerged entry nozzle with electric current pulse [J]. J. Mater. Process. Tech., 2018, 259: 341 |
| [108] | Dai W B, Zhou X L, Yang X, et al. Formation of dense inclusion buildup on submerged entry nozzle by electric current pulse [J]. Acta Metall. Sin. (Engl. Lett., 2016, 29: 500 |
| [109] | Dai W B, Yang X, Zhou X L, et al. Influence of electric current pulses on prevention of nozzle clogging [J]. J. Univ. Sci. Technol. Liaoning, 2016, 39: 12 |
| [109] | 戴文斌, 杨 鑫, 周秀丽等. 利用脉冲电流控制水口堵塞的研究 [J]. 辽宁科技大学学报, 2016, 39: 12 |
| [110] | Sun Y, Ma B Y, Yu J K. Effect of an applied electric field on the clogging of continuous casting nozzle [J]. Continuous Cast., 2008, (6): 11 |
| [110] | 孙 勇, 马北越, 于景坤. 施加电场对连铸水口防堵塞性能的影响 [J]. 连铸, 2008, (6): 11 |
| [111] | Kawamoto M. Recent development of steelmaking process in Sumitomo metals [J]. J. Iron Steel Res. (Int.), 2011, 18(S2: 28 |
| [112] | Feng S C, Wang Y H, Ling H Z, et al. Clean steel production status in Sumitomo Metal [J]. World Iron Steel, 2012, 12(4): 21 |
| [112] | 冯士超, 王艳红, 梁慧智等. 住友金属洁净钢生产工艺技术现状 [J]. 世界钢铁, 2012, 12(4): 21 |
/
| 〈 |
|
〉 |