Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation

  • Jizhao LIU ,
  • Hefei HUANG ,
  • Zhenbo ZHU ,
  • Awen LIU ,
  • Yan LI
Expand
  • 1.Shanghai Institute of Applied Physics, Chinese Academy of Sciences, Shanghai 201800, China
    2.School of Nuclear Science and Technology, University of Chinese Academy of Sciences, Beijing 100049, China
    3.School of Physical Science and Technology, ShanghaiTech University, Shanghai 201210, China

Received date: 2019-09-26

  Revised date: 2019-12-11

  Online published: 2019-12-23

Supported by

National Natural Science Foundation of China(11605271);National Natural Science Foundation of China(11975304);National Natural Science Foundation of China(91126012)

Abstract

Ion irradiation experiments are of importance for investigating irradiation damage of reactor structural materials. However, estimating the irradiation hardening of ion-irradiated materials is difficult due to the limitation of ion penetration depth. In recent years, nanoindentation test has been widely used to study the irradiation hardening of materials, because the continuous stiffness measurement (CSM) mode can obtain the relationship between nanohardness and indentation depth at a very small penetration depth. In this work, the average nanohardness of Hastelloy N alloy irradiated by xenon ion at room temperature was tested by this mode. The results showed that the nanohardness in the irradiated samples was larger than that in the unirradiated sample and this value of irradiated samples is saturated when the irradiation dose is in the range of 0.5~3.0 dpa. Based on the Nix-Gao model, the indentation size effects (ISE) of unirradiated and irradiated samples were separated from nanohardness measured by nanoindentation. The volume law of mixture model (VLM) was subsequently applied to simulate the measured nanohardness. As the depth of indentation increases, the plasticity affected region (PAR) includes both irradiation damage layer and matrix. Interface parameter was introduced to correct the volume of matrix deformation. The results indicated that the improved VLM model leads to a characteristic relation for the depth dependence of nanohardness that is in excellent agreement with nanoindentation experiments.

Cite this article

Jizhao LIU , Hefei HUANG , Zhenbo ZHU , Awen LIU , Yan LI . Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation[J]. Acta Metall Sin, 2020 , 56(5) : 753 -759 . DOI: 10.11900/0412.1961.2019.00324

References

1 Liu P P, Wan F R, Zhan Q. A model to evaluate the nano-indentation hardness of ion-irradiated materials [J]. Nucl. Instrum. Methods Phys. Res., 2015, 342B: 13
2 Gao J, Huang H F, Liu J Z, et al. Synergistic effects on microstructural evolution and hardening of the Hastelloy N alloy under subsequent He and Xe ion irradiation [J]. J. Appl. Phys., 2018, 123: 205901
3 Huang H F, Li J J, Li D H, et al. TEM, XRD and nanoindentation characterization of xenon ion irradiation damage in austenitic stainless steels [J]. J. Nucl. Mater., 2014, 454: 168
4 Lu Y P, Huang H F, Gao X Z, et al. A promising new class of irradiation tolerant materials: Ti2ZrHfV0.5Mo0.2 high-entropy alloy [J]. J. Mater. Sci. Technol., 2019, 35: 369
5 Liu X B, Wang R S, Ren A, et al. Evaluation of radiation hardening in ion-irradiated Fe based alloys by nanoindentation [J]. J. Nucl. Mater., 2014, 444: 1
6 Takayama Y, Kasada R, Sakamoto Y, et al. Nanoindentation hardness and its extrapolation to bulk-equivalent hardness of F82H steels after single- and dual-ion beam irradiation [J]. J. Nucl. Mater., 2013, 442(Suppl.1): S23
7 Huang H F, Li D H, Li J J, et al. Nanostructure variations and their effects on mechanical strength of Ni-17Mo-7Cr alloy under xenon ion irradiation [J]. Mater. Trans., 2014, 55: 1243
8 Nix W D, Gao H J. Indentation size effects in crystalline materials: A law for strain gradient plasticity [J]. J. Mech. Phys. Solids, 1998, 46: 411
9 Yang Y T, Zhang C H, Meng Y C, et al. Nanoindentation on V-4Ti alloy irradiated by H and He ions [J]. J. Nucl. Mater., 2015, 459: 1
10 Wei Y P, Liu P P, Zhu Y M, et al. Evaluation of irradiation hardening and microstructure evolution under the synergistic interaction of He and subsequent Fe ions irradiation in CLAM steel [J]. J. Alloys Compd., 2016, 676: 481
11 Xu C L, Zhang L, Qian W J, et al. The studies of irradiation hardening of stainless steel reactor internals under proton and xenon irradiation [J]. Nucl. Eng. Technol., 2016, 48: 758
12 Kasada R, Takayama Y, Yabuuchi K, et al. A new approach to evaluate irradiation hardening of ion-irradiated ferritic alloys by nano-indentation techniques [J]. Fusion Eng. Des., 2011, 86: 2658
13 Xiao X Z, Yu L. Comparison of linear and square superposition hardening models for the surface nanoindentation of ion-irradiated materials [J]. J. Nucl. Mater., 2018, 503: 110
14 Kareer A, Prasitthipayong A, Krumwiede D, et al. An analytical method to extract irradiation hardening from nanoindentation hardness-depth curves [J]. J. Nucl. Mater., 2018, 498: 274
15 Hosemann P, Kiener D, Wang Y Q, et al. Issues to consider using nano indentation on shallow ion beam irradiated materials [J]. J. Nucl. Mater., 2012, 425: 136
16 Burnett P J, Rickerby D S. The mechanical properties of wear-resistant coatings: I: Modelling of hardness behaviour [J]. Thin Solid Films, 1987, 148: 41
17 Olivier W C, Pharr G M. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments [J]. J. Mater. Res., 1992, 7: 1564
18 Zhu Z B, Huang H F, Liu J Z, et al. Xenon ion irradiation induced hardening in inconel 617 containing experiment and numerical calculation [J]. J. Nucl. Mater., 2019, 525: 32
19 Lee E H, Oliver W C, Mansur L K. Hardness measurements of Ar+-beam treated polyimide by depth-sensing ultra low load indentation [J]. J. Mater. Res., 1993, 8: 377
20 Chen H C, Hai Y, Liu R D, et al. The irradiation hardening of Ni-Mo-Cr and Ni-W-Cr alloy under Xe26+ ion irradiation [J]. Nucl. Instrum. Methods Phys. Res., 2018, 421B: 50
21 Liu J Z, Huang H F, Gao J, et al. Defects evolution and hardening in the Hastelloy N alloy by subsequent Xe and He ions irradiation [J]. J. Nucl. Mater., 2019, 517: 328
22 Sammuels L E, Mulhearn T O. An experimental investigation of the deformed zone associated with indentation hardness impressions [J]. J. Mech. Phys. Solids, 1957, 5: 125
23 Saleh M, Zaidi Z, Ionescu M, et al. Relationship between damage and hardness pro?les in ion irradiated SS316 using nanoindentation―Experiments and modelling [J]. Int. J. Plast., 2016, 86: 151
24 Zhang Z X, Hasenhuetl E, Yabuuchi K, et al. Evaluation of helium effect on ion-irradiation hardening in pure tungsten by nano-indentation method [J]. Nucl. Mater. Energy, 2016, 9: 539
25 Rickerby D S, Burnett P J. Correlation of process and system parameters with structure and properties of physically vapour-deposited hard coatings [J]. Thin Solid Films, 1988, 157: 195
Outlines

/