Microstructure and Corrosion Behavior of Fe-15Mn-5Si-14Cr-0.2C Amorphous Steel
Received date: 2019-08-19
Revised date: 2019-12-11
Online published: 2019-12-23
Supported by
National Natural Science Foundation of China(51661017);China Scholarship Council(201808625027);Outstanding Youth Funds of Gansu Province(17JR5RA108);Hongliu Outstanding Youth Funds of Lanzhou University of Technology
Amorphous steels exhibit ultra-high strength but room-temperature brittleness and strain-softening behavior as loading, which restricted the application of amorphous steels as high-performance structural material. Developing in situ crystals is an effective way to toughen the amorphous alloys. However, the crystals may sacrifice the corrosion resistance of amorphous steels. In this work, austenite and ferrite duel phases were introduced to the amorphous phase, via transformation induced plasticity (TRIP) of the austenite as loading, to enhance the ductility and improve the work-hardening behavior; and via the synergy of ferrite and amorphous phase to ensure the corrosion resistance. A novel amorphous steel Fe-15Mn-5Si-14Cr-0.2C was fabricated by magnetic suspension melting in a water-cooled copper crucible, and negative pressure suction casting into a copper mold. The microstructure and mechanical properties of the amorphous steel were characterized by XRD, EBSD and the electronic universal testing machine. The corrosion behavior in artificial seawater was studied on an electrochemical work station with a three-electrode system, and the corrosion morphology and corrosion products were characterized by SEM with EDS analysis. The results showed that the as-cast amorphous steel consisted of the amorphous matrix, CFe15.1 super-cooled austenite and Fe-Cr ferrite phases. From surface to inner, amorphous phases mainly exist in the margin, while crystalline phases are abundantly distributed in the center. The amorphous steel exhibited excellent comprehensive mechanical properties at room temperature, and its yield strength, fracture strength and plastic strain were up to 978 MPa, 2645 MPa and 35.8%, respectively. In artificial seawater, compared with 304 stainless steel, the amorphous steel showed high self-corrosion potential, low self-corrosion current density and high polarization resistance, large resistance arc radius, only one high frequency resistance arc and low corrosion kinetic rate. Moreover, the stable and dense passivation film was observed on the corrosion surface. Their excellent corrosion resistance and mechanical properties endow the amorphous steel with the potential to become a novel corrosion-resistant structural material for marine engineering.
Key words: amorphous steel; microstructure; mechanical property; corrosion behavior
Yanchun ZHAO , Xuejing MAO , Wensheng LI , Hao SUN , Chunling LI , Pengbiao ZHAO , Shengzhong KOU , Peter K. Liaw . Microstructure and Corrosion Behavior of Fe-15Mn-5Si-14Cr-0.2C Amorphous Steel[J]. Acta Metall Sin, 2020 , 56(5) : 715 -722 . DOI: 10.11900/0412.1961.2019.00275
