Formation of Sliver Defects in Single CrystalCastings of Superalloys

  • Dexin MA ,
  • Fu WANG ,
  • Weitai XU ,
  • Wenliang XU ,
  • Yunxing ZHAO
Expand
  • 1. Wedge Central South Research Institute, Shenzhen 518045, China
    2. Powder Metallurgy Research Institute, Central South University, Changsha 410083, China
    3. School of Mechanic and Electronic Engineering, Xi’an Jiao Tong University, Xi’an 710049, China

Received date: 2019-09-02

  Revised date: 2019-10-29

  Online published: 2019-12-13

Supported by

Supported by National Natural Science Foundation of China(91860103);Shenzhen Peacock Plan(20150128085205453)

Abstract

In the casting components of superalloys with increasing content of the refractory elements the occurrence of sliver defects becomes rather frequent. In comparison to the other grain defects such as stray grains and freckles, the sliver defect was less well understood and its formation mechanism is still unclear. In the present work, the origins of the sliver defects in the single crystal (SC) castings were investigated. In the metallographic detection, sliver grains can be identified to be miss-alignments of isolated, individual primary dendrite on the SC matrix. The sliver defects originated from the tearing of the existing dendrite stems in the mush zone, revealing a clear starting point of sliver defect. The cracks of the dendrites were filled by the interdendritic residual melt, which finally solidified into γ′-stripes. The tearing of some existing dendrite stems can be attributed to the adhesion of shell mold that hinders the shrinkage of the columnar dendrites on the casting surface. The second reason for the dendrite tearing is the insertion of oxide residues which significantly weakens the strength of the dendrite stems. Due to the support of the neighboring columnar dendrites, the tilting of the broken dendrites is limited, so that the grain boundary between a sliver and the matrix structure has normally a low angle. The structure and formation mechanisms of sliver defects were discussed in comparison with other defects such as stray grains, freckles and low angle grain boundaries. The corresponding methods were proposed to avoid sliver defects in production of SC superalloy castings.

Cite this article

Dexin MA , Fu WANG , Weitai XU , Wenliang XU , Yunxing ZHAO . Formation of Sliver Defects in Single CrystalCastings of Superalloys[J]. Acta Metall Sin, 2020 , 56(3) : 301 -310 . DOI: 10.11900/0412.1961.2019.00287