| 1 | Inoue A. High strength bulk amorphous alloys with low critical cooling rates (Overview) [J]. Mater. Trans., 1995, 36: 866 |
| 2 | Hofmann D C. Shape memory bulk metallic glass composites [J]. Science, 2010, 329: 1294 |
| 3 | Qiao J C, Wang Q, Pelletier J M, et al. Structural heterogeneities and mechanical behavior of amorphous alloys [J]. Prog. Mater. Sci., 2019, 104: 250 |
| 4 | Wang W H. The nature and properties of amorphous matter [J]. Prog. Phys., 2013, 33(5): 177 |
| 4 | 汪卫华. 非晶态物质的本质和特性 [J]. 物理学进展, 2013, 33(5): 177 |
| 5 | Pan J, Zhang M, Chen Q, et al. Study of anticorrosion ability of Fe43.7Co7.3Cr14.7Mo12.6C15.5B4.3Y1.9 bulk metallic glass in strong acid solutions [J]. Rare Met. Mater. Eng., 2008, 37: 805 |
| 5 | 潘 杰, 张 猛, 谌 祺等. FeCoCrMoCBY块体非晶合金在强酸介质中的耐蚀性能 [J]. 稀有金属材料与工程, 2008, 37: 805 |
| 6 | Fan H B, Zheng W, Wang G Y, et al. Corrosion behavior of Fe41Co7Cr15Mo14C15B6Y2 bulk metallic glass in sulfuric acid solutions [J]. Metall. Mater. Trans., 2011, 42A: 1524 |
| 7 | Gostin P F, Gebert A, Schultz L. Comparison of the corrosion of bulk amorphous steel with conventional steel [J]. Corros. Sci., 2010, 52: 273 |
| 8 | Naka M, Hashimoto K, Inoue A, et al. Corrosion-resistant amorphous Fe-C alloys containing chromium and/or molybdenum [J]. J. Non-Cryst. Solids, 1979, 31: 347 |
| 9 | Jayaraj J, Kim K B, Ahn H S, et al. Corrosion mechanism of N-containing Fe-Cr-Mo-Y-C-B bulk amorphous alloys in highly concentrated HCl solution [J]. Mater. Sci. Eng., 2007, A449-451: 517 |
| 10 | Pardo A, Merino M C, Otero E, et al. Influence of Cr additions on corrosion resistance of Fe- and Co-based metallic glasses and nanocrystals in H2SO4 [J]. J. Non-Cryst. Solids, 2006, 352: 3179 |
| 11 | Chen J, Wang J Z, Chen B B, et al. Tribocorrosion behaviors of Inconel 625 alloy sliding against 316 steel in seawater [J]. Tribol. Trans., 2010, 54: 514 |
| 12 | Hu X F, Jiang H C, Zhao M J, et al. Microstructure and mechanical properties of welded joint of a Fe-Cr-Ni-Mo steel with high-strength and high-toughness [J]. Acta Metall. Sin., 2018, 54: 1 |
| 12 | 胡小锋, 姜海昌, 赵明久等. 一种Fe-Cr-Ni-Mo高强高韧合金钢焊接接头的组织和力学性能 [J]. 金属学报, 2018, 54: 1 |
| 13 | Hakiki N B, Boudin S, Rondot B, et al. The electronic structure of passive films formed on stainless steels [J]. Corros. Sci., 1995, 37: 1809 |
| 14 | Zhi J H, Wang Y, Li J H, et al. Microsturcture and high temperature mechanical properties of martensitic stainless steel [J]. Heat Treat. Met., 2018, 43(3): 68 |
| 14 | 支金花, 王 裕, 李继红等. 1Cr12Ni2W1MolV马氏体不锈钢的组织和高温力学性能 [J]. 金属热处理, 2018, 43(3): 68 |
| 15 | Cao C N. Principles of Electrochemistry of Corrosion [M]. Beijing: Chemical Industry Press, 2008: 99 |
| 15 | 曹楚南. 腐蚀电化学原理 [M]. 北京: 化学工业出版社, 2008: 99 |
| 16 | Stern M, Geary A L. Electrochemical polarization I. A theoretical analysis of the shape of polarization curves [J]. J. Electrochem. Soc., 1957, 104: 56 |
| 17 | Li J W, Yang L J, Ma H R, et al. Improved corrosion resistance of novel Fe-based amorphous alloys [J]. Mater. Des., 2016, 95: 225 |
| 18 | Hua N B, Chen W Z, Wang Q T, et al. Tribocorrosion behaviors of a biodegradable Mg65Zn30Ca5 bulk metallic glass for potential biomedical implant applications [J]. J. Alloys Compd., 2018, 745: 111 |
| 19 | Wen P, Li C F, Zhao Y, et al. First principles calculation of occupancy, bonding characteristics and alloying effect of Cr, Mo, Ni in bulk α-Fe(C) [J]. Acta Phys. Sin., 2014, 63(19): 197101 |
| 19 | 文 平, 李春福, 赵 毅等. Cr, Mo, Ni在α-Fe(C)中占位、键合性质及合金化效应的第一性原理研究 [J]. 物理学报, 2014, 63(19):197101 |
| 20 | Li L, Xing S B. Catalytic effect analysis of metallic catalyst during diamond single crystal synjournal [J]. Acta Metall. Sin. (Engl. Lett)., 2014, 27: 161 |
| 21 | Wang Y F, Li Y K, Sun C, et al. Electronic theoretical model of static and dynamic strength of steels [J]. Acta Phys. Sin., 2014, 63(12): 126101 |
| 21 | 王云飞, 李云凯, 孙 川等. 钢动静态强度计算的电子理论模型 [J]. 物理学报, 2014, 63(12): 126101 |
| 22 | Wang Y, Li C F, Lin Y H. Electronic theoretical study of the influence of Cr on corrosion resistance of Fe-Cr Alloy [J]. Acta Metall. Sin., 2017, 53: 622 |
| 22 | 王 垚, 李春福, 林元华. Cr对Fe-Cr合金耐蚀性能影响的电子理论研究 [J]. 金属学报, 2017, 53: 622 |
| 23 | Souza C A C, Ribeiro D V, Kiminami C S. Corrosion resistance of Fe-Cr-based amorphous alloys: An overview [J]. J. Non-Cryst. Solids, 2016, 442: 56 |
| 24 | Huang C B, Lu Z P, Yang W. Anodic dissolution and passiyation of an Fe-Ni base alloy in hot concentrated caustic solutions [J]. Corros. Sci. Pro. Technol., 2001, 13(Suppl.): 514 |
| 24 | 黄春波, 吕战鹏, 杨 武. Fe-Ni基合金在热浓碱溶液中的阳极溶解与钝化行为 [J]. 腐蚀科学与防护技术, 2001, 13(增刊): 514 |
| 25 | Chen P, Qin F X, Zhang H F, et al. Corrosion behaviors of bulk amorphous alloy Cu-Zr-Ti-Sn and its crystallized form in 3.5% NaCl solution [J]. Acta Metall. Sin., 2004, 40: 207 |
| 25 | 陈 鹏, 秦凤香, 张海峰等. 块状非晶合金Cu-Zr-Ti-Sn在3.5%NaCl溶液中的腐蚀行为 [J]. 金属学报, 2004, 40: 207 |
| 26 | Hu Y P, Ping K B, Yan Z J, et al. First-principles calculations of structure and magnetic properties of α-Fe(Si) phase precipitated in the Finemet alloy [J]. Acta Phys. Sin., 2011, 60(10): 107504 |
| 26 | 胡玉平, 平凯斌, 闫志杰等. Finemet合金析出相α-Fe(Si)结构与磁性的第一性原理计算 [J]. 物理学报, 2011, 60(10): 107504 |
| 27 | Han Y, Kong F L, Han F F, et al. New Fe-based soft magnetic amorphous alloys with high saturation magnetization and good corrosion resistance for dust core application [J]. Intermetallics, 2016, 76: 18 |
| 28 | Machmeier P, Matuszewski T, Jones R, et al. Effect of chromium additions on the mechanical and physical properties and microstructure of Fe-Co-Ni-Cr-Mo-C ultra-high strength steel: Part I [J]. J. Mater. Eng. Perform., 1997, 6: 279 |
| 29 | Botta W J, Berger J E, Kiminami C S, et al. Corrosion resistance of Fe-based amorphous alloys [J]. J. Alloys Compd., 2014, 586(Suppl. 1): S105 |
| 30 | Qu S P, Cheng B Z, Dong L H, et al. Corrosion behavior of 2205 steel in simulated hydrothermal area [J]. Acta Metall. Sin., 2018, 54: 1094 |
| 30 | 屈少鹏, 程柏璋, 董丽华等. 2205钢在模拟深海热液区中的腐蚀行为 [J]. 金属学报, 2018, 54: 1094 |
/
| 〈 |
|
〉 |