References

[1] Carney C A, Beech J. The origin of sliver defects in single crystal turbine blades [A]. Solidification Processing [C]. London: Institute of Metals, 1987: 33
[2] Shi Z X, Liu S Z, Li J R. Sliver formation mechanism of single crystal superalloy during directional solidification proscess [J]. Hot Work. Technol., 2013, 42(13): 31
[2] 史振学, 刘世忠, 李嘉荣. 单晶高温合金定向凝固过程中条带的形成机制 [J]. 热加工工艺, 2013, 42(13): 31
[3] Avedon J W, Tenant P A, Foss B J, et al. On the origin of sliver defects in single crystal investment castings [J]. Acta Mater., 2013, 61: 5162
[4] Zhang J, Lou L H. Basic research in development and application of cast superalloy [J]. Acta Metall. Sin., 2018, 54: 1637
[4] 张 健, 楼琅洪. 铸造高温合金研发中的应用基础研究 [J]. 金属学报, 2018, 54: 1637
[5] Ma D X, Wang F, Sun H Y, et al. Study on sliver defects in single crystal castings of superalloys [J]. Foundry, 2019, 68: 567
[5] 马德新, 王 富, 孙洪元等. 高温合金单晶铸件中条纹晶缺陷的试验研究 [J]. 铸造, 2019, 68: 567
[6] Paul U, Sahm P R, Goldschmidt D. Inhomogeneities in single-crystal components [J]. Mater. Sci. Eng., 1993, A173: 49
[7] Meyer M, Dedecke D, Paul U, et al. Undercooling related casting defects in single crystal turbine blades [A]. Superalloys 1996 [C]. New York: TMS, 1996: 471
[8] Ma D X, Bührig-Polaczek A. Application of a heat conductor technique in the production of single-crystal turbine blades [J]. Metall. Mater. Trans., 2009, 40B: 738
[9] Zhang X L, Zhou Y Z, Jin T, et al. Study on the tendency of stray grain formation of Ni-based single crystal superalloys [J]. Acta Metall. Sin., 2012, 48: 1229
[9] 张小丽, 周亦胄, 金 涛等. 镍基单晶高温合金杂晶形成倾向性的研究 [J]. 金属学报, 2012, 48: 1229
[10] Zhang H Q, Zhang J, Li Y F, et al. Stray grain formation in casting platform of third generation Ni-base single crystal superalloy [J]. Foundry, 2014, 63: 128
[10] 张宏琦, 张 军, 李亚峰等. 一种第三代镍基单晶高温合金铸件截面突变处的杂晶形成过程 [J]. 铸造, 2014, 63: 128
[11] Ma D X. Development of single crystal solidification technology for production of superalloy turbine blades [J]. Acta Metall. Sin., 2015, 51: 1179
[11] 马德新. 高温合金叶片单晶凝固技术的新发展 [J]. 金属学报, 2015, 51: 1179
[12] Ma D X, Zhang Q Y, Wang H Y, et al. Influence of process condition on the stray grain formation in the single crystal blades of Ni-base superalloy DD483 [J]. Foundry, 2017, 66: 439
[12] 马德新, 张琼元, 王海洋等. 工艺条件对镍基高温合金DD483单晶叶片中杂晶缺陷的影响 [J]. 铸造, 2017, 66: 439
[13] Ma D X, Wang F, Sun H Y, et al. Experimental investigations on stray grain defects in single crystal castings of superalloys [J]. Foundry, 2019, 68: 558
[13] 马德新, 王 富, 孙洪元等. 高温合金单晶铸件中杂晶缺陷的试验研究 [J]. 铸造, 2019, 68: 558
[14] Giamei A F, Kear B H. On the nature of freckles in nickel base superalloys [J]. Metall. Trans., 1970, 1: 2185
[15] Copley S M, Giamei A F, Johnson S M, et al. The origin of freckles in unidirectionally solidified castings [J]. Metall. Trans., 1970, 1: 2193
[16] Auburtin P B L. Determination of the influence of growth front angle on freckle formation in superalloys [D]. Vancouver, Canada: The University of British Columbia, 1998
[17] Auburtin P, Wang T, Cockcroft S L, et al. Freckle formation and freckle criterion in superalloy castings [J]. Metall. Mater. Trans., 2000, 31B: 801
[18] Beckermann C, Gu J P, Boettinger W J. Development of a freckle predictor via rayleigh number method for single-crystal nickel-base superalloy castings [J]. Metall. Mater. Trans., 2000, 31A: 2545
[19] Yang W H, Chang K M, Chen W, et al. Freckle criteria for the upward directional solidification of alloys [J]. Metall. Mater. Trans., 2001, 32A: 397
[20] Tin S, Pollock T M. Predicting freckle formation in single crystal Ni-base superalloys [J]. J. Mater. Sci., 2004, 39: 7199
[21] Reed R C. The Superalloys: Fundamentals and Applications [M]. London: Cambridge University Press, 2006: 140
[22] Ma D X, Wu Q, Bührig-Polaczek A. Some new observations on freckle formation in directionally solidified superalloy components [J]. Metall. Mater. Trans., 2012, 43B: 344
[23] Ma D X. Freckle formation during directional solidification of complex castings of superalloys [J]. Acta Metall. Sin., 2016, 52: 426
[23] 马德新. 定向凝固的复杂形状高温合金铸件中的雀斑形成 [J]. 金属学报, 2016, 52: 426
[24] Ma D X. Development of dendrite array growth during alternately changing solidification condition [J]. J. Crystal Growth, 2004, 260: 580
[25] Newell M, Devendra K, Jennings P A, et al. Role of dendrite branching and growth kinetics in the formation of low angle boundaries in Ni-base superalloys [J]. Mater. Sci. Eng., 2005, A412: 307
[26] D'Souza N, Newell M, Devendra K, et al. Formation of low angle boundaries in Ni-based superalloys [J]. Mater. Sci. Eng., 2005, A413-414: 567
Outlines

/